Abstract:
그래핀 코팅층을 포함하는 동축 케이블 및 제조방법이 개시된다. 본 발명의 일 실시예에 따른 동축 케이블은 코어에 위치하는 금속 선재; 금속 선재와 동종 또는 이종 금속과, 제1 그래핀이 혼합된 형태를 갖는 것으로, 금속 선재 표면에 도금 형성되는 복합도금층; 및 복합도금층 표면에 제2 그래핀이 코팅 형성되는 그래핀 코팅층을 포함한다.
Abstract:
Disclosed are a barrier film composite based on graphene and a method for manufacturing the same. The barrier film composite according to an embodiment of the present invention is a barrier film composite having a first barrier layer, a second barrier layer, and a graphene layer stacked, wherein the first barrier layer includes an inorganic material, and the second barrier layer includes an organic polymer material.
Abstract:
Disclosed is a method of manufacturing a metal foam-graphite heat dissipating sheet. According to an embodiment of the present invention, the method of manufacturing a metal foam-graphite heat dissipating sheet includes: a first step of coating the surface of porous metal foam having multiple pores with functionalized graphene oxide or reduced graphene oxide; and a second step of inserting expandable graphite particles in at least some of the pores.
Abstract:
본 발명은, 본 발명은, 이온저장층과 전해질층 사이에 그래핀층을 형성하고, 또는 이온저장층과 전해질층 사이 및 기판위에 그래핀 투명전극을 형성한 전기변색소자를 제공하는 것이며, 그래핀층에 패턴을 형성하여 전기변색되는 부분을 제한하여 변색되는 영역이 소정의 패턴을 갖도록 할 수도 있다. 본 발명에 따른 전기변색소자의 그래핀 전극은, 그래핀 혹은 기능화된 그래핀으로 사용하여, 이온저장층과 전해질층 사이에 그래핀층을 형성시켜 전극의 손상을 방지하였으며, 또한 기존 그래핀 전극이 가지고 있던 낮은 전기전도도 문제를 해결하였고, 균일성을 확보하며 내화학성을 증가시킨다.
Abstract:
PURPOSE: A method for manufacturing a graphene hybrid film is provided to maintain a low level surface roughness of a hexagonal boron nitride layer by forming the layer using a catalyst-free substrate and to improve the quality of graphene. CONSTITUTION: A method for manufacturing a graphene hybrid film(100) comprises: a step of forming a hexagonal boron nitride layer(130) on a catalyst-free substrate(110); a step of forming a metal catalyst layer(150) on the hexagonal boron nitride layer; a step of supplying carbon to the metal catalyst layer and forming one or more lower graphene layers(170) and upper graphene layers(190) at the lower portion and the upper portion of the metal catalyst layer, respectively; and a step of removing the metal catalyst layer and the upper graphene layer. The catalyst free substrate is selected among a Si substrate, a Si/Si02 substrate, a sapphire substrate, a quartz substrate, and a glass substrate. The metal catalyst layer is one or more metals or alloys selected from a group consisting of silicon, Ni, Co, Fe, Pt, Au, Al, Cr, Cu, Mg, Mn, Mo, Rh, Si, Ta, Ti, W, U, V, Zr, brass, bronze, white copper, stainless steel, and Ge.