Abstract:
본 발명에 따른 휘발성 유기화합물의 발생을 최소화한 그라프트 공중합체의 제조방법은 고무질 중합체 라텍스와 그라프트 단량체 혼합물을 중합개시제 존재하에 중합하여 제1 그라프트 공중합체 라텍스를 제조하는 제1단계; 및 상기 제1 그라프트 공중합체 라텍스에 잔량의 그라프트 단량체 혼합물 투입과 동시에 제1차 중합개시제를 2 내지 5 시간에 걸쳐 연속적으로 투입한 후, 제2차 중합개시제를 투입하여 중합하는 제2단계로 이루어진다. 휘발성 유기화합물, 그라프트 공중합체, 중합개시제, g-ABS, 유화중합
Abstract:
A methacrylate-styrene-perfluoroacrylate terpolymer is provided to improve surface contamination while maintaining transparency and to solve problems on degradation of transparency and coating defective, low reusability and use of an organic agent for coating. A methacrylate-styrene-perfluoroacrylate terpolymer comprises methacrylate component 60-97 weight%, and styrene compound component and perfluorinated acrylate component 3-40 weight%. The styrene compound component and perfluorinated acrylate component has a weight ratio of 55/45 - 60/40. A method for the methacrylate-styrene-perfluoroacrylate terpolymer comprises the steps of: injecting an initiator and a molecular weight modifier in a monomer mixture of methacrylate monomer, styrene monomer and perfluorinated acrylate; and perfluorinated acrylate the monomer mixture in aqueous dispersion and polymerizing them at 70-120 °C for 2-8 hours.
Abstract:
An impact modifier is provided to improve impact strength, rubbing characteristic, and scratch resistance without deteriorating transparency. An impact modifier is prepared by graft-polymerizing 30-55 parts by weight of methacrylate-based monomer on 45-70 parts by weight of rubbery polymer having a particle size of 150-250 nm. The rubber polymer is obtained by polymerizing 0.1-1 parts by weight of an antioxidant and 100 parts by weight of a monomer mixture comprising 30-45wt% of diene-based monomer and 55-70wt% of alkyl acrylate.
Abstract:
본 발명에 따른 광택도 조절이 용이한 아크릴로니트릴-부타디엔-스티렌(ABS) 수지의 제조방법은 응집 고무 라텍스에 아크릴로니트릴과 스티렌으로 이루어진 모노머 혼합물을 중합하여 아크릴로니트릴-부타디엔-스티렌(ABS) 수지를 제조하는 데에 있어서, 상기 응집 고무 라텍스로서 1000 내지 2500 Å의 종자 고무 라텍스에 입자경 비대화제를 투입하여 화학적 응집을 행하는 단계와 기어펌프(Gear pump)에 의한 기계적 교반력을 이용한 기계적 응집을 행하는 단계를 병행하여 응집 제조된 응집 고무 라텍스를 사용함으로써, 용이하게 아크릴로니트릴-부타디엔-스티렌(ABS) 수지의 광택도를 조절할 수 있을 뿐만 아니라, 우수한 내충격성과 유동성을 그대로 유지한 아크릴로니트릴-부타디엔-스티렌(ABS) 수지를 제조할 수 있다. 입자경 비대화제, 응집 고무 라텍스, 화학적 응집, 기계적 응집, 광택도, 내충격성, 유동성
Abstract:
A methacrylate copolymer is provided to shorten a melting time in a resin processing while not affecting specific physical properties of a vinyl chloride resin, and to reduce generation of ungelled materials and flown mark. A method for manufacturing a methacrylate copolymer for processing aids of vinylchloride resin comprises the steps of: polymerizing a monomer mixture in the presence of a water-soluble initiator and an emulsifier to prepare polymer latex, wherein the monomer mixture comprises methyl methacrylate 60-85 weight%, alkyl acrylate-based compound 15-30 weight% and epoxide-based compound 1-10 weight%; and solidifying the polymer latex.
Abstract:
An emulsion polymerization method of acrylic resins is provided to produce the acrylic resins in an absence of an emulsifier by using comonomer having a self-emulsifying activity. An emulsion polymerization method of acrylic resins without using an emulsifier includes a step of emulsion-polymerizing alkyl (meth)acrylate in an absence of an emulsifier using an unsaturated acid-containing monomer as comonomer. The unsaturated acid-containing monomer is a carboxyl group-containing monomer. The carboxyl group-containing monomer is at least one selected from the group comprising acrylic acid, methacrylic acid, methyl acrylic acid, itaconic acid, crotonic acid, fumaric acid, and maleic acid.
Abstract:
본 발명의 나노복합체는 (A) 고무 변성 그라프트 공중합체 100 중량부; 및 (B) 콜로이달 금속(산화물) 나노입자 0.1∼50 중량부로 이루어진다. 상기 나노 복합체를 포함한 열가소성 나노복합재 수지 조성물은 선형 공중합체의 가공성을 그대로 유지하면서 충격강도, 인장강도, 모듈러스 등의 기계적 물성이 향상된 효과를 얻을 수 있다. 나노복합체, 고무 변성 그라프트 공중합체, 콜로이달 금속 나노입자, 열가소성 나노복합재
Abstract:
Provided is an acrylic impact reinforcing agent, which has an improved impact reinforcing effect and excellent powder characteristics while maintaining excellent weather resistance, and is useful for a vinyl chloride-based resin composition. The acrylic impact reinforcing agent has a core-shell structure comprising: 60-95 parts by weight of an acrylic rubber-based core containing an alkyl acrylate and an unsaturated carboxy ester compound; and 5-40 parts by weight of a shell containing an alkyl methacrylate and graft polymerized to the rubber-based core. The alkyl acrylate includes a C1-C8 alkyl acrylate, such as methyl acrylate, ethyl acrylate, propyl acrylate, butyl acrylate, hexyl acrylate or 2-ethylhexy acrylate.
Abstract:
본 발명에 따른 투명 연질 아크릴계 수지는 메타크릴레이트계 모노머, 알킬 아크릴레이트계 모노머 및 스티렌계 모노머를 포함하는 단량체 혼합물을 중합하여 굴절률이 1.49 ± 0.005 이고, 유리전이온도가 10 내지 20℃인 제1 중합체를 제조하는 제1단계, 상기 제1 중합체에 유리전이온도가 0 내지 10℃가 되는 조성으로 상기 단량체 혼합물을 적가 투입하여 그라프트 성장 반응시켜 제2 중합체를 제조하는 제2단계 및 상기 제2 중합체에 유리전이온도가 60 내지 90℃가 되는 조성으로 상기 단량체 혼합물을 투입, 중합하여 제3 중합체를 제조하는 제3단계에 의하여 제조되는 것을 특징으로 한다. 아크릴계 수지, 중합, PMMA, 유리전이온도, 연질