TRIBOCERAMIC COMPOUND
    278.
    发明申请
    TRIBOCERAMIC COMPOUND 审中-公开
    TRIBOCERAMIC化合物

    公开(公告)号:WO2009041795A4

    公开(公告)日:2009-05-22

    申请号:PCT/LV2008000009

    申请日:2008-09-26

    Inventor: KESNERS MARIS

    Abstract: The present invention relates to the machine buiding industry and it is used for coating of friction surfaces by triboceramics to decrease wear and to reduce the friction coefficient. The triboceramic compound contains oxides - magnesium oxide MgO, silica SiO2, alumine Al2O3, calcium oxide CaO, ferric oxide Fe2O3, being in the chemical composition of serpentine and talc, the natural and/or synthesized heat unprocessed and/or dehydrated minerals - serpentine, talc, clinochlore, magnesite, quartz and aluminium hydroxide are introduced forming a mixture with the following composition of oxides, in mass %: SiO2-46-54; MgO - 26-32, Al2O3- 2-5; Fe2O3 - 1,0-1,5; CaO - 0,1-0,3, water H2O - 5 or less.

    Abstract translation: 本发明涉及机器制造行业,并且其被用于通过摩擦陶瓷涂覆摩擦表面以减少磨损并降低摩擦系数。 该三硼化陶瓷化合物含有氧化物 - 氧化镁MgO,二氧化硅SiO2,铝Al2O3,氧化钙CaO,氧化铁Fe2O3,其化学组成为蛇纹石和滑石,天然和/或合成热未加工和/或脱水矿物 - 蛇纹石, 导入滑石,斜绿泥石,菱镁矿,石英和氢氧化铝,形成具有以下质量百分比的氧化物组成的混合物的混合物:SiO 2 -46-54; MgO-26-32,Al 2 O 3 -2-5; Fe2O3 - 1,0-1,5; CaO - 0,1-0,3,水H2O - 5或更少。

    LUBRICATION OF MAGNESIUM WORKPIECES FOR HOT FORMING
    279.
    发明申请
    LUBRICATION OF MAGNESIUM WORKPIECES FOR HOT FORMING 审中-公开
    用于热成型的镁工件的润滑

    公开(公告)号:WO2008095150A1

    公开(公告)日:2008-08-07

    申请号:PCT/US2008/052737

    申请日:2008-02-01

    Abstract: The elevated temperature forming of magnesium based alloy workpieces by stretching, drawing, bending (or the like) a surface of the heated workpiece over the forming surface of a forming tool is improved by forming an integral adherent layer of magnesium hydroxide on the tool- contacted surface(s) of the magnesium alloy workpiece. The magnesium hydroxide layer may be formed by treating the surface(s) of the sheet with an aqueous salt solution (e.g., sodium chloride) at a temperature and for a time to form a protective layer of desired thickness (e.g., up to about thirty micrometers). If desired, an additional layer of forming lubricant, such as a film comprising boron nitride, may be applied to the magnesium hydroxide layer.

    Abstract translation: 通过在成形工具的成形表面上通过拉伸,拉伸,弯曲(或类似)加热的工件的表面在镁合金工件上升高的温度形成,通过在工具接触上形成一体的氢氧化镁粘附层 镁合金工件的表面。 氢氧化镁层可以通过在温度和温度下用盐水溶液(例如氯化钠)处理片材的表面而形成,以形成所需厚度的保护层(例如,高达约三十 微米)。 如果需要,可以向氢氧化镁层施加附加的成形润滑剂层,例如包含氮化硼的膜。