POLYESTER FILM
    1.
    发明专利
    POLYESTER FILM 审中-公开

    公开(公告)号:JP2004010793A

    公开(公告)日:2004-01-15

    申请号:JP2002167425

    申请日:2002-06-07

    Abstract: PROBLEM TO BE SOLVED: To provide a polyester film excellent in flexibility and bleed-out resistance. SOLUTION: The polyester film contains 0.1-45wt% of a branched compound the number of whose ether bond (-O-) units other than epoxy groups is 3-100 per molecule and whose molecular weight is 200-4,000. COPYRIGHT: (C)2004,JPO

    POLYESTER FILM FOR LAMINATE
    3.
    发明专利

    公开(公告)号:JP2001122988A

    公开(公告)日:2001-05-08

    申请号:JP30351899

    申请日:1999-10-26

    Abstract: PROBLEM TO BE SOLVED: To obtain a polyester film for laminates excellent in environmental resistance, printability, high design property and emboss processability. SOLUTION: This polyester film comprises a polyester containing ethylene terephthalate unit and/or ethylene naphthalate as a main constituent and contains a coloring agent. In the film, maximum heat shrinkage stress is within the range of 0.01-5.0 Mpa and lightness L* value of film surface, chromaticity (a)* value and chromaticity (b)* value are specified.

    POLYESTER FILM FOR METAL PLATE CLADDING FABRICATION

    公开(公告)号:JP2000129008A

    公开(公告)日:2000-05-09

    申请号:JP11265899

    申请日:1999-04-20

    Abstract: PROBLEM TO BE SOLVED: To obtain a film excellent in adherence after retort processing and taste characteristics by using ethylene terephthalate and/or ethylene naphthalate units as constituents and a specific amount of cyclohexanedimethanol as a copolymerization component. SOLUTION: Polyester film A contains ethylene terephthalate and/or ethylene naphthalate units as constituents and 1-40 mol% of cyclohexanedimethanol. This film has a melting point of 246 deg.C or higher and preferably contains 0.01-3 wt.% of an inorganic or organic particle with an average particle diameter of 0.01-5 μm and a degree of anomaly of 1.1 or more. A laminated film is obtained by laminating polyester B, which contains ethylene terephthalate and/or ethylene naphthalate units as constituents and 0.01-4 mol% of cyclohexanedimethanol as a copolymerization component, to polyester A to express taste characteristics and heat resistance.

    POLYLACTIC ACID FILM AND LAMINATE USING IT
    5.
    发明专利

    公开(公告)号:JP2004256795A

    公开(公告)日:2004-09-16

    申请号:JP2004011731

    申请日:2004-01-20

    Abstract: PROBLEM TO BE SOLVED: To provide a film having excellent hand-cutting properties, in particular one having good transparency which is suitably applicable to an easy-openable packaging material for foodstuffs, medicines, etc., to provide an adhesive tape having excellent hand-cutting properties, and to provide, in addition, a material which is favorable in sanitation from the aspect of having a fungicidal property, antibacterial activity and the like. SOLUTION: The film is a polylactic acid film wherein haze is ≤20%, a melting point is ≥150°C and the value of breaking strength (MPa)×thickness (μm) is in the range of 100-2,100. A laminate comprising at least two layers consisting of a layer A composed of the polylactic acid film and a sealant layer (layer B), and having 50-700 g tear starting strength, is also provided. The packaging film and the adhesive tape are obtained by using the polylactic acid film. COPYRIGHT: (C)2004,JPO&NCIPI

    POLYESTER FILM FOR LAMINATION
    6.
    发明专利

    公开(公告)号:JP2001200073A

    公开(公告)日:2001-07-24

    申请号:JP2000011354

    申请日:2000-01-20

    Abstract: PROBLEM TO BE SOLVED: To prepare a polyester film for lamination which is excellent not only in environmental friendliness but also in embossability and foldability. SOLUTION: In the expansion and contraction curve of the polyester film in the temperature rise under a load of 0.1 Mpa, T1 and T2 of the film satisfy the relation represented by the equation: T2-T1>=8( deg.C), wherein T1( deg.C) is the highest temperature at which the slope of the expansion and contraction curve in the temperature rise changes from a negative value to a positive value; and T2( deg.C) is the temperature at which the expansion in the temperature rise reaches 25%.

