열전소자용 전극 및 그 제조방법
    21.
    发明公开
    열전소자용 전극 및 그 제조방법 有权
    用于热电设备的电极及其制造方法

    公开(公告)号:KR1020110071874A

    公开(公告)日:2011-06-29

    申请号:KR1020090128564

    申请日:2009-12-22

    CPC classification number: H01L35/14 H01L35/18 H01L35/20 H01L35/34

    Abstract: PURPOSE: An electrode for a thermoelectric device and a manufacturing method thereof are provided to obtain a dense sinter by rapidly raising a temperature with a discharge sintering method. CONSTITUTION: Ni powder and Mo powder are weighted to comprise Ni1-XMoX(0.5

    Abstract translation: 目的:提供一种用于热电装置的电极及其制造方法,以通过用放电烧结法快速升高温度来获得致密的烧结体。 构成:将Ni粉末和Mo粉末称重为Ni1-XMoX(0.5 <= X <1)。 将Ni粉末和Mo粉末混合以包含Ni1-XMoX(0.5 <= X <1)。 将Ni粉末和Mo粉末的混合粉末(120)填充到模具(110)中,并设置在放电等离子体烧结装置的室(100)中。 通过对混合粉末进行加压并对室内进行抽真空来施加DC脉冲。 将混合粉末加热到低于Ni和Mo的定影温度的烧结温度。混合粉末在烧结温度下用放电等离子体加压和烧结。 通过冷却室获得Ni1-XMoX(0.5 <= X <1)烧结体。

    고밀도 탄화붕소 소결체의 제조방법
    22.
    发明公开
    고밀도 탄화붕소 소결체의 제조방법 有权
    制造高密度硼砂烧结体和高密度硼砂烧结体的方法

    公开(公告)号:KR1020110018997A

    公开(公告)日:2011-02-25

    申请号:KR1020090076517

    申请日:2009-08-19

    Abstract: PURPOSE: A producing method of a high density boron carbide sintered body and the high density boron carbide sintered body are provided to prevent the generation of pores and voids among grains. CONSTITUTION: A producing method of a high density boron carbide sintered body comprises the following steps: inserting boron carbide powder into a mold inside a furnace, and pressurizing to obtain a molded body; exhausting impurity gas from the furnace by operating a pump; increasing the temperature of the furnace for volatilizing boric oxides from the surface of the boron carbide powder; exhausting the volatilized boric oxides to the outside; increasing the temperature of the furnace to the constant sintering temperature; pressurizing the molded body of the boron carbide powder, and sintering boron carbide; and cooling the furnace.

    Abstract translation: 目的:提供高密度碳化硼烧结体和高密度碳化硼烧结体的制造方法,以防止颗粒之间产生孔隙和空隙。 构成:高密度碳化硼烧结体的制造方法,包括以下步骤:将碳化硼粉末插入炉内的模具内,加压成型体; 通过操作泵从炉中排出杂质气体; 从碳化硼粉末表面提高挥发氧化硼的炉子的温度; 将挥发的硼氧化物排出外部; 将炉子的温度提高到恒定的烧结温度; 对碳化硼粉末的成形体进行加压,烧结碳化硼; 并冷却炉。

    가공성 세라믹 복합체 및 그 제조방법
    23.
    发明公开
    가공성 세라믹 복합체 및 그 제조방법 有权
    可加工的陶瓷复合材料及其制造方法

    公开(公告)号:KR1020180014285A

    公开(公告)日:2018-02-08

    申请号:KR1020160096115

    申请日:2016-07-28

    Abstract: 본발명은기계적특성과가공성이개량된 BN-SiN계가공성세라믹복합체및 그제조방법을개시한다. 본발명에의해제조된 BN-SiN계가공성세라믹복합체는, 질화붕소(BN) 30.0 내지 70.0 중량%, 질화규소(SiN) 27.6 내지 64.4 중량%, 산화이트륨(YO) 1.8 내지 4.2 중량% 및알루미나(AlO) 0.6 내지 1.4 중량%를포함하는조성비로이루어지며, 200 내지 500 MPa 범위의굽힘강도와, 2.0 ~ 5.0/℃범위의열팽창계수를지니는것을특징으로한다. 이러한특징에따르면, 고강도이면서고정밀미세가공이가능하여직경 40㎛의홀(hole) 등과같이치수정밀도가요구되는정밀기계부품이나전자부품등의다양한산업에활용이가능하며, 특히실리콘과열팽창계수가유사하여예컨대, 반도체검사용프로브카드에미세프로브를고정시키는핵심부품인프로브카드용가이드등과같은반도체분야의정밀부품에유효하게채택가능한소재로제공할수 있다.

