公开(公告)号:KR1020100109677A
公开(公告)日:2010-10-11
申请号:KR1020090028051
申请日:2009-04-01
Applicant: 강원대학교산학협력단 , 한국건설기술연구원 , (주)삼우아이엠씨
IPC: C04B18/08 , C04B24/04 , C04B28/04 , C04B103/30
CPC classification number: Y02W30/92 , C04B18/08 , C04B28/02 , C04B2103/302 , C04B2111/00068 , C04B2111/0075 , C04B2201/05
Abstract: PURPOSE: A concrete composition for road pavement repairing is provided to reduce the water-cement rate by inserting an early-strength type water reducing agent and ultrafine fly ash. CONSTITUTION: A concrete composition for road pavement repairing for an early traffic opening contains 10~20wt% of ultrafine fly ash and 0.5~1wt% of early-strength type water reducing agent for 312~420kg of quick-setting cement. The ultrafine fly ash includes more than 6,000 grains of particles. The early-strength type water reducing agent includes a polycarboxylic acid based water reducing agent. The water-cement rate of the composition is 36~41wt%.
Abstract translation: 目的:通过插入早强型减水剂和超细粉煤灰,提供道路修补的混凝土组合物,以降低水泥率。 构成:早期交通开放路面修复的具体构成包含超细粉煤灰10〜20wt%,早强型减水剂0.5〜1wt%,速凝水泥312〜420kg。 超细粉煤灰包含6,000多颗颗粒。 早强型减水剂包括基于多元羧酸的减水剂。 组合物的水泥率为36〜41wt%。
-
202.소수성 폴리머 개질 조강 콘크리트 조성물 및 이를 이용한 콘크리트 구조물의 보수공법 有权
Title translation: 含高分子聚合物的高强度混凝土复合材料及使用复合材料的混凝土结构的修复方法公开(公告)号:KR100975586B1
公开(公告)日:2010-08-13
申请号:KR1020100031836
申请日:2010-04-07
Applicant: 주식회사 이레하이테크이앤씨 , 남경건설(주)
CPC classification number: C04B24/005 , C04B16/065 , C04B28/184 , C04B2201/05 , E04G23/02
Abstract: PURPOSE: A hydrophobic polymer modified blister steel concrete composition, and a repairing method of a concrete structure using thereof are provided to use a hydrophobic polymer copolymerized with ethylene-vinyl acetate to extend the curing time of concrete. CONSTITUTION: A hydrophobic polymer modified blister steel concrete composition contains 5~25wt% of cement binding material, 30~60wt% of fine aggregate, 20~50wt% of coarse aggregate, 0.5~5wt% of water, and 0.1~6wt% of hydrophobic polymer. The hydrophobic polymer includes hydrophobic acryl and an ethylene vinyl acetate emulsion. The hydrophobic acryl includes 1,1-dichloroethane, 2-hydroxy ethyl acrylate, 2-methoxycarbonyl -1-propene, and a reactive initiator.
Abstract translation: 目的:提供一种疏水性聚合物改性泡罩钢混凝土组合物及其使用的混凝土结构的修复方法,以使用与乙烯 - 乙酸乙烯酯共聚的疏水性聚合物来延长混凝土的固化时间。 构成:疏水聚合物改性起泡钢混凝土组合物含有5〜25wt%的水泥粘合剂,30〜60wt%的细骨料,20〜50wt%的粗骨料,0.5〜5wt%的水和0.1〜6wt%的疏水性 聚合物。 疏水性聚合物包括疏水性丙烯酸酯和乙烯 - 乙酸乙烯酯乳液。 疏水性丙烯酰基包括1,1-二氯乙烷,2-羟基乙基丙烯酸酯,2-甲氧基羰基-1-丙烯和反应性引发剂。
-
203.
