公开(公告)号:KR1020140085247A
公开(公告)日:2014-07-07
申请号:KR1020120155602
申请日:2012-12-27
Applicant: 제일모직주식회사
CPC classification number: C08G64/06 , B29C47/0021 , B29C47/92 , B29C2947/92152 , B29C2947/92209 , B29C2947/92647 , B29C2947/92704 , C08G64/307 , C08G64/04 , C08G64/1608 , C08G64/28 , C08J5/18 , C08L69/00
Abstract: A polycarbonate resin for a film of the present invention comprises: a repeat unit represented by chemical formula 1 of claim 1; a repeat unit represented by chemical formula 2 of claim 1; and a repeat unit represented by chemical formula 3 of claim 1, and is characterized by having the weight-average molecular weight of 15,000-60,000 g/mol and the flow index of 3-40 g/10 min. The polycarbonate resin for a film has excellent scratch resistance, tensile elongation, chemical resistance and heat resistance and is able to manufacture a film of a roll shape without a protective film.
Abstract translation: 本发明的膜用聚碳酸酯树脂包括:由权利要求1的化学式1表示的重复单元; 由权利要求1的化学式2表示的重复单元; 和由权利要求1的化学式3表示的重复单元,其特征在于重均分子量为15,000-60,000g / mol,流动指数为3-40g / 10min。 用于膜的聚碳酸酯树脂具有优异的耐擦伤性,拉伸伸长率,耐化学性和耐热性,并且能够制造没有保护膜的辊状膜。
-
公开(公告)号:KR1020140077581A
公开(公告)日:2014-06-24
申请号:KR1020120146546
申请日:2012-12-14
Applicant: 제일모직주식회사
CPC classification number: C08L69/00 , C08K5/0066 , C08K5/523
Abstract: A polycarbonate resin composition according to the present invention comprises: a polycarbonate component including an aromatic polycarbonate resin and a copolymerized polycarbonate resin including a repetitive unit represented by chemical formula 1 and a repetitive unit represented by chemical formula 2; and a flame retardant. The polycarbonate resin composition has a scratch width of 310 μm or less as measured by a Ball-type Scratch Profile (BSP) test; a pencil hardness rating of F or higher; a flame retardancy level of V-0 or higher as measured on a 2.0 mm-thick specimen according to UL94; and a transmittance of 80% or more as measured in accordance with ASTM D1003. The polycarbonate resin composition can exhibit excellent scratch resistance, flame retardancy and transparency. In chemical formula 2, R_1 and R_2 are each independently substituted or unsubstituted C1 to C6 alkyl groups, and a and b are each independently an integer from 1 to 4.
Abstract translation: 根据本发明的聚碳酸酯树脂组合物包括:包含芳族聚碳酸酯树脂的聚碳酸酯组分和包含由化学式1表示的重复单元和由化学式2表示的重复单元的共聚聚碳酸酯树脂; 和阻燃剂。 聚碳酸酯树脂组合物通过球形划痕(BSP)试验测得的刮擦宽度为310μm以下。 铅笔硬度等级F以上; 根据UL94在2.0mm厚的样品上测量的V-0或更高的阻燃水平; 并且根据ASTM D1003测量的透光率为80%以上。 聚碳酸酯树脂组合物可以表现出优异的耐刮擦性,阻燃性和透明性。 在化学式2中,R 1和R 2各自独立地为取代或未取代的C1至C6烷基,a和b各自独立地为1至4的整数。
-
公开(公告)号:KR1020130078603A
公开(公告)日:2013-07-10
申请号:KR1020110147628
申请日:2011-12-30
Applicant: 제일모직주식회사
Abstract: PURPOSE: A manufacturing method of polycarbonate is provided to offer the polycarbonate which improves the physical property including low temperature impact intensity, weather-resistant, and high temperature stability etc. CONSTITUTION: A manufacturing method of polycarbonate comprises: a step which polymerizes an aromatic series dihydroxy compound and diaryl carbonate under the presence of a first catalyst; a step which inputs an end-capping agent; a step which inputs an acid compound. The manufacturing method additionally comprises a step which inputs additives after the step which inputs the acid compound. The polymerization reaction is a fusion polymerization reaction. The end-capping agent is inputted as the amount of 100-6,000 ppm for the aromatic dihydroxy compound.
