저농도 구리이온이 함유된 용액으로부터 구리이온 제거방법
    21.
    发明公开
    저농도 구리이온이 함유된 용액으로부터 구리이온 제거방법 有权
    从低浓度铜溶液中除去铜离子的方法

    公开(公告)号:KR1020130128080A

    公开(公告)日:2013-11-26

    申请号:KR1020120051839

    申请日:2012-05-16

    CPC classification number: C22B15/0089 C22B3/42

    Abstract: The present invention relates to a method for removing copper ions, wherein the method includes: a step (a) of selectively absorbing and removing the copper ions from a mixed solution, which contains the copper ions and at least one or two metal ions selected from nickel ions, cobalt ions, and iron ions, using an ion exchange resin which is a chelate resin having an iminodiacetic acid functional group; and a step (b) of recovering copper by detaching the copper from the ion exchange resin in which the copper ions are absorbed. The present invention also relates to the copper which is detached and recovered from the ion exchange resin, which the copper ions are absorbed in, by the method using an eluent containing 2 to 12 vol% of sulfuric acid. [Reference numerals] (AA) Solution including nickel, cobalt, iron, and low concentration copper;(BB) Sulfuric acid/sodium hydroxide;(CC) pH adjustment;(DD) Copper attachment;(EE) Resin/solution separation;(FF) Ion exchange resin;(GG) Solution;(HH) Eluant;(II) Detachment;(JJ) Nickel/cobalt recovery process;(KK) Resin/eluant separation;(LL) Ion exchange resin;(MM) Copper-containing solution;(NN) Copper recovery process

    Abstract translation: 本发明涉及一种去除铜离子的方法,其中所述方法包括:从包含铜离子和至少一种或两种选自以下的金属离子的混合溶液中选择性吸收和除去铜离子的步骤(a) 镍离子,钴离子和铁离子,使用具有亚氨基二乙酸官能团的螯合树脂的离子交换树脂; 以及通过从其中吸收铜离子的离子交换树脂中分离出铜而回收铜的步骤(b)。 本发明还涉及通过使用含有2〜12体积%的硫酸的洗脱液的方法从离子交换树脂中分离和回收铜离子的铜。 (AA)溶液包括镍,钴,铁和低浓度铜;(BB)硫酸/氢氧化钠;(CC)pH调节;(DD)铜附着;(EE)树脂/溶液分离; FF)离子交换树脂;(GG)溶液;(HH)洗脱剂;(II)分离;(JJ)镍/钴回收方法;(KK)树脂/洗脱剂分离;(LL)离子交换树脂;(MM) 含铜溶液;(NN)铜回收工艺

    광미로부터 매트와 슬래그를 얻는 방법
    22.
    发明授权
    광미로부터 매트와 슬래그를 얻는 방법 有权
    从尾矿中获取物质和泥浆的方法

    公开(公告)号:KR101325204B1

    公开(公告)日:2013-11-04

    申请号:KR1020110094982

    申请日:2011-09-21

    CPC classification number: Y02P10/212

    Abstract: 본 발명은 광미로부터 매트와 슬래그를 얻는 방법에 관한 것으로, 광미 100중량부, 알루미나 및 산화철 소스 물질 50 내지 200중량부 및 탄산칼슘 소스 물질 50 내지 200중량부를 혼합하여 혼합물을 얻는 단계와; 상기 혼합물을 용융제련하여 매트와 슬래그를 얻는 단계를 포함한다.

    수직형 소성로를 이용한 자열 소성체 제조방법
    23.
    发明授权
    수직형 소성로를 이용한 자열 소성체 제조방법 有权
    立式炉自热烧结体的制造方法

