기능성 신발
    11.
    发明公开
    기능성 신발 有权
    功能鞋

    公开(公告)号:KR1020110047324A

    公开(公告)日:2011-05-09

    申请号:KR1020090103908

    申请日:2009-10-30

    CPC classification number: A43B13/203 A43B3/0015 A43B7/06 A43B7/32 A43B21/285

    Abstract: PURPOSE: Functional shoes are provided to improve energy conversion efficiency and to endure external force repeated during walking. CONSTITUTION: Functional shoes comprise: a shoes body(110); an elastic airbag(120) which repeats contraction and expansion by an external force applied during walking; an air channel tube(130) which inhales air from an inlet and discharges air to an outlet; a check valve(140) preventing the suction of the air from the outlet during inflation of the elastic airbag and the exhaustion of the air to the inlet during contraction of the elastic airbag; a turbine(150) which is formed within the air channel tube and revolves; a generator(160) generating electromotive force by the rotation of the turbine; and an output terminal(170) which outputs electrical energy to the outside of the shoes body.

    Abstract translation: 目的:提供功能性鞋,以提高能量转换效率,并承受步行期间重复的外力。 构成:功能鞋包括:鞋体(110); 弹性气囊(120),其通过在步行期间施加的外力重复收缩和膨胀; 空气通道管(130),其从入口吸入空气并将空气排放到出口; 止回阀(140),其在所述弹性气囊的充气期间防止来自所述出口的空气的吸入,并且在所述弹性气囊的收缩期间空气向所述入口排出; 涡轮(150),其形成在所述空气通道管内并旋转; 通过涡轮机的旋转产生电动势的发电机(160) 以及向鞋体的外部输出电能的输出端子(170)。

    센서 및 액추에이터용 비납계 압전 세라믹 조성물 및 그 제조방법
    12.
    发明授权
    센서 및 액추에이터용 비납계 압전 세라믹 조성물 및 그 제조방법 有权
    用于传感器和执行器的无铅压电陶瓷的组成及其制造方法

    公开(公告)号:KR101012143B1

    公开(公告)日:2011-02-07

    申请号:KR1020080108951

    申请日:2008-11-04

    Abstract: 본 발명은 납이 함유되지 않은 비납계 압전 세라믹 조성물과 그의 제조방법에 관한 것으로서, 보다 상세하게는 센서 및 액추에이터에 적용될 수 있는 우수한 전기기계결합계수 및 압전특성을 지닌 납이 함유되지 않은 압전 세라믹 조성물 및 그 제조방법에 관한 것이다.
    본 발명의 압전 센서 및 액추에이터용 비납계 압전 세라믹 조성물은 x Na(Nb
    0.8 Ta
    0.2 )O
    3 - y K(Nb
    0.8 Ta
    0.2 )O
    3 - z Li(Nb
    0.8 Ta
    0.2 )O
    3 의 분말 1mol 대비 a mol의 비율로 Li
    2 CO
    3 가 첨가된 조성을 갖되, 상기 x는 0.47 이상 0.53 이하이고, y는 0.98-x이고, z는 0.02이며, a는 0.01이다. 보다 바람직하게는 상기 x는 0.51이다.
    비납계, 압전, 세라믹조성물, 하소, 재하소, 소결,

    고변위 적층형 압전액츄에이터용 저온소결 압전 자기 조성물
    13.
    发明授权
    고변위 적층형 압전액츄에이터용 저온소결 압전 자기 조성물 有权
    用于低温烧结的高性能多层陶瓷致动器的压电陶瓷组合物

