SOLAR CELL MODULE
    1.
    发明申请
    SOLAR CELL MODULE 审中-公开
    太阳能电池模块

    公开(公告)号:WO2011090321A3

    公开(公告)日:2011-12-29

    申请号:PCT/KR2011000399

    申请日:2011-01-20

    CPC classification number: H01L31/0481 C08K5/0016 H01L31/048 Y02E10/50

    Abstract: The present invention relates to a solar cell module, comprising: a solar cell; an encapsulation layer which protects the solar cell; and an adhesive layer which is interposed between the encapsulation layer and the solar cell, and which has adhesive force for attaching the encapsulation layer to the solar cell, wherein said adhesive force is weakened by a stimulus applied by an external source during the repair of the encapsulation layer.

    Abstract translation: 太阳能电池模块技术领域本发明涉及一种太阳能电池模块,其包括: 保护太阳能电池的封装层; 以及介于所述封装层和所述太阳能电池之间并且具有用于将所述封装层附接到所述太阳能电池的粘合力的粘合层,其中所述粘合力在所述修复期间由外部源施加的刺激而减弱 封装层。

    FABRICATION METHOD OF OPTICAL THIN FILM DEVICE SHOWING NONLINEAR CURRENT BEHAVIOR AND PHOTO TRANSISTOR USING THE OPTICAL DEVICE
    3.
    发明公开
    FABRICATION METHOD OF OPTICAL THIN FILM DEVICE SHOWING NONLINEAR CURRENT BEHAVIOR AND PHOTO TRANSISTOR USING THE OPTICAL DEVICE 审中-公开
    使用光学器件显示非线性电流行为和光电晶体的光学薄膜器件的制造方法

    公开(公告)号:KR20100012783A

    公开(公告)日:2010-02-08

    申请号:KR20080101118

    申请日:2008-10-15

    Abstract: PURPOSE: A method for manufacturing an optical device with a thin film type nonlinear current characteristic is provided to obtain a nonlinear current characteristic using the optical device which reacts with the light from a light emitting diode. CONSTITUTION: A zinc oxide is deposited by a sputtering method using a zinc oxide target(S100). A deposition process is performed under an argon atmosphere without the oxygen injection. The nitrogen is additionally injected in a deposition thickness of 50 to 1000 nm. A thermal process is performed under the oxygen atmosphere after a thin film deposition process(S110). The thermal process is performed by an in-situ method using a growth chamber in a vacuum state or an ex-situ process using a thermal chamber outside the vacuum state. A deposition temperature is between a room temperature and 400 degrees centigrade. The temperature of the thermal process is between 100 to 600 degrees centigrade.

    Abstract translation: 目的:提供一种制造具有薄膜型非线性电流特性的光学器件的方法,以使用与来自发光二极管的光反应的光学器件来获得非线性电流特性。 构成:使用氧化锌靶通过溅射法沉积氧化锌(S100)。 在氩气氛下进行沉积工艺,而不注入氧气。 另外以50至1000nm的沉积厚度注入氮气。 在薄膜沉积工艺之后,在氧气氛下进行热处理(S110)。 热处理通过使用真空状态的生长室的原位方法或使用真空状态之外的热室进行的非原位方法进行。 沉积温度在室温和400摄氏度之间。 热处理温度介于100至600摄氏度之间。