    Abstract: PURPOSE: Provided is an environmental-friendly method for making a cathode plate for a lithium secondary battery, which uses an aqueous H2O2-containing solution that is not harmful to human bodies to form high-viscosity slurry suitable for coating on a cathode collector. CONSTITUTION: The method for making a cathode plate comprises: a step(1) for dissolving vanadium pentoxide into an aqueous H2O2-containing solution; a step(3,4) for adding a conductive agent to form a gel; a step(5) for removing moisture from the gel; and a step(6) for coating the gel onto a cathode collector and then drying. Particularly, the aqueous solution comprises 5 to 20 wt% of H2O2. The conductive agent may be added together with a binder, and the conductive agent is preferably super-p and the binder is preferably carboxymethyl cellulose.

    Abstract translation: 目的:提供一种用于制造锂二次电池阴极板的环保方法,其使用对人体无害的含H 2 O 2水溶液形成适于涂覆在阴极集电体上的高粘度浆料。 构成:制造阴极板的方法包括:将五氧化二钒溶解在含水H 2 O 2溶液中的步骤(1) 用于添加导电剂以形成凝胶的步骤(3,4); 用于从凝胶中除去水分的步骤(5); 以及用于将凝胶涂布到阴极集电体上然后干燥的步骤(6)。 特别地,水溶液含有5〜20重量%的H 2 O 2。 导电剂可以与粘合剂一起加入,导电剂优选为超级p,粘合剂优选为羧甲基纤维素。

Patent Agency Ranking