    公开(公告)号:KR100977420B1

    公开(公告)日:2010-08-24

    申请号:KR1020080108969

    申请日:2008-11-04

    Abstract: 본 발명은 압전 자기 조성물에 관한 것으로서, 압전변위제어용으로 적층형 압전 액츄에이터에 사용될 수 있는 높은 전기기계결합계수(k
    p )와 압전상수(d
    33 )를 갖는 압전 자기 조성물에 관한 것이다.
    본 발명의 조성물은 안정한 ABO
    3 구조를 갖는 0.4Pb(Mg
    1/3 Nb
    2/3 )O
    3 -0.25PbZrO
    3 -0.35PbTiO
    3 의 100중량부 대비, 0.05 중량부의 Li
    2 CO
    3 , 0.01 중량부의 Bi
    2 O
    3 , 1 중량부의 PbO 및 d중량부의 CuO가 첨가된 압전 자기 조성물로서, 상기 d는 0 초과 0.5이하의 범위이며, 보다 바람직하게는 상기 d는 0.3이다.
    CuO를 첨가함에 따라 전기기계결합계수(k
    p ) 및 압전상수(d
    33 )가 증가하는 한편 소결온도는 950 ℃로 낮출수 있었으며, 따라서 보다 값싼 은 전극을 사용할 수 있는 적층형 압전액츄에이터에 응용될 수 있는 압전 자기 조성물 및 그 제조방법을 제공한다.
    압전세라믹스, 액츄에이터, 압전변위소자, 적층세라믹스, 저온소성

    전기영동증착을 이용한 적층형 세라믹 소자의 공극 밀봉방법
    14.
    发明授权
    전기영동증착을 이용한 적층형 세라믹 소자의 공극 밀봉방법 失效
    一种使用电泳沉积法在共烧多层陶瓷器件中密封电极与陶瓷层之间气隙的新方法

    公开(公告)号:KR100960855B1

    公开(公告)日:2010-06-07

    申请号:KR1020080052416

    申请日:2008-06-04

    Abstract: 본 발명은 전기영동증착을 이용한 적층형 세라믹 소자의 공극 밀봉 방법에 관한 것으로 동시 소성이 요구되는 적층형 세라믹 소자의 제조 시 부 전극과 세라믹 테이프로 구성되는 적층체들 사이에 발생되는 세라믹테이프와 전극 사이의 단차를 줄일 수 있으며 고 적층체를 제조하기 위해서 적층형 세라믹 소자의 상층부와 하층부에 포함된 내부 전극의 변형이 없이 간편하게 일체화된 고적층형 세라믹 소자를 제조할 수 있는 공정에 관한 것이다.
    세라믹 적층 소자 공극 밀봉 전기영동증착

    적층 벤딩형 압전소자 및 이를 이용한 에너지 발생 장치
    16.
    发明公开
    적층 벤딩형 압전소자 및 이를 이용한 에너지 발생 장치 无效
    使用多层弯曲型压电装置的能量产生装置

    公开(公告)号:KR1020100045655A

    公开(公告)日:2010-05-04

    申请号:KR1020080104694

    申请日:2008-10-24

    CPC classification number: H01L41/0973 H01L41/083 H01L41/187 H02N2/0005

    Abstract: PURPOSE: A stacked bending type piezoelectric device and an energy generation device using the same are provided to successively generate energy by overlapping the attenuation section of voltage signal. CONSTITUTION: A metal plate(120) is stacked on one side of a piezoelectric device(110) which is based on a ceramic. The ceramic-based piezoelectric device and one end of the metal plate are bent. A bending part(b) is formed. The piezoelectric device and the metal plate are adhered by a resin adhesion layer(130). The resin adhesion layer fixes the metal plate and the piezoelectric device.

    Abstract translation: 目的:提供堆叠式弯曲型压电装置和使用该压电装置的能量产生装置,以通过与电压信号的衰减部分重叠来连续产生能量。 构成:金属板(120)层叠在基于陶瓷的压电元件(110)的一侧。 陶瓷基压电元件和金属板的一端弯曲。 形成弯曲部(b)。 压电装置和金属板通过树脂粘合层(130)粘合。 树脂粘合层固定金属板和压电装置。

    비납계 압전 세라믹스 조성물 및 그 제조방법
    17.
    发明授权
    비납계 압전 세라믹스 조성물 및 그 제조방법 有权
    비납계압전세라믹스조성물및그제조방법

