Method for producing polyurethane foam
    13.
    发明专利
    Method for producing polyurethane foam 审中-公开
    生产聚氨酯泡沫的方法

    公开(公告)号:JP2007191679A

    公开(公告)日:2007-08-02

    申请号:JP2006167722

    申请日:2006-06-16

    Abstract: PROBLEM TO BE SOLVED: To provide a method for producing a polyurethane foam having high foam strength and low rebound resilience.
    SOLUTION: The polyurethane foam having density of 0.1 g/cm
    3 or more contains a polyol A, which is a polyester-polyol having a hydroxyl value of 45-115 mg KOH/g and being obtained by polycondensing a polyhydric alcohol component containing a polyhydric alcohol having a side chain and a polybasic acid component, and polyol B, which is a polyether-polyol having 3 functional groups and a hydroxyl value of 15-40 mg KOH/g. The method of producing the polyurethane foam comprises reacting a polyol component, in which the weight ratio of polyol A to polyol B is 1.2-3, with a polyisocyanate component.
    COPYRIGHT: (C)2007,JPO&INPIT

    Abstract translation: 解决的问题:提供具有高泡沫强度和低回弹性的聚氨酯泡沫塑料的制造方法。 < P>解决方案:密度为0.1g / cm 3以上的聚氨酯泡沫体含有多元醇A,其为羟值为45〜115mg KOH / g的聚酯多元醇,为 通过缩聚含有侧链和多元酸组分的多元醇的多元醇组分和作为具有3个官能团和羟值为15-40mg KOH / g的聚醚多元醇的多元醇B获得的。 制备聚氨酯泡沫的方法包括使多元醇组分(其中多元醇A与多元醇B的重量比为1.2-3)与多异氰酸酯组分反应。 版权所有(C)2007,JPO&INPIT

    Foam
    14.
    发明专利
    Foam 审中-公开

    公开(公告)号:JP2004169017A

    公开(公告)日:2004-06-17

    申请号:JP2003368799

    申请日:2003-10-29

    Inventor: SAWAI MINORU

    Abstract: PROBLEM TO BE SOLVED: To provide a foam with sufficient strength and simultaneously having moderate elasticity and high rebound resilience. SOLUTION: The foam with a storage modulus of 1.7-2.5 MPa obtained from dynamic viscoelasticity at 25°C and 10 Hz frequency, and tanδ of 0.01-0.14, a member of shoe sole made of the foam and the shoe sole having the foam with rebound resilience of 36-80%. The foam exhibits wear-out amount of 100 mg or less in DIN wear test under conditions of pressing force of 7.5 N of a disk form test piece of 18 cm diameter and 10 mm thickness to an abrasive cloth, and 100% modulus of 1.2 MPa and a polyurethane foam is manufactured by a reaction of a polyol component and a isocyanate compound. COPYRIGHT: (C)2004,JPO

    Foam
    15.
    发明专利
    Foam 审中-公开

    公开(公告)号:JP2004161987A

    公开(公告)日:2004-06-10

    申请号:JP2003110573

    申请日:2003-04-15

    Inventor: SAWAI MINORU

    Abstract: PROBLEM TO BE SOLVED: To provide foam having sufficient strength and having soft and good touch and low impact resilience at the same time. SOLUTION: In the foam, the density is ≥0.1 g/cm 3 and the glass transition point is one and the glass transition point exists in a temperature range of -20 to 60°C and the storage elastic modulus (E') obtained from dynamic viscoelasticity at 10 Hz frequency and 25°C is 0.5-2 MPa and tan δ is 0.16-0.5. The member for shoe sole is composed of the foam. The shoe sole has the foam. The shoes have the shoe soles. COPYRIGHT: (C)2004,JPO

    DEINKING
    16.
    发明专利
    DEINKING 失效

    公开(公告)号:JPH10298883A

    公开(公告)日:1998-11-10

    申请号:JP10312897

    申请日:1997-04-21

    Applicant: KAO CORP

    Abstract: PROBLEM TO BE SOLVED: To obtain a high-quality reclaimed pulp and enable improvement of circulation ratio of white water by using a specific alkylene oxide adduct of a higher alcohol or a higher fatty acid (ester) as a deinking agent. SOLUTION: Ink is released from waste paper in the presence of one or more kinds of deinking agents selected from a group of the formula R1 O(AO)p H [R1 is a 14-24C alkyl or alkenyl or 8-14C alkyl or alkylpheyl; AO represents an oxyethylene (EO) and an oxypropylene (PO) and EO average addition mole number is 20-300 and EO/PO addition mole ratio is 1-7; (p) is a number satisfying the above relationship in EO and PO] or the formula R2 [COO(AO)m R3 ]n [(n) is an integer of >=1; R2 is a residue obtained by eliminating all COOH from a 14-24C carboxylic acid; R3 is H or a 1-20C alkyl or alkenyl; AO is EO and PO and EO average addition mole number is the same mole number as the above and EO/PO addition mole ratio is the same mole ratio as the above; (m) is a number satisfying the above relationship in EO and PO) and then, pulp is washed at 40-80 deg.C.

