광파이버를 이용한 전류 및 전압 동시측정장치 및 방법
    21.
    发明公开
    광파이버를 이용한 전류 및 전압 동시측정장치 및 방법 失效
    同时通过使用光纤同时测量电流和电压的装置及其相关方法

    公开(公告)号:KR1020040020345A

    公开(公告)日:2004-03-09

    申请号:KR1020020051939

    申请日:2002-08-30

    Abstract: PURPOSE: An apparatus for simultaneously measuring a current and a voltage by using an optical fiber and a method for the same are provided, which are installed more easier than a conventional electric transformer or a conventional crystal optic sensor. CONSTITUTION: An apparatus for simultaneously measuring a current and a voltage by using an optical fiber includes a laser(1), a first polarization plate(2), a polarization modulator(3), a sensor head(4), a second polarization plate(5), an optical detector(6), a lock-in amplifier(8) and a converting block. The laser(1) generates a laser beam and the first polarization plate(2) deflects the laser beam generated from the laser(1) at a predetermined angle. The polarization modulator(3) generates an electrical signal for the reference voltage and periodically modulates the linear polarized light into a circular polarized light. The sensor head(4) induces the changes of the linear polarized light for the current and the circular polarized light for the voltage. The second polarization plate(5) makes the output light of the sensor head(4) to be polarized at a predetermined angle. The optical detector(6) changes the output light of the second polarization plate(5) into an electrical signal. The lock-in amplifier(8) measures the amount of changes of the circular light by receiving the electrical signal of the polarization modulator(3) and the optical detector(6). And, the converting block converting the amount of polarization changes of the lock-in amplifier(8) into the values of a current and the voltage.

    Abstract translation: 目的:提供一种通过使用光纤同时测量电流和电压的装置及其方法,其比常规电变压器或常规晶体光学传感器更容易安装。 构成:通过使用光纤同时测量电流和电压的装置包括激光器(1),第一偏振片(2),偏振调制器(3),传感器头(4),第二偏振片 (5),光学检测器(6),锁定放大器(8)和转换块。 激光器(1)产生激光束,并且第一偏振板(2)使从激光器(1)产生的激光束以预定角度偏转。 偏振调制器(3)产生用于参考电压的电信号,并将线性偏振光周期性地调制为圆偏振光。 传感器头(4)引起用于电流的线偏振光和用于电压的圆偏振光的变化。 第二偏振板(5)使传感器头(4)的输出光以预定角度偏振。 光检测器(6)将第二偏振板(5)的输出光改变为电信号。 锁定放大器(8)通过接收偏振调制器(3)和光学检测器(6)的电信号来测量圆形光的变化量。 并且,转换块将锁定放大器(8)的极化变化量转换成电流和电压值。

    광섬유를 이용한 도플러 편이 측정장치
    22.
    发明公开
    광섬유를 이용한 도플러 편이 측정장치 无效
    通过使用光纤测量多普勒频移的装置

    公开(公告)号:KR1020030053105A

    公开(公告)日:2003-06-28

    申请号:KR1020010083143

    申请日:2001-12-22

    CPC classification number: G01B9/02023 G01D5/268 G01D5/353 G02B2006/12111

    Abstract: PURPOSE: An apparatus for measuring Doppler shift by using an optical fiber is provided to measure correctly the Doppler shift regardlessly of the external vibration by improving the sensitivity of a sensor. CONSTITUTION: A Doppler shift measurement apparatus includes a collecting lens(10), a Doppler shift sensor(20), and a beam detector(36). The collecting lens is used for collecting the scattered light generated from a laser beam. The Doppler shift sensor receives the scattered light from the collecting lens and analyzes the multiple reflection of the scattered light and the frequency of the scattered light. The beam detector is connected to the Doppler shift sensor. The Doppler shift sensor includes an inlet portion(22) for receiving the scattered light, an optical fiber coupler(24) formed at a rear portion of the inlet portion, an optical fiber splitter(28) for splitting the scattered light, and a circulation portion for circulating partially the scattered light.