    公开(公告)号:KR100875479B1

    公开(公告)日:2008-12-22

    申请号:KR1020070056769

    申请日:2007-06-11

    Abstract: A composition and a manufacturing method of lead-free piezoelectric ceramics are provided to improve the piezoelectricity characteristic by adding Li2CO3 and Na2CO3 to the ceramic composition. The manufacturing method of the lead-free piezoelectric ceramic composition comprises the following steps: the step that mixes and pulverizes the sample of the Na2CO3, K2CO3, Li2CO3, Nb2O5, and Ta2O5 and dries and burns; the step that re-burns the burned sample; the step for remixing, re-pulverizing the sample; the step for sintering and molding the dried sample. Li2CO3 and Na2CO3 are added to the ceramic composition of (NaxK0.95-xLi0.05)(Nb0.95Ta0.05)O3.

    Abstract translation: 提供无铅压电陶瓷的组成和制造方法,以通过向陶瓷组合物中加入Li 2 CO 3和Na 2 CO 3来改善压电特性。 无铅压电陶瓷组合物的制备方法包括以下步骤:将Na 2 CO 3,K 2 CO 3,Li 2 CO 3,Nb 2 O 5和Ta 2 O 5的样品混合并粉碎并干燥和灼烧; 重烧烧伤样本的步骤; 重新混合,重新粉碎样品的步骤; 烧结和模制干燥样品的步骤。 (Na x K 0.95-x Li 0.05)(Nb 0.95 Ta 0.05)O 3的陶瓷组合物中添加Li 2 CO 3和Na 2 CO 3。

    탄소나노튜브 전극을 이용한 염료감응형 태양전지 모듈 및그 제조방법
    18.
    发明授权
    탄소나노튜브 전극을 이용한 염료감응형 태양전지 모듈 및그 제조방법 有权
    染料敏化太阳能电池模块和使用碳纳米管电极的制造方法

    公开(公告)号:KR100834475B1

    公开(公告)日:2008-06-05

    申请号:KR1020060119439

    申请日:2006-11-30

    CPC classification number: Y02E10/542 Y02P70/521

    Abstract: 본 발명은 탄소나노튜브 전극을 이용한 염료감응형 태양전지 모듈에 관한 것으로서, 상,하부 투명기판과; 상,하부 투명기판의 내측 표면에 형성된 도전성 투명전극과; 상기 상부 도전성 투명전극 위에 형성되며, 등간격으로 다수개가 형성되는 것으로 그 표면에는 염료가 흡착된 산화물반도체 다공질 음극전극과; 상기 하부 도전성 투명전극 위에 박막형태로 형성된 것으로 상기 음극전극에 대응하는 양극부로서의 탄소나노튜브층으로 된 상대전극과; 상기 상,하부 도전성 투명전극 위에 상기 음극전극 및 이에 대응되는 상대전극으로 이루어진 단위전극 사이에 형성되는 것으로 광감응되어 발생하는 전자를 포집하는 그리드전극과; 상기 상,하부 도전성 투명전극 위에 형성되며, 상기 그리드전극과 전기적으로 연결되어 상기 그리드전극으로부터 이동된 전자를 외부로 전달시키는 연결전극과; 상기 음극전극과 상대전극 사이에 충전되는 전해질;을 포함하여 구성되는 것을 특징으로 하는 탄소나노튜브 전극을 이용한 염료감응형 태양전지 모듈 및 이의 제조방법을 기술적 요지로 한다. 이에 따라, 단위 염료감응형 태양전지를 모듈의 형태로 복수개로 형성시키고, 그리드전극 및 연결전극을 이용하여 전자를 포집하고 이동시킴에 따라 태양전지의 효율이 높고, 대면적의 탄소나노튜브를 이용한 염료감응형 태양전지를 제공할 수 있어, 실용화 가능성이 높은 효과가 있으며, 또한, 유연성이 있고, 전기전도성이 있는 탄소나노튜브 전극을 상대전극, 그리드전극 및 연결전극으로 사용함으로써, 기존의 금속 전극의 문제점인 전해질에 의해 용해되거나, 산화 등에 의한 열화가 나타나는 현상이 없으므로, 전기적, 화학적으로 안정한 모듈을 제공할 수 있는 이점이 있다.
    탄소나노튜브 염료감응형 태양전지 상대전극 연결전극 그리드전극

