公开(公告)号:KR1020020011520A
公开(公告)日:2002-02-09
申请号:KR1020000044836
申请日:2000-08-02
Applicant: 한국화학연구원
IPC: B01J19/00
CPC classification number: B01J19/0006 , B01J19/0046 , B01J2219/00695
Abstract: PURPOSE: A synthesis equipment of chemical composition for searching composition ratio of fluorescent substance and preparing powder thereof is provided, which can prepare fluorescent substance of homogeneous composition by preparing precursor for metal oxide of fluorescent substance from liquid and can prepare powder that has crystallinity even at low temperature and easily dispersed. CONSTITUTION: The reactor comprises a liquid storage system(10), a reaction system and a precursor recovery equipment(40). In the liquid storage system(10) many tanks(11) and rotating speed detecting motors(21) controlled by computer are installed to feed liquid to reaction equipment. The reaction equipment consists of a thermostatic bath(30) that is insulated by insulating material(32), in which a tubular reactor(31) is installed to receive liquid and conduct reaction. The reacted material is fed through a detector(41) of sediment in liquid and a micro-filter(42) to precursor recovery equipment(40), finally to a filtrate recovery device(43) that is kept at vacuum by a vacuum pump(44).
Abstract translation: 目的:提供一种用于搜索荧光物质组成比和制备粉末的化学组成的合成设备,其可以通过从液体制备荧光物质的金属氧化物的前体制备均匀组成的荧光物质,并且可以制备具有结晶度的粉末,即使在 低温易分散。 构成:反应器包括液体储存系统(10),反应系统和前体回收设备(40)。 在液体存储系统(10)中,安装了许多由计算机控制的罐(11)和转速检测电动机(21),以将液体供给反应设备。 反应设备包括由绝缘材料(32)绝缘的恒温槽(30),其中安装有管状反应器(31)以接收液体并进行反应。 将反应的材料通过液体中的沉淀物的检测器(41)和前体回收设备(40)的微滤器(42)进料到最终通过真空泵保持真空的滤液回收装置(43) 44)。
-
公开(公告)号:KR1020010109030A
公开(公告)日:2001-12-08
申请号:KR1020000030148
申请日:2000-06-01
Applicant: 한국화학연구원
IPC: C09K11/78
CPC classification number: C09K11/7728 , C04B35/50 , C04B35/64 , C09K11/7731 , Y02B20/181
Abstract: 본 발명은 가돌륨옥사이드계 적색 형광체 및 그 제조방법에 관한 것으로서, 더욱 상세하게는 형광체 모체로 사용하는 가돌륨옥사이드(Gd
2 O
3 )에 활성제로서 유로피움옥사이드(Eu
2 O
3 )를 첨가하고, 여기에 산화아연(ZnO), 탄산리튬(Li
2 CO
3 ), 탄산칼슘(CaCO
3 ), 산화마그네슘(MgO), 산화갈륨(Ga
2 O
3 ), 수산화알루미늄(Al(OH)
3 ) 중에서 선택된 부활제를 첨가함으로써, 저속전자선에서 발광휘도가 우수하고 고진공에서도 안정한 물성을 가지며 저전압 전자선 여기에 의해 구동하는 전계 방출 디스플레이(Field Emission Display, FED)에 적합한 다음 화학식 1로 표시되는 새로운 가돌륨옥사이드계 적색 형광체 및 그 제조방법에 관한 것이다.
Gd
2-Xy O
3 : Eu
X ,M
y
상기 화학식 1에서: 0.005≤X≤0.5 이고, 0≤y≤1.0 이며, M은 Zn, Li, Ca, Mg, Ga 및 Al 중에서 선택된 원소이다.-
公开(公告)号:KR1020000075149A
公开(公告)日:2000-12-15
申请号:KR1019990019588
申请日:1999-05-29
Applicant: 한국화학연구원
IPC: C09K11/54
CPC classification number: C09K11/623 , C09K11/595 , C09K11/646 , C09K11/676
Abstract: PURPOSE: A zinc silicate based green fluorescent material having excellent luminous efficiency in vacuum ultraviolet and stable physical properties under high vacuum and method of preparing the same by doping zinc silicate with manganese oxide and, if necessary, with a co-activator selected from aluminum oxide, gallium oxide and titanium oxide are provided which are suitable for plasma display panels (PDP) due to the short afterglow time. CONSTITUTION: The zinc silicate based green fluorescent material of formula; Zn2-aSi1-bO4 : aMn, bM, wherein a and b are 0 ≤ a ≤ 0.15, 0 ≤ b ≤ 0.02, respectively, and M is an element selected from Al, Ga and Ti is prepared by mixing silicate prepared using zinc oxide and silica as phosphor raw material with manganese oxide and a co-activator selected for aluminum oxide, gallium oxide and titanium oxide, calcining at 1,100 to 1,350°C, heating at 900 to 1,200°C under reducing atmosphere and grinding.
