POLYESTER MULTILAYERED INJECTION MOLDED ARTICLE

    公开(公告)号:JP2003260759A

    公开(公告)日:2003-09-16

    申请号:JP2002061691

    申请日:2002-03-07

    Abstract: PROBLEM TO BE SOLVED: To obtain a polyester multilayered injection molded article capable of being used for parts of devices and electric appliances for home, parts of office automation equipment and parts for data communication equipment which are excellent in noise insulation characteristics by utilizing a polyester resin capable of simplifying a process by injection molding. SOLUTION: The polyester multilayered injection molded article has a structure of a skin layer (A) and a core layer (B). The skin layer comprises a composite consisting of 99-40 wt.% of a polyester (A1) and 1-60 wt.% of a reinforcing filler (A2). The core layer comprises a composite consisting of 100-40 wt.% of a thermoplastic elastomer (B1) and 0-60 wt.% of a reinforcing filler (B2). COPYRIGHT: (C)2003,JPO

    RESIN COMPOSITION AND MOLDED PRODUCT MADE OF THE SAME

    公开(公告)号:JP2003253106A

    公开(公告)日:2003-09-10

    申请号:JP2002052438

    申请日:2002-02-27

    Abstract: PROBLEM TO BE SOLVED: To provide a resin composition which is excellent in a crystallization property and heat resistance, and a molded product made of the same. SOLUTION: The resin composition contains a (A) polylactic acid resin and a (B) polyacetal resin. The polylactic acid resin comprises the same resin (A-1) containing the both of a poly L-lactic acid resin having an L-lactic unit as a main component and a poly D-lactic acid resin having a D-lactic acid unit as a main component and/or a (A-2) block copolymer consisting of a poly L- lactic acid segment having an L-lactic acid unit as a main component and a poly D-lactic acid segment having a D-lactic acid as a main component. The molded product is made of the resin composition. COPYRIGHT: (C)2003,JPO

    METHOD FOR PRODUCING POLYBUTYLENE TEREPHTHALATE

    公开(公告)号:JP2001114884A

    公开(公告)日:2001-04-24

    申请号:JP29311699

    申请日:1999-10-15

    Abstract: PROBLEM TO BE SOLVED: To provide a method for producing a polybutylene terephthalate having improved quality by which, when terephthalic acid containing acetic acid, and 1,4-butanediol are used as raw materials, and an esterification reaction and a polycondensation reaction following the reaction are carried out, the retardation of the polycondensation can be extremely reduced to carry out the polycondensation reaction smoothly, and the 1,4-butanediol distilled off at the polycondensation reaction can be effectively recovered and utilized in the esterification step as it is. SOLUTION: This method for producing the polybutylene terephthalate by subjecting the terephthalic acid containing the acetic acid and the 1,4-butanediol to the esterification reaction, and further subjecting the reaction product to the polycondensation reaction is characterized in that an alkaline compound is added to the reaction mixture at an arbitrary step before finishing the polycondensation reaction.

    METHOD FOR PRODUCING POLYESTER
    17.
    发明专利

    公开(公告)号:JP2001114879A

    公开(公告)日:2001-04-24

    申请号:JP29311599

    申请日:1999-10-15

    Abstract: PROBLEM TO BE SOLVED: To provide a method for efficiently producing a polyester having a low concentration of a carboxy terminal group, excellent in hydrolysis resistance and containing a small amount of a foreign matter. SOLUTION: This method for producing the polyester is characterized by carrying out an esterification reaction or an ester-interchange reaction under a reduced pressure, and adding an alkaline compound to the reaction mixture at an arbitrary step before the finishing of the polymerization reaction when producing the polyester by using a dicarboxylic acid component comprising an aromatic dicarboxylic acid or an ester-forming derivative, and a diol component consisting essentially of 1,4-butanediol in the presence of a catalyst, and carrying out the esterification reaction or the ester-interchange reaction, and the polycondensation reaction following it.

    POLYESTER RESIN COMPOSITION
    18.
    发明专利

    公开(公告)号:JP2000212408A

    公开(公告)日:2000-08-02

    申请号:JP32753899

    申请日:1999-11-17

    Abstract: PROBLEM TO BE SOLVED: To obtain a composition capable of giving a molded article excellent in rigidity, impact resistance, heat resistance and chemical resistance by incorporating a phyllosilicate salt having exchangeable cations existing between layers replaced by organic onium ions and an impact modifier each in a specific amount into a thermoplastic polyester resin. SOLUTION: Into 100 pts.wt. of a thermoplastic polyester resin (A) are incorporated 0.1-40 pts.wt. of a phyllosilicate salt (B) having exchangeable cations existing between layers replaced by organic onium ions and 1-50 pts.wt. of an impact modifier (C). Preferably, at least 80% of the component B exists in the component A phase and the component B is previously dispersed in the component A before the impact modifier is added. Further are added 2-100 pts.wt. of a fibrous inorganic filler, 0.01-5 pts.wt. of a hindered phenol compound, an organic phosphite or phosphonite compound, and 0.05-10 pts.wt. of a compound having a functional group reactive with the thermoplastic polyester.

    THERMOPLASTIC RESIN COMPOSITION FOR SHEET OR CARD

    公开(公告)号:JP2000169723A

    公开(公告)日:2000-06-20

    申请号:JP34342998

    申请日:1998-12-02

    Abstract: PROBLEM TO BE SOLVED: To obtain a thermoplastic resin composition which gives a sheet hardly exhibiting warpage, etc., even when embossed and which exhibits excellent mold release characteristics in card production by compounding a thermoplastic resin with specified amounts of an inorganic platy filler having a specified average particle size and a mold release agent. SOLUTION: This composition is prepared by compounding 100 pts.wt. thermoplastic resin with 0.5-25 pts.wt. inorganic platy filler having an average particle size of 0.5-20 μm and 0.01-5 pts.wt. mold release agent. Preferably, the thermoplastic resin has a total light transmission (per 2 mm thickness, according to ASTM D1003) of 50% or higher and/or a glass transition temperature of 70-170 deg.C. Preferable examples of the thermoplastic resin are PS, a styrene- acrylonitrile copolymer, a styrene-butadiene-acrylonitrile terpolymer, a polyester, and a polycarbonate. Talc is preferable as the inorganic platy filler. Preferably, at least one mold release agent selected from among montanic acid compounds and low-molecular polyolefins is used.