    염료감응형 태양전지의 구조 및 그 제조방법
    19.
    发明授权
    염료감응형 태양전지의 구조 및 그 제조방법 有权
    染料敏化太阳能电池的结构及其制造方法

    公开(公告)号:KR100790405B1

    公开(公告)日:2008-01-02

    申请号:KR1020060067416

    申请日:2006-07-19

    Abstract: A structure of a dye-sensitized solar cell and a manufacturing method thereof are provided to prevent a short between an anode and a cathode even though a gap between the anode and the cathode is narrowed by arranging the anode and the cathode in a concave groove. A dye-sensitized solar cell is comprised of a top substrate(101), a conductive electrode(102) formed on an inner surface of the top substrate, an oxide semiconductor porous cathode(103) formed over the conductive electrode, a relative electrode as a positive polar section corresponding to the cathode electrode, and an electrolyte(105) gap-filled between the cathode and the relative electrode. A dye is absorbed into a surface of the oxide semiconductor porous cathode. A concave groove is formed on a bottom substrate toward the relative electrode by using a coating layer resistant to a glass substrate corrosion liquid and corrosion. The relative electrode is formed in the concave groove.

    Abstract translation: 提供染料敏化太阳能电池的结构及其制造方法,以防止阳极和阴极之间的短路,即使通过将阳极和阴极布置在凹槽中而使阳极和阴极之间的间隙变窄。 染料敏化太阳能电池由上基板(101),形成在顶基板的内表面上的导电电极(102),形成在导电电极上的氧化物半导体多孔阴极(103),相对电极 对应于阴极的正极性部分和在阴极和相对电极之间间隙填充的电解质(105)。 染料被吸收到氧化物半导体多孔质阴极的表面。 通过使用耐玻璃基板腐蚀液体和腐蚀的涂层,在底部基板上朝向相对电极形成凹槽。 相对电极形成在凹槽中。

    박막 커패시터 유전체의 제조방법
    20.
    发明授权
    박막 커패시터 유전체의 제조방법 失效
    制造薄膜电容器电介质的方法

    公开(公告)号:KR100766991B1

    公开(公告)日:2007-10-15

    申请号:KR1020040112676

    申请日:2004-12-27

    Abstract: 본 발명에 따른 박막 커패시터 유전체의 제조방법은, a) 기판상의 실리콘 타겟에 탄탈륨(Ta) 금속을 반응성 가스인 산소와 반응시켜 가면서 증착하는 단계와, b) 상기 증착으로 형성된 산화탄탈륨(TaO) 박막을 산소 분위기 및 진공 분위기에서 소정 온도로 열처리하는 단계; 및 c) 상기 열처리된 Ta
    2 O
    5-x 박막을 상온까지 냉각하는 단계를 포함한 박막 커패시터 유전체의 제조방법에 있어서: 상기 단계 b)에서의 산소 분위기 및 진공 분위기 조건은 산소 주입을 50cc/min로, 진공도를 10
    -6 torr 이하로 유지하는 것을 특징으로 한다.
    이와 같은 본 발명에 의하면, RF 스퍼터링 방법으로 Ta
    2 O
    5 박막을 증착시킨 후 결정화 온도 영역으로 알려진 650∼750 ℃의 산소 및 진공 분위기에서 어닐링 처리하여 커페시터 유전체 박막을 제조하므로, 상온에서 200 ℃ 까지 유전율 변화를 측정한 결과 매우 안정한 특성을 나타내고, 4.0 ×102 (kV/cm) 이하의 전계강도 영역에서 비교적 안정한 누설전류 특성을 나타내어 메모리나 박막 커패시터용 유전체로서 채용될 경우 양호한 특성을 갖는 제품의 생산이 가능해 진다.
    커패시터, 유전체, 메모리

Patent Agency Ranking