公开(公告)号:KR100977177B1
公开(公告)日:2010-08-20
申请号:KR1020080127762
申请日:2008-12-16
Applicant: 제일모직주식회사
Abstract: 본 발명의 난연성 열가소성 수지 조성물은 (A) 폴리카보네이트 수지 1 내지 100 중량% 및 (B) 고무 변성 방향족 비닐계 공중합체 수지 0 내지 99 중량%로 이루어지는 기초수지 100 중량부에 대하여, (C) 브롬화 디페닐에탄 혼합물 0.01∼30 중량부를 포함한다. 본 발명의 난연성 열가소성 수지 조성물은 우수한 난연성뿐만 아니라, 내열성, 충격강도 및 성형성이 뛰어나다.
폴리카보네이트, 스티렌, 열가소성 수지, 할로겐, 난연성-
公开(公告)号:KR1020100073148A
公开(公告)日:2010-07-01
申请号:KR1020080131740
申请日:2008-12-22
Applicant: 제일모직주식회사
Abstract: PURPOSE: A flame retardant thermoplastic resin composition is provided to secure the stability for the fire by using a brominated diphenyl ethanol compound, and to improve the commercial availability and the heat resistance of the composition. CONSTITUTION: A flame retardant thermoplastic resin composition contains the following: 20~90 parts of rubber-reinforced polystyrene resin by weight; 10~80 parts of polyphenylene oxide resin by weight; and 0.01~30 parts of brominated diphenyl ethanol compound by weight. The rubber-reinforced polystyrene resin is a polymer containing 1~30wt% of rubber elastomer, and 70~99wt% of aromatic vinyl monomer. The polyphenylene oxide resin is poly(2,6-dimethyl,1,4-phenylene)ether.
Abstract translation: 目的:提供阻燃热塑性树脂组合物,以通过使用溴化二苯乙醇化合物来确保火灾的稳定性,并提高组合物的商业利用率和耐热性。 构成:阻燃性热塑性树脂组合物含有:20〜90重量份的橡胶增强聚苯乙烯树脂; 10〜80份聚苯醚树脂重量; 和0.01〜30份溴化二苯乙醇化合物。 橡胶增强聚苯乙烯树脂是含有1〜30重量%的橡胶弹性体和70〜99重量%的芳族乙烯基单体的聚合物。 聚苯醚树脂是聚(2,6-二甲基,1,4-亚苯基)醚。
-
公开(公告)号:KR1020100070207A
公开(公告)日:2010-06-25
申请号:KR1020080128826
申请日:2008-12-17
Applicant: 제일모직주식회사
IPC: C08K5/02
Abstract: PURPOSE: A brominated diphenyl ethane mixture and a resin composition using thereof are provided to secure the fire retardant property, the thermal stability, and the weatherability of the composition by controlling the contents of hexa bromodiphenyl ethane. CONSTITUTION: A brominated diphenyl ethane mixture produced by bromating diphenylethane contains hexa bromodiphenyl ethane, hepta bromodiphenyl ethane, and octa bromodiphenyl ethane. A producing method of the brominated diphenyl ethane mixture comprises a step of adding a brominating agent solution to a diphenylethane solution including a metal salt Lewis acid catalyst, and a step of controlling the contents of the hexa bromodiphenyl ethane into 55~85wt% by reacting the reactants at -20~50 deg C, and a step of controlling the content of a compound substituted with the odd number of diphenylethane Br into 0.01~30wt%.
Abstract translation: 目的:提供溴化二苯乙烷混合物及其使用的树脂组合物,以通过控制六溴二苯基乙烷的含量来确保组合物的阻燃性,耐热性和耐候性。 构成:通过溴化二苯乙烷生产的溴化二苯乙烷混合物含有六溴二苯乙烷,七溴二苯乙烷和八溴二苯乙烷。 溴化二苯乙烷混合物的制备方法包括将溴化剂溶液加入到包含金属盐路易斯酸催化剂的二苯乙烷溶液中的步骤,以及通过使六溴代二苯基乙烷的含量控制在55〜85wt% 反应物在-20〜50℃,将以奇数二苯基乙烷Br取代的化合物的含量控制在0.01〜30重量%的步骤。
-
公开(公告)号:KR100943662B1
公开(公告)日:2010-02-22
申请号:KR1020070137409
申请日:2007-12-26
Applicant: 제일모직주식회사
Abstract: 본 발명의 열안정성과 가공성이 우수한 열가소성 수지 조성물은 (A) (A
1 ) 에폭시기 포함 비닐공중합체 5∼100 중량% 및 (A
2 ) 고무강화 스티렌계 공중합 수지 0∼95 중량%로 이루어지는 에폭시기가 포함되어 있는 비닐계 고분자 30∼99 중량%; (B) 폴리에스테르 수지 1∼70 중량%; 상기 (A) + (B) 100 중량부에 대하여, (C) 브롬 함유 난연제 3∼20 중량부; 및 (D) 실란 화합물로 표면 개질된 안티몬 0.1∼6 중량부로 이루어지는 것을 특징으로 한다.
