Method of making heat exchanger coil
    111.
    发明授权
    Method of making heat exchanger coil 失效
    制造换热器盘管的方法

    公开(公告)号:US4186474A

    公开(公告)日:1980-02-05

    申请号:US693587

    申请日:1976-06-07

    Applicant: Louis P. Hine

    Inventor: Louis P. Hine

    Abstract: The copper inlet and outlet tube arrangements for an essentially all aluminum coil comprised of aluminum fins, hairpin tubes, and return bends, are ultrasonically soldered to open ends of the hairpin tubes at the same time as the return bends are soldered to the hairpin tubes in an ultrasonic soldering bath; with any bonds of the copper inlet and outlet tube arrangements, such as connections to an expansion device and a connection to a suction header being located at an elevation above the solder bath to preclude contamination of the bath from the bonds.

    Abstract translation: 用于由铝翅片,发夹管和返回弯头组成的基本上所有铝线圈的铜入口和出口管布置在回弯弯管焊接到发夹管的同时被超声波焊接到发夹管的开口端 超声波焊接浴; 具有铜入口和出口管布置的任何连接,例如到膨胀装置的连接以及与抽吸集管的连接位于焊料槽上方的高度处,以防止熔池从粘结中被污染。

    Soldered joint and method
    112.
    发明授权
    Soldered joint and method 失效
    焊接接头和方法

    公开(公告)号:US3957289A

    公开(公告)日:1976-05-18

    申请号:US498704

    申请日:1974-08-19

    Abstract: The present invention relates to the making of an evaporator or condenser construction wherein ends of heat exchange tubes extending through heat exchange plates or fins are joined with return bend connectors. The ends of the tubes are provided with flared cups that telescopically receive the ends of return bend connectors. Nibs are formed on the outer surface of and extend outwardly a predetermined amount from the outer surface of the return bend connectors near the ends thereof. Grooves are formed on said outer surface and extend longitudinally between each nib and the end of the connector. When the end of a return bend connector is inserted into a flared cup, an interference fit between the nibs and the cup centers the end of the connector in the cup and frictionally retains the tube and the return bend in assembled relation when the assembly is inverted and thereafter submerged in a solder bath. The grooves provide vents for hot gases during the soldering operation.

    Abstract translation: 本发明涉及蒸发器或冷凝器结构的制造,其中延伸穿过热交换板或翅片的热交换管的端部与回弯接头连接。 管的端部设置有可伸缩地容纳返回弯曲连接器的端部的扩口杯。 在返回弯曲连接器的靠近其端部的外表面上形成有一个预定量的外表面并且向外延伸的笔尖。 沟槽形成在所述外表面上并且在每个尖端和连接器的端部之间纵向延伸。 当返回弯曲连接器的端部插入喇叭形杯中时,笔尖和杯子之间的过盈配合将连接器的端部中心,并且当组件反转时摩擦地将管子和返回弯头保持组装关系 然后浸没在焊料槽中。 沟槽在焊接操作期间为热气体提供通风口。

    JOINING TOOL WITH INDUCTIVE HEATING DEVICE AND METHOD FOR INDUCTIVELY HEATING A JOINING MEMBER
    117.
    发明申请
    JOINING TOOL WITH INDUCTIVE HEATING DEVICE AND METHOD FOR INDUCTIVELY HEATING A JOINING MEMBER 审中-公开
    带有感应加热装置的加工工具和用于感应加热成员的方法

    公开(公告)号:WO2017121823A1

    公开(公告)日:2017-07-20

    申请号:PCT/EP2017/050605

    申请日:2017-01-12

    Abstract: Joining tool (10) for inductively heating an, at least in some portions, inductively heatable joining member (18), wherein the joining tool (10) has a joining head (12) having a holding device (28) for holding the joining member (18). The joining tool (10) further has an inductive heating device (36), wherein an electric coil (40) of the inductive heating device (36) is arranged such that a joining member (18) held in the holding device (28) can be inductively heated. The inductive heating device (36) here has a heat exchanger tube (50).