公开(公告)号:KR1020090085451A
公开(公告)日:2009-08-07
申请号:KR1020080011354
申请日:2008-02-04
Applicant: (주)제이엔티아이엔씨
Inventor: 노재호
CPC classification number: E01C11/005 , C04B7/32 , C04B22/143 , C04B2103/54 , C04B2111/0075 , C04B2111/72 , C04B2201/05 , E01C7/35
Abstract: An early-strength polymer cement paste composition and a constructing and repairing method for pavement using the same are provided to show excellent durability and to secure driving stability and amenities. An early-strength polymer cement paste composition is composed of 100wt% of polymeric admixture solution and 20-200wt% of early-strength admixture solution. The content of the early-strength admixture solution is 70-130wt%. The polymeric admixture solution consists of 40-100wt% of gypsum, 0-60wt% of cement and 20-120wt% of polymeric solution.
Abstract translation: 提供早期强度的聚合物水泥浆料组合物以及使用其的路面施工和修复方法,以显示出优异的耐久性和确保驾驶的稳定性和便利性。 早期强度聚合物水泥浆组合物由100重量%的聚合物混合溶液和20-200重量%的早强混合溶液组成。 早强混合溶液的含量为70-130wt%。 聚合物混合溶液由40-100wt%的石膏,0-60wt%的水泥和20-120wt%的聚合物溶液组成。
-
公开(公告)号:KR101911009B1
公开(公告)日:2018-10-25
申请号:KR1020180026487
申请日:2018-03-06
Applicant: 연후산업 주식회사
IPC: C04B28/14 , C04B7/02 , C04B7/32 , C04B14/06 , C04B22/10 , C04B24/26 , E01C11/00 , C04B111/34 , C04B111/00 , C04B111/72
CPC classification number: C04B28/14 , C04B7/02 , C04B7/323 , C04B14/06 , C04B22/10 , C04B24/26 , C04B2111/0075 , C04B2111/343 , C04B2111/72 , C04B2201/05 , E01C11/005
Abstract: 본발명은내마모성및 균열저항성이우수한조강개질시멘트콘크리트조성물및 이를이용한도로포장보수·보강공법에관한것으로, 조강형결합재 1∼45중량%, 잔골재 5∼80중량%, 굵은골재 5∼80중량%, 기능개선혼화제 0.01∼30중량% 및물 1∼40중량%를포함한다. 상기조강형결합재는보통포틀랜드시멘트 20~90중량%, 칼슘또는마그네슘설포알루미네이트 3~45중량%, 트리칼슘알루미네이트시멘트 1~30중량%, 이산화규소 1~30중량%, 석고 1~20중량%, 하이드록시탄산마그네슘 0.1~20중량%, 알루민산스트론듐 0.01~15중량% 및알루미노실리케이트 0.01~15중량%를포함하고, 상기기능개선혼화제는메틸메타크릴레이트-스티렌공중합체 30∼99중량%, 폴리에틸렌옥사이드 0.1∼30중량%, 메틸아크릴레이트-비닐아세테이트공중합체 0.1∼25중량%, 부타디엔고무 0.1∼25중량%, 플루오린실란 0.1∼25중량%, 폴리칼본산계감수제 0.01~10중량% 및실리콘계소포제 0.01~10중량%를포함하는것을특징으로하는것이다. 본발명에의하면, 포졸란반응에의하여시멘트의초기수화및 조직의치밀화를촉진하여밀실한콘크리트를만들수 있어콘크리트의내마모성및 부착강도를개선하며, 특히팽창재와수축저감제를사용함으로써건조수축에의한표면균열및 팽창파괴현상을방지하는효과를얻었고내구성을크게향상시킬수 있다.
-
公开(公告)号:KR101888601B1
公开(公告)日:2018-08-14
申请号:KR1020170101455
申请日:2017-08-10
Applicant: 정진영
Inventor: 정진영
IPC: C04B14/04 , C04B24/38 , C04B28/16 , C04B7/02 , C04B7/32 , C04B111/00 , C04B103/14 , C04B103/30 , C04B103/22
CPC classification number: C04B14/042 , C04B7/02 , C04B7/323 , C04B24/38 , C04B28/16 , C04B2103/14 , C04B2103/22 , C04B2103/34 , C04B2111/0012 , C04B2201/05
Abstract: 본발명은틱소트로피성능을나타내는초속경시멘트조성물및 그조성물을이용한초속경콘크리트조성물에관한것으로, 더욱상세하게는상기초속경시멘트조성물은시멘트혼합물, 무수석고, 경화촉진제, 유동화제, 응결지연제및 개질제로이루어지며, 상기개질제는아타펄자이트와구아검이 1:0.5 내지 1 중량부로혼합되어이루어진다. 상기의성분으로이루어지는틱소트로피성능을나타내는초속경시멘트조성물은개질제로아타펄자이트와구아검의혼합물이사용되어틱소트로피성능이부여되며, 경사면과같은부위에대한우수한작업성및 시공성을나타내며, 과도한유동화제의사용없이도초기강도를발현할수 있는초속경콘크리트조성물을제공한다.
