MINERAL FILLED POLYPROPYLENE COMPOSITION
    12.
    发明申请
    MINERAL FILLED POLYPROPYLENE COMPOSITION 有权
    矿物填充聚丙烯组合物

    公开(公告)号:US20160319118A1

    公开(公告)日:2016-11-03

    申请号:US15105492

    申请日:2014-12-15

    Abstract: The present disclosure relates to a polypropylene composition for the production of molded articles, such as finished parts for the automotive industry, has melt flow rate (230° C., 2.16 kg) of at least 25 g/10 min and comprising: (A) 50-95% of a composition having an intrinsic viscosity of the fraction soluble in xylene at 25° C. of 3.0-5.0 dl/g; and (A1) 70-95% of a propylene homopolymer having a polydispersity index (PI) of 4.3-10, a fraction insoluble in xylene at 25° C. higher than 90% and an MFR (230° C., 2.16 kg) of 100-250 g/10 min; (A2) 5-30% of a copolymer of propylene with 36-44% of ethylene-derived units; (B) optionally up to 45% of a heterophasic propylene polymer, having an MFR (230° C., 2.16 kg) of 10-25 g/10 min, a flexural modulus higher than 1400 MPa, comprising 5-20% of a copolymer rubber component and 80-95% of a matrix propylene polymer component; (C) 2-10% of an ethylene based elastoplastic copolymer; and (D) optionally up to 20% of talc.

    Abstract translation: 用于生产模制品的聚丙烯组合物,例如用于汽车工业的成品,其熔体流动速率(230℃,2.16Kg)为至少25g / 10min,包括:(A)50-95% 在25℃下可溶于二甲苯的级分的特性粘度为3.0-5.0dl / g的组合物,其组成为:(Al)70-95%的多分散指数(PI)为4.3〜10的丙烯均聚物, 在25℃下不溶于二甲苯的馏分高于90%,MFR(230℃,2.16Kg)为100-250g / 10min; (A2)5-30%丙烯与36-44%乙烯衍生单元的共聚物; (B)任选多达45%的多相丙烯聚合物,MFR(230℃,2.16Kg)为10-25g / 10min,弯曲模量高于1400MPa,并且包含5-20%的共聚物橡胶 组分和80-95%的基质丙烯聚合物组分; (C)2-10%的乙烯基弹性共聚物; 和(D)任选地最多20%的滑石。

    PROPYLENE TERPOLYMER
    13.
    发明申请

    公开(公告)号:US20220033596A1

    公开(公告)日:2022-02-03

    申请号:US17275939

    申请日:2019-09-04

    Abstract: A terpolymer compositions made from or containing: A) From 80 wt % to 97 wt %; of a first propylene, ethylene, 1-butene terpolymer having: i) the content of ethylene derived units ranging from 0.5 wt % to 3.2 wt %; ii) the content of 1-butene derived units ranging from 7.2 wt % to 14.8 wt %; and B) From 20 wt % to 3 wt %; of a second propylene, ethylene, 1-butene terpolymer having: i) the content of ethylene derived units ranging from 0.5 wt % to 3.2 wt %; ii) the content of 1-butene derived units ranging from 14.4 wt % to 26.5 wt %; and the terpolymer composition having the melt flow rate, MFR, measured according to ISO 1133 at 230° C. with a load of 2.16 kg, ranging from 3.0 g/10 min to 20.0 g/10 min; the sum of the amounts of A) and B) being 100 wt %.

    NUCLEATED PROPYLENE POLYMER COMPOSITION
    14.
    发明申请

    公开(公告)号:US20190322850A1

    公开(公告)日:2019-10-24

    申请号:US16341584

    申请日:2017-10-05

    Abstract: A nucleated propylene polymer composition made from or containing: A) a propylene homopolymer; B) a copolymer of propylene with ethylene derived units; the nucleated composition having a fraction soluble in xylene at 25° C. between 9.0 and 21.0 wt %, an intrinsic viscosity of the fraction soluble in xylene at 25° C. between 1.0 and 1.9 dl/g, a total melt flow rate between 1.5 and 5 g/10 min and the value of the relation (I): 22.5+0.2*MFR−1.2*Xs+0.2*IV  (I) is higher than 5.9; wherein MFR is the melt flow rate of the nucleated composition; IV is the intrinsic viscosity of the fraction soluble in xylene at 25° C.; and Xs is the fraction soluble in xylene at 25° C., the amount of A+B is equal to 100 wt %, and the nucleating agent is selected from the group consisting of aromatic or aliphatic carboxylic acids, aromatic metal phosphates, sorbitol derivatives and talc.