    Abstract translation: 目的:提供一种通过使用光纤测量多普勒频移的装置,通过提高传感器的灵敏度,正确地测量多普勒频移,无论外部振动如何。 构成:多普勒频移测量装置包括收集透镜(10),多普勒频移传感器(20)和光束检测器(36)。 收集透镜用于收集由激光束产生的散射光。 多普勒频移传感器接收来自收集透镜的散射光,并分析散射光的多重反射和散射光的频率。 光束检测器连接到多普勒频移传感器。 多普勒频移传感器包括用于接收散射光的入口部分(22),形成在入口部分后部的光纤耦合器(24),用于分散散射光的光纤分离器(28) 用于部分地散射散射光的部分。

    형강의 용접부분 도료 코팅 방지용 테이프부착 장치 및 방법
    23.
    发明公开
    형강의 용접부분 도료 코팅 방지용 테이프부착 장치 및 방법 有权
    焊接部分焊接部位的涂料附着胶带附着装置及其方法

    公开(公告)号:KR1020030053083A

    公开(公告)日:2003-06-28

    申请号:KR1020010083116

    申请日:2001-12-22

    CPC classification number: C09J2203/31

    Abstract: PURPOSE: Provided is a tape attachment equipment for paint coating prevention in a welding part of a section steel which lets the welding part attached by a tape to secure the welding part so that it bars zinc paint from being attached to the welding part. CONSTITUTION: The tape attachment equipment for paint coating prevention in the welding part of the section steel comprises the parts of: a fixing part(20) which lets a tape(14,16) held before attaching, in which the tape covers upper and lower side of the transferred section steel; a tape cutting part(22) which cuts the tape after attaching; and an upper(24) and a lower(26) roller for compression which let the tape attached effectively.

    Abstract translation: 目的:提供一种用于在钢的焊接部分中防止涂漆的胶带附着设备,其使焊接部分通过胶带附接以固定焊接部分,使得锌涂料不粘附到焊接部件。 构成:用于在钢板焊接部分防止涂漆的胶带附着装置包括以下部分:固定部分(20),其使胶带(14,16)在连接之前保持,其中胶带覆盖上部和下部 转移段钢; 安装后切割带的带切割部分(22); 以及用于压缩的上(24)和下(26)辊,其使带有效地附接。

    티타늄화합물피막의제조방법
    24.
    发明授权
    티타늄화합물피막의제조방법 失效
    生产钛化合物涂层的方法

    公开(公告)号:KR100298599B1

    公开(公告)日:2001-11-22

    申请号:KR1019980053862

    申请日:1998-12-09

    Inventor: 정재인 박형국

    Abstract: 본 발명은 시계와 같은 대인 장식용 제품의 장식성 향상 및 공구나 기계류 그리고 금형제품과 같은 제품의 수명향상을 위하여 이에 이용되는 부속판 등에 스퍼터링 증발원을 이용하여 반응성 스퍼터링에 의한 티타늄 화합물 피막을 형성시키는 방법에 관한 것으로, 불활성가스와 반응성 가스가 혼합된 가스 분위기에서 증발원으로 티타늄 타겟이 장착된 스퍼터링 증발원을 이용하고 글로우 방전을 이용하여 이루어지는 티타늄 화합물 피막의 제조방법에 있어서, 증발원으로 비평형 마그네트론 스퍼터링 증발원을 이용하되, 전자석의 전류를 2~5A로 하고, 기판전류를 1.5mA/cm
    2 이상으로 조절하여 제조하는 것을 특징으로 하여, 밀착력과 색상의 밝기 등과, 피막의 특성이 대폭 향상될 뿐만 아니라, 150℃ 이하의 저온에서도 피막제조가 가능하여 기존 방식으 로 불가능하였던 플라스틱과 같은 온도에 민감한 소재에도 코팅이 가능하기 때문에 소재의 선택 폭을 넓힐 수 있는 효과가 있다.

