公开(公告)号:DE19845317A1
公开(公告)日:2000-04-06
申请号:DE19845317
申请日:1998-10-01
Applicant: BASF AG
Inventor: FISCHER MICHAEL , WEBER MARTIN , GINSS CHRISTOPHE , BERZ STEPHAN , KRES NORBERT
IPC: C08J5/04 , C08F265/04 , C08F279/02 , C08K3/40 , C08K5/00 , C08K7/14 , C08L25/08 , C08L25/12 , C08L25/14 , C08L51/00 , C08L51/06 , C08L55/02 , C08L67/02 , C08L67/03 , C08L101/10 , C08L25/06 , C08L33/20
Abstract: The invention relates to a fiber-reinforced thermoplastic moulding material containing the following ingredients in relation to the sum of ingredients A-D and optionally E and F, representing a total of 100 wt. %: d) 10-97 wt. % of at least one aromatic polyester as ingredient A; e) 1-50 wt. % of at least one particle-shaped grafted copolymer with a soft phase glass transition temperature that is lower than 0 DEG C and an average particle size of 50-1000 nm as ingredient B; f) 1-50 wt. % of at least one copolymer made of monomers c1) 50-90 wt. % of at least one vinyl aromatic monomer as ingredient C1 and c2) 10-25 wt. % acrylonitrile and/or methacrylonitrile as ingredient C2, as ingredient C; 1-50 wt. % glass fibers as ingredient D; f) 0-25 wt. % other ingredients that are compatible, can be mixed in a homogenous manner with ingredients A and/or C and can be dispersed therein, as ingredient E; f) 0-10 wt. % usual additives such as UV stabilizers, oxidation retarders, lubricating agents and release agents as ingredient F. The invention also relates to moulded parts made from said moulding materials and used in the interiors of motor vehicles. The invention further relates to the use of moulding materials in the production of moulded parts.
-
公开(公告)号:DE19840274A1
公开(公告)日:2000-03-09
申请号:DE19840274
申请日:1998-09-03
Applicant: BASF AG
Inventor: FISCHER MICHAEL , FISCH HERBERT , JUNG NORBERT , TECHRITZ KLAUS
Abstract: Thermoplastic molding materials containing (wt.%): (A) polyester (5-99); (B) an aminosilane compound and an epoxy polymer pretreated fiber forming filler (1-50); (C) an elastic rubber polymerizate (0-30); (D) an additional additive (0-40), where the sum of (A) to (D) = 100% are new. Independent claims are included for: (1) A molded body obtainable from the thermoplastic molding materials; (2) a laser addressed molded body obtainable from the thermoplastic molding materials; (3) KGZ internal and external parts obtainable from the thermoplastic molding materials.
-
公开(公告)号:DE59700372D1
公开(公告)日:1999-09-30
申请号:DE59700372
申请日:1997-01-22
Applicant: BASF AG
Inventor: FISCHER MICHAEL , KOCH JUERGEN
IPC: B29D7/00 , C08F293/00
Abstract: A block copolymer obtainable by reactingA) monomers selected from the group consisting of styrene, alpha-methylstyrene, acrylonitrile, methacrylonitrile, methyl methacrylate and maleic anhydride to form blocks A having a glass transition temperature Tg of more than 0° C. andB) monomers selected from the group consisting of n-butyl acrylate, methyl acrylate and 2-ethylhexyl acrylate to form blocks B having a glass transition temperature Tg of less than 0° C.at from 100 to 160° C. in the presence of free-radical initiators and N-oxyl radicals.
-
公开(公告)号:MX9803723A
公开(公告)日:1998-09-30
申请号:MX9803723
申请日:1998-05-11
Applicant: BASF AG
Inventor: FISCHER MICHAEL , KOCH JURGEN
IPC: B29D7/00 , C08F293/00 , B29D07/00
Abstract: La presente invencion se refiere a un copolímero en bloques obtenible mediante la reaccion de: A) monomeros seleccionados del grupo que consiste en estireno, alfa-metilestireno, acrilonitrilo, metacrilonitrilo, metacrilato de metilo, y anhídrido maléico para formar bloques A con una temperatura de transicion del vidrio TV demás de 0 degree C. y B) monòmeros seleccionados del grupo que consiste en acrilato de n-butilo, acrilato de metilo y acrilato de 2-etilhexilo para formar bloques B con una temperatura de transicion del vidrio TV de menos de 0 degree C. desde 100 a 170 degree C en presencia de iniciadores radicales libres y radicales N-oxilo.
-
公开(公告)号:AU1593997A
公开(公告)日:1997-08-20
申请号:AU1593997
申请日:1997-01-22
Applicant: BASF AG
Inventor: FISCHER MICHAEL , KOCH JURGEN
IPC: B29D7/00 , C08F293/00
Abstract: A block copolymer obtainable by reactingA) monomers selected from the group consisting of styrene, alpha-methylstyrene, acrylonitrile, methacrylonitrile, methyl methacrylate and maleic anhydride to form blocks A having a glass transition temperature Tg of more than 0° C. andB) monomers selected from the group consisting of n-butyl acrylate, methyl acrylate and 2-ethylhexyl acrylate to form blocks B having a glass transition temperature Tg of less than 0° C.at from 100 to 160° C. in the presence of free-radical initiators and N-oxyl radicals.
-
-
-
-