    Abstract translation: (10),用于至少部分地感应加热可感应加热的接合构件(18),其中接合工具(10)具有接合头部(12),接合头部(12)具有保持装置 (28),用于保持连接构件(18)。 接合工具(10)还具有感应加热装置(36),其中感应加热装置(36)的电线圈(40)布置成使得保持在保持装置(28)中的接合构件(18)可以 被感应加热。 感应加热装置(36)在此具有热交换管(50)。

    FLUXLESS BRAZING METHOD
    118.
    发明申请
    FLUXLESS BRAZING METHOD 审中-公开
    无流体钎焊法

    公开(公告)号:WO2017080771A1

    公开(公告)日:2017-05-18

    申请号:PCT/EP2016/075155

    申请日:2016-10-20

    Abstract: The invention relates to a method of manufacturing a heat exchanger, joined by brazing in a controlled atmosphere brazing process, comprising the steps of: (a)providing of the components to be brazed together of which at least one is made from an aluminium alloy brazing sheet product comprising of a core alloy clad on one or both sides with a Al-Si alloy brazingfiller material, the Al- Si alloy brazing filler material has been pre-treated by means of etching with an alkaline or acidic etchant, and wherein the Al-Si alloy brazing filler material has the following composition, consisting of, in wt.%: Si 5% to 15%, Mg 0.10% to 3%, Fe up to 0.8%, Cu up to 0.3%, Mn up to 0.8%, Zn up to 0.25%, Ti up to 0.3%, balance aluminium, (b)assembling the components into an assembly, (c)brazing the assembly without applying brazing flux onto the assembly components, and brazing the whole assembly in a dry inert gas atmosphere at a brazing temperature, and wherein the oxygen content of the dry inert gas atmosphere is less than 35 ppm, and cooling of the brazed assembly.

    Abstract translation: 本发明涉及一种制造热交换器的方法,所述热交换器通过在受控气氛钎焊工艺中钎焊而连接,所述方法包括以下步骤:(a)提供待钎焊在一起的部件,其至少部分地 一种由铝合金钎焊片材产品制成,所述铝合金钎焊片材产品包括在一侧或两侧包覆有铝硅合金钎焊填充材料的芯合金,所述铝硅合金钎焊填充材料已通过碱性蚀刻进行预处理 或酸性蚀刻剂,并且其中所述Al-Si合金钎焊填充材料具有以下组成,其包含以重量%计:Si 5%至15%,Mg 0.10%至3%,Fe最高达0.8%,Cu最高至 0.3%,Mn高达0.8%,Zn高达0.25%,Ti高达0.3%,余量为铝,(b)将组件组装成组件,(c)在不将钎焊剂施加到组件上的情况下硬焊组件, 将整个组件在钎焊温度下在干燥的惰性气体气氛中钎焊,并且其中, 干燥的惰性气体气氛小于35 ppm,并冷却钎焊组件。

    쉘앤튜브 열교환기
    119.
    发明申请
    쉘앤튜브 열교환기 审中-公开
    壳管热交换器

    公开(公告)号:WO2016159450A1

    公开(公告)日:2016-10-06

    申请号:PCT/KR2015/007094

    申请日:2015-07-08

    Abstract: 본 발명은 원통 형상의 동체로 된 쉘과, 상기 쉘의 내부를 구획하도록 설치되고, 서로 마주보도록 복수의 튜브삽입홀이 각각 관통 형성된 한 쌍의 튜브시트와, 상기 튜브시트 사이를 연결하도록 서로 마주보는 상기 튜브삽입홀 각각에 용접 결합되는 복수의 튜브를 포함하는 쉘앤튜브 열교환기에 있어서, 상기 튜브와 동일한 직경으로 형성되고, 상기 튜브시트 각각의 튜브삽입홀 내부로 각각 삽입되는 원통 형상으로 된 복수의 튜브접합부재와, 장형의 용접와이어를 일정한 길이로 절단한 후 링형상으로 제작되고, 상기 튜브 각각의 양단 외주에 각각 삽입되는 복수의 링와이어를 더 포함하고, 상기 튜브시트 각각은, 서로 마주보는 면에 상기 튜브삽입홀로부터 외주방향을 향해 접합부가 형성되도록 소정의 거리만큼 이격된 환형의 튜브시트홈이 함몰 형성되고, 상기 튜브 각각은, 양단이 상기 튜브접합부재의 마주보는 각각의 일단에 접촉함과 동시에 상기 튜브시트홈의 함몰된 간격 범위 내에 각각 위치하도록 상기 튜브시트의 마주보는 각각의 튜브삽입홀에 삽입되고, 상기 튜브접합부재의 내부로 삽입된 용접토치를 이용하여 상기 튜브시트 각각에 상기 링와이어를 용가재로 하여 상기 튜브접합부재와 용접결합되는 것을 특징으로 하는 쉘앤튜브 열교환기이다.