-
公开(公告)号:KR101839251B1
公开(公告)日:2018-04-26
申请号:KR1020160174926
申请日:2016-12-20
Applicant: 주식회사 포스코 , 재단법인 포항산업과학연구원
CPC classification number: Y02P40/143 , C01F11/46 , B09B3/00 , C04B7/153 , C04B22/141 , C04B22/146 , C04B2201/05 , Y02W30/52 , Y02W30/94
Abstract: 본발명은제철공정에서발생하는재생황산과 CaO 성분을다량함유한탈황슬래그미분말을이용하여보통시멘트또는슬래그시멘트의혼화재용알칼리석고제조방법및 이에의해제조된알칼리석고, 상기알칼리석고를포함하는시멘트용혼화재, 슬래그시멘트및 콘크리트조성물을제공하며, 상기알칼리석고는 CaO를포함하는탈황슬래그슬러리에황산을첨가하여반응시켜석고를제조하되, 상기반응이슬러리의 pH가알칼리영역내에서일어나도록황산을첨가하여제조된다.
-
207.시멘트 혼화재와 그 제조방법 및 상기 시멘트 혼화재를 포함한 시멘트 및 상기 시멘트 혼화재를 포함한 콘크리트 有权
Title translation: 水泥外加剂及其生产方法,以及包括水泥外加剂和含有水泥外加剂的混凝土的水泥公开(公告)号:KR1020170098431A
公开(公告)日:2017-08-30
申请号:KR1020160020302
申请日:2016-02-22
Applicant: 주식회사 영월이엔에스 , 신유근 , (주) 리포스
Inventor: 신유근
CPC classification number: Y02W30/91 , Y02W30/92 , Y02W30/93 , Y02W30/94 , C04B18/064 , C04B18/12 , C04B18/141 , C04B18/30 , C04B2201/05
Abstract: 본발명은시멘트혼화재와그 제조방법및 상기시멘트혼화재를포함한시멘트및 상기시멘트혼화재를포함한콘크리트에관한것으로서, 본발명에따른시멘트혼화재의제조방법은산화칼슘(CaO), 황산칼슘(CaSO) 및탄산칼슘(CaCO)을포함하는건식탈황석고와탄산칼슘(CaCO), 이산화규소(SiO)를포함하는폐수또는청수를 1차혼합및 교반하는단계, 상기건식탈황석고와폐수를 2차혼합및 교반하여혼합분말을제조하는단계, 상기혼합분말을성형하는단계, 상기혼합분말을숙성시키는단계및 상기혼합분말을건조시키는단계를포함하는것을특징으로한다.
Abstract translation: 本发明的水泥外加剂,和作为制造的方法,并且涉及一种混凝土含水泥和含有上述水泥外加剂,用于根据本发明,钙(CaO),硫酸钙(硫酸钙)和碳氧化物生产水泥掺和剂的过程中的水泥掺和剂 通过干式脱硫石膏和碳酸钙(碳酸钙),废水或含有含钙二氧化硅(SiO),碳酸钙(CaCO)主混合的步骤和搅拌下,将干法脱硫石膏和废水中的二次混合和搅拌淡水 准备混合粉末的工序,混合粉末的成形工序,熟化混合粉末的工序和干燥混合粉末的工序。
-
208.
