EXTREMELY THIN COMPOSITE CONTINUOUS SHEET AND PRODUCTION THEREOF

    公开(公告)号:JPH07205373A

    公开(公告)日:1995-08-08

    申请号:JP304894

    申请日:1994-01-17

    Abstract: PURPOSE:To improve surface smoothness, thermal characteristics and mechanical characteristics by constituting both surface layer parts of an extremely thin composite continuous sheet of PPS having specific thickness or more and constituting the inner layer thereof of a composite layer of PPS and a glass fiber fabric and setting the degree of crystallization of PPS to specific % or more and the crystal size thereof due to X-rays diffraction thereof to a specific value or more. CONSTITUTION:An extremely thin composite continuous sheet consist of PPS and a glass fiber fabric having a monofilament diameter of 10mum or less and containing 20000/in or more of glass fibers and has a thickness of 100mum or less. Both surface layer parts of the extremely thin composite continuous sheet is composed of a single PPS layer of which the thickness is at least 1/10 or more that of the sheet and the inner layer part thereof is constituted of a composite layer of PPS and a glass fiber fabric and the degree of crystallization of PPS is 40% or more and the crystal size thereof due to X-rays diffraction is 60nm or more. By this constitution, the extremely thin composite continuous sheet for a printed wiring board excellent in surface smoothness and thermal characteristics is obtained.

    RETORT POLYOLEFIN FILM
    12.
    发明专利

    公开(公告)号:JPH07166006A

    公开(公告)日:1995-06-27

    申请号:JP31648593

    申请日:1993-12-16

    Abstract: PURPOSE:To obtain a film which meets all of the requirements for a semiretort film and is used as a heat seal layer of a packaging bag by specifying the mixed resin and its amount of addition. CONSTITUTION:A polypropylene copolymer (A) having a melting point of 130-150 deg.C is mixed with a low-density polyethylene (B) and a hydrogenated block copolymer (C) composed of at least one block of a polymer based on a vinylaromatic compound and at least one block of a hydrogenated polymer based on a conjugated diene compound in a weight ration of component B to component C of 1:1 to 20:1. Component A is a random copolymer of propylene with an alpha-olefin, and ethylene or butene-1 is particularly desirable as the alpha- olefin. An example of component C is a styrene/ethylene/butylene/styrene copolymer.

    BIAXIALLY ORIENTED POLYESTER FILM FOR MOLDING CONTAINER AND METHOD FOR PRODUCING THE FILM

    公开(公告)号:JP2004010711A

    公开(公告)日:2004-01-15

    申请号:JP2002164282

    申请日:2002-06-05

    Abstract: PROBLEM TO BE SOLVED: To provide a biaxially oriented polyester film for molding containers excellent in environmental resistance, printability, dimensional stability, microwave oven resistance and molding processability. SOLUTION: The biaxially oriented polyester film is composed of a polyester consisting mainly of ethylene terephthalate units and/or ethylene naphthalate units, having a melting point of ≥245°C. In this film, the elongation at break at 150°C, the stress under 200% elongation at 150°C and the heat shrinkage at 150°C are specified, respectively. COPYRIGHT: (C)2004,JPO

    LAMINATED FILM
    14.
    发明专利

    公开(公告)号:JP2001260281A

    公开(公告)日:2001-09-25

    申请号:JP2001003495

    申请日:2001-01-11

    Abstract: PROBLEM TO BE SOLVED: To provide a laminated film capable of being suitably utilized for a film-like or a sheet-like industrial material, agricultural material, a packaging material or the like to be used by printing and having excellent recyclability. SOLUTION: The laminated film comprises at least three layers of a layer (a layer A) partly or entirely dissolvable by an acid or an alkali aqueous solution treatment, a polymer layer (a layer B) capable of being separated and recovered from the layer A by the acid or the alkali aqueous solution treatment, and a layer to be printed (a layer C).

    POLYESTER FILM FOR VAPOR DEPOSITION

    公开(公告)号:JP2000119414A

    公开(公告)日:2000-04-25

    申请号:JP29047498

    申请日:1998-10-13

    Abstract: PROBLEM TO BE SOLVED: To provide a polyester film for vapor deposition excellent in vapor deposition workability and gas barrier properties. SOLUTION: This film is composed of a polyester A comprising a dicarboxylic acid component having terephthalic acid and isophthalic acid as the main components, and a glycol component having ethylene glycol as the main component, the polyester A having a 1,3-bis(2-hydroxyethoxy) benzene component in the range of 0.1-10 wt.%.

