公开(公告)号:DE3733342A1
公开(公告)日:1989-04-13
申请号:DE3733342
申请日:1987-10-02
Applicant: BASF AG
Inventor: HOENL HANS DR , JENNE HELMUT DR , MATERN RUEDIGER
-
公开(公告)号:DE3732176A1
公开(公告)日:1989-04-06
申请号:DE3732176
申请日:1987-09-24
Applicant: BASF AG
Inventor: HOENL HANS DR
IPC: C08F287/00 , C08K3/04 , C08L25/06 , C08L53/02 , H01B1/24
Abstract: The invention relates to an electroconductive thermoplastic moulding composition containing, in each case based on the moulding composition comprising A + B + C, A from 96 to 60% by weight of at least one polymer containing styrene and/or substituted styrene, B from 2 to 20% by weight of at least one linear block copolymer containing hydrogenated styrene and butadiene, whose total styrene content, based on B, is in the range from 40 to 60% by weight, where from 5 to 25% by weight of the block copolymer is in the form of block polystyrene and the remainder of the styrene is incorporated randomly in from 60 to 40% by weight of hydrogenated butadiene, and where the block copolymer C has a mean molecular weight (weight average) of from 50,000 to 200,000 and furthermore containing C from 2 to 20% by weight of electroconductive black. The moulding composition is used for the production of mouldings.
-
公开(公告)号:DE3620008A1
公开(公告)日:1987-12-17
申请号:DE3620008
申请日:1986-06-13
Applicant: BASF AG
Inventor: HOENL HANS DR , MITTNACHT HANS DR
-
公开(公告)号:DE3365349D1
公开(公告)日:1986-09-18
申请号:DE3365349
申请日:1983-12-02
Applicant: BASF AG
Inventor: HOENL HANS DR
IPC: C08F279/02
-
公开(公告)号:DE3425457A1
公开(公告)日:1986-01-23
申请号:DE3425457
申请日:1984-07-11
Applicant: BASF AG
Inventor: HOENL HANS DR , ECHTE ADOLF DR
Abstract: The invention relates to a moulding composition containing a hard matrix A essentially comprising a polymer of a vinylaromatic monomer in a proportion of from 70 to 95 % by weight, based on the moulding composition of A+B, and a soft phase B, distributed therein, in a proportion of from 5 to 30 % by weight, based on the moulding composition of A+B, which has a mean particle size in the range from 0.1 to 1.5 mu m (number average). The soft phase is a graft copolymer comprising the vinylaromatic monomer of the polymer building up the hard matrix and an elastomeric styrene-butadiene two-block copolymer. The vinylaromatic monomer for building up the hard matrix A comprises ring-alkylated styrenes such that the soft phase B contains more than 70% (number average) of shell particles.
-
公开(公告)号:DE19624827A1
公开(公告)日:1998-01-02
申请号:DE19624827
申请日:1996-06-21
Applicant: BASF AG
-
公开(公告)号:DE3787191D1
公开(公告)日:1993-10-07
申请号:DE3787191
申请日:1987-03-31
Applicant: BASF AG
Inventor: BRONSTERT KLAUS DR , HOENL HANS DR , ECHTE ADOLF DR , KLAERNER PETER DR
IPC: C08F2/16 , C08F2/38 , C08F279/02 , C08F285/00
Abstract: Translucent polystyrene which has been impact-modified using rubber is prepared by polymerising styrene compounds in the presence of a rubber containing thiol groups.
-
公开(公告)号:DE3778683D1
公开(公告)日:1992-06-04
申请号:DE3778683
申请日:1987-02-09
Applicant: BASF AG
Inventor: HOENL HANS DR
Abstract: Thermoplastic moulding compsns. (I) comprises, on (A)+(B) (1) (A) 50-95 wt.% resin matrix formed, calculated on (A), from (a1) 98-50 wt.% styrene, (a2) 2-50 wt.% acrylonitrile, (B) 50-5 wt.% soft phase, evenly distributed in the resin matrix, comprising graft copolymer from (a1), (a2) and a styrene-butadiene block copolymer (II) of 50-95 wt.% styrene and 50-5 wt.% butadiene on (II) having wt. ave. mol. wt. 50,000-300000 (also given as 50,000-400000); or (2) (A) 60-90 wt.% resin matrix formed from (a1) 95-70 wt.% styrene, (a2) 5-30 wt.% acrylonitrile, (B) 40-10 wt.% soft phase, distributed as in (1), comprising a graft copolymer from (a1), (a2) and (II) of 55-90 wt.% styrene and 45-10 wt.% butadiene, wt.-ave. mol. wt. of the (II) being 50,000-400,000; or (3) (A) 60-90 wt.% resin matrix formed from (a1) 90-70 wt.% styrene, (a2) 10-30 wt.% acrylonitrile; (B) 40-10 wt.% soft phase, distributed as in (1), comprising a graft copolymer from (a1), (a2) and 60-85 wt.% styrene and 40-15 wt.% butadiene, wt.-ave. mol. wt. of the (II) being 50,000-400,000 or (4) (A) 60-90 wt.% resin matrix formed from (a1) 85-70 wt.% styrene, (a2) 15-30 wt.% acrylonitrile, (B) 40-10 wt.% soft phase, distributed as in (1) comprising graft copolymer from (a1) (a2) and (II) as in (3). Pref. (I) consist of (A) and (B).
-
公开(公告)号:DE3821886A1
公开(公告)日:1990-02-08
申请号:DE3821886
申请日:1988-06-29
Applicant: BASF AG
Inventor: HOENL HANS DR , KRESS GERHARD DR
IPC: C08K3/08 , C08J3/20 , C08J3/22 , C08K3/02 , C08K7/06 , C08L101/00 , G21F1/10 , H01B1/22 , H01R13/658 , H05K9/00
Abstract: Mouldings containing electroconductive fillers or fillers which attenuate in electromagnetic radiation and containing fillers which are not homogeneously distributed, and process for their preparation by moulding granule mixtures.
-
公开(公告)号:DE3804544A1
公开(公告)日:1989-08-24
申请号:DE3804544
申请日:1988-02-13
Applicant: BASF AG
Inventor: HOENL HANS DR , MUELLER WOLFGANG F DR , JENNE HELMUT DR , MOEDERSHEIM NORBERT
-
-
-
-
-
-
-
-
-