    고진공마그네트론스퍼터링방법
    25.
    发明授权
    고진공마그네트론스퍼터링방법 失效
    高真空磁控溅射法

    公开(公告)号:KR100295617B1

    公开(公告)日:2001-10-26

    申请号:KR1019980057576

    申请日:1998-12-23

    Inventor: 박형국 정재인

    Abstract: 본 발명은 진공 증착법 중의 하나인 마그네트론 스퍼터링에서 타겟 주위에 이온과 전자를 공급시켜 고진공에서도 마그네트론 스퍼터링을 작동시킬 수 있도록 한 고진공 마그네트론 스퍼터링방법에 관한 것으로, 마그네트론 스퍼터링장치를 사용하여 마그네트론 스퍼터링 작업을 행함에 있어서, 타겟(18)을 향하여 설치되어 방전가스를 공급하는 가스주입구(12)의 주위에 필라멘트(9)를 설치하고, 상기 필라멘트(9)의 주위에 양극(8)과 영구자석(7)을 설치한 후, 상기 필라멘트(9)에 전원을 공급하고 상기 양극(8)에 전압을 공급함으로써, 상기 필라멘트(9)에서 발생되는 전자와 상기 영구자석(7)의 자기장에 의해 이온화된 방전가스 이온이 상기 타겟(18)을 향하여 공급되도록 함을 특징으로 한다.

    냉연강판 실시간 표면조도 측정방법
    26.
    发明公开
    냉연강판 실시간 표면조도 측정방법 无效
    实时测量冷轧钢板表面粗糙度的方法

    公开(公告)号:KR1020010060790A

    公开(公告)日:2001-07-07

    申请号:KR1019990063232

    申请日:1999-12-28

    CPC classification number: B21B38/00 B21B2261/14 G01B11/30

    Abstract: PURPOSE: A method for real-time measuring the surface roughness of a cold rolled steel sheet is provided to measure the surface roughness of the steel sheet by measuring intensity and scattering distribution of specular reflecting light scattered using an infrared rays CCD after entering an infrared ray laser to the steel sheet. CONSTITUTION: In a method for real-time measuring the surface roughness of a cold rolled steel sheet, the method is characterized in that the surface roughness of the steel sheet which is within the range of 1.2 to 1.8 microns is measured using the following Mathematical Expression that is standardized by measuring an intensity (Is) and a scattering distribution of specular reflecting light scattered using an infrared rays CCD after entering an infrared ray laser light to the steel sheet, and measuring pixel numbers at the point that is 1/2 of the intensity (Is) of specular reflecting light: (Mathematical Expression) where Is is an intensity of specular reflecting light, σ is an RMS surface roughness, θ is a laser incidence angle, λ is a laser wavelength, and Pn is a pixel number at the point that is 1/2 of the intensity of specular reflecting light.

    Abstract translation: 目的:提供一种用于实时测量冷轧钢板的表面粗糙度的方法,通过测量进入红外线后使用红外线CCD散射的镜面反射光的强度和散射分布来测量钢板的表面粗糙度 激光到钢板。 构成:在冷轧钢板的表面粗糙度的实时测定方法中,该方法的特征在于,使用以下数学式求出钢板的表面粗糙度在1.2〜1.8微米的范围内 通过测量在对钢板进入红外线激光后使用红外线CCD散射的镜面反射光的强度(Is)和散射分布进行标准化,并且测量在该钢板的1/2的点处的像素数 镜面反射光的强度(Is):(数学表达式)其中,Is是镜面反射光的强度,σ是RMS表面粗糙度, 是激光入射角,λ是激光波长,Pn是在镜面反射光的强度的1/2的点处的像素数。