Abstract translation: 目的:一种基于硅酸锌的绿色荧光材料,其在真空紫外线中具有优异的发光效率并且在高真空下具有稳定的物理性能,并且通过用氧化锰掺杂硅酸锌和如果需要,使用选自氧化铝的共活化剂 提供了由于余辉时间短而适用于等离子体显示面板(PDP)的氧化镓和氧化钛。 构成:式中的硅酸锌基绿色荧光物质; Zn2-aSi1-bO4:aMn,bM,其中a和b分别为0≤a≤0.15,0≤b≤0.02,并且M是选自Al,Ga和Ti的元素,通过混合使用氧化锌制备的硅酸盐 二氧化硅作为氧化锰的荧光体原料和用于氧化铝,氧化镓和氧化钛的共活化剂,在1100〜1350℃下煅烧,在还原气氛下在900〜1200℃下加热研磨。
-
公开(公告)号:KR1020000074761A
公开(公告)日:2000-12-15
申请号:KR1019990018916
申请日:1999-05-25
Applicant: 한국화학연구원
IPC: C09K11/54
CPC classification number: C09K11/595 , C09K11/646
Abstract: PURPOSE: A process for preparing a Zn2SiO4:Mn green light-emitting fluorescent substance having narrow particle size distribution, almost truly spherical form and low coagulating property and excellent in fluorescent intensity is provided which produces the fluorescent substance being widely applicable to the display industry including an electronic display such as cathode-ray tubes and field emission displays. CONSTITUTION: In the preparation of an orthosilicic acid zinc-based green light emitting fluorescent substance, a basic catalyst and water are added to 0.05 to 2 mol/L ethanol diluted solution of tetraethyl orthosilicic acid and filtered. The filtrate is dispersed in a Zinc component- and Mn component-containing solution and added with oxalic acid or oxalate to give precipitated mixtures, which are dried and heat treated under reducing atmosphere to give the fluorescent substance powder.
Abstract translation: 目的:制备粒径分布窄,几乎真实球形,凝固性低,荧光强度优异的Zn2SiO4:Mn绿色发光荧光体的制造方法,其荧光物质广泛适用于显示工业,包括 诸如阴极射线管和场发射显示器的电子显示器。 构成:在正硅酸锌系绿色发光荧光物质的制备中,向0.05〜2mol / L四乙基正硅酸乙醇稀释溶液中加入碱性催化剂和水,并过滤。 将滤液分散在含锌组分和Mn组分的溶液中并加入草酸或草酸盐,得到沉淀的混合物,将其在还原气氛下进行干燥和热处理,得到荧光物质粉末。
-
公开(公告)号:KR100270409B1
公开(公告)日:2000-11-01
申请号:KR1019980043244
申请日:1998-10-15
Applicant: 한국화학연구원
Abstract: 본 발명은 티탄산란타늄계 적색 형광체 및 그 제조방법에 관한 것으로서, 더욱 상세하게는 형광체 모체인 티탄산란타늄계 화합물(La
2 Ti
x O
y )에 공부활제로 수산화알루미늄과 염화프라세오디움을 첨가함으로써 발광특성에서 발광휘도와 색순도가 우수하고 고진공에서도 안정한 물성을 가지며 저전압 전자선 여기에 의해 구동하는 전계 방출 디스플레이(Field Emission Display, FED)에 적합하도록 고휘도를 갖는 다음 화학식 1로 표시되는 티탄산란타늄계 적색 형광체 및 그 제조방법에 관한 것이다.
La
2 Ti
x O
y :aPr,bAl
상기 화학식 1에서 2≤x≤3, 7≤y≤9, 0.0005≤a≤0.004 이고, 0<b≤0.3 이다.-
公开(公告)号:KR1020000018337A
公开(公告)日:2000-04-06
申请号:KR1019980035889
申请日:1998-09-01
Applicant: 한국화학연구원
CPC classification number: C09K11/623 , C01P2002/70 , C01P2004/03 , C04B35/64 , C04B2235/3286 , C09K11/574
Abstract: PURPOSE: A process for preparing a green luminescent, phosphorescent composition using a wet precipitation method is provided which produces the title phosphor excellent in luminescent strength. CONSTITUTION: The process of producing green luminescent phosphor of ZnGa2O4: Mn comprises the steps of adding a base to gallium-containing solution to precipitate hydroxide; by heat treating the solution to convert to a GaO(OH) sediment; dispersing the sediment in a manganese component-containing zinc compound solution; adding oxalic acid and a base thereto to give a mixed sediment; filtering, drying, and calcining. The process has the advantages of producing the phosphor at a low temperature and preventing environment pollution.
