Propylene based polymer composition

    公开(公告)号:US11124636B2

    公开(公告)日:2021-09-21

    申请号:US16610332

    申请日:2018-04-12

    Abstract: A propylene polymer composition made from or containing: a) from 35 wt % to 65 wt %, based upon the total weight of the propylene polymer composition, of a propylene 1-hexene copolymer containing from 10.2 to 13.0% by weight, based upon the weight of the propylene 1-hexene copolymer, of 1-hexene derived units and having a Melt Flow Rate (MFR, measured according to ASTM D 1238, 230° C./2.16 kg, (at 230° C., with a load of 2.16 kg)) from 3.5 to 12.0 g/10 min; b) from 35 wt % to 65 wt %, based upon the total weight of the propylene polymer composition, of a propylene ethylene copolymer containing from 1.5 wt % to 6.5 wt %, based upon the weight of the propylene ethylene copolymer, of ethylene derived units and having a Melt Flow Rate (MFR, measured according to ASTM D 1238, 230° C./2.16 kg, (at 230° C., with a load of 2.16 kg)) from 3.5 to 12.0 g/10 min.

    Propylene polymer compositions
    15.
    发明授权
    Propylene polymer compositions 有权
    丙烯聚合物组合物

    公开(公告)号:US09181424B2

    公开(公告)日:2015-11-10

    申请号:US14349711

    申请日:2012-10-05

    Abstract: Propylene polymer compositions comprising: A) from 70 wt % to 95 wt %, of a random copolymer of propylene with ethylene, containing from 1.5 wt % to 4.5 wt %, of ethylene derived units, having a content of fraction insoluble in xylene at 25° C. of not less than 93%; B) from 5 wt % to 35 wt %, of a copolymer of propylene with ethylene, containing from 7.0 wt % to 17.0 wt % of ethylene derived units; the sum A+B being 100; wherein the melt flow rate, MFR. (Melt Flow Rate according to ASTM 1238, condition L, i.e. 230° C. and 2.16 kg load) ranges from 40 g/10 min and 130 g/10 min; and wherein the relation (I) is fulfilled: 10

    Abstract translation: 丙烯聚合物组合物,其包含:A)70重量%至95重量%的丙烯与乙烯的无规共聚物,其含有1.5重量%至4.5重量%的乙烯衍生单元,其含量在25℃不溶于二甲苯 ℃不低于93%; B)5重量%至35重量%的丙烯与乙烯的共聚物,其含有7.0重量%至17.0重量%的乙烯衍生单元; 总和A + B为100; 其中熔体流动速率MFR。 (根据ASTM 1238的熔体流动速率,条件L,即230℃和2.16kg负荷)为40g / 10min和130g / 10min; 并且其中满足关系式(I):10

    POLYPROPYLENE FIBER
    16.
    发明申请
    POLYPROPYLENE FIBER 审中-公开
    聚丙烯纤维

    公开(公告)号:US20150191852A1

    公开(公告)日:2015-07-09

    申请号:US14408023

    申请日:2013-06-13

    Abstract: Fibers comprising a polypropylene obtainable by a process comprising the steps of: (i) polymerizing propylene in the presence of a catalyst system comprising the product obtained by contacting the following components: (a) a solid catalyst component comprising a magnesium halide, a titanium compound having at least a Ti-halogen bond and at least two electron donor compounds one of which being present in an amount from 40 to 90% by mol with respect to the total amount of donors and selected from succinates and the other being selected from 1,3 diethers, (b) an aluminum hydrocarbyl compound, and (c) optionally an external electron donor compound, to obtain a polypropylene precursor having a melt flow rate MFR1; (ii) subjecting the thus-obtained polypropylene precursor to visbreaking to obtain a visbroken polypropylene having a melt flow rate MFR2; (iii) spinning the visbroken polypropylene obtained in the previous step; wherein MFR2 is comprised between from 15 to 40 g/10 min, the ratio MFR2/MFR1 is comprised between 8 and 18, both MFR1 and MFR2 being measured according to ISO method 1133 (230° C., 2.16 kg).

    Abstract translation: 包含聚丙烯的纤维包括以下步骤:(i)在催化剂体系存在下聚合丙烯,所述催化剂体系包含通过使以下组分接触获得的产物:(a)固体催化剂组分,其包含卤化镁,钛化合物 具有至少一个Ti-卤素键和至少两个电子给体化合物,其中一种以相对于供体总量为40-90%摩尔量存在,选自琥珀酸盐,另一种选自1, 3个二醚,(b)铝烃基化合物和(c)任选的外电子给体化合物,得到熔体流动速率MFR 1的聚丙烯前体; (ii)将由此获得的聚丙烯前体进行减粘裂化以得到熔体流动速率MFR 2的减粘裂化聚丙烯; (iii)纺丝上一步获得的耐磨破坏聚丙烯; 其中MFR 2在15至40g / 10min之间,MFR 2 / MFR 1的比率在8和18之间,MFR 1和MFR 2均根据ISO方法1133(230℃,2.16kg)测量。