    Abstract translation: 本发明公开了一种具有改进的机械性能和可加工性的BN-SiN可加工的陶瓷复合材料及其制造方法。 本发明制造的基于BN-的SiN加工性陶瓷复合物,氮化硼(BN)30.0〜70.0%(重量),硅氮化物(氮化硅)27.6至64.4%(重量)氧化钇(YO)1.8氧化铝4.2%(重量)的(ALO ),弯曲强度为200〜500MPa,热膨胀系数为2.0〜5.0 /。 根据这些特性,高强度,并且可以在各种工业,例如高精度精细加工可以利用能够通过精密机械零件等需要尺寸精度的电子部件,如直径40㎛uihol(空穴),并且尤其是硅和热膨胀的类似系数 通过,例如,它可以提供一个可能在半导体材料的精密零件,如探针卡指南显微探针固定到探针卡用于半导体的核心部分有效通过。

    고온주입 열분해법에 의한 CoSb3 나노입자 제조방법
    24.
    发明授权
    고온주입 열분해법에 의한 CoSb3 나노입자 제조방법 有权
    通过热注射热解制备COSB3纳米颗粒的方法

    公开(公告)号:KR101395690B1

    公开(公告)日:2014-05-15

    申请号:KR1020130096573

    申请日:2013-08-14

    Abstract: The present invention relates to a method for manufacturing CoSb3 nanoparticles by a hot-injection pyrolysis method which is, more specifically, capable of manufacturing CoSb3 nanoparticles in a single phase without phase separation from two compounds each of which contains metal elements having different thermal decomposition temperature from each other; and is capable of improving thermal performance through the CoSb3 nanoparticles by obtaining the CoSb3 nanoparticles with high purity and having a particle diameter in nano-unit and adjusting the particle diameter of the particle at the same time. In addition, the present invention relates to the method for manufacturing CoSb3 nanoparticles by the hot-injection pyrolysis which is capable of reducing manufacturing costs since the CoSb3 nanoparticles can be manufactured only with a short time reaction and minimizing risk during production.

    Abstract translation: 本发明涉及一种通过热喷射热解法制造CoSb3纳米颗粒的方法,该方法更具体地是能够从两种化合物制备单相中的CoSb 3纳米颗粒,每种化合物含有不同热分解温度的金属元素 从彼此; 并且通过获得高纯度的CoSb 3纳米颗粒并且具有纳米单位的粒径并同时调节颗粒的粒径,能够通过CoSb 3纳米颗粒改善热性能。 此外,本发明涉及通过热喷射热解制造CoSb 3纳米颗粒的方法,其能够降低制造成本,因为CoSb 3纳米颗粒可以仅在短时间反应下制造并且最小化生产过程中的风险。

    구리 전극을 포함하는 열전소자 및 그 제조방법
    25.
    发明授权
    구리 전극을 포함하는 열전소자 및 그 제조방법 有权
    具有铜电极的热电器件及其制造方法相同

    公开(公告)号:KR101323097B1

    公开(公告)日:2013-10-30

    申请号:KR1020110120543

    申请日:2011-11-17

    Abstract: 본 발명은, CoSb
    3 열전반도체의 제1면과 제2면에 제1 금속 플레이트, 제2 금속 플레이트 및 구리(Cu) 전극이 순차적으로 적층되어 접합된 구조를 가지며, 상기 제1 금속 플레이트는 알루미늄 금속 또는 알루미늄 합금으로 이루어지고, 상기 제2 금속 플레이트는 티타늄(Ti), 지르코늄(Zr) 및 텅스텐 중에서 선택된 1종 이상의 금속 또는 티타늄(Ti), 지르코늄(Zr) 및 텅스텐 중에서 선택된 1종 이상의 금속을 포함하는 합금으로 이루어진 열전소자 및 그 제조방법에 관한 것이다. 본 발명에 의하면, 열전반도체와 전극 계면에서 크랙(crack)이나 보이드(void)와 같은 결함이 거의 없으며 계면 정합이 잘 이루어져 인장력에 대한 강성이 우수하고, 열전반도체와 전극의 계면에서 들뜨거나 하는 등의 부정합이 작아 계면 분리가 일어나지 않으므로 고온에서의 신뢰성이 높다.