    PROPYLENE BASED POLYMER COMPOSITION
    16.
    发明申请

    公开(公告)号:US20180362748A1

    公开(公告)日:2018-12-20

    申请号:US16061258

    申请日:2016-11-22

    Abstract: A propylene polymer composition made from or containing: a) from about 40 wt % to about 80 wt % of a propylene 1-hexene copolymer containing from about 5.5 to about 9.0% by weight, based upon the total weight of the propylene 1-hexene copolymer, of 1-hexene derived units and having a Melt Flow Rate (MFR, measured according to ASTM D 1238 at 230° C., with a load of 2.16 kg) from about 3.5 to about 12.0 g/10 min; and b) from about 20 wt % to about 60 wt % of a propylene ethylene copolymer containing from about 1.5 wt % to about 6.5 wt % based upon the total weight of the propylene ethylene copolymer, of ethylene derived units, and having a Melt Flow Rate (MFR, measured according to ASTM D 1238, at 230° C., with a load of 2.16 kg) from about 3.5 to about 12.0 g/10 min; the sum of a) and b) being 100.

    COMPOSITION COMPRISING PROPYLENE-ETHYLENE-1-BUTENE TERPOLYMERS

    公开(公告)号:US20180237623A1

    公开(公告)日:2018-08-23

    申请号:US15750772

    申请日:2016-07-19

    Abstract: A polyolefin composition made from or containing: A) from 19 wt % to 50 wt % of a propylene ethylene copolymer having an ethylene derived units content ranging from 1.5 wt % to 6.0 wt; B) from 50 wt % to 81 wt % of a propylene ethylene 1-butene terpolymer having an ethylene derived units content ranging from 1.5 wt % and 6.0 wt % and 1-butene derived units content of between 4.8 wt % and 12.4 wt %; wherein the ratio C2 wt %/C4 wt % is between 0.22 and 3.0, where C2 wt % is the weight percent of ethylene derived units and C4 wt % is the weight percent of 1-butene derived units; the content of xylene soluble fraction at 25° C. is between 2 and 15 wt %; molecular weight distribution (MWD), expressed in terms of Mw/Mn, greater than 4.0; recoverable compliance at 200° C. having a maximum value between 800 and 1200 seconds, lower than 65×10−5 Pa−1.

    BOPP MULTILAYER FILM
    19.
    发明申请

    公开(公告)号:US20220032593A1

    公开(公告)日:2022-02-03

    申请号:US17311076

    申请日:2019-11-18

    Abstract: A BOPP multilayer film having at least three layers made from or containing a nucleated propylene polymer composition having: A) from 77 wt % to 91 wt %, of a propylene homopolymer having a fraction insoluble in xylene at 25° C. higher than 95%; B) from 9 wt % to 23 wt %, of a copolymer of propylene with from 28.0 wt % to 42.0 wt % of ethylene derived units; and C) a nucleating agent selected from aromatic or aliphatic carboxylic acids, aromatic metal phosphates, sorbitol derivatives and talc, wherein the composition has an intrinsic viscosity (IV) of the fraction soluble in xylene at 25° C. between 1.0 dl/g and 1.9 dl/g, a fraction soluble (Xs) in xylene at 25° C. between 9.0 wt % and 21.0 wt %, a total melt flow rate (MFR) between 1.5 and 5 g/10 min and the value of the relation (I): 22.5+0.2*MFR−1.2*Xs+0.2*IV  (I) higher than 5.9.

    HEAT-SHRINKABLE LABEL
    20.
    发明申请

    公开(公告)号:US20200255609A1

    公开(公告)日:2020-08-13

    申请号:US16758763

    申请日:2018-10-31

    Abstract: A heat-shrinkable label made from or containing a terpolymer film containing propylene, ethylene and 1-hexene, wherein the terpolymer has: (i) a content of ethylene derived units ranging from 0.5 wt % to 5.0 wt %, (ii) a content of 1-hexene derived units ranging from 1.0 wt % to 6.0 wt %, (iii) a melt flow rate (MFR) (ISO 1133 230° C., 2.16 kg) ranging from 0.5 to 20 g/10 min, and (iv) a polydispersity index (P.I.) ranging from 2.0 to 7.0.