Abstract:
본 발명은 자연 해수를 전해액으로 사용하여 양극산화반응에 의해 티타늄 금속 지지체에 결정형의 티타니아를 고정화시킨 광감응 소재를 제조한다. 그리고, 이 광감응 소재를 광어노드로 활용하여 수소발생률이 우수한 광전기화학적 수소제조장치를 제공한다. 또한, 본 발명은 상기 광감응 소재를 광촉매로 하는 6가 크롬 환원장치를 제공함으로써, 수중에 존재하는 대표적인 독성물질인 6가 크롬을 광화학반응에 의해 상대적으로 독성이 약한 3가 크롬으로 환원처리하게 된다.
Abstract:
PURPOSE: A metal-structure, a metal-structured catalyst, a metal-structured catalyst module and their preparation methods for a possible application in a compact reformer are provided to uniformly form a metallic oxidation layer through an electrochemical surface treatment. CONSTITUTION: A preparation method for a possible application in a compact reformer comprises the steps of: removing and cleaning a surface containment of a metallic supporter; performing electrochemical surface treatment to form a metallic oxidation layer by adjusting the applied voltage in electrolyte and the concentration of the electrolyte; and performing the heat treatment under oxidizing environment to form a metallic oxidation layer.
Abstract:
본 발명은 자열개질에 의한 천연가스로부터 피셔-트롭쉬 액화공정용 합성가스(H 2 /CO≒2) 제조에 사용되는 개질촉매 및 그 제조방법과 이를 이용한 피셔-트롭쉬 액화공정용 합성가스의 제조방법에 관한 것으로, 그 주된 목적은 주된 반응으로 메탄 또는 천연가스를 부분산화반응하고 부가되는 반응으로 수증기개질반응과 (역)수성가스전이반응{(reverse) water gas shift reaction, (R)WGS}에 의해 수소와 일산화탄소로 전환하면서, 피셔-트롭쉬 공정(Fischer-Tropsch Process)에 적합한 수소와 일산화탄소 비율(H 2 /CO≒2)을 얻는데 필요한 촉매 조성과 반응조건을 제시하는 데 있다. 본 발명의 구성은 고표면적 알루미나 담체와, 알루미나 담체 100wt% 대비 니켈금속 1~20wt%, 세륨금속 1 ~ 15wt%로 조성된 피셔-트롭쉬 액화공정용 촉매 및 그 제조방법과 이를 이용한 합성가스 제조방법을 그 기술적 사상의 특징으로 한다. 피셔-트롭쉬 액화공정, 자열개질, 촉매, 합성가스, 고표면적 알루미나 담체, 니켈, 세륨
Abstract:
본 발명은 피셔-트롭쉬 액화공정용 합성가스 제조공정에 사용되는 메탄 자열개질촉매 및 이를 이용한 메쉬형 촉매층, 그리고 이를 이용한 피셔-트롭쉬용 합성가스 제조방법에 관한 것으로, 그 주된 목적은 주된 반응으로 메탄 또는 천연가스를 부분산화반응하고 부가되는 반응으로 수증기개질반응과 (역)수성가스전이반응{(reverse) water gas shift reaction, (R)WGS}에 의해 수소와 일산화탄소로 전환하면서, 피셔-트롭쉬 공정(Fischer-Tropsch Process)에 적합한 수소와 일산화탄소 비율(H 2 /CO≒2)을 얻는데 필요한 촉매 및 촉매층과 이를 이용한 반응조건을 제시하는 데 있다. 본 발명의 구성은 고표면적 알루미나 담체와, 촉매 전체 무게 대비 팔라듐 금속 2~4wt%로 조성된 피셔-트롭쉬 액화공정용 합성가스 제조 촉매 및 이 촉매를 메쉬형 금속판을 불규칙 유로를 유발하면서 원하는 촉매양에 따라 용이하게 그 수의 조절이 가능한 형태로 적층한 촉매층, 그리고 이를 이용한 합성가스 제조방법을 그 기술적 사상의 특징으로 한다. 자열개질, 팔라듐, 피셔-트롭쉬용 합성가스, 메쉬형 촉매층, 촉매부분산화반응
Abstract:
본 발명은 금속 구조체 촉매 및 그 제조방법에 관한 것으로, 그 목적은 반응의 고활성과 액상 생성물에 대한 높은 수율, 그리고 반응열에 대한 높은 안정성을 보이는 금속 구조체 촉매 및 그 제조방법을 제공하는 데 있다. 본 발명의 구성은 피셔-트롭쉬 반응을 이용하여 일산화탄소와 수소로 이루어진 합성가스로부터 가솔린, 디젤, 왁스 등을 제조하는 방법에 있어서, 금속 구조체 위에 피셔-트롭쉬 반응 촉매가 워시 코팅된 금속 구조체를 이용하여 피셔-트롭쉬 반응에 의해 일산화탄소와 수소로 이루어진 합성가스로부터 가솔린, 디젤, 왁스 등을 제조하는데 사용되는 금속 구조체 촉매 및 그 제조방법을 그 기술적 사상의 특징으로 한다. 피셔-트롭쉬 반응, 피셔-트롭쉬 반응 촉매, 금속 구조체 촉매, 액체 연료
Abstract:
A reforming catalyst, a manufacturing method thereof, and a method of producing synthetic gas for the fischer-tropsch process using the same are provided to offer the reforming catalyst improving selectivity of carbon monoxide and hydrogen and to maintain high catalytic activity. In a catalyst for fischer-tropsch process, a reforming catalyst used in production of synthetic gas(H2/CO≒2) for a fischer-tropsch process through autothermal reforming of natural gas includes a component consisting of a high surface area alumina carrier, 1~20 wt% of a nickel metal, 1~15 wt% of a cerium metal on the basis of 100 wt% of the alumina carrier. The high surface area alumina carrier is a gamma alumina of which specific surface area is bigger than 100m^2/g.