公开(公告)号:KR101750831B1
公开(公告)日:2017-06-26
申请号:KR1020160150381
申请日:2016-11-11
CPC classification number: Y02P40/143 , Y02W30/92 , Y02W30/94 , C04B7/17 , C04B18/08 , C04B18/141 , C04B22/064 , C04B28/065 , C04B2103/302 , C04B2201/05
Abstract: 본발명은콘크리트의조기강도및 장기강도가향상되고, 점성이낮아시공성과압송성이좋으며, 수화열이적게방출되어온도균열및 수축균열을저감시킬수 있는저점성저발열결합재및 이를이용한저점성저발열고강도콘크리트조성물에관한것이다.본발명은「저점성시멘트 40~50wt%; 고로슬래그미분말 20~30wt%; 플라이애시 10~25wt%; 및무기계활성화재 1.0~5.0wt%; 를포함하는저점성저발열결합재」를제공한다.
Abstract translation: 本发明提高了早期强度和混凝土的长期强度,高度和压送通过使用水化热特性粘度,低建设,低seongjeo加热高强度混凝土被释放sikilsu减小的收缩温度裂缝和低seongjeo加热开裂粘合剂和更少它 本发明涉及一种组合物,其包含“低粘度水泥40至50重量% 20〜30重量%的高炉矿渣粉末; 粉煤灰10至25重量%; 和1.0-5.0重量%的无机活化剂; “低熔点硫化剂”
-
公开(公告)号:KR101708214B1
公开(公告)日:2017-02-21
申请号:KR1020160132594
申请日:2016-10-13
Applicant: 주식회사 하나레미콘
Inventor: 우영삼
IPC: C04B18/14 , C04B18/08 , C04B28/04 , C04B28/08 , C04B28/02 , C04B16/06 , C04B14/06 , C04B14/30 , C04B14/36 , C04B22/14
CPC classification number: Y02W30/92 , Y02W30/94 , C04B18/141 , C04B14/06 , C04B14/30 , C04B14/365 , C04B16/06 , C04B18/08 , C04B22/143 , C04B28/021 , C04B28/04 , C04B28/082 , C04B2201/05
Abstract: 본발명은친환경레미콘조성물및 그제조방법에관한것으로, 골재, 결합재, 물및 혼화제를혼합한혼합물에강도증진재및 유해물질저감재를포함하는것을기술적특징으로하며, 시멘트사용량감소에따른초기강도저하를개선할수 있을뿐만아니라 6가크롬, 중금속등 유해물질발생을저감시킬수 있는장점이있으며, 아파트, 빌딩, 단독주택등의건축물에사용할수 있다.
-
公开(公告)号:KR101706272B1
公开(公告)日:2017-02-13
申请号:KR1020160105484
申请日:2016-08-19
Applicant: (주) 캐어콘
IPC: C04B18/06 , C04B18/14 , C04B7/32 , E01D22/00 , E04G23/02 , C04B103/44 , C04B111/72 , C04B103/30
CPC classification number: Y02W30/92 , Y02W30/94 , C04B18/061 , C04B7/323 , C04B18/146 , C04B2103/306 , C04B2103/44 , C04B2111/72 , C04B2201/05 , E01D22/00 , E04G23/02
Abstract: 본발명의콘크리트보수용모르타르조성물은유동층보일러애시 1 ~ 20 중량%; 시멘트 5 ~ 30 중량%; 실리카흄 1 ~ 4 중량%; 속경 CSA(Calcium Sulfo-Aluminate) 1 ~ 8 중량%; 멜라민계유동화제 0.2 ~ 0.6 중량%; 팽창재 2 ~ 5 중량%; 증점제 0.01 ~ 0.1 중량%; 골재 40 ~ 60 중량%;를포함한다. 유동층보일러애시는 SiO: 3.49 ~ 18.6 중량%; NaO : 0.05 ~ 0.32 중량%; MgO : 0.87 ~ 3.31 중량%; KO : 0.08 ~ 0.69 중량%; CaO : 29.7 ~ 58.2 중량%; FeO: 0.26 ~ 3.54 중량%; AlO: 0.28 ~ 7.47 중량%; SO: 14.6 ~ 26.0 중량%; 잔여고형물 : 10.6 ~ 20.9 중량%를포함하는것이바람직하다.
-
-
-
-
-
-
-
-
-