Abstract:
A polyolefin composition made from or containing (I) 75-95 wt % of a thermoplastic polyolefin made from or containing (A) 18-30 wt % of a propylene copolymer with 1.0-6.0 wt. % of CH2═CHR comonomer, having a melt flow rate (MFR) ranging from 30 to 60 g/10 min; and (B) 70-82 wt % of a propylene copolymer with 20-35 wt. % of CH2═CHR comonomer, and optionally a diene, wherein the thermoplastic polyolefin has i) a xylene soluble fraction equal to or greater than 70 wt. %; and ii) a MFR from 0.2 to 15.0 g/10 min, and (II) 5-25 wt % of a polybutene component, having a flexural modulus equal to or lower than 60 MPa and made from or containing a butene-1 copolymer with ethylene and optionally a comonomer of formula CH2═CHR1, wherein the copolymer having i) up to and including 20 wt % of ethylene-or comonomer-derived units; and ii) Mw/Mn equal to or lower than 3.
Abstract:
A process for producing a polybutene-1 composition including the step of: blending A) from 99.5 to 99.9% by weight, with respect to the total weight of A)+B), of a butene-1 polymer which is brought to a molten state or maintained in a molten state during the blending step; and B) from 0.1 to 0.5% by weight, with respect to the total weight of A)+B), of an alkanoyl hydrazine; wherein the resulting polybutene-1 composition, having a crystallization temperature TcC satisfying the following relation: T c C ≥ T c A + 5 where TcA is the crystallization temperature of the butene-1 polymer A).
Abstract:
A polyolefin composition made from or containing:
A) 5-35% by weight of a propylene homopolymer; B) 20-50% by weight of an ethylene homopolymer; and C) 30-60% by weight of a terpolymer of ethylene, propylene and 1-butene derived units.
Abstract:
A polymer composition made from or containing:
A) from 70 wt % to 95 wt % of a propylene polymer composition made from or containing:
A1) from 15 wt % to 35 wt % of a propylene 1-butene copolymer; and A2) from 65 wt % to 85 wt % of a propylene ethylene 1-butene terpolymer; and
B) from 5.0 wt % to 30.0 wt % of a copolymer of 1-butene and ethylene containing from 3.0 wt % to 4.2 wt % of ethylene derived units, based upon the total weight of the copolymer of 1-butene and ethylene, wherein the sum of the amounts of A) and B) being 100 wt %.
Abstract:
Polyolefin compositions made from or containing:(A) about 5 to about 35% by weight of a propylene-based polymer containing about 90% by weight or more of propylene units and containing about 10% by weight or less of a fraction soluble in xylene at 25° C. (XSA);(B) about 25 to about 50% by weight, of a copolymer of ethylene and a C3-C8 alpha-olefin containing from about 0.1% to about 15% by weight of alpha-olefin units and containing about 75% by weight or less of a fraction soluble in xylene at 25° C. (XSB); and(C) about 30 to about 60% by weight, of a copolymer of ethylene and propylene containing from about 45% to about 75% by weight of ethylene units and containing from about 55% to about 95% by weight, of a fraction soluble in xylene at 25° C. (XSC).
Abstract:
Polyolefin compositions suitable for injection moulded items e.g. for impact bumpers and car interiors comprising from 30% to 90% by weight of an heterophasic propylene polymer composition (A); and from 10% to 70% by weight of a multimodal ethylene/C6-C12 alpha olefin copolymer (B); having density from 0.850 to 0.920 g/cm3, total comonomer content from 6% to 30% by weight, Mw/Mn from 4 to 20; intrinsic viscosity in decalin at 135° C. from 1.0 to 4.0 dL/g, and comprising an HDPE fraction (HDPE % wt) up to 30% wt; further comprising up to 50% by weight of a filler (C) and optionally, in amount up to 10% by weight with respect to the overall composition, an impact modifier masterbatch component (D) consisting of a ultra-soft heterophasic copolymer component.
Abstract:
A propylene polymer composition made from or containing a) from 20 wt % to 44 wt % of a propylene 1-hexene copolymer, containing from 5.0 wt % to 8.3 wt % of 1-hexene derived units, b) from 25 wt % to 45 wt % of a propylene 1-hexene ethylene terpolymer, and c) from 25 wt % to 50 wt % of a propylene ethylene copolymer, wherein the Melt Flow Rate of components a)+b)+c) is from 3.5 to 12.0 g/10 min.
Abstract:
A polyolefin composition made from or containing:
(I) 50-95% by weight of a heterophasic polyolefin composition made from or containing: (A) 10-40% by weight of a propylene polymer selected from the group consisting of propylene homopolymers and copolymers of propylene with an alpha-olefin, having 1.0-6.0% by weight of units deriving from the alpha-olefin, wherein the propylene polymer (A) having a melt flow rate (MFRA) ranging from 20 to 60 g/10 min.; and (B) 60-90% by weight of a copolymer of propylene with an alpha-olefin, having 20-35% by weight of units deriving from the alpha-olefin, wherein the fraction of the heterophasic polyolefin composition (I) soluble in xylene at 25° C. (XS(I)) is equal to or higher than 60% by weight; and (II) 5-50% by weight of a propylene-ethylene copolymer having 12-25% by weight of units deriving from ethylene.
Abstract:
A polyolefin composition made from or containing:
(A) 18-35% by weight of a copolymer of propylene with an alpha-olefin, wherein the copolymer contains 2.0-4.0% by weight of the alpha-olefin and has a melt flow rate (MFRA) ranging from 30 to 60 g/10 min; and (B) 65-82% by weight of a copolymer of propylene with an alpha-olefin, and optionally a diene, wherein the copolymer is made from or containing 20-35% by weight of the alpha-olefin, wherein
the polyolefin composition is made from or containing a fraction that is soluble in xylene at 25° C. (XS(tot)) in an amount higher than 70% by weight; the amounts of (A), (B), and the fraction soluble in xylene at 25° C. (XS(tot)) are based on the total weight of the polyolefin composition; and the melt flow rate (MFR) of the polyolefin composition ranges from 0.2 to 2.0 g/10 min.
Abstract:
Multilayer film (BOPP) structure containing at least: A) a skin (outer) layer substantially consisting of a crystalline low seal Initiation temperature propylene copolymer; B) a tie layer substantially consisting of a butene-1 copolymer having flexural modulus (MEF) of 75 MPa or less; C) a core layer substantially consisting of one or more polypropylene homopolymers designed for BOPP.