    Method for producing pigment dispersion for color filter
    17.
    发明专利
    Method for producing pigment dispersion for color filter 审中-公开
    生产彩色滤光片色素分散液的方法

    公开(公告)号:JP2013037059A

    公开(公告)日:2013-02-21

    申请号:JP2011170878

    申请日:2011-08-04

    Abstract: PROBLEM TO BE SOLVED: To provide a method for producing a pigment dispersion for a color filter which is capable of forming a cured film excellent in contrast and developability, and to provide a coloring composition for a color filter which contains the pigment dispersion obtained by the method.SOLUTION: There are provided: a method for producing a pigment dispersion for a color filter comprising (1) a step of obtaining a preliminary dispersion by dispersing a mixture which contains [1] an organic pigment, an ester-based organic solvent, a graft polymer (A) containing a constitutional unit derived from vinylpyrrolidone in the main chain and a constitutional unit derived from (meth)acrylate ester in the side chain until the volume median particle diameter of the organic pigment is 20 to 50 nm and (2) a step of obtaining a dispersion by mixing the resulting preliminary dispersion and a polyamine dispersant (B) having an acid value of 10 to 30 mgKOH/g and an amine value of 5 to 50 mgKOH/g; and a coloring composition for a color filter containing a pigment dispersion obtained by the method [2].

    Abstract translation: 要解决的问题:提供一种能够形成对比度和显影性优异的固化膜的滤色器用颜料分散体的制造方法,提供含有颜料分散体的滤色器用着色组合物 通过该方法获得。 提供了一种用于制造用于滤色器的颜料分散体的方法,包括(1)通过分散含有[1]有机颜料,酯类有机溶剂的混合物获得预分散体的步骤 在主链中含有衍生自乙烯基吡咯烷酮的结构单元的接枝聚合物(A)和源自侧链(甲基)丙烯酸酯的结构单元直到有机颜料的体积中值粒径为20〜50nm,( 2)通过混合得到的预分散体和酸值为10〜30mgKOH / g,胺值为5〜50mgKOH / g的多胺分散剂(B),得到分散液的步骤; 以及含有通过方法[2]得到的颜料分散体的滤色剂着色组合物。 版权所有(C)2013,JPO&INPIT

    Method for producing pigment dispersion for color filter
    18.
    发明专利
    Method for producing pigment dispersion for color filter 有权
    生产彩色滤光片色素分散液的方法

    公开(公告)号:JP2013037058A

    公开(公告)日:2013-02-21

    申请号:JP2011170872

    申请日:2011-08-04

    Abstract: PROBLEM TO BE SOLVED: To provide a method for producing a pigment dispersion for a color filter which is capable of forming a cured film excellent in contrast and developability, and to provide a coloring composition for a color filter which contains the pigment dispersion obtained by the method.SOLUTION: There is provided a method for producing a pigment dispersion comprising: (1) a step of obtaining a dispersion by dispersing a mixture which contains [1] an organic pigment, an ester-based organic solvent, a graft polymer (A) containing a constitutional unit derived from vinylpyrrolidone in the main chain and a constitutional unit derived from (meth)acrylate ester in the side chain and a polyamine dispersant (B) having an acid value of 10 to 30 mgKOH/g and an amine value of 5 to 50 mgKOH/g; and (2) a step of obtaining a pigment dispersion by removing at least a part of a graft polymer (A) and a polyamine dispersant (B) which are not adsorbed on the organic pigment from the resulting dispersion, a method for producing a pigment dispersion for a color filter in which the weight ratio [(A)+(B)/organic pigment] is 0.7 to 1.3 in the step (1) and 0.2 to 0.5 in the step (2), and a coloring composition for a color filter containing a pigment dispersion obtained by the method [2].