Abstract translation: 目的:提供聚碳酸酯的制造方法,提供改善包括低温冲击强度,耐候性和高温稳定性等的物理性能的聚碳酸酯。构成:聚碳酸酯的制造方法包括:将芳族系列 二羟基化合物和碳酸二芳基酯在第一催化剂存在下反应; 输入端帽剂的步骤; 输入酸化合物的步骤。 该制造方法还包括在输入酸化合物的步骤之后输入添加剂的步骤。 聚合反应是聚合反应。 对于芳族二羟基化合物,封端剂的输入量为100-6,000ppm。
-
公开(公告)号:KR1020130056127A
公开(公告)日:2013-05-29
申请号:KR1020110121903
申请日:2011-11-21
Applicant: 제일모직주식회사
CPC classification number: C08G64/06 , C08G64/307 , G02B1/04 , C08L69/00
Abstract: PURPOSE: A polycarbonate is provided to have excellent scratch resistance, chemical resistance, flexibility, room temperature/low temperature impact strength, and heat resistance. CONSTITUTION: A polycarbonate comprises repeating units represented by chemical formula 1, chemical formula 2, and chemical formula 3. In chemical formula 1 and 2, each of R1 and R2 is independently C1-C6 alkyl group, each of a and b is an integer from 0-4. In chemical formula 3, each of R1 and R2 is a substituted or unsubstituted C1-C6 alkyl group; each of a and b is independently an integer from 1-4. In chemical formula 3, each of R1 and R2 is independently a substituted or unsubstituted C1-C6 alkyl group. The polycarbonate has a molar ratio of Ch1(M1):Ch2(M2):Ch3(M3)=10-85mol%:5-30mol%:10-80mol%.
Abstract translation: 目的:提供聚碳酸酯以具有优异的耐刮擦性,耐化学性,柔韧性,室温/低温冲击强度和耐热性。 构成:聚碳酸酯包含由化学式1,化学式2和化学式3表示的重复单元。在化学式1和2中,R 1和R 2各自独立地为C 1 -C 6烷基,a和b各自为整数 从0-4。 在化学式3中,R 1和R 2各自为取代或未取代的C 1 -C 6烷基; a和b各自独立地为1-4的整数。 在化学式3中,R 1和R 2各自独立地为取代或未取代的C 1 -C 6烷基。 Ch1(M1):Ch2(M2):Ch3(M3)= 10-85mol%:5-30mol%:10-80mol%的摩尔比。
-
公开(公告)号:KR1020130031702A
公开(公告)日:2013-03-29
申请号:KR1020110095429
申请日:2011-09-21
Applicant: 제일모직주식회사
CPC classification number: C08G64/083 , C08L69/00
Abstract: PURPOSE: Polycarbonate is provided to have excellent fire retardancy, chemical resistance, thermal resistance, shock absorbency, and flexibility, while maintaining transparency. CONSTITUTION: Polycarbonate comprises formula 1, formula 2, formula 3 and formula 4 in recurring units. In the formulas above, each of R1 and R2 is a substituted or non-substituted C-C6 alkyl group, a substituted or non-substituted C3-C6 cycloalkyl group, a substituted or non-substituted C6-C12 aryl group, or a halogen atom. In the formulas above, R3 is a substituted or non-substituted C1-6 alkyl group, a substituted or non-substituted C6-12 aryl group, and a substituted or non-substituted C7-20 aralkyl group. In the formulas above, each of a and b each is an integer ranging from 0 to 4, and n is 0 or 1.
Abstract translation: 目的:提供聚碳酸酯具有优异的阻燃性,耐化学性,耐热性,抗冲击性和柔韧性,同时保持透明度。 构成:聚碳酸酯包含重复单元的式1,式2,式3和式4。 在上式中,R 1和R 2各自为取代或未取代的C 1 -C 6烷基,取代或未取代的C 3 -C 6环烷基,取代或未取代的C 6 -C 12芳基或卤素 原子。 在上式中,R 3是取代或未取代的C 1-6烷基,取代或未取代的C 6-12芳基,以及取代或未取代的C 7-20芳烷基。 在上式中,a和b各自为0〜4的整数,n为0或1。
-
公开(公告)号:KR1020120067193A
公开(公告)日:2012-06-25
申请号:KR1020100128654
申请日:2010-12-15
Applicant: 제일모직주식회사
Abstract: PURPOSE: A manufacturing method of a flame-retardant aromatic polycarbonate resin is provided to improve flame retardancy by adding small amount of a phosphoric based compound, and to improve transparency by minimizing heat history number of the resin. CONSTITUTION: A manufacturing method of a flame-retardant aromatic polycarbonate resin comprises a step of melt-polymerizing aromatic dihydroxy compound and carbonate diester mixture, extruding by adding a diphosphate-based phosphate-based compound into a melted polymer. The diphosphate-based phosphate-based compound has a structure in chemical formula 1. In chemical formula 1, R^1-R^20 is respectively hydrogen, C1-6 linear or branched alkyl, and n is 0.5-50, and B is respectively C1-12 alkyl group, and q is respectively 0,1 or 2, and X is a single bond, C=O, S, O, SO2, C(CH3)2, C1-5 alkylene, C2-5 alklidene, C5-6 cycloalkylidene, or C6-12 arylene.
