公开(公告)号:ES2342552T3
公开(公告)日:2010-07-08
申请号:ES06017533
申请日:2006-08-23
Applicant: SIEMENS AG
Inventor: BARNIKEL JOCHEN DR , SCHMITZ FRIEDHELM
Abstract: Álabe de turbina (120, 130) de una turbina con un sistema de recubrimiento, que presenta al menos una capa adhesiva (3) aplicada directamente a la pieza constructiva (1) y en especial una capa de protección calorífuga (4) configurada sobre la capa adhesiva (3), caracterizado porque la capa adhesiva (3) se compone de entre el 22% y el 36% en peso de Cr, entre el 15% y el 30% en peso de Ni, Fe como base, como máximo 55 ppm de Al, opcionalmente entre el 1% y el 3% en peso de Si.
-
公开(公告)号:CA2548973A1
公开(公告)日:2005-06-23
申请号:CA2548973
申请日:2004-12-01
Applicant: SIEMENS AG
Inventor: SCHMITZ FRIEDHELM , WIEGHARDT KAI
Abstract: The invention relates to the use of a thermal insulating layer (7) for a housing of a steam turbine in order to even out the deformation behaviour of different components based on different heatings of the components.
-
公开(公告)号:DE50006157D1
公开(公告)日:2004-05-27
申请号:DE50006157
申请日:2000-05-12
Applicant: SIEMENS AG
Inventor: SCHMITZ FRIEDHELM
Abstract: A steam turbine component coated with a protective layer can be exposed to hot vapor. The component has a metallic base body, to which the protective layer is bonded by diffusion in order to increase the resistance of the base material to oxidation. The protective layer contains aluminum and has a thickness of less than 50 mum. The protective coating can be formed by applying an aluminum pigment to the base body and maintaining the component at a predetermined temperature.
-
14.
公开(公告)号:DE10009426A1
公开(公告)日:2001-08-30
申请号:DE10009426
申请日:2000-02-28
Applicant: SIEMENS AG
Inventor: BARNIKEL JOCHEN , REITZNER KARL UVE , SCHMITZ FRIEDHELM
Abstract: In a process to treat drinking water, a water (5) supply (15) system (3) has an added biocide (11) into which an agent (21) is introduced to reduce the biocide (11). The reduction agent is especially an oxidation agent (21) which has a stronger biocidal action than does the biocide (11). The oxidation agent is especially hydrogen peroxide. An independent claim is included for a water (5) supply system (3) containing a biocide (11) agent, with a pipe (15) to an outlet (15). A reservoir (23) feeds (25) hydrogen peroxide (21) to the water pipe (15).
-
公开(公告)号:DE19536218A1
公开(公告)日:1997-04-03
申请号:DE19536218
申请日:1995-09-28
Applicant: SIEMENS AG
Inventor: SCHMITZ FRIEDHELM , WOJACZYK HANS-GUENTER
Abstract: The method involves mechanical loading of the tested combustion chamber brick (19). The brick is supported in a tension-free condition by a pair of holders (2,6) adapted to the shape of the brick. The mechanical loading is provided by a defined force (F), exerted on the brick in the region between the holders. Preferably one of the holders (2) is fixed in position and the other is movable together with pressure elements (10,11), for matching the component size tolerance range and variations from the ideal shape.
-
公开(公告)号:DE58908611D1
公开(公告)日:1994-12-08
申请号:DE58908611
申请日:1989-08-10
Applicant: SIEMENS AG
Inventor: CZECH NORBERT , SCHMITZ FRIEDHELM
-
公开(公告)号:AT110116T
公开(公告)日:1994-09-15
申请号:AT90106913
申请日:1990-04-11
Applicant: SIEMENS AG
Inventor: SCHMITZ FRIEDHELM
IPC: C21D9/50
-
公开(公告)号:DE3861836D1
公开(公告)日:1991-04-04
申请号:DE3861836
申请日:1988-07-25
Applicant: SIEMENS AG
Inventor: SCHMITZ FRIEDHELM
-
公开(公告)号:DE3766507D1
公开(公告)日:1991-01-17
申请号:DE3766507
申请日:1987-01-09
Applicant: SIEMENS AG
Inventor: SCHMITZ FRIEDHELM
Abstract: These pipes (1) of austenitic, ferritic or austenitic-ferritic non- rusting steels are annealed after the longitudinal seam (2) has been welded. In the process according to the invention, the pipes (1) are only partially solution-annealed in the region of the weld seam (2) and of the heat-affected zone (3) or in a region (4) going slightly beyond the former. This allows even annealing temperatures of, for example, above 1200 DEG C and long holding times, whereby optimised solution-annealing and a better equalisation of segregations of the corrosion resistance-determining elements chromium and molybdenum in the region of the weld seam can be achieved. The only partial heating of the weld seam, for example by means of focused infrared emitters, prevents deformation of the pipes under the action of gravity during the annealing, in spite of the high annealing temperature. As a result, the corrosion resistance of the weld seam (3) can approach the value of the base material. Defined alloying with nitrogen from the surrounding atmosphere can further improve the corrosion resistance. Production of high-quality thin-walled pipes which can be tested for damage is also facilitated.
-
公开(公告)号:DE3913973A1
公开(公告)日:1990-10-31
申请号:DE3913973
申请日:1989-04-27
Applicant: SIEMENS AG
Inventor: SCHMITZ FRIEDHELM
IPC: C21D9/50
-
-
-
-
-
-
-
-
-