    公开(公告)号:KR101048527B1

    公开(公告)日:2011-07-12

    申请号:KR1020080083243

    申请日:2008-08-26

    CPC classification number: C22B1/22 C22B1/2413

    Abstract: 본 발명은 횡단면이 원형, 타원형 또는 다각형으로 상부보다 하부가 넓은 테이퍼 형상이며 탄소를 함유하는 펠렛으로 충전된 소성로, 펠렛 투입부, 배출부, 공기 조절부를 포함하여 이루어지는 것을 특징으로 하는 수직형 자열 소성로에 관한 것이다.
    그리고 본 발명은 상기 수직형 자열 소성로에 탄소를 함유하는 펠렛을 충전 시켜 예열한 후 상기 예열된 펠렛을 충전시킨 소성로의 내부에 탄소를 함유하는 펠렛을 연속적으로 투입하고, 상기 탄소를 함유하는 펠렛이 자열 소성되어 생성된 자열 소성체가 하부로 연속적으로 배출하는 단계를 포함하는 자열 소성체 제조방법에 관한 것이다.
    상기 소성로를 이용하여 소성체를 제조하는 방법은 추가적인 가열 없이 소성 시 생성되는 열만으로 펠렛을 자열 소성 할 수 있는 점에서 경제적인 이점이 있다.
    자열소성, 수직형 소성로, 석탄폐석, 석탄회, 폐주물사

    Abstract translation: 本发明垂直串烧成炉,其包括横截面,包括圆形,椭圆形或多边形具有比上部宽锥形填充有含有碳焙烧炉,粒料输入单元,所述放电单元,所述空调单元粒料一个下 Lt。

    합성매트로부터 유가금속의 침출방법
    24.
    发明公开
    합성매트로부터 유가금속의 침출방법 有权
    合成材料中有价值金属的浸出方法

    公开(公告)号:KR1020100068928A

    公开(公告)日:2010-06-24

    申请号:KR1020080127446

    申请日:2008-12-15

    CPC classification number: C22B15/0071 C22B3/08 C22B23/025 C22B23/0407

    Abstract: PURPOSE: A leaching method of the valuable metal from synthetic mat is provided to reduce a manufacturing cost by using the sulfuric acid in leaching. CONSTITUTION: A leaching method of the valuable metal from synthetic mat comprises: a step of leaching a synthetic mat with valuable metals by adding hydrocarbon compound under a sulfuric acid solution; a step of producing the slurry by adding the synthetic mat with valuable metals and the phase change material aliphatic hydrocarbon compound under a sulfuric acid solution; a step of leaching the slurry by pressurizing it and increasing temperatures; and a step of collecting the leaching solution. The synthetic mat containing valuable metals comprises copper, nickel, cobalt, iron and sulfur. The concentration of the sulfuric acid solution is 1~10%.

    Abstract translation: 目的:提供合成垫中贵重金属的浸出方法,通过使用硫酸浸出来降低制造成本。 构成:从合成垫中浸取有价值金属的方法包括:通过在硫酸溶液下加入烃化合物来浸出具有有价值金属的合成垫的步骤; 通过将有价金属的合成垫和相变材料脂族烃化合物加入到硫酸溶液中来制备浆料的步骤; 通过对浆料进行加压并提高温度来浸出浆料的步骤; 以及收集浸出液的步骤。 含有有价金属的合成垫包括铜,镍,钴,铁和硫。 硫酸溶液浓度为1〜10%。

    심해저 망간단괴로부터 제조된 매트상의 유가금속 침출방법
    25.
    发明公开
    심해저 망간단괴로부터 제조된 매트상의 유가금속 침출방법 有权
    使用氢氯酸溶液作为大气压力下的浸出溶液从深海洋锰矿生产的细粒料中选择性地浸出有价值金属的方法

    公开(公告)号:KR1020050008061A

    公开(公告)日:2005-01-21

    申请号:KR1020030047747

    申请日:2003-07-14

    Inventor: 박경호 남철우

    Abstract: PURPOSE: To provide a method for leaching valuable metals from a matte produced from deep ocean manganese nodules, wherein the method reduces facility cost and operation cost by simplifying leaching process, saves energy by leaching the valuable metals under the atmospheric pressure and reuses the recovered sulfur by recovering sulfur of the matte as a simple substrate sulfur. CONSTITUTION: In a method for leaching valuable metals from a matte comprising copper, nickel, cobalt, iron and sulfur as an intermediate product produced from deep ocean manganese nodules, the method comprises a step of injecting the matte into a hydrochloric acid solution used as a leaching solution in an amount of 10 g of the matte per liter of the hydrochloric acid solution having a hydrochloric acid concentration of 2N to 6N under the atmospheric pressure, thereby leaching the matte at a temperature of 80 to 90 deg.C to selectively dissolve nickel, cobalt and iron only except copper from the matte; and a step of recovering non-oxidized sulfur as a simple substance sulfur(S¬0) after leaching.

