Abstract: PROBLEM TO BE SOLVED: To provide a component with a coating system which comprises an adhesion layer directly provided on the component and a heat insulation layer formed on the adhesion layer, where the internal diffusion between the base material of the component and the adhesion layer is suppressed to the minimum; further, the degree of the mixing therebetween required for the optimum adhesion of the adhesion layer is secured, and also, the characteristics of the base material in the component are not hindered. SOLUTION: In this invention, an adhesion layer 3 comprises 22 to 36 wt.% Cr, 15 to 30 wt.% Ni, ≤55 ppm Al, and Fe as a base. COPYRIGHT: (C)2008,JPO&INPIT
Abstract translation: 要解决的问题:为了提供一种涂覆系统的部件,其包括直接设置在部件上的粘合层和形成在粘合层上的绝热层,其中部件的基材和 粘附层被抑制到最小; 此外,确保了粘合层最佳粘合所需的混合程度,并且也不会妨碍部件中的基材的特性。 解决方案:在本发明中,粘合层3包含22至36重量%的Cr,15至30重量%的Ni,≤55ppm的Al和作为碱的Fe。 版权所有(C)2008,JPO&INPIT
-
公开(公告)号:WO2012059325A3
公开(公告)日:2012-10-11
申请号:PCT/EP2011068215
申请日:2011-10-19
Applicant: SIEMENS AG , SCHMITZ FRIEDHELM , STAMM WERNER
Inventor: SCHMITZ FRIEDHELM , STAMM WERNER
IPC: C23C30/00 , B32B15/01 , C22C19/00 , C22C19/05 , C22C30/00 , C23C4/08 , C23C14/14 , C23C28/00 , F01D5/28
CPC classification number: C22C19/058 , B32B15/01 , B32B15/04 , C22C19/05 , C22C30/00 , C23C28/30 , C23C28/321 , C23C28/3215 , C23C28/345 , C23C28/3455 , C23C30/00 , F01D5/288 , F05C2201/0463 , F05D2300/132 , F05D2300/15 , Y02T50/67 , Y10T428/12618
Abstract: Known protective coatings having a high Cr content, as well as silicon, have brittle phases that become additionally brittle under the influence of carbon during use. The protective coating according to the invention has the composition of 24% to 26% cobalt (Co), 10% to 12% aluminum (Al), 0.2% to 0.5% yttrium (Y), 12% to 14% chromium (Cr), and the remainder nickel.
Abstract translation: 具有已知的保护层的Cr浓度高,而在脆性相,其额外成为碳的使用过程中的影响下脆的添加硅形式。 根据本发明的保护层的组成是24%至26%钴(Co),10%至12%的铝(Al),0.2%至0.5%的钇(Y),12% - 14%的铬(Cr), 其余为镍。
-
公开(公告)号:WO2011086046A2
公开(公告)日:2011-07-21
申请号:PCT/EP2011050222
申请日:2011-01-10
Applicant: SIEMENS AG , SCHMITZ FRIEDHELM , STAMM WERNER
Inventor: SCHMITZ FRIEDHELM , STAMM WERNER
CPC classification number: C22C19/056 , C22C19/07 , C23C28/321 , C23C28/3215 , C23C28/345 , C23C28/3455 , C23C30/00 , F01D5/288 , F05C2201/0463 , F05D2230/90 , F05D2300/15 , Y02T50/67 , Y10T428/12618
Abstract: Known protective layers having a high Cr content, as well as silicon, have brittle phases that become additionally brittle under the influence of carbon during use. The protective layer according to the invention has the composition of 31% to 35% cobalt (Co), 10% to 13% aluminum (Al), 0.1% to 0.7% yttrium (Y), and/or at least one equivalent metal from the group comprising scandium and the rare earth elements, 31% to 35% chromium (Cr), 0.1% to 0.5% silicon, and the remainder nickel.
Abstract translation: 已知的具有高Cr含量的保护涂层和另外的硅形成脆性相,其在使用期间在碳的影响下另外脆化。 根据本发明的保护层的组成是31%至33%的钴(Co),10%至13%的铝(Al),0.1%至0.7%的钇(Y)和/或选自下组,其包括至少一个当量的金属 钪和稀土元素,31%至35%的铬(Cr),0.1%至0.5%的硅,余量为镍。
-
公开(公告)号:PL1869292T3
公开(公告)日:2013-05-31
申请号:PL06708745
申请日:2006-03-13
Applicant: SIEMENS AG
Inventor: HAJE DETLEF , RÖTTGER DIETMAR , SCHMITZ FRIEDHELM
-
公开(公告)号:DE502006006582D1
公开(公告)日:2010-05-12
申请号:DE502006006582
申请日:2006-08-23
Applicant: SIEMENS AG
Inventor: BARNIKEL JOCHEN DR , SCHMITZ FRIEDHELM
Abstract: The turbine blade (1) comprises a substrate (2) and a coating system having an adhesive layer (3) directly applied on the blade and heat insulating layer (4) formed on the adhesive layer having multiple layers. The heat-insulating layer contains ceramic. A first layer of the adhesive layer applied on the component formed as barrier layer for a layer formed on the first layer. The barrier layer minimizes inter diffusion between the component and the adhesive layer.
-
公开(公告)号:IN175649B
公开(公告)日:1995-07-29
申请号:IN683CA1990
申请日:1990-08-08
Applicant: SIEMENS AG
Inventor: CZECH NORBERT , SCHMITZ FRIEDHELM
-
公开(公告)号:AT61101T
公开(公告)日:1991-03-15
申请号:AT88111976
申请日:1988-07-25
Applicant: SIEMENS AG
Inventor: SCHMITZ FRIEDHELM
-
公开(公告)号:ES2342552T3
公开(公告)日:2010-07-08
申请号:ES06017533
申请日:2006-08-23
Applicant: SIEMENS AG
Inventor: BARNIKEL JOCHEN DR , SCHMITZ FRIEDHELM
Abstract: Álabe de turbina (120, 130) de una turbina con un sistema de recubrimiento, que presenta al menos una capa adhesiva (3) aplicada directamente a la pieza constructiva (1) y en especial una capa de protección calorífuga (4) configurada sobre la capa adhesiva (3), caracterizado porque la capa adhesiva (3) se compone de entre el 22% y el 36% en peso de Cr, entre el 15% y el 30% en peso de Ni, Fe como base, como máximo 55 ppm de Al, opcionalmente entre el 1% y el 3% en peso de Si.
-
公开(公告)号:CA2548973A1
公开(公告)日:2005-06-23
申请号:CA2548973
申请日:2004-12-01
Applicant: SIEMENS AG
Inventor: SCHMITZ FRIEDHELM , WIEGHARDT KAI
Abstract: The invention relates to the use of a thermal insulating layer (7) for a housing of a steam turbine in order to even out the deformation behaviour of different components based on different heatings of the components.
-
公开(公告)号:DE50006157D1
公开(公告)日:2004-05-27
申请号:DE50006157
申请日:2000-05-12
Applicant: SIEMENS AG
Inventor: SCHMITZ FRIEDHELM
Abstract: A steam turbine component coated with a protective layer can be exposed to hot vapor. The component has a metallic base body, to which the protective layer is bonded by diffusion in order to increase the resistance of the base material to oxidation. The protective layer contains aluminum and has a thickness of less than 50 mum. The protective coating can be formed by applying an aluminum pigment to the base body and maintaining the component at a predetermined temperature.
-
-
-
-
-
-
-
-
-