    Abstract translation: 本发明涉及一种管壳式热交换器,其包括:壳体,其构造为圆柱形主体; 安装成限定壳体内部的一对管板,多个管插入孔,通过每个管板形成为彼此相对; 以及分别彼此相对地焊接/耦合到管插入孔的多个管,以便在管板之间连接,其中管壳式热交换器还包括多个管接合构件,多个管接合构件 形成为具有与管相同的直径,其插入到各管板的相应的管插入孔中并且具有圆柱形状,以及多个环形线,其通过将长焊丝切割成预定的 长度并给出相同的环形,并插入相应管的两端的外周; 相应的管板具有通过相互面对的凹陷表面形成的环形管板槽,以便间隔预定距离,使得从管插入孔朝向外周形成接合部分; 各管的两端与彼此面对的管接合构件的一端相接触,并且将各管插入到要位于缩进间隔范围内的管片的相应管插入孔中 的管板槽; 并且使用插入到管接合构件中的焊接接触和使用环形线作为填充金属,将各个管与管接合构件一起焊接/联接到相应的管板。

    ろう付方法
    120.
    发明申请
    ろう付方法 审中-公开
    制动方法

    公开(公告)号:WO2016093017A1

    公开(公告)日:2016-06-16

    申请号:PCT/JP2015/082035

    申请日:2015-11-13

    Abstract:  量産設備に容易に適用でき、作業工程の簡素化が容易であり、ろう付接合の品質を安定可能なろう付方法を提供する。Mg:0.2%未満に規制され残部Al及び不可避不純物からなる化学成分を有する心材層(B)と、Si:4.0~13.0%、Bi:0.01~0.3%を必須に含み、更にLi:0.004~0.08%及びBe:0.006~0.12%のうち1種又は2種を含み、Mg:0.1%未満に規制され残部Al及び不可避不純物からなる化学成分を有し、心材層(C)の少なくとも一方の面にクラッドされたろう材層(B)とを有するブレージングシート(2)を含む被処理物(1)を準備する。ろう材層(B)が内側被接合部(12)及び外側被接合部(13)の両方に存在するように被処理物(1)を組み立てる。外側被接合部(13)のろう材層(B)上にフラックス(3)を塗布した後、不活性ガス雰囲気下で被処理物(1)を加熱してろう付を行う。

    Abstract translation: 本发明提供一种能够容易地应用于大规模生产设备的钎焊方法,其中可以容易地简化操作步骤并且可以稳定钎焊的质量。 制备待处理物体(1),所述待处理物体包括钎焊片(2),其包括:具有Mg限制在小于0.2%的化学组成的芯材料层(C),其余部分 的Al和不可避免的杂质; 和具有基本上含有4.0-13.0%Si和0.01-0.3%Bi的化学组成的钎料层(B),并且还含有0.004-0.08%的Li和/或0.006-0.12%的Be,其中Mg被限制在 小于0.1%,其余由Al和不可避免的杂质构成,钎料层(B)包覆芯材层(C)的至少一个表面。 被加工物(1)组装成使得钎焊材料层(B)存在于内部接合部(12)和外部接合部(13)中。 将助熔剂(3)施加到外部接合部(13)的钎料层(B)上,并将待处理物体(1)在惰性气体气氛中加热钎焊。