무기계 그라우팅 재료의 제조방법과 무기계 그라우팅 재료를 이용한 콘크리트 균열 보수방법
    12.
    发明公开
    무기계 그라우팅 재료의 제조방법과 무기계 그라우팅 재료를 이용한 콘크리트 균열 보수방법 有权
    无机组合材料及其制造方法,以及重复混凝土裂缝的方法

    公开(公告)号:KR1020130134058A

    公开(公告)日:2013-12-10

    申请号:KR1020120057305

    申请日:2012-05-30

    CPC classification number: C04B14/28 C04B2103/0001 E04G23/02

    Abstract: The present invention relates to an inorganic grouting material with enhanced densification and watertightness of an existing inorganic grouting material by mixing inorganic grouting materials and microorganisms which are able to form fine calcium carbonate powder and making the microorganisms form calcium carbonate particles among microcracks and micropores in the inorganic grouting material; a method for manufacturing the same, and a method for repairing concrete cracks using the material. The method for manufacturing the inorganic grouting material and a method for repairing the concrete cracks using the same according to the present invention comprise: a step of adding urea to water and preparing a culture medium (S1); a step of adding microorganisms into the culture medium, which forms calcium carbonate, culturing the microorganisms until the concentration of the microorganisms in the culture medium is optimized, and generating a proper culture medium (S2); a step of adding inorganic particles such as cement or geopolymers to the proper culture medium (S3); a injecting the microorganism-mixed inorganic grouting material into the concrete cracks and curing the grouting material (S4); and a step of making the surface of the cured grouting material come in contact with a solution containing urea as a carbonate ion source and a calcium source and incubating for a predetermined time and promoting fine calcium carbonate powder of the microorganisms (S5). [Reference numerals] (AA) Start;(BB) Prepare an inorganic grouting material;(CC) Concentration of microorganisms = set concentration ?;(DD) Repair concrete cracks;(EE) End;(S1) Prepare a culture medium;(S2) Add and culture the microorganisms;(S3) Add inorganic particles into a proper culture medium;(S4) Inject/cure the grouting material to concrete cracks;(S5) Apply urea and a calcium source on the surface of the grouting material

    Abstract translation: 本发明涉及通过混合无机灌浆材料和能够形成细小碳酸钙粉末的微生物,使现有的无机灌浆材料具有增强的致密化和水密性的无机灌浆材料,并使微生物在微裂纹和微孔中形成碳酸钙颗粒 无机灌浆材料; 其制造方法,以及使用该材料修复混凝土裂缝的方法。 根据本发明的无机灌浆材料的制造方法和修补混凝土裂缝的方法包括:向水中加入尿素并制备培养基的步骤(S1); 将微生物添加到形成碳酸钙的培养基中,培养微生物直到培养基中微生物的浓度最优化并产生适当的培养基(S2)的步骤; 向合适的培养基中加入水泥或地质聚合物等无机粒子的步骤(S3); 将微生物混合无机灌浆材料注入混凝土中,使灌浆材料发生破裂并固化(S4); 以及使固化的灌浆材料的表面与含有作为碳酸根离子源和钙源的尿素的溶液接触并保温预定时间并促进微生物的微细碳酸钙粉末的步骤(S5)。 (参考号)(AA)开始;(BB)准备无机​​灌浆材料;(CC)微生物浓度=设定浓度;;(DD)修复混凝土裂缝;(EE)结束;(S1)准备培养基; S2)添加培养微生物;(S3)将无机颗粒加入合适的培养基中;(S4)将灌浆材料注入/固化为混凝土裂缝;(S5)在灌浆材料表面涂上尿素和钙源

    크기 조절이 가능한 단분산성 나노입자 어레이 제조방법, 이에 의하여 제조된 나노입자 어레이와 그 응용
    13.
    发明公开
    크기 조절이 가능한 단분산성 나노입자 어레이 제조방법, 이에 의하여 제조된 나노입자 어레이와 그 응용 无效
    用于制造具有可调大小的单分散性纳米粒子阵列的方法,由其制造的纳米粒子阵列及其应用

