ALPHA,B TI BASE - AL, SN, ZR, MO, CR ALLOYS

    公开(公告)号:AU3287884A

    公开(公告)日:1985-05-09

    申请号:AU3287884

    申请日:1984-09-10

    Abstract: Process for improving the crack growth behavior of titanium alloys containing substantial beta stabilizers and at least 3% molybdenum, such as Ti-6-2-4-6. The process includes the steps of forging above the beta transus temperature, cooling at a controlled rate through the beta transus temperature, heating to a temperature between 50 DEG -150 DEG F. below the beta transus temperature, cooling the alloy at a rate in excess of that produced by air cooling, and aging the material between about 900 DEG F. and 1100 DEG F. The resultant material has substantially improved crack growth behavior when contrasted with material processed according to the prior art.

    TITANIUM-BASED ALLOY HAVING IMPROVED CRACK GROWTH BEHAVIOUR

    公开(公告)号:GB2148940A

    公开(公告)日:1985-06-05

    申请号:GB8425444

    申请日:1984-10-09

    Abstract: Process for improving the crack growth behavior of titanium alloys containing substantial beta stabilizers and at least 3% molybdenum, such as Ti-6-2-4-6. The process includes the steps of forging above the beta transus temperature, cooling at a controlled rate through the beta transus temperature, heating to a temperature between 50 DEG -150 DEG F. below the beta transus temperature, cooling the alloy at a rate in excess of that produced by air cooling, and aging the material between about 900 DEG F. and 1100 DEG F. The resultant material has substantially improved crack growth behavior when contrasted with material processed according to the prior art.

    3.
    发明专利
    未知

    公开(公告)号:DK516084A

    公开(公告)日:1985-05-01

    申请号:DK516084

    申请日:1984-10-30

    Abstract: Process for improving the crack growth behavior of titanium alloys containing substantial beta stabilizers and at least 3% molybdenum, such as Ti-6-2-4-6. The process includes the steps of forging above the beta transus temperature, cooling at a controlled rate through the beta transus temperature, heating to a temperature between 50 DEG -150 DEG F. below the beta transus temperature, cooling the alloy at a rate in excess of that produced by air cooling, and aging the material between about 900 DEG F. and 1100 DEG F. The resultant material has substantially improved crack growth behavior when contrasted with material processed according to the prior art.

    4.
    发明专利
    未知

    公开(公告)号:IT8423406D0

    公开(公告)日:1984-10-31

    申请号:IT2340684

    申请日:1984-10-31

    Abstract: Process for improving the crack growth behavior of titanium alloys containing substantial beta stabilizers and at least 3% molybdenum, such as Ti-6-2-4-6. The process includes the steps of forging above the beta transus temperature, cooling at a controlled rate through the beta transus temperature, heating to a temperature between 50 DEG -150 DEG F. below the beta transus temperature, cooling the alloy at a rate in excess of that produced by air cooling, and aging the material between about 900 DEG F. and 1100 DEG F. The resultant material has substantially improved crack growth behavior when contrasted with material processed according to the prior art.

    5.
    发明专利
    未知

    公开(公告)号:IT1177103B

    公开(公告)日:1987-08-26

    申请号:IT2340684

    申请日:1984-10-31

    Abstract: Process for improving the crack growth behavior of titanium alloys containing substantial beta stabilizers and at least 3% molybdenum, such as Ti-6-2-4-6. The process includes the steps of forging above the beta transus temperature, cooling at a controlled rate through the beta transus temperature, heating to a temperature between 50 DEG -150 DEG F. below the beta transus temperature, cooling the alloy at a rate in excess of that produced by air cooling, and aging the material between about 900 DEG F. and 1100 DEG F. The resultant material has substantially improved crack growth behavior when contrasted with material processed according to the prior art.

    TITANIUM-BASED ALLOY HAVING IMPROVED CRACK GROWTH BEHAVIOUR

    公开(公告)号:GB2148940B

    公开(公告)日:1987-05-28

    申请号:GB8425444

    申请日:1984-10-09

    Abstract: Process for improving the crack growth behavior of titanium alloys containing substantial beta stabilizers and at least 3% molybdenum, such as Ti-6-2-4-6. The process includes the steps of forging above the beta transus temperature, cooling at a controlled rate through the beta transus temperature, heating to a temperature between 50 DEG -150 DEG F. below the beta transus temperature, cooling the alloy at a rate in excess of that produced by air cooling, and aging the material between about 900 DEG F. and 1100 DEG F. The resultant material has substantially improved crack growth behavior when contrasted with material processed according to the prior art.

    7.
    发明专利
    未知

    公开(公告)号:NO844031L

    公开(公告)日:1985-05-02

    申请号:NO844031

    申请日:1984-10-09

    Abstract: Process for improving the crack growth behavior of titanium alloys containing substantial beta stabilizers and at least 3% molybdenum, such as Ti-6-2-4-6. The process includes the steps of forging above the beta transus temperature, cooling at a controlled rate through the beta transus temperature, heating to a temperature between 50 DEG -150 DEG F. below the beta transus temperature, cooling the alloy at a rate in excess of that produced by air cooling, and aging the material between about 900 DEG F. and 1100 DEG F. The resultant material has substantially improved crack growth behavior when contrasted with material processed according to the prior art.

    PROCESSING FOR TITANIUM ALLOYS
    9.
    发明专利

    公开(公告)号:CA1229249A

    公开(公告)日:1987-11-17

    申请号:CA456768

    申请日:1984-06-18

    Abstract: Improved Processing for Titanium Alloys Process for improving the crack growth behavior of titanium alloys containing substantial beta stabilizers and at least 3% molybdenum, such as Ti-6-2-4-6. The process includes the steps of forging above the beta transus temperature, cooling at a controlled rate through the beta transus temperature, heating to a temperature between 50-150.degree.F below the beta transus temperature, cooling the alloy at a rate in excess of that produced by air cooling, and aging the material between about 900.degree.F and 1100.degree.F. The resultant material has substantially improved crack growth behavior when contrasted with material processed according to the prior art.