公开(公告)号:AT343646T
公开(公告)日:2006-11-15
申请号:AT02764807
申请日:2002-07-30
Applicant: BASF AG
Inventor: BARTL JUERGEN , GRITTMANN ERNST-JUERGEN , GUENTHER ERHARD , GERKE HEINZ-UDO , KLENZ RAINER
Abstract: A laminate including a decorative material (A), a layer of cellular polyisocyanate/polyaddition elastomer (B) giving an outstanding Soft-Touch-Effect to a decorative, e.g. leather surface, combined with excellent residual elasticity is new. A composite structural unit (sic) including a decorative material (A), a layer of cellular polyisocyanate/polyaddition elastomer (CPIE) (B) of residual pressure deformation (sic) of 25% in accordance with DIN 53572, using a 40x40x30 mm test body without a silicone coating, with testing at constant deformation, where the test body is 40% compressed and held in a recirculated air facility (sic) for 22 hours at 80 deg C, after withdrawal from the facility the test device is held for 2 hours in the compressed state, cooled to room temperature, and the test body is withdrawn from the test device, and 10 minutes 30 seconds after withdrawal the height of the test body is measured to 0.1 mm accuracy, and a layer of back sprayed (sic) thermoplastic C. An Independent claim is also included for preparation of the laminate involving placing the material A in a tool mold (sic) with material A on both sides of the tool wall, using a cellular polyisocyanate/polyaddition elastomer (CPIE) (B) of residual pressure deformation (sic) of 25% in accordance with DIN 53572, and a 40x40x30 mm test body without a silicone coating as described above, with final measurement of the height of the test body to an accuracy of 0.1 mm.
-
公开(公告)号:AT280035T
公开(公告)日:2004-11-15
申请号:AT01943251
申请日:2001-04-17
Applicant: BASF AG
Inventor: ROESCH JOACHIM , HUEFFER STEPHAN , IGL GEORG , BARTL JUERGEN , TAEGER TILMAN LUEDECKE , KLENZ RAINER , GINSS CHRISTOPHE , GUENTHER ERHARD , LIESE MICHAELA
IPC: B32B37/10 , B29C45/14 , B29C45/16 , B29C70/68 , B32B5/18 , B32B7/04 , B32B9/02 , B32B37/15 , D06N7/04 , B32B31/10 , B32B31/30 , B29K711/08
Abstract: The invention relates to a process for the production of a multilayered composite element which comprises a layer of leather, a layer of a hard component formed from a polymer, which is bonded to the leather layer in certain areas, and a layer of a soft component, which is arranged between the leather component and the hard component, which comprises laying the leather against one mold surface of a mold, positioning the soft component on the leather, and molding the polymer acting as hard component onto the leather layer and the soft component layer at a pressure of at least 50 bar, preferably greater than 100 bar, in particular greater than 180 bar, and at a temperature of greater than 100° C., preferably from 180 to 280° C., in particular from 200 to 250° C., by bonding the leather and the hard component to one another in certain areas at least, with temperature of the mold surface of the mold being controlled, at least during the bonding. The invention furthermore relates to a composite element obtainable by the process. The composite element is extremely robust, has a soft touch surface and is inexpensive to produce.
-
公开(公告)号:AT246591T
公开(公告)日:2003-08-15
申请号:AT00979509
申请日:2000-10-25
Applicant: BASF AG
Inventor: HUEFFER STEPHAN , ROESCH JOACHIM , IGL GEORG , BARTL JUERGEN , HOMES ANGELIKA
IPC: B60R13/02 , B29C43/20 , B29C44/14 , B29C45/14 , B29C45/73 , B29C45/78 , B29C47/02 , B29C70/68 , B29K101/12 , B29K105/04 , B29L9/00 , B32B7/04 , B32B9/02 , B32B37/15 , C14B7/04 , D06N3/00 , B32B31/30 , B29K711/08
Abstract: The invention relates to a method for producing a three-dimensional molded part that comprises a carrier produced from a thermoplastic polymer and a leather layer applied on said carrier. Said leather and said thermoplastic polymer are linked by means of a tool that has a molding surface on which the leather comes to rest at a pressure of at least 50 bar, preferably of more than 100 bar, especially more than 180 bar, and at a temperature of more than 100 DEG C, preferably 180 to 280 DEG C, especially 200 to 250 DEG C, with the molding surface of the tool that rests against the leather being tempered. The invention provides a method for intimately linking the carrier and the leather layer. The molded articles produced by the inventive method have a substantially improved resistance to the effects of temperature or moisture variations.
-
公开(公告)号:DE10019605A1
公开(公告)日:2001-10-25
申请号:DE10019605
申请日:2000-04-20
Applicant: BASF AG
Inventor: ROESCH JOACHIM , HUEFFER STEPHAN , IGL GEORG , BARTL JUERGEN , TAEGER TILMANN
IPC: B32B37/10 , B29C45/14 , B29C45/16 , B29C70/68 , B32B5/18 , B32B7/04 , B32B9/02 , B32B37/15 , D06N7/04 , B32B31/20 , B29C44/12 , D06N3/00 , C14B7/02
Abstract: Die Erfindung betrifft ein Verfahren zur Herstellung eines mehrschichtigen Verbundkörpers, welcher eine Schicht aus Leder umfasst, eine abschnittsweise mit der Schicht aus Leder verbundene Schicht einer aus einem Polymeren gebildeten Hartkomponente, sowie einer zwischen Leder- und Hartkomponente angeordneten Schicht aus einer Weichkomponente, dadurch gekennzeichnet, das das Leder an einer Formfläche eines Werkzeugs angelegt wird, auf dem Leder die Weichkomponente positioniert wird und das als Hartkomponente wirkende Polymere bei einem Druck von mindestens 50 bar, vorzugsweise mehr als 100 bar, insbesondere mehr als 180 bar, und einer Temperatur von mehr als 100 DEG C, vorzugsweise 180 bis 280 DEG C, insbesondere 200 bis 250 DEG C, auf die Schicht aus Leder und die Schicht der Weichkomponente aufgeformt wird, in der Weise, daß das Leder und die Hartkomponente zumindest abschnittsweise miteinander verbunden werden, wobei während des Aufformens der Hartkomponente die Formfläche des Werkzeugs temperiert wird. DOLLAR A Ferner betrifft die Erfindung einen mit dem Verfahren erhältlichen Verbundkörper. Der Verbundkörper ist äußerst robust, weist eine Oberfläche mit einem "soft touch" auf und ist kostengünstig herzustellen.
-
-
-