    公开(公告)号:KR1020120123183A

    公开(公告)日:2012-11-08

    申请号:KR1020120005865

    申请日:2012-01-18

    CPC classification number: B82B3/0038 B82Y40/00 C08J3/24 C08J7/04 C23C26/00

    Abstract: PURPOSE: A manufacturing method of mono-dispersible nano particle array, a nano-particle array manufactured by the same and applications thereof are provided to evaporating the mono-dispersible nano-particle array by using a block copolymer lithography mode. CONSTITUTION: A manufacturing method of mono-dispersible nano particle array comprises the following step: combining metal ion to a polymer by contacting the polymer to the metal ion. The polymer is a block copolymer of two or more polymers. One or more block copolymers has electric charge opposite to the metal self-assembling the block copolymer; dipping the block copolymer in the metal ion solution; combining the polymer with the metal ion in the metal ion solution; and removing the block copolymer.

    Abstract translation: 目的:提供单分散纳米颗粒阵列的制造方法,由其制造的纳米粒子阵列及其应用,以通过使用嵌段共聚物光刻模式来蒸发单分散性纳米粒子阵列。 构成:单分散纳米颗粒阵列的制造方法包括以下步骤:通过使聚合物与金属离子接触来将金属离子与聚合物组合。 聚合物是两种或更多种聚合物的嵌段共聚物。 一种或多种嵌段共聚物具有与金属自组装嵌段共聚物相反的电荷; 将嵌段共聚物浸入金属离子溶液中; 将聚合物与金属离子溶液中的金属离子结合; 并除去嵌段共聚物。

    무기계 그라우팅 재료의 제조방법과 무기계 그라우팅 재료를 이용한 콘크리트 균열 보수방법
    15.
    发明授权
    무기계 그라우팅 재료의 제조방법과 무기계 그라우팅 재료를 이용한 콘크리트 균열 보수방법 有权
    无机灌浆材料及其制造方法,以及混凝土裂缝解决方法

    公开(公告)号:KR101343086B1

    公开(公告)日:2014-01-16

    申请号:KR1020120057305

    申请日:2012-05-30

    Abstract: 본 발명은 탄산칼슘 미분말을 형성할 수 있는 미생물을 무기계 그라우팅 재료에 혼입하여 무기계 그라우팅 재료 내에 있는 미세균열과 미세공극 사이에서 미생물이 탄산칼슘 입자를 형성하도록 하고, 이로써 기존 무기계 그라우팅 재료의 치밀성 및 수밀성을 증가시킬 수 있는 무기계 그라우팅 재료 및 그 제조방법과 이 재료를 이용한 콘크리트 균열 보수방법에 관한 것으로, 본 발명에 따른 무기계 그라우팅 재료의 제조방법 및 이를 이용한 콘크리트 균열 보수방법은 물에 요소를 첨가하여 배양액을 준비하는 단계(S1)와; 상기 배양액에 탄산칼슘을 형성하는 기능을 갖는 미생물을 투입하고, 배양액 내의 미생물의 농도가 적정화 될 때까지 배양하여 적정 배양액을 생성하는 단계(S2)와; 상기 적정 배양액에 시멘트 또는 지오폴리머 등의 무기계 입자를 첨가하는 단계(S3)와; 상기 미생물 혼입 무기계 그라우팅 재료를 콘크리트 균열에 주입하여 그라우팅 재료를 경화시키는 단계(S4)와; 상기 경화된 그라우팅 재료 표면에 탄산 이온의 공급원인 요소와 칼슘원을 동시에 첨가한 수용액을 접촉시킨 후 설정 시간 동안 방치하여 미생물의 탄산칼슘 미분말 형성 작용을 촉진하는 단계(S5)로 이루어진다.