    질화티타늄 박막의 제조방법
    27.
    发明公开
    질화티타늄 박막의 제조방법 失效
    硝基钛薄膜的制备方法

    公开(公告)号:KR1020010017223A

    公开(公告)日:2001-03-05

    申请号:KR1019990032613

    申请日:1999-08-09

    Inventor: 정재인 박형국

    CPC classification number: C01B21/076 C01G23/00 C23C14/0641

    Abstract: PURPOSE: A method for preparing titanium nitride thin film is provided which is able to prevent deterioration of characteristics thereof such as an adhesive property and brightness of color according to distance increase between evaporation source and base plate. CONSTITUTION: The titanium nitride thin film is prepared by using a sputtering evaporation source having a titanium target and a glow discharge under a mixture gas of an inert gas and a reactive gas atmosphere, wherein non-equivalent magnetron sputtering evaporation source is used as the evaporation source and two evaporation sources(2)(2') are placed in opposite side of each other and the strength of the magnetic field at the center part of a base plate(4) is controlled to be more than 15 gauss by inducing a magnetic field of two electromagnets(3)(3') to be put together near the base plate(4) and wrap the base plate(4).

    Abstract translation: 目的:提供一种用于制备氮化钛薄膜的方法,其能够防止根据蒸发源和基板之间的距离增加的颜色的粘合性和亮度等特性的劣化。 构成:通过使用具有钛靶的溅射蒸发源和在惰性气体和反应气体气氛的混合气体下的辉光放电来制备氮化钛薄膜,其中使用非等效磁控溅射蒸发源作为蒸发 源极和两个蒸发源(2)(2')放置在彼此的相对侧,并且通过诱导磁场将基板(4)的中心部分处的磁场的强度控制为大于15高斯 将两个电磁体(3)(3')的场放在基板(4)附近并包裹基板(4)。

    도금강판의파우더링성평가방법
    28.
    发明授权
    도금강판의파우더링성평가방법 失效
    供应涂料评价方法

    公开(公告)号:KR100262671B1

    公开(公告)日:2000-08-01

    申请号:KR1019970071705

    申请日:1997-12-22

    Abstract: PURPOSE: An evaluation method for the powdering property of a plated steel plate is provided, which can evaluate the powdering property even though the thickness of plated steel plate is changed by using scratch without any additional bending device and can evaluate the property repeatedly, thereby improving the reliability of evaluation. CONSTITUTION: The evaluation method is as follows: (i) form a scratch of a fixed depth on the plated layer of electroplated steel plate by increasing vertical drag force to 0-200 N using diamond tip of scratch tester equipped with sonic wave measuring device for causing ablation of powder (powdering) of plated layer; (ii) quantify the powdering degree by scotch tape; and (iii) evaluate the powdering degree by the quantified degree.

    Abstract translation: 目的:提供一种电镀钢板的粉化特性的评价方法,即使在没有任何附加的弯曲装置的情况下,通过刮擦来改变镀覆钢板的厚度,也能够评价粉化性,能够重复地评价其特性, 评估的可靠性。 规定:评估方法如下:(i)通过使用装备有声波测量装置的划痕测试仪的金刚石尖端将垂直牵引力增加至0-200N,在电镀钢板的镀层上形成固定深度的划痕 引起镀层粉末(粉化)的消融; (ii)通过透明胶带量化粉化度; 和(iii)以量化度评估粉化程度。

    이온빔을이용한고진공마그네트론스퍼터링방법
    29.
    发明公开
    이온빔을이용한고진공마그네트론스퍼터링방법 失效
    使用离子束喷射高真空磁体的方法

