LIQUID MATERIAL APPLYING APPARATUS, SEALING APPARATUS FOR SUBSTRATE AND APPARATUS AND METHOD OF MANUFACTURING SUBSTRATE USING THE APPARATUSES

    公开(公告)号:JP2002233806A

    公开(公告)日:2002-08-20

    申请号:JP2001030443

    申请日:2001-02-07

    Applicant: SONY CORP

    Abstract: PROBLEM TO BE SOLVED: To provide a liquid material applying apparatus capable of applying a liquid material uniformly, precisely and efficiently on a substrate or a laminated material in every corner, a sealing apparatus for substrate, which is capable of sealing the substrate and the laminated material while surely preventing the incorporation of bubbles or the generation of air pool, and an apparatus for manufacturing the high quality substrate, formed by fully sealing the whole surface of the laminated material and a manufacturing method thereof. SOLUTION: The liquid material applying apparatus for applying the liquid material on a prescribed position of the substrate 21 or the laminated material 22 is provided with syringes 5, 6 and 7 each possessing at least >=1 sets of coating nozzles each composed of a cylindrical nozzle and a slit nozzle and holding the liquid material inside, a triaxial moving means 8 for moving the sylinges 5, 6 and 7 in the X, Y, and Z directions, which cross each other at the right angle, a detecting means for detecting the position of the substrate 21 or the laminated material 22 in the Z axial direction and a moving means 23 for moving the substrate 21 or the laminated material 22 in the Z axial direction.

    DISPLAY DEVICE AND ITS MANUFACTURING METHOD

    公开(公告)号:JP2002221916A

    公开(公告)日:2002-08-09

    申请号:JP2001017801

    申请日:2001-01-26

    Applicant: SONY CORP

    Abstract: PROBLEM TO BE SOLVED: To provide an upper surface light-emission type display device having a good contrast and a manufacturing method of the display device suitable for the manufacture of this display device. SOLUTION: While forming light emitting elements 3 on a supporting substrate 1, black matrixes 13 are formed on a transparent counter substrate 11. The supporting substrate 1 and the counter substrate 11 are stuck together in the state of sealing the display elements 3 with an adhesion resin 21, and filling the adhesion resin 21 between the supporting substrate 1 and the counter substrate 11. On this occasion, the supporting substrate 1 and the counter substrate 11 are aligned so that the formation surface of the black matrixes 13 in the counter substrate 11 may be oppositely placed in the formation surface of the light emitting elements 3 in the supporting substrate 1, and that the black matrixes 13 may be disposed by oppositely placing them between the light emitting elements 3. This alignment is performed by disposing an alignment mark 7 formed on the formation surface of the light emitting elements 3 in the supporting base plate 1, and an alignment mark 17 formed on the counter substrate 11 in the predetermined state.

    DISPLAY DEVICE AND ITS MANUFACTURING METHOD

    公开(公告)号:JP2002221911A

    公开(公告)日:2002-08-09

    申请号:JP2001015424

    申请日:2001-01-24

    Applicant: SONY CORP

    Abstract: PROBLEM TO BE SOLVED: To provide a method for manufacturing a display device which can suppress the contamination of air bubbles inside the sealing and has high productivity. SOLUTION: A light emitting element 2 is formed on a substrate film 101. Then unhardened sealing resin 13 is supplied onto a light emitting element 2 forming surface of the substrate film 101. The substrate film 101 and a sealing film 104 which are arranged with the space by holding the sealing resin 13 and the light emitting element 2 therebetween are pressurized to each other via the sealing resin 13 by a pressing mechanism 303 successively from these end part sides to stick the substrate film 101 and the sealing film 104 together at an upstream side of a moving direction of the pressed part while holding the space between substrate film 101 and the sealing film 104 at a downstream side of the moving direction of the pressed part to the substrate film 101. Thereafter the sealing resin 13 in a state charged into a cladded part between the substrate film and the sealing film, is hardened.

    ORGANIC ELECTRIC-FIELD LIGHT-EMITTING ELEMENT

    公开(公告)号:JP2001135482A

    公开(公告)日:2001-05-18

    申请号:JP31207099

    申请日:1999-11-02

    Applicant: SONY CORP

    Abstract: PROBLEM TO BE SOLVED: To provide an electric-field light-emitting element which can increase light-emitting efficiency by the application of an existing material, emits light stably for a long time and achieves blue light-emission with high brightness and excellent chromaticity. SOLUTION: In a single-hetero-type organic EL element with a structure in which an ITO transparent electrode 5, a hole-transport layer 4, an electron- transport layer 2 and a metallic electrode 1 are laminated in order on a glass substrate 6, between the above hole-transport layer 4 and the electron-transport layer 2, a hole-block layer 33 containing vasophenantroline derivatives expressed by the following general formula 1, concretely for example, is formula 2, ethyl radical is shown as Et is arranged. In this way, the recombination of electron- hole in a hole-transportable light-emitting layer 4b can be promoted.

