Applicant: UNITED TECHNOLOGIES CORP
Inventor: BERZIK DOUGLAS MICHEAL , BRODI GEORGE , O CONELL THOMAS EDWARD
CPC classification number: C22F1/183
-
公开(公告)号:DK516084D0
公开(公告)日:1984-10-30
申请号:DK516084
申请日:1984-10-30
Applicant: UNITED TECHNOLOGIES CORP
Inventor: BERCZIK DOUGLAS MICHAEL , BRODI GEORGE , O'CONNELL THOMAS EDWARD
Abstract: Process for improving the crack growth behavior of titanium alloys containing substantial beta stabilizers and at least 3% molybdenum, such as Ti-6-2-4-6. The process includes the steps of forging above the beta transus temperature, cooling at a controlled rate through the beta transus temperature, heating to a temperature between 50 DEG -150 DEG F. below the beta transus temperature, cooling the alloy at a rate in excess of that produced by air cooling, and aging the material between about 900 DEG F. and 1100 DEG F. The resultant material has substantially improved crack growth behavior when contrasted with material processed according to the prior art.
-
公开(公告)号:NO164720C
公开(公告)日:1990-11-07
申请号:NO844031
申请日:1984-10-09
Applicant: UNITED TECHNOLOGIES CORP
Inventor: BERCZIK DOUGLAS MICHAEL , BRODI GEORGE , O'CONELL THOMAS EDWARD
Abstract: Process for improving the crack growth behavior of titanium alloys containing substantial beta stabilizers and at least 3% molybdenum, such as Ti-6-2-4-6. The process includes the steps of forging above the beta transus temperature, cooling at a controlled rate through the beta transus temperature, heating to a temperature between 50 DEG -150 DEG F. below the beta transus temperature, cooling the alloy at a rate in excess of that produced by air cooling, and aging the material between about 900 DEG F. and 1100 DEG F. The resultant material has substantially improved crack growth behavior when contrasted with material processed according to the prior art.
-
公开(公告)号:NO164720B
公开(公告)日:1990-07-30
申请号:NO844031
申请日:1984-10-09
Applicant: UNITED TECHNOLOGIES CORP
Inventor: BERCZIK DOUGLAS MICHAEL , BRODI GEORGE , O'CONELL THOMAS EDWARD
Abstract: Process for improving the crack growth behavior of titanium alloys containing substantial beta stabilizers and at least 3% molybdenum, such as Ti-6-2-4-6. The process includes the steps of forging above the beta transus temperature, cooling at a controlled rate through the beta transus temperature, heating to a temperature between 50 DEG -150 DEG F. below the beta transus temperature, cooling the alloy at a rate in excess of that produced by air cooling, and aging the material between about 900 DEG F. and 1100 DEG F. The resultant material has substantially improved crack growth behavior when contrasted with material processed according to the prior art.
-
公开(公告)号:ZA847963B
公开(公告)日:1985-05-29
申请号:ZA847963
申请日:1984-10-11
Applicant: UNITED TECHNOLOGIES CORP
Inventor: BERCZIK DOUGLAS MICHAEL , BRODI GEORGE , O'CONNELL THOMAS EDWARD
Abstract: Process for improving the crack growth behavior of titanium alloys containing substantial beta stabilizers and at least 3% molybdenum, such as Ti-6-2-4-6. The process includes the steps of forging above the beta transus temperature, cooling at a controlled rate through the beta transus temperature, heating to a temperature between 50 DEG -150 DEG F. below the beta transus temperature, cooling the alloy at a rate in excess of that produced by air cooling, and aging the material between about 900 DEG F. and 1100 DEG F. The resultant material has substantially improved crack growth behavior when contrasted with material processed according to the prior art.
-
公开(公告)号:DE3438495A1
公开(公告)日:1985-05-09
申请号:DE3438495
申请日:1984-10-19
Applicant: UNITED TECHNOLOGIES CORP
Inventor: BERCZIK DOUGLAS MICHAEL , BRODI GEORGE , O'CONNELL THOMAS EDWARD
Abstract: Process for improving the crack growth behavior of titanium alloys containing substantial beta stabilizers and at least 3% molybdenum, such as Ti-6-2-4-6. The process includes the steps of forging above the beta transus temperature, cooling at a controlled rate through the beta transus temperature, heating to a temperature between 50 DEG -150 DEG F. below the beta transus temperature, cooling the alloy at a rate in excess of that produced by air cooling, and aging the material between about 900 DEG F. and 1100 DEG F. The resultant material has substantially improved crack growth behavior when contrasted with material processed according to the prior art.
-
-
-
-
-