Abstract:
The present disclosure relates to a multilayer film characterized by one or more skin layers comprising propylene/ethylene copolymers characterized by the following features: an ethylene derived units content of between 1.0 wt % and 15.0% wt %; and a molecular weight distribution (MWD), expressed in terms of Mw/Mn, of greater than 4.0;a content of xylene soluble fraction (XS) and an ethylene derived units content (C2) that fulfills the following relationship: XS
Abstract:
The present disclosure generally relates to a hot melt adhesive polyolefin composition comprising a high melt flow, butene-1 copolymer suitable to be used as a glue in the paper and packaging industry, in furniture manufacturing, e.g. for edgebands, square edges and softforming, for paneling in high moisture environments, and as a glue in tufted or needle punched carpets.
Abstract:
The present disclosure relates to a propylene ethylene 1-butene terpolymer wherein:(i) the content of ethylene derived units ranges from 1.1 wt % to 1.9 wt %, (ii) the content of 1-butene ranges from 5.0 wt % to 9.0 wt %, (iii) the melting point (Tm) of the non-nucleated terpolymer ranges from 125° C. to 137° C.; and (iv) the xylene soluble fraction at 25° C. is lower than 8.0 wt %.
Abstract:
A container comprising a propylene, ethylene, 1-hexene terpolymer wherein in the terpolymer: (i) the content of ethylene derived units ranges from 0.5 wt % to 2.0 wt %; (ii) the content of 1-hexene derived units ranges from 1.5 wt % to 5.5 wt %; (iii) the content of ethylene derived units fulfills the following equation (I); C2
Abstract:
The present technology relates to a pre-polymerized catalyst component for the polymerization of olefins, characterized by a non-stereospecific solid catalyst component comprising Ti, Mg and a halogen and an amount of a (co)polymer of an alpha-olefin CH2═CHR1, where R is a C1-C12 hydrocarbon group ranging from 0.1 to 500 g per g of said solid catalyst component. In some embodiments, the (co)polymer is characterized by an isotacticity, expressed in terms isotactic pentads, of higher than 60 molar % and an intrinsic viscosity, measured in tetraline at 135° C., of at least 1.0 dL/g.
Abstract:
A liquid phase process for the polymerization of butene-1 carried out in the presence of a catalyst comprising (a) a solid catalyst component comprising Mg, Ti and an electron donor compound of the following formula (I) in which the R groups, equal to or different from each other, are C1-C10 hydrocarbon groups; (b) an aluminium alkyl cocatalyst and (c) an external electron donor.
Abstract:
A polyolefin composition comprising: A) from 65 wt % to 85 wt %, of a propylene/ethylene/1-butene terpolymer wherein: i) the content of ethylene derived units ranges from 0.6 wt % to 2.5 wt; ii) the content of 1-butene derived units ranges from 6 wt % to 12 wt %; iii) the fraction soluble in xylene at 25° C. ranges from 3.5 wt % to 20 wt %; B) from 15 wt % to 35 wt % of a propylene/ethylene copolymer having a content of ethylene derived units ranging from 10 wt % to 40 wt %; the copolymer optionally can contains 1-butene derived units in an amount less than 1 wt %; the sum A)+B) being 100.
Abstract:
Process for the polymerization of butene-1 carried out in the presence of a catalyst comprising (a) a solid catalyst component comprising Mg, Ti and an electron donor compound of the following formula (I) In which the R groups equal to or different from each other, are C1-C15 hydrocarbon groups, the R1-R2 groups, equal to or different from each other, are hydrogen, halogen or C1-C15 hydrocarbon groups, optionally containing an heteroatom selected from halogen, P, S, N and Si, n and m are integer from 0 to 3 with the proviso that at least one of them is different from 0; (b) An aluminium alkyl cocatalyst and (c) an external electron donor
Abstract:
Polyolefin compositions suitable for injection molded items e.g. for impact bumpers and car interiors comprising from 30% to 90% by weight of an heterophasic propylene polymer composition (A); and from 10% to 70% by weight of a multimodal ethylene/butene-1 copolymer (B); having density from 0.850 to 0.935 g/cm3, total comonomer content from 6% to 30% by weight, Mw/Mn from 4 to 20; intrinsic viscosity in decalin at 135° C. from 1.0 to 4.0 dL/g, and comprising an HDPE fraction (HDPE % wt) up to 30% wt; further comprising from 0 to 50% by weight of a filler (C) and optionally, in amount up to 10% by weight with respect to the overall composition, an impact modifier masterbatch component D consisting of an ultra-soft heterophasic copolymer component.
Abstract:
A propylene polymer composition made from or containing a) from 20 wt % to 44 wt % of a propylene 1-hexene copolymer, containing from 5.0 wt % to 8.3 wt % of 1-hexene derived units, b) from 25 wt % to 45 wt % of a propylene 1-hexene ethylene terpolymer, and c) from 25 wt % to 50 wt % of a propylene ethylene copolymer, wherein the Melt Flow Rate of components a)+b)+c) is from 3.5 to 12.0 g/10 min.