    OPTICAL ELEMENT AND BASE BODY FOR OPTICAL ELEMENT

    公开(公告)号:JP2000260559A

    公开(公告)日:2000-09-22

    申请号:JP5805099

    申请日:1999-03-05

    Applicant: SONY CORP

    Inventor: KIJIMA YASUNORI

    Abstract: PROBLEM TO BE SOLVED: To provide a long-life optical element capable of extracting the luminescence of an organic EL element transmitted by a substrate to the exterior with high efficiency and capable of obtaining high brightness by low-voltage driving, and provide a base body for the optical element. SOLUTION: A substrate 21 is prepared by cutting into thin pieces an assembly of optical fibers 15 made of quartz glass or a polymer, a whole cut surface thereof is covered with an organic material or an inorganic material, the surface roughness thereof is finished into 300 nm or less, and pixels PX are formed thereon. The luminescence of such an element comes into each fiber of the optical fiber group and then becomes easy to transmit while being confined therein through the total reflection, and can be efficiently extracted to the exterior as transmitted light.

    ELECTROLUMINESCENCE ELEMENT
    127.
    发明专利

    公开(公告)号:JPH11204259A

    公开(公告)日:1999-07-30

    申请号:JP298698

    申请日:1998-01-09

    Applicant: SONY CORP

    Inventor: KIJIMA YASUNORI

    Abstract: PROBLEM TO BE SOLVED: To provide an electroluminescence element increasing luminous efficiency, stably luminescing for a long period, and capable of emitting high- luminance, good-chromaticity blue by applying existing materials. SOLUTION: An indium tin oxide(ITO) transparent electrode 5, a hole transportation layer 4, an electron transportation layer 2 and a metal electrode 1 are laminated in this order on a glass substrate 6 to form a single hetero-type organic EL element, and a hole block layer 33 is provided between the hole transportation layer 4 and the electron transportation layer 2, thereby the recombination between electrons and holes on a hole transportation luminous layer 4b can be accelerated.

    MANUFACTURE OF OPTICAL ELEMENT
    128.
    发明专利

    公开(公告)号:JPH1187056A

    公开(公告)日:1999-03-30

    申请号:JP23954897

    申请日:1997-09-04

    Applicant: SONY CORP

    Abstract: PROBLEM TO BE SOLVED: To provide a method of manufacturing an optical element wherein an amorphous luminous layer can be formed surely with good controllability even in the case of using a luminous material or the like such as one which decomposes partly when it is vaporized. SOLUTION: A luminous layer has a stratified region containing a host luminous material and guest luminous material, the host luminous material has a vaporization temperature higher than that of the guest luminous material, and of electron/hole transportability at least the electron transportability is provided in an optical element, in a method of its manufacture by using a physical gas phase growth device 40 provided with a luminous material storage vessel (heating board) 30, so as to prevent mixing of the host luminous material with the guest luminous material, and so as to bring the host/guest luminous material into contact, after the host/guest luminous material is stored in the luminous material storage vessel 30, by heating it, the stratified region of the luminous layer is formed by the physical gas phase growth method.

    ORGANIC ELECTROLUMINESCENCE ELEMENT
    129.
    发明专利

    公开(公告)号:JPH09306670A

    公开(公告)日:1997-11-28

    申请号:JP11585896

    申请日:1996-05-10

    Applicant: SONY CORP

    Abstract: PROBLEM TO BE SOLVED: To provide an organic electroluminescent element with high stability with the passage of time by using a chemically stable material as an cathode material. SOLUTION: An about 100nm thick ITO anode 12 is formed on a 30mm×30mm transparent glass substrate 10. An about 50nm thick hole transporting layer 14 comprising TPD (N,N'-diphenyl-N,N'-di(3-methylphenyl)4,4'- diaminobiphenyl) and an about 50nm thick luminescent layer 16 comprising Alq3 (tris(8-quinolinol)aluminium) are stacked in order on the luminescent portion on the ITO anode 10. An about 20nm thick Sb cathode 18 using Sb as a cathode material is formed on the luminescent layer 16.

    BINUCLEAR METALLIC COMPLEX ITS PRODUCTION AND OPTICAL ELEMENT

    公开(公告)号:JPH09165390A

    公开(公告)日:1997-06-24

    申请号:JP34810095

    申请日:1995-12-15

    Applicant: SONY CORP

    Abstract: PROBLEM TO BE SOLVED: To obtain a new binuclear metallic complex useful as a material for an electroluminescent element excellent in brightness and chromaticity by reacting a ligand comprising phenylbenzoxazole or quinoline moiety having SH or OH group with a metallic salt. SOLUTION: This complex is a new binuclear metallic complex of formula: M2 (L -S)m (L -O)n X4-m-n [M is a group II A or group II B element in the periodic table; L and L and the moiety of formula I (R is an atom adjacent to an aromatic nitrogen atom and/or forms a cyclic structure in combination with a part of R ;R forms a cyclic structure in combination with an aromatic nitrogen atom and/or an atom adjacent to this) or formula II (R is the same kind as R ;R is the same kind as R ); X is an anion;(m) is 1-4; (n) is 0-3] or formula: M2 (L -S)m (L -S)n X4-m-n and useful as a material having an high fluorescent property and an excellent electron transportability for preparing a optical element such as an organic electroluminescent element or the like luminous in high brightness at various chromaticities.