고무강화 스티렌계 수지, 폴리에스테르, 난연성, 열안정성, 가공성, 표면 개질된 산화 안티몬-
105.
公开(公告)号:KR1020090073620A
公开(公告)日:2009-07-03
申请号:KR1020070141607
申请日:2007-12-31
Applicant: 제일모직주식회사
IPC: C09K21/02
Abstract: A capsulated inorganic retardant is provided to improve heat resistance and dispersibility in thermal processing with a polymer resin by encapsulating antimony oxide, and to ensure excellent flame-retardant performance. A capsulated inorganic retardant is one that the whole and a part of the surface of the antimony oxide is coated with an epoxy resin. The antimony oxide is antimony trioxide(Sb2O3) or antimony pentaoxide(Sb2O5). The epoxy resin has a structure of the following chemical formula 1 or 2. A method for manufacturing the capsulated inorganic retardant comprises the steps of: mixing an epoxy resin, antimony oxide and emulsifier to prepare emulsion; injecting a hardener in the emulsion and performing inverse emulsion; and mixing and reacting the emulsified solution at 30-150 °C.
Abstract translation: 提供了一种封装的无机阻燃剂,以通过包封氧化锑来改善热处理中的耐热性和分散性,并确保优异的阻燃性能。 封装的无机阻燃剂是氧化锑表面的整个和一部分涂覆有环氧树脂的阻燃剂。 氧化锑是三氧化锑(Sb 2 O 3)或五氧化二锑(Sb 2 O 5)。 环氧树脂具有以下化学式1或2的结构。封装无机阻燃剂的制造方法包括以下步骤:将环氧树脂,氧化锑和乳化剂混合以制备乳液; 在乳液中注入固化剂并进行反相乳液; 并在30-150℃下使乳化溶液混合和反应。
-
公开(公告)号:KR1020090069673A
公开(公告)日:2009-07-01
申请号:KR1020070137409
申请日:2007-12-26
Applicant: 제일모직주식회사
Abstract: A flame-retardant thermoplastic resin composition is provided to improve processability and thermal stability while maintaining impact resistance and fire retardancy and to be suitable for the molding of large-sized products. A flame-retardant thermoplastic resin composition with excellent thermal stability and workability comprises (A) a styrene-based polymer 30~99 weight% including an epoxy group; (B) polyester resin 1~70 weight%; based on (A) + (B) of 100.0 parts by weight, (C) a brome-containing flame retardant 3~20 parts by weight; and (D) an antimony 0.1~6 parts by weight surface-modified with a silane compound. The styrene-based polymer(A) consists of (A1) an epoxy group-containing vinyl copolymer 5~100 weight% and (A2) a rubber-reinforced styrene-based copolymer resin 0~95 weight%.
Abstract translation: 提供阻燃热塑性树脂组合物以改善加工性能和热稳定性,同时保持耐冲击性和阻燃性,并且适合于大型产品的成型。 具有优异的热稳定性和加工性的阻燃性热塑性树脂组合物包含(A)包含环氧基的苯乙烯类聚合物30〜99重量% (B)聚酯树脂1〜70重量%; 基于(A)+(B)为100.0重量份,(C)含溴的阻燃剂为3〜20重量份; 和(D)用硅烷化合物表面改性的0.1〜6重量份的锑。 苯乙烯类聚合物(A)由(A1)含有环氧基的乙烯基共聚物5〜100重量%和(A2)橡胶强化苯乙烯系共聚物树脂0〜95重量%组成。
-
公开(公告)号:KR100830418B1
公开(公告)日:2008-05-20
申请号:KR1020070021841
申请日:2007-03-06
Applicant: 제일모직주식회사
Abstract: A thermoplastic resin composition suitable for the external material of an electrical product or an electronic product is provided to improve impact resistance remarkably. A thermoplastic resin composition comprises 30-99 parts by weight of a styrene-based polymer containing an epoxy group which comprises 5-100 wt% of a vinyl copolymer containing an epoxy group, and 0-95 wt% of a rubber reinforced styrene-based copolymer resin; and 1-70 parts by weight of a polyester resin. Preferably the vinyl copolymer containing an epoxy group is prepared by copolymerizing 0.001-5.0 mol% of an unsaturated epoxy-based compound containing an epoxy group and 95-99.999 mol% of a vinyl-based compound; and the styrene-based polymer contains 0.001-5.0 mo% of an epoxy group.
