METHOD AND SYSTEM FOR PRODUCING AN INFRARED TRANSMITTING FIBER
    4.
    发明申请
    METHOD AND SYSTEM FOR PRODUCING AN INFRARED TRANSMITTING FIBER 审中-公开
    用于生产红外发射光纤的方法和系统

    公开(公告)号:WO2008084030A1

    公开(公告)日:2008-07-17

    申请号:PCT/EP2008/050099

    申请日:2008-01-07

    CPC classification number: C03B37/023 C03B2201/84 C03B2205/20 C03C13/041

    Abstract: The invention relates to a method for producing an infrared transmitting fiber (50) comprising the steps of providing a preform (20) of the infrared transmitting fiber (50) to be produced, said preform (20) comprising a receptacle, which is the precursor of the fiber's cladding, and a solid solution provided inside said receptacle, said solid solution being the precursor of the fiber's core; heating the fiber's preform (20) up to a temperature in which the receptacle softens and the solid solution melts; collecting the flow generated by the softened receptacle; drawing the fiber (50) from the collected flow.

    Abstract translation: 本发明涉及一种用于生产红外线传输光纤(50)的方法,包括以下步骤:提供待生产的红外线传输光纤(50)的预成型件(20),所述预成型件(20)包括作为前体的容器 的纤维包层,以及设置在所述容器内的固溶体,所述固溶体是纤维芯的前体; 将纤维的预成型件(20)加热到容器软化和固溶体熔化的温度; 收集软化容器产生的流量; 从收集的流中抽出纤维(50)。

    PROCESS FOR PRODUCING MICRO-OPTICAL ELEMENTS OR A FIBRE END IN THE FORM OF A MICRO-OPTICAL ELEMENT, AND THE USE OF SUCH ELEMENTS
    5.
    发明申请
    PROCESS FOR PRODUCING MICRO-OPTICAL ELEMENTS OR A FIBRE END IN THE FORM OF A MICRO-OPTICAL ELEMENT, AND THE USE OF SUCH ELEMENTS 审中-公开
    用于生产微型光学元件或光纤年底微光学元件和这些元素的使用形式

    公开(公告)号:WO1995029277A1

    公开(公告)日:1995-11-02

    申请号:PCT/EP1995001560

    申请日:1995-04-25

    Abstract: The invention concerns a process for producing micro-optical elements or a fibre end in the form of a micro-optical element, a base material being shaped to form the required micro-optical element. As a process by which elements can be produced and reproduced in larger batches, are transparent with low loss levels over a greater (i.e. wider band) spectral range than prior art elements, are not restricted in their possible surface geometry and are inexpensive to manufacture, a crystalline or polycrystalline fibre or section thereof which is substantially absorption-free in the spectral range 0.4 - 30 mu m and is produced from a base material of a solid solution, is shaped to produce micro-optical elements with that spectral range. The invention also concerns advantageous uses and applications of the disclosed micro-optical elements.

    Abstract translation: 本发明描述了用于生产微光学元件的或在微光学元件的形式的纤维端部的方法,其中起始材料形成为微光学元件的形状的方法。 提供一种方法,可以用在大批量是透明超过相比于现有技术和更宽的频带的光谱区域具有低的损失较大,没有在它们的表面几何形状的限制,它们是便宜地制造可再现的元素来产生 是用于生产微光学元件用的光谱范围从0.4到30微米的,单晶或多晶纤维或其一部分是自由的吸收基本上在该光谱范围内,这是从在固体溶液的起始材料制成的 使模子。 此外,本发明涉及有利用途和微光学元件的应用。

    VERFAHREN ZUR HERSTELLUNG VON SYNTHETISCHEM QUARZGLAS SOWIE QUARZGLAS FÜR DEN EINSATZ ALS MANTELMATERIAL EINER OPTISCHEN FASER
    6.
    发明申请
    VERFAHREN ZUR HERSTELLUNG VON SYNTHETISCHEM QUARZGLAS SOWIE QUARZGLAS FÜR DEN EINSATZ ALS MANTELMATERIAL EINER OPTISCHEN FASER 审中-公开
    工艺生产合成石英玻璃和石英玻璃用作表面材料光纤ONE

    公开(公告)号:WO2013087678A1

    公开(公告)日:2013-06-20

    申请号:PCT/EP2012/075197

    申请日:2012-12-12

    Abstract: Es ist ein Verfahren zur Herstellung von synthetischem Quarzglas bekannt, umfassend die Verfahrensschritte: (a) Umsetzen eines eine kohlenstoffhaltige Siliziumverbindung enthaltenden Einsatzmaterials mit Sauerstoff in einer Reaktionszone zu SiO 2 -Partikeln, (b) Abscheiden der SiO 2 -Partikel auf einer Ablagerungsfläche unter Bildung eines Kohlenstoff und Hydroxylgruppen enthaltenden, porösen SiO 2 -Sootkörpers, (c) Trocknen des porösen SiO 2 -Sootkörpers, und (d) Verglasen zu dem synthetischen Quarzglas durch Erhitzen des Sootkorpers auf eine Verglasungstemperatur. Um hiervon ausgehend ein Verfahren anzugeben, das eine kostengünstige Herstellung von Quarzglas durch Pyrolyse oder Hydrolyse einer kohlenstoffhaltigen Siliziumverbindung unter Einsatz eines kohlenstoffhaltigen Einsatzmaterials ermöglicht, wird erfindungsgemäß vorgeschlagen, dass ein Sootkörper mit einem Kohlenstoffgehalt im Bereich von 1 Gew.-ppm bis 50 Gew.-ppm erzeugt wird.

    Abstract translation: 它是用于制造合成石英玻璃的方法是已知的,包括以下步骤:(a)沉积表面2个颗粒上的SiO的含碳硅与氧的原料在反应区中,以SiO 2颗粒,含化合物的(b)中沉积反应以形成碳 和含羟基的,多孔的SiO 2烟灰体,(c)干燥所述多孔的SiO 2烟灰体,和(d)玻璃化由Sootkorpers加热到玻璃化温度的合成石英玻璃。 要指定此基础上的方法,其允许通过热解或水解廉价生产的石英玻璃的硅化合物,使用将碳质原料含碳,本发明提出了具有以重量计在1个重量ppm的范围内的碳含量,以50份微粉体 ppm的被生成。