Abstract:
An enzymatic hydrogen production apparatus for water decomposition using an anodized tubular TiO2 electrode, a solar cell, and a nanofiltration membrane is provided to produce hydrogen economically using sunlight by applying a solar cell and the nanofiltration membrane used as an ion bridge, thereby maximizing the hydrogen generation efficiency. A hydrogen production apparatus(1) for water decomposition comprises an anodized TiO2 electrode(13), an anode electrolyte(14), a cathode(15), a cathode electrolyte(16), a nanofiltration membrane(17), and a solar cell(18). The anodized TiO2 electrode is formed by integrally and densely laying up titania(13B) as a transition metal oxide layer in a tubular shape on the surface of a metal titanium support, thereby bonding the titania as the transition metal oxide layer to the surface of the metal titanium support. The anode electrolyte has the anodized TiO2 electrode immersed thereinto. The cathode is formed of metal having corrosiveness with respect to an acidic or alkaline solution. The cathode electrolyte has the cathode immersed thereinto. The cathode electrolyte is a mixed solution of a buffer solution with a pH range of 7 to 10, an electron carrier, and an enzyme. The nanofiltration membrane is connected to both end portions of the anode electrolyte and cathode electrolyte to provide a moving passage of ions between two solutions. The solar cell connects the anodized TiO2 electrode and cathode.
Abstract:
PURPOSE: A method for fabricating bundles of plastic optical fibers coated with optical catalyst is provided to remove efficiently coating layers of the plastic optical fibers and form bundles of plastic optical fibers without the coating layers. CONSTITUTION: A predetermined solvent is prepared to remove a coating layer of a plastic optical fiber(S10). The plastic optical fiber is dipped into the predetermined solvent(S20). A core of the plastic optical fiber is cleaned by using distilled water(S30). The core of the plastic optical fiber is coated by using an optical catalyst(S40). A dry process for the coated core is performed(S50). The above processes are repeatedly performed to form a bundle of plastic optical fibers(S60). The bundle of plastic optical fibers is formed by using a plurality of optical fibers(S70). A polishing process for end portions of the optical fibers is performed(S80).
Abstract:
본 발명은 니켈/티타니아 혼합광촉매 및 그 제조방법과 이 촉매를 유리구슬에 코팅시킨 유리구슬담지체 및 그 코팅방법에 관한 것으로, 그 목적은 광촉매에 있어서, 정공-전자쌍의 재결합을 억제 또는 방지하는 것과 띠에너지의 값을 낮춰서 빛의 활용범위를 높여주거나, 띠에너지의 값이 다소 커지더라도 화학물질과 촉매간의 추진에너지가 커지도록 하는 혼합광촉매 및 그 제조방법과 이 촉매를 유리구슬에 코팅시킨 유리구슬담지체 및 그 코팅방법을 제공하는 것이다. 본 발명의 구성은 55.6~99wt%티타니아, 44.4~1wt%니켈로 조성되는 니켈/티타니아 혼합광촉매를 제조하기 위하여 냉각공정; 교반 및 첨가공정; 교반공정; 박막제거공정; 감압증발공정과; 진공냉각공정과; 건조공정을 거쳐 광촉매를 제조하며, 이를 다시 유리 담지체에 광촉매를 코팅시켜 유리구슬담지체를 제조한다.