    Abstract translation: 要解决的问题:提供一种能够形成对比度和显影性优异的固化膜的滤色器用颜料分散体的制造方法,提供含有颜料分散体的滤色器用着色组合物 通过该方法获得。 提供一种颜料分散体的制造方法,其特征在于:(1)通过将含有[1]有机颜料,酯系有机溶剂,接枝聚合物(1)的混合物分散而获得分散体的工序; A),在主链中含有衍生自乙烯基吡咯烷酮的结构单元和源自侧链中的(甲基)丙烯酸酯的结构单元和酸值为10〜30mgKOH / g的多胺分散剂(B)和胺值 为5至50mgKOH / g; 和(2)通过从所得分散体除去不吸附在有机颜料上的接枝聚合物(A)和多胺分散剂(B)的至少一部分而获得颜料分散体的步骤,制备颜料的方法 步骤(1)中重量比[(A)+(B)/有机颜料]为0.7〜1.3,步骤(2)中为0.2〜0.5)的滤色器的分散液,以及颜色的着色组合物 含有通过方法[2]得到的颜料分散体的过滤器。 版权所有(C)2013,JPO&INPIT

    Compound metal oxide calcined body
    19.
    发明专利
    Compound metal oxide calcined body 有权
    化合物金属氧化物计算体

    公开(公告)号:JP2009158167A

    公开(公告)日:2009-07-16

    申请号:JP2007332592

    申请日:2007-12-25

    CPC classification number: Y02E60/122

    Abstract: PROBLEM TO BE SOLVED: To provide a compound metal oxide calcined body becoming a positive electrode active material in which smooth movement of Li becomes possible, which is superior in a molding property in forming a positive electrode, and superior in high speed discharge characteristics by heating a spray-granular body and making it porous.
    SOLUTION: This is the porous and granular compound metal oxide calcined body which is obtained by calcining the granular body, after a granular body is obtained from a slurry containing metal oxide (a), metal compound (b), and a solvent by a spray-granulation. The metal oxide (a) and the metal compound (b) are hardly soluble in the solvent, the calcining is carried out after a heat-insulating process that the granular body obtained by the spray-granulation is heated in a range of the decomposition temperature ±200° of the metal compound (b), and the metal compound (b) is made to be the compound metal oxide calcined body containing a non-metal element component released at least in the heat-insulating process.
    COPYRIGHT: (C)2009,JPO&INPIT

    Abstract translation: 要解决的问题:为了提供一种复合金属氧化物煅烧体,其成为能够平滑移动Li的正极活性材料,其在形成正极时的成型性能优异,并且高速放电性优异 特征通过加热喷雾颗粒体并使其多孔化。 解决方案:这是通过煅烧颗粒体获得的多孔和颗粒状复合金属氧化物煅烧体,在从含有金属氧化物(a),金属化合物(b)和溶剂的浆料获得颗粒体之后 通过喷雾造粒。 金属氧化物(a)和金属化合物(b)几乎不溶于溶剂,在通过喷雾造粒得到的粒状体在分解温度的范围内加热的绝热处理之后进行煅烧 金属化合物(b)的±200°,金属化合物(b)被制成含有至少在隔热工艺中释放的非金属元素成分的复合金属氧化物煅烧体。 版权所有(C)2009,JPO&INPIT

    Manufacturing method of polyurethane foam
    20.
    发明专利
    Manufacturing method of polyurethane foam 审中-公开
    聚氨酯泡沫的制造方法

    公开(公告)号:JP2008138091A

    公开(公告)日:2008-06-19

    申请号:JP2006325964

    申请日:2006-12-01

    Inventor: SAWAI MINORU

    Abstract: PROBLEM TO BE SOLVED: To provide a manufacturing method of a polyurethane foam exhibiting high foam strengths, low impact resilience and resistance to water absorption, a polyurethane foam obtained by the manufacturing method, a shoe sole composed of the polyurethane foam and a shoe having the shoe sole.
    SOLUTION: The manufacturing method of the polyurethane foam comprises causing a polyol component comprised of a polyester polyol and a polyether polyol to react with a polyisocyanate component in the co-presence of a catalyst comprised of an imidazole compound represented by formula (I) and 1,4-diazabicyclo[2.2.2]octane (TEDA) and a foam stabilizer.
    COPYRIGHT: (C)2008,JPO&INPIT

    Abstract translation: 解决问题的方法为了提供具有高泡沫强度,低回弹性和耐吸水性的聚氨酯泡沫的制造方法,通过该制造方法得到的聚氨酯泡沫,由聚氨酯泡沫制成的鞋底和 鞋子鞋底。 解决方案:聚氨酯泡沫的制造方法包括使由聚酯多元醇和聚醚多元醇组成的多元醇组分与多异氰酸酯组分反应,共催化剂由式(I)表示的咪唑化合物 )和1,4-二氮杂双环[2.2.2]辛烷(TEDA)和泡沫稳定剂。 版权所有(C)2008,JPO&INPIT