公开(公告)号:DE3525749A1
公开(公告)日:1987-01-29
申请号:DE3525749
申请日:1985-07-19
Applicant: BASF AG
Inventor: OEHSEN UBBO VON DR , STECHER KARLHEINZ DR , KOEHLER WALDEMAR DR , MUELLER BERTHOLD DR , BRUNNMUELLER FRITZ DR , SCHNEIDER ROLF DR
Abstract: A process for the thermolytic cleavage of formamide to give hydrocyanic acid and water over alumina or alumina/silica moldings subjected to final sintering or over high temperature corrosion-resistant stainless steel packings in the presence of atmospheric oxygen possesses, in particular, high HCN selectively and a high formamide conversion.
-
公开(公告)号:DE3629477A1
公开(公告)日:1988-03-03
申请号:DE3629477
申请日:1986-08-29
Applicant: BASF AG
Inventor: LEUTNER BERND DR , MUELLER BERTHOLD DR , VOLKENBORN WILHELM DIPL ING
Abstract: Cavities in mining are filled by introducing a mixture consisting of a slurry or sludge which evolves CO2, foams and solidifies and predominantly comprises alpha-hemihydrate, alpha-CaSO4. 0.5 H2O, an alkali metal or alkaline earth metal carbonate and water, by a method in which the mixture is mixed with a bisulfate-containing aqueous solution or suspension of one or more metals before being introduced into the cavities to be filled.
-
-
公开(公告)号:DE3778276D1
公开(公告)日:1992-05-21
申请号:DE3778276
申请日:1987-08-22
Applicant: BASF AG
Inventor: LEUTNER BERND DR , MUELLER BERTHOLD DR , VOLKENBORN WILHELM
Abstract: In the filling of mine cavities using a mixt. of CO2-evolving, foaming and setting slurry of mainly alpha hemihydrate, alkaline (ne earth) carbonate and water, the novelty is that, prior to introduction into the cavities, the mixt. is mixed with a hydrogen sulphate-contg. aq. soln. or suspension of one or more metals.
-
公开(公告)号:AT74888T
公开(公告)日:1992-05-15
申请号:AT87112204
申请日:1987-08-22
Applicant: BASF AG
Inventor: LEUTNER BERND DR , MUELLER BERTHOLD DR , VOLKENBORN WILHELM
-
公开(公告)号:DE3684372D1
公开(公告)日:1992-04-23
申请号:DE3684372
申请日:1986-07-07
Applicant: BASF AG
Inventor: VON OEHSEN UBBO DR , STECHER KARLHEINZ DR , KOEHLER WALDEMAR DR , MUELLER BERTHOLD DR , BRUNNMUELLER FRITZ DR , SCHNEIDER ROLF DR
Abstract: Thermolytic cracking of formamide (I) to HCN and H2O is carried out by introducing superheated (I) gas at 300-480 deg.C under reduced pressure of 1-350 mbar and with 0.1-10 vol.% air into a reactor with a nest of tubes and passing at 450-590 deg.C and an average dwell time of 0.01-0.25 s over highly sintered mouldings, consisting of 50-100 wt.% Al2O3 and 50-0 wt. % SiO2 or over Cr-Ni stainless steel mouldings, which are resistant to high temp. corrosion. (I) is introduced at 300-400 deg.C and 50-150 mbar with 1.0-3.0 vol.% air; and cracked at 500-540 deg.C witha dwell time of 0.01-0.15 s.. The mouldings consist of 85-95 wt.% Al2O3 and 15-5 wt.% SiO2; or of 18-21 wt.% Cr, 9-13 wt.% Ni, 0-3 wt.% and the rest Fe.
-
-
-
-
-