    고온화학기상증착용 버블링 장치
    26.
    发明公开
    고온화학기상증착용 버블링 장치 有权
    用于高温化学气相沉积的泡泡机

    公开(公告)号:KR1020130104908A

    公开(公告)日:2013-09-25

    申请号:KR1020120026857

    申请日:2012-03-16

    Abstract: PURPOSE: A bubbling device for high temperature chemical vapor deposition is provided to manufacture target substances by applying various kinds of substances and to facilitate the vaporization of liquid-phase materials at a relatively low temperature. CONSTITUTION: A bubbling device for high temperature chemical vapor deposition comprises a material storage part (102), a bubble gas supply part, a first heating unit, a bubble gas inlet (116), and a material gas outlet (118). The material storage part stores liquid-phase materials. The bubble gas supply part supplies bubble gas to bubble the materials. The first heating unit heats the materials bubbled by the bubble gas to vaporize. The bubble gas inlet is a passage to introduce the bubble gas into the material storage part. The material gas outlet is a passage to supply materials gas formed by vaporizing the materials from the material storage part to a reaction chamber of a high-temperature chemical vapor deposition device.

    Abstract translation: 目的:提供用于高温化学气相沉积的鼓泡装置,通过应用各种物质制造目标物质,并促进液相材料在较低温度下的蒸发。 构成:用于高温化学气相沉积的鼓泡装置包括材料储存部分(102),气泡气体供应部分,第一加热单元,气泡气体入口(116)和材料气体出口(118)。 材料储存部存储液相材料。 泡沫气体供应部分提供泡沫气体来泡沫材料。 第一加热单元加热泡沫气体鼓泡的物质蒸发。 泡沫气体入口是将气泡引入材料储存部分的通道。 原料气体出口是通过将材料从材料储存部分蒸发到高温化学气相沉积装置的反应室而形成的材料的通道。

    고강도 뼈분쇄기 및 그 제조방법
    27.
    发明公开
    고강도 뼈분쇄기 및 그 제조방법 有权
    其制造方法及其制造方法

    公开(公告)号:KR1020120084456A

    公开(公告)日:2012-07-30

    申请号:KR1020110005826

    申请日:2011-01-20

    Abstract: PURPOSE: A bone grinder and a manufacturing method thereof are provided to enhance bone grinding efficiency. CONSTITUTION: A manufacturing method of a bone grinder is as follows. Zirconia(ZrO2) 90-99.9 mole % and yttria(Y2O3) 0.1-10 mole % are mixed and shattered into pieces(S110). Pressure is applied to the mixed and shattered powder in one direction(S120). The molded mixture passes through cold water pressure molding(S130). The molded product is annealed(S140). The annealed product is processed using CAD/CAM(S150). The produce is sintered in an oxidizing atmosphere(S160).

    Abstract translation: 目的:提供骨磨机及其制造方法以提高骨磨削效率。 构成:骨磨机的制造方法如下。 将90-99.9摩尔%的氧化锆(ZrO 2)和氧化钇(Y 2 O 3)0.1-10摩尔%混合并粉碎成片(S110)。 在一个方向上对混合粉碎的粉末施加压力(S120)。 模制的混合物通过冷水压力成型(S130)。 模制产品退火(S140)。 使用CAD / CAM处理退火产品(S150)。 将产物在氧化气氛中烧结(S160)。

    머시너블 흑색 세라믹 복합체 및 그 제조방법
    28.
    发明公开
    머시너블 흑색 세라믹 복합체 및 그 제조방법 有权
    具有黑色可制造性的陶瓷复合材料及其制造方法

    公开(公告)号:KR1020120043294A

    公开(公告)日:2012-05-04

    申请号:KR1020100104523

    申请日:2010-10-26

    Abstract: PURPOSE: A machinable black ceramic complex and a manufacturing method thereof are provided to enhance crystal state by using a hot pressing process. CONSTITUTION: A machinable black ceramic complex comprises zirconia(ZrO2), boron nitride(BN), yttrium oxide(Y2O3), and alumina(Al2O3). The zirconia(ZrO2) and boron nitride(BN) are contained 78-96 weight%. The yttrium oxide(Y2O3) is contained 3-12 weight% and the alumina (Al2O3) is contained 1-10 weight%. The machinable black ceramic complex has a flexural strength of 120-160MPa and a thermal expansion coefficient of 6.0-9.0×10^-6/degree Celsius. A manufacturing method of the machinable black ceramic composite comprises next steps: mixing material powders; charging compound powder in a mold of a furnace; sintering and hot pressing the compound powder; obtaining machinable ceramic composite by cooling the furnace; placing the machinable ceramic composite and carbon group powder in a crucible; charging the crucible into the furnace; exhausting impurity gas within the furnace; processing a thermal process to make the ceramic black; and obtaining the machinable black ceramic composite by cooling the furnace.

