lC TRAY용 대전방지 코팅 조성물
    14.
    发明公开
    lC TRAY용 대전방지 코팅 조성물 有权
    涂料组合物,用于防止IC托盘的静电

    公开(公告)号:KR1020130099439A

    公开(公告)日:2013-09-06

    申请号:KR1020120020947

    申请日:2012-02-29

    CPC classification number: C09D155/02 C09D5/24 C09D109/06 C09D125/10

    Abstract: PURPOSE: An antistatic coating composition for an IC tray is provided to manufacture a product in various colors and to solve dust and contaminant problems as the antistatic coating composition is capable of realizing permanent antistatic property and does not use particles, such as carbon black. CONSTITUTION: An antistatic coating composition for an IC tray comprises 100.0 parts by weight of a copolymer resin, 10 to 30 parts by weight of polyether block amides, 0.1 to 1 part by weigh to a UV stabilizer, 0.1 to 1 part by weight of antioxidant, and 0.1 to 0.5 part by weight of a dispersing agent. The copolymer resin is formed 60 to 90 parts by weight of an acrylonitrile-butadiene-styrene copolymer (ABS) resin; and 10 to 60 parts by weight of a styrene-ethylene-butylene-styrene (SEBS) resin or a styrene-butylene-styrene (SBS) resin.

    Abstract translation: 目的:提供用于IC托盘的抗静电涂料组合物,以制造各种颜色的产品并解决灰尘和污染问题,因为抗静电涂料组合物能够实现永久抗静电性能,并且不使用诸如炭黑的颗粒。 构成:用于IC托盘的抗静电涂料组合物包含100.0重量份的共聚物树脂,10-30重量份的聚醚嵌段酰胺,0.1-1重量份的UV稳定剂,0.1-1重量份的抗氧化剂 ,和0.1〜0.5重量份的分散剂。 共聚物树脂形成60至90重量份的丙烯腈 - 丁二烯 - 苯乙烯共聚物(ABS)树脂; 和10至60重量份的苯乙烯 - 乙烯 - 丁烯 - 苯乙烯(SEBS)树脂或苯乙烯 - 丁烯 - 苯乙烯(SBS)树脂。

    이차전지용 음극 활물질 및 이의 제조방법
    16.
    发明公开
    이차전지용 음극 활물질 및 이의 제조방법 有权
    负极活性物质二次电池及其制造方法

    公开(公告)号:KR1020170055750A

    公开(公告)日:2017-05-22

    申请号:KR1020150158908

    申请日:2015-11-12

    Abstract: 본발명은, 이차전지용음극활물질및 이의제조방법에관한것으로, 보다구체적으로, 나노실리콘; 탄소전구체; 및계면활성제를혼합하여혼합조성물을제조하는혼합조성물의제조단계; 및상기혼합조성물을열처리하여실리콘-탄소복합재료를형성하는실리콘-탄소복합재료의형성단계; 를포함하고, 상기계면활성제는, 상기탄소전구체 100 중량부에대해 1 내지 200 중량부로포함되고, 상기나노실리콘은, 상기탄소전구체 100 중량부에대해 5 내지 100 중량부로포함되는, 이차전지용음극활물질의제조방법및 이차전지용음극활물질에관한것이다. 본발명은, 나노실리콘과탄소전구체의표면을안정화시켜균일한혼합을유도하여, 전지성능및 수명저하를방지할수 있는이차전지용음극활물질을제공할수 있다.

    Abstract translation: 二次电池用负极活性物质及其制造方法技术领域本发明涉及二次电池用负极活性物质及其制造方法,更具体而言,涉及二次电池用负极活性物质, 碳前体; 和表面活性剂以制备混合组合物; 并且通过对混合组合物进行热处理来形成硅 - 碳复合材料; 其中基于100重量份的碳前体,表面活性剂的含量为1至200重量份,并且相对于100重量份的碳前体,纳米硅的含量为5至100重量份, 和二次电池用负极活性物质。 本发明可以提供用于二次电池的负极活性材料,其稳定纳米硅和碳前体的表面以引起均匀混合,从而防止电池性能和寿命。