    THERMOPLASTIC POLYESTER FILM
    16.
    发明专利

    公开(公告)号:JPH11322963A

    公开(公告)日:1999-11-26

    申请号:JP15375598

    申请日:1998-05-19

    Abstract: PROBLEM TO BE SOLVED: To prepare a thermoplastic polyester film which is excellent in perfume retention and heat sealability by using a specific dicarboxylic acid component and a glycol component. SOLUTION: This polyester film is based on a polyester A formed from a dicarboxylic acid component contg. at least 80 wt.% terephthalic acid component and/or 2, 6-naphthalenedicarboxylic acid component and a glycol component contg. 35-100 wt.% 1,3-propanediol, has a plane orientation factor fn of 0-0.03, and pref. has the surface roughness Ra of 0.01-0.5 μm. Pref., polyester film A contains 0.5 wt.% or lower particles. Inorg. particles, org. particles, or the like, having an average particle size of 0.001-8 μm can be used. Pref., polyester film A has a heat of fusion ΔHu in differential scanning calorimetry of 5-40 lug and is laminated to polyester B having an m.p. of 200-260 deg.C.

    LAMINATED FILM FOR PACKAGING AND LAMINATE FOR PACKAGING

    公开(公告)号:JPH11245346A

    公开(公告)日:1999-09-14

    申请号:JP5355798

    申请日:1998-03-05

    Abstract: PROBLEM TO BE SOLVED: To obtain a balanced laminated film for packaging which is good in environmental and working-environmental properties in the application of a water-dispersion type anchor-coating agent without using an organic solvent, and in the adhesion, transparency, and gas barrier properties after being boiled, and a laminate for packaging. SOLUTION: In a laminated film for packaging in which polyvinylidene chloride is laminated on a backing film through an anchor-coating agent, the agent contains a water-dispersion type polyester-polyurethane resin and a water- dispersion type aliphatic polyisocyanate compound as main components and is incorporated with a silane coupling agent. A laminate for packaging is constituted by laminating another film on the polyvinylidene chloride coating surface of the laminated film.

    BIAXIALLY ORIENTED FILM AND LAMINATED FILM

    公开(公告)号:JPH1160754A

    公开(公告)日:1999-03-05

    申请号:JP15268398

    申请日:1998-06-02

    Abstract: PROBLEM TO BE SOLVED: To obtain a resin film excellent in durability, wear resistance and resistance to Gelbo properties by using a specific aliphatic polyketone as an essential constituent, and allowing the polyketone to include a specified amount of inorganic and/or organic particles having a particle diameter within a specific range. SOLUTION: This biaxially oriented film is obtained by using a polymer formed out of constituents consisting essentially of an aliphatic polyketone containing >=80 mol.%, preferably >=90 mol.%, especially preferably 95 mol.% constituent unit of the formula [(r) is H or methyl, preferably H; R is H or a 1-4C alkyl, preferably H or methyl], and including 0.001-10 wt.% inorganic and/or organic particles having 0.01-10 μm, preferably 0.01-5 μm, especially preferably 0.01-3 μm particle diameter expressed in terms of weight ratio. Preferably, the thickness fluctuation of the film is

    GAS BARRIER FILM AND PACKAGING MATERIAL

    公开(公告)号:JPH10323928A

    公开(公告)日:1998-12-08

    申请号:JP7632598

    申请日:1998-03-24

    Abstract: PROBLEM TO BE SOLVED: To provide a gas barrier film having gas barrier property, durable barrier property at a high humidity adhesive property of coated film, and printability. SOLUTION: In the film comprising a coated film containing inorganic plate- like particles and water soluble or dispersible polymer as main component on at least one surface of a thermoplastic resin base material, surface roughness parameter Rt/Ra of the coated film is 25 or less, and number of waviness in a range of 25 to 100 μm of a diameter of a surface of the coated film is 1 to 150 pieces/mm .

    GAS BARRIER FILM AND MANUFACTURE THEREOF

    公开(公告)号:JPH10166516A

    公开(公告)日:1998-06-23

    申请号:JP26426097

    申请日:1997-09-29

    Abstract: PROBLEM TO BE SOLVED: To realize a film, which has gas barrier properties even under highly humid state and, at the same time, keeps the adhesion between the film and a base material and the gas barrier properties even after the lamination of the film to the base material by a method wherein an amine compound represented by a specified formula is included in a coating film. SOLUTION: A gas barrier film is produced by forming a coating film, which is mainly made of inorganic laminar compound and water-soluble polymer and includes an amine compound represented by a formula, where R1 is hydrogen, 1-6C alkyl chain or its substitution product, aryl chain or its substitution product, R2 is hydrogen, 1C or more alkyl chain or its substitution product, aryl chain or its substitution product and R3 is 1C or more alkyl chain or its substitution product, aryl chain or its substitution product. In order to form a coating film onto a thermoplastic resin base material, the coating film is formed out of a dispersion prepared by dispersing the constituent components of the coating film in various solutions by gravure coating and then dried by a heat roll contacting method or the like in order to obtain the desired coating film.