Abstract:
전고체형 필름 일차전지 및 그 제조 방법에 관하여 개시한다. 본 발명에 따른 필름 일차전지는 제1 고분자 필름 및 제1 전도층으로 구성되는 제1 고분자 집전체 필름과, 상기 제1 전도층 위에 형성된 제1 전극층과, 제2 고분자 필름 및 제2 전도층으로 구성되는 제2 고분자 집전체 필름과, 상기 제2 전도층 위에 형성된 제2 전극층과, 상기 제1 전극층과 제2 전극층과의 사이에 형성되어 있고 수계 전해액을 포함하는 고분자 전해질층을 포함한다. 필름, 일차전지, 고분자 집전체 필름, 수계 전해액, 전고체형, 고분자 전해질
Abstract:
A novel dithiafuvalenes compound, a method for preparing the same compound, and a dye-sensitized solar cell using dye comprising the same compound are provided to form the dye-sensitized solar cell having various kinds of colors. A dye-sensitized solar cell includes a semiconductor electrode(10), a facing electrode(20), and an electrolyte solution(30) inserted between the semiconductor electrode and the facing electrode. The semiconductor electrode is formed with a transparent conductive glass substrate(12) and a nano-particle metal oxide layer(14) formed on the transparent conductive glass substrate. The facing electrode includes a conductive glass substrate(22) and a platinum layer(24).
Abstract:
나노입자(nano-particle)가 충진된 상반전(phase inversion) 고분자 전해질 제조 방법을 제시한다. 본 발명에 따르면, 고분자 매트릭스(polymer matrix)와 무기 충진제를 용매에 용해시켜 만든 슬러리(slurry)를 캐스팅(casting)한 직후 즉시 흐르는 물 속에 함침하여 내부 기공이 크게 발달된 다공성 고분자 막 형성하고, 고분자 막에 전해액을 함침시켜 고분자 전해질을 제조한다. 이에 따라, 고용량 소형 리튬(Li) 2차전지에 적용하여 우수한 전지 특성을 얻을 수 있는 고분자 전해질을 제공할 수 있다. 리튬 2차전지, 충진, 캐스팅, 상반전 기법, 폴리머 매트릭스
Abstract:
염료감응 태양전지의 나노 입자 산화물 전극 형성 방법을 제공한다. 본 발명은 산성 또는 염기성에서 분산이 잘되는 나노 입자 산화물 콜로이드 용액에 각각 염기성 수용액 및 산성 용액을 첨가하여 산-염기 반응에 의해 염 형태의 나노 입자 산화물 페이스트를 형성한다. 이어서, 상기 나노 입자 산화물 페이스트를 기판에 코팅한 후, 150℃ 이하의 저온에서 건조시켜 염료감응 태양전지의 나노 입자 산화물 전극을 형성한다. 이에 따라, 본 발명은 고분자를 첨가하지 않고도 점도가 높은 저온코팅용 나노 입자 산화물 페이스트를 산-염기 화학에 기초하여 제조할 수 있고, 이를 통하여 저온에서도 나노 입자 산화물 전극을 형성할 수 있다.
Abstract:
본 발명은 메탈 나이트라이드를 주성분으로 하는 리튬 이차전지용 음극 조성물 및 그 제조 방법에 관하여 개시한다. 본 발명에 따른 리튬 이차전지용 조성물을 제조하기 위하여 메탈 나이트라이드 활물질에 도전제 및 결합제를 혼합하여 슬러리를 제조한다. 상기 슬러리를 집전체에 코팅한다. 상기 코팅된 슬러리를 건조시킨다.
Abstract:
PURPOSE: A method for preparing lithium-cobalt-manganese based oxides for a lithium secondary battery is provided to improve the structure stability and electrochemical properties including discharge capacity of the resulted oxides through a simplified and economic process using a combustion process. CONSTITUTION: The method for preparing lithium-cobalt-manganese based oxides comprises: preparing an aqueous solution of salts of lithium, cobalt and manganese (10); heating the aqueous solution to form a gel (20); combusting the gel to form powdered oxides (30); treating the powdered oxides with heat to form a powder of Li£CoxLi(1/3-X/3)Mn(2/3-2x/3)|O2, wherein 0.05
Abstract:
PURPOSE: Provided is a composite polymer electrolyte for lithium secondary battery which has significantly improved ionic conductivity, thin thickness and reinforced mechanical property. CONSTITUTION: The composite polymer electrolyte(10) for a lithium secondary battery is manufactured by the method comprising the steps of: preparing a first polymer matrix(12) comprised of a first porous polymer having a first pore size; obtaining a solution of a single-ion conductor, mineral and second porous polymer having a second pore size lower than the first pore size in a cosolvent; coating the solution on the first polymer matrix to form a second polymer matrix(14); and impregnating an electrolytic solution(16) into the first polymer matrix(12) and the second polymer matrix(14).
Abstract:
아크릴로니트릴계 고분자와 양이온성 고분자가 혼합된 고분자 브렌드를 이용한 비수계 이차전지용 고분자 전해질 및 그 제조 방법에 관하여 개시한다. 본 발명에 따른 고분자 전해질의 제조 방법에서는 아크릴로니트릴 반복 단위를 포함하는 고분자 및 양이온성 고분자를 브렌딩하여 고분자 브렌드를 준비한다. 상기 고분자 브렌드 및 무기물을 공용매에 용해시켜 고분자 브렌드 용액을 제조한다. 상전환법에 의해 상기 고분자 브렌드 용액으로부터 다공성 고분자 필름을 형성한다. 상기 다공성 고분자 필름을 리튬염이 용해된 전해액에 함침시킨다.
Abstract:
PURPOSE: Provided is an environmental-friendly method for making a cathode plate for a lithium secondary battery, which uses an aqueous H2O2-containing solution that is not harmful to human bodies to form high-viscosity slurry suitable for coating on a cathode collector. CONSTITUTION: The method for making a cathode plate comprises: a step(1) for dissolving vanadium pentoxide into an aqueous H2O2-containing solution; a step(3,4) for adding a conductive agent to form a gel; a step(5) for removing moisture from the gel; and a step(6) for coating the gel onto a cathode collector and then drying. Particularly, the aqueous solution comprises 5 to 20 wt% of H2O2. The conductive agent may be added together with a binder, and the conductive agent is preferably super-p and the binder is preferably carboxymethyl cellulose.
Abstract translation:目的:提供一种用于制造锂二次电池阴极板的环保方法,其使用对人体无害的含H 2 O 2水溶液形成适于涂覆在阴极集电体上的高粘度浆料。 构成:制造阴极板的方法包括:将五氧化二钒溶解在含水H 2 O 2溶液中的步骤(1) 用于添加导电剂以形成凝胶的步骤(3,4); 用于从凝胶中除去水分的步骤(5); 以及用于将凝胶涂布到阴极集电体上然后干燥的步骤(6)。 特别地,水溶液含有5〜20重量%的H 2 O 2。 导电剂可以与粘合剂一起加入,导电剂优选为超级p,粘合剂优选为羧甲基纤维素。