公开(公告)号:KR1020130021527A
公开(公告)日:2013-03-06
申请号:KR1020110083820
申请日:2011-08-23
Applicant: 한국산업기술대학교산학협력단 , (주)폴리원테크놀로지
Abstract: PURPOSE: A resin composition is provided to have moderate surface resistance and excellent physical and mechanical properties without generating carbon dusts. CONSTITUTION: A resin composition comprises a modified polyphenylene oxide, high impact polystyrene, and general purpose polystyrene; a glass fiber; and a silicone-based coupling agent. The composition ratio of the polyphenylene oxide, high impact polystyrene, and general purpose polystyrene in the base resin is 70-90 weight%:5-20weight%:5-20 weight% in order. The included amount of the glass fiber is 5-30 parts by weight based on 100.0 parts by weight of the resin base.
Abstract translation: 目的:提供树脂组合物以具有中等的表面电阻和优异的物理和机械性能而不产生碳粉尘。 构成:树脂组合物包含改性聚苯醚,高抗冲聚苯乙烯和通用聚苯乙烯; 玻璃纤维; 和硅氧烷基偶联剂。 基础树脂中聚苯醚,高抗冲聚苯乙烯和通用聚苯乙烯的组成比为70-90重量%:5-20重量%:5-20重量%。 玻璃纤维的含量相对于树脂基质的100.0重量份为5-30重量份。
-
公开(公告)号:KR101367648B1
公开(公告)日:2014-02-28
申请号:KR1020110083820
申请日:2011-08-23
Applicant: 한국산업기술대학교산학협력단 , (주)폴리원테크놀로지
Abstract: 본 발명은 변성 폴리페닐렌 옥사이드(modified polyphenylene oxide), 하이 임팩트 폴리스티렌(high impact polystyrene) 및 범용 폴리스티렌(general purpose polystyrene)을 포함하는 수지 베이스; 유리섬유(glass fiber); 및 실리콘계 커플링제를 포함하는 수지 조성물에 관한 것이다.
본 발명을 통하여 우수한 내열성, 기계적 특성 및 물리적 특성을 유지하면서, 적합하면서도 일정한 표면 저항을 갖는 수지 조성물을 얻을 수 있다.-
公开(公告)号:KR101312985B1
公开(公告)日:2013-10-01
申请号:KR1020110053426
申请日:2011-06-02
Applicant: 한국산업기술대학교산학협력단 , (주)폴리원테크놀로지
IPC: C08L23/04 , C08L31/04 , C08K3/04 , C08L101/12
Abstract: 본 발명은 대전방지용 반도전성 수지 조성물 및 그 제조방법에 관한 것으로, 더욱 상세하게는, 폴리에틸렌, 에틸렌 비닐 아세테이트 및 카본 블랙을 적절히 포함하는 대전방지용 반도전성 수지 조성물 및 그 제조방법에 관한 것이다. 본 발명을 통해 개선된 표명 저항을 지니면서도 인장강도와 신장률의 물리적 특성이 우수하고 압출가공성이 뛰어난 대전방지용 반도전성 수지 조성물 및 그의 제조방법을 제공한다.
-
公开(公告)号:KR1020130099439A
公开(公告)日:2013-09-06
申请号:KR1020120020947
申请日:2012-02-29
Applicant: 한국산업기술대학교산학협력단 , (주)폴리원테크놀로지
IPC: C09D109/06 , C09D5/00 , C09D5/24 , C09D133/24
CPC classification number: C09D155/02 , C09D5/24 , C09D109/06 , C09D125/10
Abstract: PURPOSE: An antistatic coating composition for an IC tray is provided to manufacture a product in various colors and to solve dust and contaminant problems as the antistatic coating composition is capable of realizing permanent antistatic property and does not use particles, such as carbon black. CONSTITUTION: An antistatic coating composition for an IC tray comprises 100.0 parts by weight of a copolymer resin, 10 to 30 parts by weight of polyether block amides, 0.1 to 1 part by weigh to a UV stabilizer, 0.1 to 1 part by weight of antioxidant, and 0.1 to 0.5 part by weight of a dispersing agent. The copolymer resin is formed 60 to 90 parts by weight of an acrylonitrile-butadiene-styrene copolymer (ABS) resin; and 10 to 60 parts by weight of a styrene-ethylene-butylene-styrene (SEBS) resin or a styrene-butylene-styrene (SBS) resin.
