11.
公开(公告)号:HUT70710A
公开(公告)日:1995-10-30
申请号:HU9403461
申请日:1993-05-26
Applicant: BASF AG
Inventor: ALICKE GERHARD , WEILBACHER MANFRED , WOLFF BERNARDO , HEINEN HARTMUT , DIETZEN FRANZ-JOSEF , WEBER REINHOLD , HAHN MANFRED
Abstract: PCT No. PCT/EP93/01320 Sec. 371 Date Nov. 22, 1994 Sec. 102(e) Date Nov. 22, 1994 PCT Filed May 26, 1993 PCT Pub. No. WO93/24560 PCT Pub. Date Dec. 9, 1993.Process for the production of foam boards having a minimum thickness of 20 mm and a cross-sectional area of at least 50 cm2 by extruding a mixture of the styrene polymer, from 1 to 10% by weight, based on the styrene polymer, of a blowing agent, wherein the blowing agent contains at least one ether from the group consisting of dimethyl ether, methyl ethyl ether and methyl vinyl ether.
-
12.
公开(公告)号:HU9403461D0
公开(公告)日:1995-03-28
申请号:HU9403461
申请日:1993-05-26
Applicant: BASF AG
Inventor: ALICKE GERHARD , WEILBACHER MANFRED , WOLFF BERNARDO , HEINEN HARTMUT , DIETZEN FRANZ-JOSEF , WEBER REINHOLD , HAHN MANFRED
Abstract: PCT No. PCT/EP93/01320 Sec. 371 Date Nov. 22, 1994 Sec. 102(e) Date Nov. 22, 1994 PCT Filed May 26, 1993 PCT Pub. No. WO93/24560 PCT Pub. Date Dec. 9, 1993.Process for the production of foam boards having a minimum thickness of 20 mm and a cross-sectional area of at least 50 cm2 by extruding a mixture of the styrene polymer, from 1 to 10% by weight, based on the styrene polymer, of a blowing agent, wherein the blowing agent contains at least one ether from the group consisting of dimethyl ether, methyl ethyl ether and methyl vinyl ether.
-
公开(公告)号:NO309194B1
公开(公告)日:2000-12-27
申请号:NO954782
申请日:1995-11-24
Applicant: BASF AG
Inventor: CALLENS JULIEN N R , BIESEN ALFONS J S VAN , WOLFF BERNARDO , ALICKE GERHARD , WEBER REINHOLD , DIETZEN FRANZ-JOSEF , HAHN KLAUS
IPC: C08J9/12
Abstract: PCT No. PCT/EP94/01631 Sec. 371 Date Nov. 21, 1995 Sec. 102(e) Date Nov. 21, 1995 PCT Filed May 20, 1994 PCT Pub. No. WO94/28058 PCT Pub. Date Dec. 8, 1994Extruded foam boards produced using halogen-free blowing agents from a styrene polymer thermoplastic matrix having a Vicat softening temperature VST B 50 of at most 100 DEG and a melt index MVI 200/5 of at least 5 ml/10 min are at least 20 mm, preferably more than 50 mm and in particular from 80 to 200 mm, thick. Preferred blowing agents for producing the foam boards are carbon dioxide alone, as well as mixtures of carbon dioxide and ethanol and/or dimethyl ether.
-
公开(公告)号:ES2114198T3
公开(公告)日:1998-05-16
申请号:ES94916977
申请日:1994-05-20
Applicant: BASF AG
Inventor: CALLENS JULIEN N R , VAN BIESEN ALFONS J S , WOLFF BERNARDO , ALICKE GERHARD , WEBER REINHOLD , DIETZEN FRANZ-JOSEF
IPC: C08J9/12
Abstract: PCT No. PCT/EP94/01631 Sec. 371 Date Nov. 21, 1995 Sec. 102(e) Date Nov. 21, 1995 PCT Filed May 20, 1994 PCT Pub. No. WO94/28058 PCT Pub. Date Dec. 8, 1994Extruded foam boards produced using halogen-free blowing agents from a styrene polymer thermoplastic matrix having a Vicat softening temperature VST B 50 of at most 100 DEG and a melt index MVI 200/5 of at least 5 ml/10 min are at least 20 mm, preferably more than 50 mm and in particular from 80 to 200 mm, thick. Preferred blowing agents for producing the foam boards are carbon dioxide alone, as well as mixtures of carbon dioxide and ethanol and/or dimethyl ether.
-
公开(公告)号:DE59405594D1
公开(公告)日:1998-05-07
申请号:DE59405594
申请日:1994-05-20
Applicant: BASF AG
Inventor: CALLENS JULIEN , VAN BIESEN ALFONS , WOLFF BERNARDO , ALICKE GERHARD , WEBER REINHOLD , DIETZEN FRANZ-JOSEF , HAHN KLAUS
IPC: C08J9/12
Abstract: PCT No. PCT/EP94/01631 Sec. 371 Date Nov. 21, 1995 Sec. 102(e) Date Nov. 21, 1995 PCT Filed May 20, 1994 PCT Pub. No. WO94/28058 PCT Pub. Date Dec. 8, 1994Extruded foam boards produced using halogen-free blowing agents from a styrene polymer thermoplastic matrix having a Vicat softening temperature VST B 50 of at most 100 DEG and a melt index MVI 200/5 of at least 5 ml/10 min are at least 20 mm, preferably more than 50 mm and in particular from 80 to 200 mm, thick. Preferred blowing agents for producing the foam boards are carbon dioxide alone, as well as mixtures of carbon dioxide and ethanol and/or dimethyl ether.