Abstract translation: 目的:提供一种使用湿沉淀法制备绿色发光性磷光组合物的方法,其产生发光强度优异的标题荧光体。 构成:生产ZnGa2O4:Mn的绿色荧光体的方法包括以下步骤:向含镓溶液中加入碱以沉淀氢氧化物; 通过热处理溶液转化为GaO(OH)沉淀物; 将沉淀物分散在含锰组分的锌化合物溶液中; 加入草酸和碱,得到混合沉淀物; 过滤,干燥和煅烧。 该方法具有在低温下生产荧光体并防止环境污染的优点。
-
公开(公告)号:KR1020000008650A
公开(公告)日:2000-02-07
申请号:KR1019980028566
申请日:1998-07-15
Applicant: 한국화학연구원
IPC: C09K11/77
CPC classification number: C09K11/7728 , C04B35/505 , C04B35/64 , C04B2235/3225 , Y02B20/181
Abstract: PURPOSE: A fluorescent substance made of yttrium oxide derivatives is provided which shows good luminance purity in a slow electron tube and stable physical property in high vacuum and can reduce the pollution since it doesn't use Cd or S. CONSTITUTION: A fluorescent substance made of yttrium oxide derivatives, (Y1-xEux)2O3, is obtained by the following steps of: dissolving yttrium nitrate(Y(NO3)3*4.7H2O) and europium nitrate(Eu(NO3)3*2.5H2O) in a solvent which comprises citric acid and ethylene glycol in the ratio of from 2:3 to 1:5, followed by esterification at the temperature of 100-150°C; heating at 350°C; sintering and pulverizing at 500-1300°C. In formula, x is between 0.02 and 0.5.
Abstract translation: 目的:提供由氧化钇衍生物制成的荧光物质,其在慢电子管中显示出良好的亮度纯度,并且在高真空中具有稳定的物理性质,并且可以减少污染,因为它不使用Cd或S.构成:制成荧光物质 通过以下步骤获得氧化钇衍生物(Y1-xEux)2O3:将硝酸钇(Y(NO 3)3·4.7H 2 O)和硝酸铕(Eu(NO 3)3·2.5H 2 O)溶解在溶剂中 包括柠檬酸和乙二醇,其比例为2:3至1:5,然后在100-150℃的温度下酯化; 在350℃加热; 在500-1300℃下烧结和粉碎。 在式中,x在0.02和0.5之间。
-
公开(公告)号:KR1019990085329A
公开(公告)日:1999-12-06
申请号:KR1019980017682
申请日:1998-05-15
Applicant: 한국화학연구원
IPC: C09K11/55
Abstract: 본 발명은 티탄산스트론튬계 적색 형광체 및 그 제조방법에 관한 것으로서, 더욱 상세하게는 형광체 모체인 티탄산스트론튬(SrTiO
3 )에 공부활제로 산화갈륨과 염화프라세오디움을 첨가함으로써 저속전자선에서 발광휘도와 색순도가 우수하고 고진공에서도 안정한 물성을 가지며 저전압 전자선 여기에 의해 구동하는 전계 방출 디스플레이(Field Emission Display, FED)에 적합하도록 고휘도를 갖는 다음 화학식 1로 표시되는 티탄산스트론튬계 적색 형광체 및 그 제조방법에 관한 것이다.
SrTiO
3 :
a Pr,
b Ga
상기 화학식 1에서 0.0005≤a≤0.01 이고, 0<b≤1.0 이다.-
公开(公告)号:KR1019990076138A
公开(公告)日:1999-10-15
申请号:KR1019980010832
申请日:1998-03-27
Applicant: 한국화학연구원
IPC: C09K11/74
Abstract: 본 발명은 니오브산이트륨(YNbO
4 )계 청색 형광체 및 그의 제조방법에 관한 것으로서, 더욱 상세하게는 형광체 모체인 니오브산이트륨에 부활제로 산화비스무스가 도핑됨으로써 저속전자관에서 발광 효율이 뛰어나며 고진공에서도 안정한 물성을 가지며 새로운 전계방출 디스플레이(field emission display, FED)에 적합한 다음 화학식 1로 표시되는 저전압용 니오브산이트륨(YNbO
4 )계 청색 형광체 및 그의 제조방법에 관한 것이다.
Y
2-ab Nb
a O
4 :
b Bi
상기 화학식 1에서 0.80≤a≤1.10 이고, 0.001≤b≤0.05 이다.-
公开(公告)号:KR1019990074383A
公开(公告)日:1999-10-05
申请号:KR1019980007929
申请日:1998-03-10
Applicant: 한국화학연구원
IPC: C04B35/80
Abstract: 본 발명은 펄스-온도구배법을 이용한 섬유강화 복합재료 제조장치에 관한 것으로, 복합 재료를 형성하기 위한 프리폼을 반응기에 집어넣고 펄스와 열구배를 동시에 제공하여 반응가스가 프리폼 내부로 단시간에 함침가능하게 함으로써, 균일한 밀도를 가지면서 치밀화가 이루어지게 되어, 고밀도의 섬유강화 복합재료를 얻을 수 있는 펄스-온도구배법을 이용한 섬유강화 복합재료 제조장치를 제공하는데 있다.