Abstract translation: 目的:提供用于IC托盘的抗静电涂料组合物,以制造各种颜色的产品并解决灰尘和污染问题,因为抗静电涂料组合物能够实现永久抗静电性能,并且不使用诸如炭黑的颗粒。 构成:用于IC托盘的抗静电涂料组合物包含100.0重量份的共聚物树脂,10-30重量份的聚醚嵌段酰胺,0.1-1重量份的UV稳定剂,0.1-1重量份的抗氧化剂 ,和0.1〜0.5重量份的分散剂。 共聚物树脂形成60至90重量份的丙烯腈 - 丁二烯 - 苯乙烯共聚物(ABS)树脂; 和10至60重量份的苯乙烯 - 乙烯 - 丁烯 - 苯乙烯(SEBS)树脂或苯乙烯 - 丁烯 - 苯乙烯(SBS)树脂。
-
公开(公告)号:KR101473523B1
公开(公告)日:2014-12-17
申请号:KR1020120020947
申请日:2012-02-29
Applicant: 한국산업기술대학교산학협력단 , (주)폴리원테크놀로지
IPC: C09D109/06 , C09D5/00 , C09D5/24 , C09D133/24
Abstract: 본발명은아크릴로니트릴-부타디엔-스티렌공중합체(Acrylonitrile-butadiene-styrene copolymer, ABS) 수지 60 내지 90중량부; 및스티렌-에틸렌-부틸렌-스틸렌(Styrene-Ethylene-Butylene-Styrene, SEBS) 또는스티렌-부틸렌-스티렌(Styrene-Butylene-Styrene, SBS) 수지 10 내지 60중량부의비율로이루어진공중합체수지혼합물 100중량부; 폴리에테르블록아미드(Polyether block amides) 10 ~ 30중량부; UV 안정제 0.1 ~ 1중량부; 산화방지제는 0.1 ~ 1중량부; 분산제 0.1 ~ 0.5중량부를포함하는 IC TRAY용대전방지코팅조성물에관한것이다. 본발명에의하면, 영구대전방지특성을구현하면서카본블랙등의입자를사용을하지않아, 다양한색상의제품이가능하고분진및 오염물질의문제도해결할수 있을뿐만아니라, 코팅된파이프의표면저항이 10~10&OHgr;의범위가되며, 파이프의인장강도및 내충격성을향상시킬수 있는 IC TRAY용대전방지코팅조성물을제공할수 있다.
-
公开(公告)号:KR1020120134500A
公开(公告)日:2012-12-12
申请号:KR1020110053426
申请日:2011-06-02
Applicant: 한국산업기술대학교산학협력단 , (주)폴리원테크놀로지
IPC: C08L23/04 , C08L31/04 , C08K3/04 , C08L101/12
Abstract: PURPOSE: An antistatic semiconductive resin composition is provided to have superior extrusion processability and excellent physical properties such as a tensile strength while having a surface resistance within a moderate range. CONSTITUTION: An antistatic semiconductive resin composition comprises polyethylene, ethylene vinyl acetate and carbon black. The sum of p+q+r, where p is the weight% of the polyethylene and the q is the weight% of the ethylene vinyl acetate and r is the weight% of the carbon black based on the total weight of the semiconductive resin composition, p is 108-2r - 118-2r q is r-18 - r-11, and r is 21-29. [Reference numerals] (S10) Putting raw material in; (S20) Mixing; (S30) Extruding; (S40) Cooling/cutting
Abstract translation: 目的:提供抗静电半导体树脂组合物,以具有优异的挤出加工性和优异的物理性能,例如抗拉强度,同时具有在适度范围内的表面电阻。 构成:抗静电半导体树脂组合物包含聚乙烯,乙烯 - 乙酸乙烯酯和炭黑。 p + q + r的总和,其中p是聚乙烯的重量%,q是乙烯乙酸乙烯酯的重量%,r是基于半导体树脂组合物的总重量的炭黑的重量% ,p为108-2r-118-2r q为r-18-r-11,r为21-29。 (附图标记)(S10)将原料放入; (S20)混合; (S30)挤压; (S40)冷却/切割
-
公开(公告)号:KR100997052B1
公开(公告)日:2010-11-29
申请号:KR1020100020188
申请日:2010-03-08
Applicant: (주)폴리원테크놀로지
Abstract: PURPOSE: A polypropylene master batch composition for a flame-retardant flexible electric wire pipe is provided to secure the excellent heat-resisting stability and UV stability by using tris(tribromoneopentyl) phosphate as a flame retardant, and to improve the impact strength. CONSTITUTION: A polypropylene master batch composition for a flame-retardant flexible electric wire pipe contains the following: 100 parts of base resin by weight formed with one compound selected from the group consisting of low-density polyethylene, linear low-density polyethylene, and high-density polyethylene; 30~70 parts of fire retardant by weight formed with tris(tribromoneopentyl) phosphate; 5~30 parts of antimony oxide by weight; 0.5~5 parts of anti-oxidant by weight; and 0.1~5 parts of distearyl thiodipropionate, octadecyl-3-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate, and zinc stearate by weight.