Abstract translation: 目的:提供阻燃性芳香族聚碳酸酯树脂的制造方法,通过添加少量的磷酸类化合物来提高阻燃性,并且通过使树脂的热历史数量最小化来提高透明性。 构成:阻燃性芳香族聚碳酸酯树脂的制造方法包括使芳族二羟基化合物和碳酸二酯混合物熔融聚合的步骤,通过将二磷酸盐基磷酸酯类化合物加入到熔融聚合物中进行挤出。 基于磷酸酯的磷酸酯类化合物具有化学式1的结构。在化学式1中,R 1〜R 20分别为氢,C 1-6直链或支链烷基,n为0.5〜50,B为 分别为C1-12烷基,q分别为0,1或2,X为单键,C = O,S,O,SO2,C(CH3)2,C1-5亚烷基,C2-5亚烷基, C5-6亚环烷基或C6-12亚芳基。
-
27.
公开(公告)号:KR101008577B1
公开(公告)日:2011-01-17
申请号:KR1020080131363
申请日:2008-12-22
Applicant: 제일모직주식회사
IPC: C07C219/16
Abstract: 본 발명의 분지형 폴리카보네이트 합성용 분지제는 하기 화학식 1로 표시되는 것을 특징으로 한다:
[화학식 1]
상기에서, R
1 및 R
2 은 각각 독립적으로 선형 또는 분지형 C
1 ∼C
30 의 알킬기,
알콕시기, C
6 ∼C
30 의 아릴기, C
1 ∼C
10 알킬치환 C
6 ∼C
30 의
아릴기이고, n은 3∼6의 정수임.
분지형 폴리카보네이트, 다관능성 분지제, 에스테르교환 반응, 말단 수산기-
公开(公告)号:KR101557541B1
公开(公告)日:2015-10-06
申请号:KR1020120155613
申请日:2012-12-27
Applicant: 제일모직주식회사
CPC classification number: C08L69/00 , C08L51/003 , C08L2205/03 , C08L51/04
Abstract: 본발명의폴리카보네이트수지조성물은청구항 1의화학식 1로표시되는반복단위, 청구항 1의화학식 2로표시되는반복단위및 청구항 1의화학식 3으로표시되는반복단위를포함하는공중합폴리카보네이트수지, 및방향족폴리카보네이트수지를포함하는폴리카보네이트성분; 및아크릴계충격보강제를포함하는것을특징으로한다. 상기폴리카보네이트수지조성물은내스크래치성, 내충격성및 내열성이우수하다.
-
公开(公告)号:KR101459130B1
公开(公告)日:2014-11-10
申请号:KR1020110147625
申请日:2011-12-30
Applicant: 제일모직주식회사
CPC classification number: C08G64/06 , C08J7/047 , C08J2369/00 , Y10T428/24942 , Y10T428/31507
Abstract: 본 발명의 플라스틱 글레이징은 기재층; 및 상기 기재층의 일면에 형성되는 코팅층으로 이루어지고, 상기 기재층은 비페닐기 함유 폴리카보네이트를 포함하며, 상기 비페닐기는 전체 폴리카보네이트중 10 내지 50 mol % 함유하는 것을 특징으로 한다.
-
公开(公告)号:KR101447269B1
公开(公告)日:2014-10-06
申请号:KR1020110121903
申请日:2011-11-21
Applicant: 제일모직주식회사
CPC classification number: C08G64/06 , C08G64/307 , G02B1/04 , C08L69/00
Abstract: 본 발명의 폴리카보네이트 수지는 하기 화학식 1, 화학식 2 및 화학식 3을 반복단위로 포함하는 것을 특징으로 한다:
[화학식 1]
[화학식 2]
(상기에서, R
1 및 R
2 는 각각 독립적으로 치환 또는 비치환된 C1 내지 C6 알킬기이며, a 및 b는 각각 독립적으로 0 내지 4의 정수이다)
[화학식 3]