    公开(公告)号:KR1020000041638A

    公开(公告)日:2000-07-15

    申请号:KR1019980057577

    申请日:1998-12-23

    Inventor: 박형국 정재인

    CPC classification number: C23C14/0052 C23C14/354 C23C14/46

    Abstract: PURPOSE: A sputtering method of high vacuum magnetron using an ion beam is provided to operate a magnetron sputtering in a high vacuum by supplying an ion around a target with using the ion beam. CONSTITUTION: An inside of a vacuum container(1) is filled with 1X10¬-4Torr by injecting an argon gas inside a discharging gas container(9) when the vacuum container(1) is reached about 1X10¬-6Torr by ventilating with a turbo molecular pump. An ion beam(6) is operated and an ion generated from the ion beam(6) is supplied to a target(7) and a substrate(3) at the same time. Because a magnetron sputtering(2) is installed to inclined face of the ion beam(6), the ion generated from the ion beam(6) is sent to the target(7) and the substrate(3) installed in the magnetron sputtering(2). When a voltage over 400V is fed to the target(7) through a voltage feeding device of sputtering(11), a plasma is generated around the target(7) by generating the magnetron sputtering(2). To inject oxygen or nitrogen in a reacting gas container(8) into the vacuum container(1) through the gas inlet(12), an intended thin film of compound is deposited.

    Abstract translation: 目的:提供使用离子束的高真空磁控管的溅射方法,通过使用离子束在靶上提供离子来在高真空中操作磁控溅射。 构成:当真空容器(1)通过涡轮通风达到约1X10-6Torr时,通过在排放气体容器(9)内注入氩气,在1×10 -4乇内填充真空容器(1)的内部 分子泵。 操作离子束(6),并且从离子束(6)产生的离子同时被供给到靶(7)和基板(3)。 由于磁控管溅射(2)安装在离子束(6)的倾斜面上,所以从离子束(6)产生的离子被传送到靶(7)和安装在磁控溅射中的基片(3) 2)。 当通过溅射(11)的电压馈送装置将超过400V的电压馈送到目标(7)时,通过产生磁控溅射(2)在靶(7)周围产生等离子体。 为了通过气体入口(12)将反应气体容器(8)中的氧气或氮气注入真空容器(1)中,沉积了预期的化合物薄膜。

    아연계 도금강판의 파우더링성 및 도금밀착성 동시 측정방법
    30.
    发明授权
    아연계 도금강판의 파우더링성 및 도금밀착성 동시 측정방법 失效
    评估钢铁中Zn- / BA涂层的粘合和粉末的方法

    公开(公告)号:KR100544626B1

    公开(公告)日:2007-11-09

    申请号:KR1019980053860

    申请日:1998-12-09

    Inventor: 박형국 정재인

    Abstract: 본 발명은 본 발명은 아연계 전기도금강판의 파우더링성 및 도금밀착성을 평가하는 방법에 관한 것으로서, 시편(1)에 다이아몬드 팁(2)으로 수직힘을 가하는 단계와; 시편이송장치(4)로 시편(1)을 이동시켜 도금층을 박리시키는 단계와; 상기 도금층이 박리될 때 발생하는 음파를 음파측정기(5)로 측정하는 단계와; 측정된 아날로그 음파신호를 아날로그/디지털 변환기(8)에 의해 디지털 신호로 변환하는 단계와; 변환된 디지털 음파신호를 컴퓨터(9)에 인가하여 도금밀착성을 측정하는 단계와; 램프(10)의 광을 시편(1)에 조사하는 단계와; 시편(1)에서 반사되는 반사광을 광파이버(6)와 광커플러(21)를 통해 디지털 카메라(7)로 포착하는 단계와; 상기 디지털 카메라(7)에 포착된 도금층의 영상을 컴퓨터(9)로 전송하는 단계와; 상기 도금층의 영상에서 파우더가 발생하는 시점의 거리와 그때 다이아몬드 팁(2)에 가해준 힘을 연관시켜 파우더가 발생하기 시작할 때의 힘으로 아연계 도금강판의 파우더링성을 측정하여 정량화 하는 단계로 이루어져 간편하고 정량화된 평가방법으로 추가장치 및 작업이 필요 없는 경제적 효과가 있는 아연계 도금강판의 파우더링성 및 도금밀착성 동시 측정방법이다.