    Abstract translation: 目的:提供可机加工的黑色陶瓷复合体及其制造方法,以通过热压加工来提高晶体状态。 构成:可加工的黑色陶瓷配合物包括氧化锆(ZrO 2),氮化硼(BN),氧化钇(Y 2 O 3)和氧化铝(Al 2 O 3)。 氧化锆(ZrO 2)和氮化硼(BN)含有78-96重量%。 氧化钇(Y 2 O 3)含有3〜12重量%,氧化铝(Al 2 O 3)含有1-10重量%。 可加工黑色陶瓷复合体的弯曲强度为120-160MPa,热膨胀系数为6.0-9.0×10 ^ -6 /摄氏度。 可加工黑色陶瓷复合体的制造方法包括以下步骤:混合材料粉末; 将复合粉末装入炉子的模具中; 烧结和热压复合粉末; 通过冷却炉获得可加工陶瓷复合材料; 将可加工的陶瓷复合材料和碳组粉末放置在坩埚中; 将坩埚装入炉中; 在炉内排出杂质气体; 加工热处理使陶瓷黑色; 并通过冷却炉获得可机加工的黑色陶瓷复合材料。

    고밀도 탄화붕소 소결체의 제조방법
    29.
    发明授权
    고밀도 탄화붕소 소결체의 제조방법 有权
    制造高密度碳化硼烧结体的方法

    公开(公告)号:KR101123391B1

    公开(公告)日:2012-03-23

    申请号:KR1020090076517

    申请日:2009-08-19

    Abstract: 본 발명은, 탄화붕소 분말을 퍼니스에 구비된 몰드에 넣고 압력을 가하여 원하는 형태의 성형체로 성형하는 단계와, 펌프를 작동시켜 퍼니스 내에 존재하는 불순물 가스를 배기하는 단계와, 상기 퍼니스의 온도를 탄화붕소 분말의 표면에 존재하는 붕소산화물이 휘발되는 온도로 상승시키는 단계와, 상기 붕소산화물이 휘발되는 온도에서 유지하여 붕소산화물을 휘발시키면서 상기 퍼니스 외부로 휘발된 붕소산화물을 배기하는 단계와, 상기 퍼니스의 온도를 붕소산화물이 휘발되는 온도보다 높고 탄화붕소의 용융 온도보다 낮은 목표하는 소결 온도로 상승시키는 단계와, 상기 소결 온도에서 탄화붕소 분말의 성형체에 압력을 가하면서 탄화붕소를 소결시키는 단계 및 퍼니스를 냉각하여 탄화붕소 소결체를 얻는 단계를 포함하는 고밀도 탄화붕소 소결체의 제조방법에 관한 것이다.
    탄화붕소(boroncarbide), 붕소산화물, 열간가압소결(hot pressing), 소결조제

    고밀도 탄화붕소 소결체의 제조방법
    30.
    发明公开
    고밀도 탄화붕소 소결체의 제조방법 有权
    高密度硼砂烧结体及其制造方法

    公开(公告)号:KR1020110107959A

    公开(公告)日:2011-10-05

    申请号:KR1020100027170

    申请日:2010-03-26

    Abstract: 본 발명은, 탄화붕소 분말을 퍼니스에 구비된 몰드에 넣고 압력을 가하여 원하는 형태의 성형체로 성형하는 단계와, 펌프를 작동시켜 퍼니스 내에 존재하는 불순물 가스를 배기하고, 환원제 가스인 수소(H
    2 ) 가스를 공급하는 단계와, 상기 퍼니스의 온도를 탄화붕소 분말의 표면에 존재하는 붕소산화물(B
    2 O
    3 )이 휘발되는 온도보다 높은 온도로 1차 상승시키는 단계와, 상기 퍼니스의 온도를 붕소산화물이 휘발되는 온도보다 높고 탄화붕소의 용융 온도보다 낮은 소결 온도로 2차 상승시키는 단계와, 상기 소결 온도에서 탄화붕소 분말의 성형체에 압력을 가하면서 환원 가스 분위기인 수소(H
    2 ) 가스 분위기에서 탄화붕소를 소결시키는 단계 및 퍼니스를 냉각하여 탄화붕소 소결체를 얻는 단계를 포함하는 고밀도 탄화붕소 소결체의 제조방법 및 이에 의해 제조된 고밀도 탄소붕소 소결체에 관한 것이다.