Abstract:
A nanocomposite is provided including layered nanoparticles and a dispersant dispersed in a curable resin, where the nanocomposite contains less than 2% by weight solvent. A composite is also provided including from about 1 to 70 weight percent of layered nanoparticles, and a dispersant, dispersed in a cured resin, and a filler embedded in the cured resin. Further, a method of preparing a nanoparticle-containing curable resin system is provided including mixing from 1 to 70 weight percent of aggregated layered nanoparticles with a curable resin and a dispersant to form a mixture. The mixture contains less than 2% by weight solvent. The method also includes milling the mixture in an immersion mill containing milling media to form a milled resin system including layered nanoparticles dispersed in the curable resin.
Abstract:
A hardcoat composition includes one or more multifunctional (meth)acrylate monomers, and a population of semi-reactive nanoparticles dispersed within the one or more multifunctional (meth)acrylate monomers. The population of semi-reactive nanoparticles have an average particle diameter in a range from 5 nm to 60 nm.
Abstract:
A hardcoat composition includes one or more multifunctional (meth)acrylate monomers, and a nanoparticle mixture dispersed within the one or more multifunctional (meth)acrylate monomers. The nanoparticle mixture includes a first population of semi-reactive nanoparticles having an average particle diameter in a range from 5 nm to 60 nm, and a second population of reactive nanoparticles having an average particle diameter in a range from 5 nm to 60 nm.
Abstract:
A hardcoat composition includes one or more multifunctional (meth)acrylate monomers, and a nanoparticle mixture dispersed within the one or more multifunctional (meth)acrylate monomers. The nanoparticle mixture includes a first population of reactive nanoparticles. The first population of reactive nanoparticles have an average particle diameter in a range from 5 nm to 60 nm, and a second population of non-reactive nanoparticles. The second population of non-reactive nanoparticles have an average particle diameter in a range from 5 nm to 60 nm.
Abstract:
A hardcoat composition includes one or more multifunctional (meth)acrylate monomers, and a nanoparticle mixture dispersed within the one or more multifunctional (meth)acrylate monomers. The nanoparticle mixture includes a first population of semi-reactive nanoparticles having an average particle diameter in a range from 5 nm to 60 nm, and a second population of reactive nanoparticles having an average particle diameter in a range from 5 nm to 60 nm.
Abstract:
A hardcoat composition includes one or more multifunctional (meth)acrylate monomers, and a population of semi-reactive nanoparticles dispersed within the one or more multifunctional (meth)acrylate monomers. The population of semi-reactive nanoparticles have an average particle diameter in a range from 5 nm to 60 nm.
Abstract:
A display film comprises a transparent glass layer including two or more co-planar glass layer segments and a thickness defined by a first major surface and a second major surface opposing the first major surface being less than 500 micrometers; interstitial polymer material separating adjacent segments; and transparent energy dissipation layer having a glass transition temperature of 27 degrees Celsius or less and a Tan Delta peak value of 0.5 or greater and being disposed on the first major surface.
Abstract:
A nanocomposite is provided including silica nanoparticles and a dispersant dispersed in a curable resin or a curing agent, where the nanocomposite contains less than 2% by weight solvent. The silica nanoparticles include nonspherical silica nanoparticles and/or spherical pyrogenic silica nanoparticles. A composite is also provided including from about 4 to 70 weight percent of silica nanoparticles, and a dispersant, dispersed in a cured resin, and a filler embedded in the cured resin. Optionally, the composite further contains a curing agent. Further, a method of preparing a nanoparticle-containing curable resin system is provided including mixing from 10 to 70 weight percent of aggregated silica nanoparticles with a curable resin and a dispersant to form a mixture. The mixture contains less than 2% by weight solvent. The method also includes milling the mixture in an immersion mill containing milling media to form a milled resin system including silica nanoparticles dispersed in the curable resin.
Abstract:
A nanocomposite is provided including silica nanoparticles and a dispersant dispersed in a curable resin or a curing agent, where the nanocomposite contains less than 2% by weight solvent. The silica nanoparticles include nonspherical silica nanoparticles and/or spherical pyrogenic silica nanoparticles. A composite is also provided including from about 4 to 70 weight percent of silica nanoparticles, and a dispersant, dispersed in a cured resin, and a filler embedded in the cured resin. Optionally, the composite further contains a curing agent. Further, a method of preparing a nanoparticle-containing curable resin system is provided including mixing from 10 to 70 weight percent of aggregated silica nanoparticles with a curable resin and a dispersant to form a mixture. The mixture contains less than 2% by weight solvent. The method also includes milling the mixture in an immersion mill containing milling media to form a milled resin system including silica nanoparticles dispersed in the curable resin.
Abstract:
A nanocomposite is provided including spherical pyrogenic silica nanoparticles dispersed in a curable resin or a curing agent. The nanocomposite contains less than 2% by weight solvent and less than 0.5% by weight dispersant based on the nanoparticle weight. A composite is also provided including from about 4 to 70 weight percent of spherical pyrogenic silica nanoparticles dispersed in a cured resin, and a filler embedded in the cured resin. Optionally, the composite further contains a curing agent. Further, a method of preparing a nanoparticle-containing curable resin system is provided including mixing from 10 to 70 weight percent of aggregated spherical pyrogenic silica nanoparticles with a curable resin to form a mixture. The mixture contains less than 2% by weight solvent and less than 0.5% by weight dispersant based on the nanoparticle weight. The method also includes milling the mixture in an immersion mill containing milling media to form a milled resin system including silica nanoparticles dispersed in the curable resin.