Abstract:
Polyolefin compositions suitable for injection moulded items e.g. for impact bumpers and car interiors comprising from 30% to 90% by weight of an heterophasic propylene polymer composition (A); and from 10% to 70% by weight of a multimodal ethylene/C6-C12 alpha olefin copolymer (B); having density from 0.850 to 0.920 g/cm3, total comonomer content from 6% to 30% by weight, Mw/Mn from 4 to 20; intrinsic viscosity in decalin at 135° C. from 1.0 to 4.0 dL/g, and comprising an HDPE fraction (HDPE % wt) up to 30% wt; further comprising up to 50% by weight of a filler (C) and optionally, in amount up to 10% by weight with respect to the overall composition, an impact modifier masterbatch component (D) consisting of a ultra-soft heterophasic copolymer component.
Abstract:
A filled polyolefin composition made from or containing 20-50 wt. % of an heterophasic polypropylene (a), 10-25 wt. % of a propylene polymer (b) having a MFR (ISO1133 230° C./2.16 Kg) higher than 800 g/10 min., 5-35 wt. % of a propylene polymer (c) having MFR (ISO1133 230° C./2.16 Kg) of 0.5-20 g/10 min. and a tensile modulus (ISO 527-1,-2) equal to or higher than 1000 MPa, 5-35 wt. % of glass fibers (d), and 0-5 wt. % of a compatibilizer (e).
Abstract:
A polyolefin composition made from or containing:
(A) 10-40% by weight of a copolymer of propylene with hexene-1, is made from or containing 1.0-6.0% by weight, based on the weight of (A), of units deriving from hexene-1 and has a melt flow rate (MFRA) measured according to ISO 1133, 230° C., 2.16 kg ranging from 20 to 60 g/10 min.; and (B) 60-90% by weight of a copolymer of propylene with an alpha-olefin of formula CH2═CHR, and optionally a diene, wherein R is H or a linear or branched C2-C8 alkyl and wherein the copolymer is made from or containing 20-35% by weight, based on the total weight of (B), of alpha-olefin,
wherein
the polyolefin composition has an amount of fraction soluble in xylene (XS(tot)) at 25° C. equal to or higher than 65% by weight, and
the amounts of (A), (B), and XS(tot) being based on the total weight of (A)+(B).
Abstract:
A copolymer of propylene with hexene-1 containing from 5 to 9% by weight of recurring units derived from hexene-1, having a melting temperature from 125 to 140° C. and Melt Flow Rate (ASTM D1238, 230/2.16 Kg) from 0.1 to 3 g/10 min., is used to produce blown films having valuable mechanical and optical properties.
Abstract:
A polypropylene composition made from or containing: A) from 50 wt % to 90 wt %; of a propylene homopolymer; B) from 10 wt % to 50 wt %; of a copolymer of propylene having from 30.0 wt % to 70.0 wt %, of ethylene derived units, based upon the total weight of the copolymer; the sum of the amount of component A) and B) being 100; the polypropylene composition having: i) an intrinsic viscosity of the fraction soluble in xylene at 25° C. between 2.2 to 4.0 dl/g; ii) a MFR L (Melt Flow Rate according to ISO 1133, condition L, at 230° C. and 2.16 kg load) from 0.5 to 100 g/10 min; iii) a xylene soluble fraction ranging from 20 wt % to 50 wt %, based upon the total weight of the polypropylene composition; wherein the polypropylene composition being obtained by a polymerization process wherein the catalyst system contains bismuth.
Abstract:
The present disclosure relates to highly filled polyolefin compositions with improved balance of properties particularly for applications where puncture and tear resistance is requested comprising a flexible heterophasic polyolefin composition (I), consisting of a crystalline polymer fraction (A) consisting of a copolymer of propylene with ethylene having a fraction insoluble in xylene at 25° C. of at least 90% by weight, and an elastomeric fraction (B) consisting of a copolymer or blend of copolymers of ethylene with propylene; the copolymer or blend containing units derived from ethylene in a quantity lower than 40% by weight. The fraction soluble in xylene at 25° C. of the polyolefin composition having an IVgpc lower than 2.5 dl/g, a broad molecular weight distribution Mw/Mn (GPC) equal to or higher than 4, and a Mz/Mw (GPC) equal to or higher than 2.5.
Abstract:
Polyolefin compositions suitable for injection molded items e.g. for impact bumpers and car interiors comprising from 30% to 90% by weight of an heterophasic propylene polymer composition (A); and from 10% to 70% by weight of a multimodal ethylene/butene-1 copolymer (B); having density from 0.850 to 0.935 g/cm3, total comonomer content from 6% to 30% by weight, Mw/Mn from 4 to 20; intrinsic viscosity in decalin at 135° C. from 1.0 to 4.0 dL/g, and comprising an HDPE fraction (HDPE % wt) up to 30% wt; further comprising from 0 to 50% by weight of a filler (C) and optionally, in amount up to 10% by weight with respect to the overall composition, an impact modifier masterbatch component D consisting of an ultra-soft heterophasic copolymer component.
Abstract:
A polyolefin composition made from or containing:
A) 5-35% by weight of a propylene ethylene copolymer; B) 20-50% by weight of an ethylene homopolymer; and C) 30-60% by weight of a terpolymer of ethylene, propylene and 1-butene derived units.
Abstract:
The present disclosure relates to a composition comprising: (A) 30-60% by weight of a soft polyolefin composition comprising 10-50% by weight of a copolymer (a) of propylene, which contains from 1-8% by weight of comonomer; 50-90% by weight of a copolymer (b) of ethylene and other alpha-olefin(s) and from 57-80% of ethylene; where the weight ratio of the content of copolymer component (b) to the fraction XS (soluble in xylene) at room temperature (about 25° C.), both (b and XS) referred to the total weight of (a)+(b), is 1.5 or less, and the intrinsic viscosity [η] of the XS fraction is 3 dl/g or more; and the total quantity of copolymerized ethylene is 30-65% by weight; (B) 5-30% of glass fiber filler; (C) 0.5%-3% by weight of a compatibilizer; and (D) 10-40% by weight of a polypropylene component selected from propylene homopolymers, propylene copolymers containing up to 5% by moles of ethylene and/or C4-C10 α-olefin(s) and combinations of such homopolymers and copolymers, with a MFR from 0.3 to 2500 g/10 min.
Abstract:
A filled polyolefin composition made from or containing a blend of a 30-70 wt. % of a first heterophasic polypropylene (HECO1) and 70-30 wt. % of a second heterophasic polypropylene (HECO2), wherein the heterophasic copolymers differ in MFR and type of comonomers, in combination with glass fibers and optionally a compatibilizer.