    POLYESTER FILM FOR OUTER SURFACE OF MOLDED CONTAINER

    公开(公告)号:JP2000297161A

    公开(公告)日:2000-10-24

    申请号:JP10608499

    申请日:1999-04-14

    Abstract: PROBLEM TO BE SOLVED: To obtain a polyester film which has a high hiding power, is free of unevenness and excellent in beautifulness and has a high abrasion resistance by incorporating a specified amount (per unit thickness) of titanium oxide containing a specified amount of an inorganic and/or an organic surface-treating agent into the same. SOLUTION: This polyester film contains titanium oxide which has an average particle size of 0.1-0.5 μm and is surface-treated with 0.01-2 wt.% inorganic and/or an organic surface-treating agent. The content of titanium oxide per unit thickness of the film is 1.2-2.5 wt.%/μm. If necessary, the film further contains 0.01-2 wt.%/μm cohesion-type inorganic particles having an average particle size of 0.01-10 μm. Preferably, a layer having a titanium oxide concentration of 2-15 wt.%/μm is formed on at least one side of the film in order to reduce the abrasion of a roll, An aluminum oxide compound or an aluminum hydroxide compound in an amount of 0.01-1.5 wt.%, based on titanium oxide, is preferable as the inorganic surface-treating agent. A silicone compound in an amount of 0.02-2 wt.% or a polyhydric alcohol compound in an amount of 0.01-1.5 wt.%, based on titanium oxide, is preferable as the organic surface- treating agent.

    LAMINATED FILM AND VAPOR DEPOSITION FILM USING THE SAME
    8.
    发明公开
    LAMINATED FILM AND VAPOR DEPOSITION FILM USING THE SAME 审中-公开
    MEHRSCHICHTFOLIE UND DAMPFBESCHICHTETE FOLIE UNTER VERWENDUNG DERSELBEN

    公开(公告)号:EP1142704A4

    公开(公告)日:2002-04-17

    申请号:EP00954976

    申请日:2000-08-24

    Abstract: The present invention relates to (1) a laminate film where, on at least one face of a substrate layer (the A layer) selected from polyester film and aliphatic polyamide film, there is provided a polyamide layer (the C layer) in which the chief component is an aromatic polyamide of glass transition temperature at least 60 DEG C, as a layer to undergo vapour deposition, and the centre-line average roughness (Ra) of the face which is to undergo vapour deposition is in the range 0.005 to 0.03 mu m, or (2) a laminate film where, on at least one face a substrate layer (the A layer) selected from polyester film and aliphatic polyamide film, there is provided a polyamide layer (the C layer) in which the chief component is an aromatic polyamide of glass. transition temperature at least 60 DEG C, as a layer to undergo vapour deposition and, between the substrate A layer and the polyamide C layer, a layer (the B layer) comprising a single polymer or a plurality of polymers of SP value 10 to 15 is interposed between the substrate A layer and the polyamide C layer; and the invention offers film for vapour-deposition which is outstanding in its processability in vapour-deposition, and in its gas barrier properties.

    Abstract translation: 本发明涉及(1)层叠膜,其中,在选自聚酯膜和脂肪族聚酰胺膜的基材层(A层)的至少一面上,设置有聚酰胺层(C层),其中, 主要组分是玻璃化转变温度至少为60℃的芳族聚酰胺,作为经历气相沉积的层,并且要经历气相沉积的面的中心线平均粗糙度(Ra)在0.005至0.03的范围内 或(2)层压膜,其中,在至少一面为选自聚酯膜和脂肪族聚酰胺膜的基材层(A层)的面上设置有聚酰胺层(C层),其中主要成分 是玻璃的芳香聚酰胺。 转变温度至少为60℃,作为经历气相沉积的层,并且在基材A层和聚酰胺C层之间,包含SP值为10至15的单一聚合物或多种聚合物的层(B层) 介于基板A层和聚酰胺C层之间; 并且本发明提供了在气相沉积加工性方面突出的气相沉积膜及其阻气性。