-
公开(公告)号:AT164607T
公开(公告)日:1998-04-15
申请号:AT94916977
申请日:1994-05-20
Applicant: BASF AG
Inventor: CALLENS JULIEN N R , VAN BIESEN ALFONS J S , WOLFF BERNARDO , ALICKE GERHARD , WEBER REINHOLD , DIETZEN FRANZ-JOSEF , HAHN KLAUS
Abstract: PCT No. PCT/EP94/01631 Sec. 371 Date Nov. 21, 1995 Sec. 102(e) Date Nov. 21, 1995 PCT Filed May 20, 1994 PCT Pub. No. WO94/28058 PCT Pub. Date Dec. 8, 1994Extruded foam boards produced using halogen-free blowing agents from a styrene polymer thermoplastic matrix having a Vicat softening temperature VST B 50 of at most 100 DEG and a melt index MVI 200/5 of at least 5 ml/10 min are at least 20 mm, preferably more than 50 mm and in particular from 80 to 200 mm, thick. Preferred blowing agents for producing the foam boards are carbon dioxide alone, as well as mixtures of carbon dioxide and ethanol and/or dimethyl ether.
-
公开(公告)号:PL171701B1
公开(公告)日:1997-06-30
申请号:PL30641193
申请日:1993-05-26
Applicant: BASF AG
Inventor: ALICKE GERHARD , WEILBACHER MANFRED , WOLFF BERNARDO , HEINEN HARTMUT , DIETZEN FRANZ-JOSEF , WEBER REINHOLD , HAHN MANFRED
Abstract: PCT No. PCT/EP93/01320 Sec. 371 Date Nov. 22, 1994 Sec. 102(e) Date Nov. 22, 1994 PCT Filed May 26, 1993 PCT Pub. No. WO93/24560 PCT Pub. Date Dec. 9, 1993.Process for the production of foam boards having a minimum thickness of 20 mm and a cross-sectional area of at least 50 cm2 by extruding a mixture of the styrene polymer, from 1 to 10% by weight, based on the styrene polymer, of a blowing agent, wherein the blowing agent contains at least one ether from the group consisting of dimethyl ether, methyl ethyl ether and methyl vinyl ether.
-
公开(公告)号:FI107051B
公开(公告)日:2001-05-31
申请号:FI955641
申请日:1995-11-23
Applicant: BASF AG
Inventor: CALLENS JULIEN N R , VAN BIESEN ALFONS J S , WOLFF BERNARDO , ALICKE GERHARD , WEBER REINHOLD , DIETZEN FRANZ-JOSEF , HAHN KLAUS
IPC: C08J9/12
Abstract: PCT No. PCT/EP94/01631 Sec. 371 Date Nov. 21, 1995 Sec. 102(e) Date Nov. 21, 1995 PCT Filed May 20, 1994 PCT Pub. No. WO94/28058 PCT Pub. Date Dec. 8, 1994Extruded foam boards produced using halogen-free blowing agents from a styrene polymer thermoplastic matrix having a Vicat softening temperature VST B 50 of at most 100 DEG and a melt index MVI 200/5 of at least 5 ml/10 min are at least 20 mm, preferably more than 50 mm and in particular from 80 to 200 mm, thick. Preferred blowing agents for producing the foam boards are carbon dioxide alone, as well as mixtures of carbon dioxide and ethanol and/or dimethyl ether.
-
公开(公告)号:PL175478B1
公开(公告)日:1999-01-29
申请号:PL31175394
申请日:1994-05-20
Applicant: BASF AG
Inventor: CALLENS JULIEN N R , VAN BIESEN ALFONS J S , WOLFF BERNARDO , ALICKE GERHARD , WEBER REINHOLD , DIETZEN FRANZ-JOSEF , HAHN KLAUS
Abstract: PCT No. PCT/EP94/01631 Sec. 371 Date Nov. 21, 1995 Sec. 102(e) Date Nov. 21, 1995 PCT Filed May 20, 1994 PCT Pub. No. WO94/28058 PCT Pub. Date Dec. 8, 1994Extruded foam boards produced using halogen-free blowing agents from a styrene polymer thermoplastic matrix having a Vicat softening temperature VST B 50 of at most 100 DEG and a melt index MVI 200/5 of at least 5 ml/10 min are at least 20 mm, preferably more than 50 mm and in particular from 80 to 200 mm, thick. Preferred blowing agents for producing the foam boards are carbon dioxide alone, as well as mixtures of carbon dioxide and ethanol and/or dimethyl ether.
-
20.
公开(公告)号:HU213640B
公开(公告)日:1997-08-28
申请号:HU9503364
申请日:1994-05-20
Applicant: BASF AG
Inventor: ALICKE GERHARD , BIESEN ALFONS J S , CALLENS JULIEN N R , DIETZEN FRANZ-JOSEF , HAHN KLAUS , WEBER REINHOLD , WOLFF BERNARDO
Abstract: PCT No. PCT/EP94/01631 Sec. 371 Date Nov. 21, 1995 Sec. 102(e) Date Nov. 21, 1995 PCT Filed May 20, 1994 PCT Pub. No. WO94/28058 PCT Pub. Date Dec. 8, 1994Extruded foam boards produced using halogen-free blowing agents from a styrene polymer thermoplastic matrix having a Vicat softening temperature VST B 50 of at most 100 DEG and a melt index MVI 200/5 of at least 5 ml/10 min are at least 20 mm, preferably more than 50 mm and in particular from 80 to 200 mm, thick. Preferred blowing agents for producing the foam boards are carbon dioxide alone, as well as mixtures of carbon dioxide and ethanol and/or dimethyl ether.
-
-
-
-
-
-
-
-
-