Abstract translation: 目的:提供一种用于阻燃柔性电线管的聚丙烯母料组合物,通过使用三(三溴新戊基)磷酸酯作为阻燃剂以确保耐冲击稳定性和UV稳定性,并提高冲击强度。 构成:用于阻燃柔性电线管的聚丙烯母料组合物包含以下组分:100重量份由选自低密度聚乙烯,线性低密度聚乙烯和高分子量的一种化合物形成的重量的基础树脂 密度聚乙烯; 30〜70重量份由三(三溴新戊基)磷酸酯形成的阻燃剂; 5〜30份氧化锑重量; 0.5〜5份抗氧化剂重量; 和0.1〜5份硫代二丙酸二硬脂酯,十八烷基-3-(3,5-二叔丁基-4-羟基苯基)丙酸酯和硬脂酸锌。
-
公开(公告)号:KR101411690B1
公开(公告)日:2014-07-03
申请号:KR1020110063681
申请日:2011-06-29
IPC: C08L101/16 , C08J5/18 , B29D7/01 , B29C47/00
Abstract: 본 발명은 산업이나 농업 용도로 사용되는 광 붕괴-생분해 복합수지와 필름 및 그 조성물에 관한 것으로, 이온교환수 100중량부에 수산화칼륨(KOH) 0.9-1.5중량부를 용해시키고 스테아르산(stearic acid) 4.0-6.0 중량부를 적가하면서 완전히 용해될 때까지 200RPM으로 교반한 다음 2.7-3.0중량부의 페릭설페이트 히드레이트(ferric sulphate hydrate)나 칼슘설페이트 히드레이트(calcium sulphate hydrate)인 금속 설페이트 히드레이트(metal sulphate hydrate)를 적가하면서 반응시켜 생성되는 침전물을 여과, 세척, 건조과정을 거치는 금속 스테아레이트(metal stearate) 제조단계와;
폴리올레핀, 폴리염화비닐, 폴리에스테르, 폴리스틸렌, 아크릭 혹은 나이론과 같은 고분자 수지 100 중량부에 상기 금속 스테아레이트 형성단계에서 제조된 금속 스테아레이트 0.1-10중량부와 아이언(iron:금속) 2,4-펜탄디온(iron 2,4-pentanedione), 티타닐 2,4-펜탄디온(titanyl 2,4-pentanedione), 지르코닐 2,4-펜탄디온(zirconyl 2,4- pentanedione), 마그네슘 2,4-펜탄디온(magnesium 2,4-pentanedione), 카퍼 2,4-펜탄디온(copper 2,4-pentanedione), 칼슘 2,4-펜탄디온(calcium 2,4-pentanedione)이나 알루미늄 2,4-펜탄디온(aluminium 2,4-pentanedione)과 같은 금속 펜탄디온 0.1-20 중량부, 자외선안정제 (UV absorber, UV stabilizer) 0.1-1.0중량부, 열산화방지제인폴리(1,2-디히드로-2,2,4-트리메틸퀴놀린) [poly(1,2-dihydro-2,2,4-trimethyl quinoline)], 2,6-디-터트-부틸-4-메틸페놀(2,6-di-tert-butyl-4-methyl phenol), 테트라키스[메틸렌(3,5-디-터트 -부틸-4-히드로옥시-히드로시나메이트)메탄 [tetrakis[methylene(3,5-di-tert-butyl-4-hydroxy-hydrocinnamate)]methane]이나 트리스(2,4-디-터트-부틸-페닐)포스파이트[tris(2,4-di-tert-butyl-phenyl) phosphite] 0.1-5중량부, 안료 0.001 내지 4.0중량부, 니켈 디메틸글리옥심 (nickel diethylglyoxime) 0.01-0.5중량부, 페놀프탈레인(phenolphthalein) 0.01-5중량부와, 랙틱애시드(lactic acid :젖산) (latic acid), 말레익안하이드리드 (maleic anhydride), 시트릭액시트(citric acid)등과 같은 분해조절컴파운드 0.1-10중량부를 통상의 헨셀 믹서, 슈퍼 믹서 또는 디스퍼션 니더에서 용융혼합하여 광붕괴-생분해 복합수지 조성물형성단계와;
상기 광 붕괴-생분해 복합수지 조성물형성단계에서 얻어진 조성물을 단축(single) 또는 이축(twin) 압출기를 이용한 용융압출 성형과정을 통해 2-3mm 크기를 갖는 광 붕괴-생분해 복합수지 펠렛으로 만드는 펠렛화 단계와;로 광 붕괴-생분해 복합수지를 얻고, 상기 펠렛화단계에서 얻어진 광 붕괴-생분해 복합수지 펠렛을 호퍼에 넣고 시트 성형용 다이가 부착되어 있는 단축 또는 이축압출 시트기에서 필름을 성형하는 필름성형단계로 광 붕괴-생분해 복합수지 필름을 얻는다.상기 펠렛화단계에서 얻어진 광 붕괴-생분해 복합수지 펠렛을 호퍼에 넣고 시트 성형용 다이가 부착되어 있는 단축 또는 이축압출 시트기에서 필름을 성형하는 필름성형단계로 제조되는 광 붕괴-생분해 복합수지 조성물 및 이를 이용한 필름을 얻는다.-
公开(公告)号:KR1020100113750A
公开(公告)日:2010-10-22