Abstract translation: 提供适用于电子产品或电子产品的外部材料的热塑性树脂组合物,以显着提高耐冲击性。 热塑性树脂组合物包含30-99重量份含有环氧基的苯乙烯基聚合物,其包含5-100重量%的含有环氧基的乙烯基共聚物和0-95重量%的橡胶增强苯乙烯基 共聚树脂; 和1-70重量份的聚酯树脂。 优选地,含有环氧基的乙烯基共聚物通过使0.001-5.0mol%的含有环氧基的不饱和环氧基化合物和95-99.999mol%的乙烯基类化合物共聚来制备; 苯乙烯类聚合物含有0.001-5.0摩尔%的环氧基。
-
公开(公告)号:KR100783022B1
公开(公告)日:2007-12-07
申请号:KR1020060117203
申请日:2006-11-24
Applicant: 제일모직주식회사
Abstract: A styrene-based thermoplastic resin composition, and a pellet prepared by extruding the composition are provided to improve impact resistance, particularly falling impact resistance, fluidity, and injection moldability without the deterioration of heat resistance and thermal stability. A styrene-based thermoplastic resin composition comprises 100 parts by weight of a rubber modified styrene-based copolymer resin; 0.01-30 parts by weight of an organic dicarbonic acid modified ethylene-based rubber; and 1-10 parts by weight of a chlorinated polymer. Preferably the rubber modified styrene-based copolymer resin comprises 20-100 parts by weight of a styrene-based graft copolymer resin; and 0-80 parts by weight of a styrene-based copolymer resin.
Abstract translation: 提供苯乙烯类热塑性树脂组合物和通过挤出组合物制备的颗粒以提高耐冲击性,特别是耐冲击性,流动性和注模成型性,而不会降低耐热性和热稳定性。 苯乙烯类热塑性树脂组合物包含100重量份的橡胶改性苯乙烯基共聚物树脂; 0.01-30重量份有机二羰基改性乙烯基橡胶; 和1-10重量份的氯化聚合物。 优选地,橡胶改性苯乙烯基共聚物树脂包含20-100重量份的基于苯乙烯的接枝共聚物树脂; 和0-80重量份的苯乙烯基共聚物树脂。
-
公开(公告)号:KR100602850B1
公开(公告)日:2006-07-19
申请号:KR1020030091833
申请日:2003-12-16
Applicant: 제일모직주식회사
Abstract: 본 발명의 난연성을 갖는 열가소성 수지 조성물은 고무 변성 스티렌계 수지(A) 40 내지 95 중량부, 폴리페닐렌 에테르계 수지(B) 60 내지 5 중량부, 스티렌계 수지(C) 10 내지 40 중량부로 이루어진 기초수지 (A)+(B)+(C) 100 중량부를 기준으로 하여 아크릴로니트릴함량이 5 내지 18 중량%인 스티렌-아크릴로니트릴 공중합체 수지(D) 2 내지 30 중량부, 알킬 포스피닉산 금속염 화합물(E) 0.5 내지 30 중량부, 방향족 인산 에스테르 화합물(F) 0 내지 30 중량부를 적용한 난연성 및 내열도가 우수한 열가소성 수지 조성물에 관한 것이다. 상기 열가소성 수지 조성물은 용도에 따라 가소제, 열안정제, 산화방지제, 광안정제, 상용화제, 안료, 염료 및/또는 무기물 첨가제를 더 포함할 수 있다.
난연성 수지 조성물, 아크릴로니트릴, 알킬 포스피닉산 금속염, 방향족 인산 에스테르, 내열도Abstract translation: 热塑性树脂组合物具有本发明的阻燃性的橡胶改性的苯乙烯类树脂(A)40〜95重量份的聚苯醚系树脂(B)60〜5重量份的苯乙烯类树脂(C)按重量计10至40份 相对于基础树脂(A)+(B)+(C)100重量份,丙烯腈含量为5〜18重量%的苯乙烯 - 丙烯腈共聚物树脂(D)2〜30重量份 将0.5至30重量份的邻苯二甲酸金属盐化合物(E)和0至30重量份的芳族磷酸酯化合物(F)应用于具有优异的阻燃性和耐热性的热塑性树脂组合物。 取决于用途,热塑性树脂组合物可进一步包含增塑剂,热稳定剂,抗氧化剂,光稳定剂,增容剂,颜料,染料和/或无机添加剂。
-
公开(公告)号:KR100568080B1
公开(公告)日:2006-04-05
申请号:KR1020020084711
申请日:2002-12-27
Applicant: 제일모직주식회사
IPC: C08L51/06
Abstract: 본 발명의 난연성 열가소성 수지 조성물은 (A) (a
1 ) 고무상 중합체 5 내지 65 중량%에 방향족비닐계 단량체 30 내지 95 중량%, 상기 방향족 비닐계와 공중합 가능한 단량체 0 내지 20 중량%, 및 가공성 및 내열성을 부가하는 단량체 0 내지 15 중량%를 첨가하여 그라프트 중합시킨 그라프트 공중합체 수지 20 내지 100 중량% 및 (a
2 ) 방향족 비닐계 단량체 60 내지 90 중량%에 상기 방향족 비닐계 단량체와 공중합 가능한 단량체 10 내지 40 중량% 및 가공성 및 내열성을 부가하는 단량체 0 내지 30 중량%를 첨가하여 공중합시킨 공중합체수지 0 내지 80 중량%로 이루어진 고무변성 스티렌계 수지 100 중량부; 및 (B) 옥사 포스포란계 화합물 15 내지 40 중량부로 이루어지는 것을 특징으로 한다.
고무변성 스티렌계 수지, 옥사 포스포란계 화합물Abstract translation: 本发明的阻燃热塑性树脂组合物包含(A)(a
-
-
-
-
-
-
-
-
-