申请号:KR1020090032221
申请日:2009-04-14
Applicant: (주)폴리원테크놀로지
Abstract: PURPOSE: A flame-retardant resin composition is provided to secure physical properties including the tensile strength and the elongation rate, and to minimize the smoke density during the fire. CONSTITUTION: A flame-retardant resin composition contains 100 parts of ethylene vinyl acetate by weight, 1~5 parts of maleic anhydride terpolymer ethylene acrylate graft resin by weight; 10~15 parts of maleic anhydride-linear low-density polyethylene grafted copolymer resin by weight; 90~150 parts of magnesium hydroxide by weight; 3~10 parts of high molecular weight silicon compound by weight; and 1~5 parts of master batch including a resin, and red-phosphorus.
Abstract translation: 目的:提供阻燃树脂组合物以确保包括拉伸强度和伸长率在内的物理性能,并使火灾期间的烟雾浓度最小化。 构成:阻燃树脂组合物含有100重量份乙烯乙酸乙烯酯,1〜5重量份马来酸酐三元共聚物乙烯丙烯酸酯接枝树脂; 10〜15份马来酸酐 - 线性低密度聚乙烯接枝共聚物树脂; 90〜150份重量的氢氧化镁; 3〜10重量份高分子量硅化合物; 和1〜5份包含树脂的母料和红磷。
-
公开(公告)号:KR1020130002621A
公开(公告)日:2013-01-08
申请号:KR1020110063681
申请日:2011-06-29
IPC: C08L101/16 , C08J5/18 , B29D7/01 , B29C47/00
Abstract: PURPOSE: A photo-sensitive-biodegradable composite resin is provided to reduce molecular weight by collision of a polymer backbone through sunlight and to have excellent biodegradability. CONSTITUTION: A photo-sensitive-biodegradable composite resin is manufactured by: a step of a manufacturing a metal stearate by filtering, washing and drying a precipitate which is obtained by dropping and reacting a stearic acid and a metal sulfate hydrate into a potassium hydrate solution; a step of melt-mixing the metal stearate and a decomposition-controlling compound into a polymer resin to form a photo-sensitive-biodegradable composite resin composition; and a step of manufacturing a photo-sensitive-biodegradable pellet by melting and extrusion molding the composition. [Reference numerals] (AA) Metal stearate manufacturing step; (BB) Photo-sensitive-biodegradable composite resin composition forming step; (CC) Pelletizing step
Abstract translation: 目的:提供光敏生物降解复合树脂,以通过聚合物主链通过阳光的碰撞来降低分子量,并具有优异的生物降解性。 构成:通过以下方法制造光敏生物降解性复合树脂:通过过滤,洗涤和干燥通过将硬脂酸和金属硫酸盐水合物滴加并反应到水合钾溶液中而获得的沉淀物来制造金属硬脂酸盐的步骤 ; 将金属硬脂酸酯和分解控制化合物熔融混合到聚合物树脂中以形成光敏生物可降解复合树脂组合物的步骤; 以及通过熔融和挤出成型制造光敏生物降解性颗粒的步骤。 (AA)金属硬脂酸酯的制造工序; (BB)光敏生物降解性复合树脂组合物的形成工序; (CC)造粒步骤
-
-
-
-
-
-
-
-
-