    Abstract translation: 目的:提供从深海锰结核产生的无光泽浸出有价值金属的方法,其中通过简化浸出过程降低设备成本和运行成本,通过在大气压下浸取有价值金属节省能源,并重新利用回收的硫 通过回收无光泽的硫作为简单的底物硫。 构成:在从含有铜,镍,钴,铁和硫的无光泽物质中浸出有价金属作为由深海锰结核产生的中间产物的方法中,该方法包括将无光泽物质注入盐酸溶液中的步骤 在大气压下,每升盐酸浓度为2N〜6N的盐酸溶液中加入10g的无光泽溶液浸出溶液,由此在80〜90℃的温度下浸出锍,以选择性地溶解镍 ,钴和铁只除了来自无光泽的铜; 以及在浸出后回收未氧化的硫作为单质硫(S0)的步骤。

    금속산화물 복합 피복 이산화티탄 광촉매의 제조 방법
    26.
    发明授权
    금속산화물 복합 피복 이산화티탄 광촉매의 제조 방법 失效
    光催化剂涂层金属氧化物和二氧化钛的生产方法

    公开(公告)号:KR100330627B1

    公开(公告)日:2002-03-29

    申请号:KR1019990055136

    申请日:1999-12-06

    Abstract: TiO광촉매의활성은 TiO미분체의입경이작을수록큰 것으로나타났기때문에 10∼20nm 이하의미세한분체가제조되고있다. 그러나, 이러한미분체는응집이일어나기쉬어광촉매의효율을저하시키거나용도를제한하는등의문제를야기시킨다. 따라서, 광촉매의활용성을고려하여미립의 TiO분말을담체에담지시켜사용되고있으며, 담체로서는제올라이트등과같은다공성물질을주로사용하고있다. 그러나, TiO의광촉매반응은빛이닿는표면부분에서만일어나므로, 다공성산화물을담체로사용하는것은그다지바람직하지못하며, 합성제올라이트와같은다공성물질은가격이비싸광촉매의가격을상승시키는요인이되고있다. 본발명은상기한바와같이동작되는종래의기술의문제점을개선하기위하여창안된것으로서, 주목적은광촉매의담체를다공성물질이아닌규석, 고령토, 납석, 장석, 점토와같은염가의천연광물로하고, 담체의표면에피복되는 TiO의광촉매활성을향상시키기위해소량의반도체성금속산화물(WO, FeO, SnO, CuO, NbO등)을복합피복하는저가형 TiO의광촉매의제조방법을제공하는것을특징으로한다.

    스피커용 자성유체의 제조방법
    27.
    发明授权
    스피커용 자성유체의 제조방법 失效
    用于制造扬声器磁场的方法

    公开(公告)号:KR100177569B1

    公开(公告)日:1999-05-15

    申请号:KR1019960031826

    申请日:1996-07-31

    Abstract: 본 발명은 스피커에 있어서 보이스코일과 플래트 사이에 내장되는 자성유체를 제3급 아민을 산화철 미립자 표면에 코팅시켜 제조하는 방법에 관한 것으로, 종래의 경우 자성유체가 불포화 알킬기를 갖는 계면활성체를 사용하여 왔던 관계로 산화철 초미립자의 표면이 쉽게 산화되고 점도의 저하와 함께 포화자화값의 감소현상을 초래하여 자성유체 효율을 저하시키는 문제점이 있었던바, 이러한 문제점을 해소하고자 본 발명은 초미립 산화철을 공침법에 의하여 상온에서 제조하여 세척하고, 계면활성제를 초미립 산화철 표면에 코팅하고 세척 건조후 호모제나이저(Homogenizer)를 이용하여 초미립 산화철을 광유에 분산시켜 제조가 이루어지는 스피커용 자성유체의 제조방법에 있어서, 계면활성제를 초미립 산화철의 표면에 코팅하는 공정이 3급 아민(Tri caprylyl amine)을 80∼90℃에서 초미립 산화철과 함께 교반 혼합시켜 이루어지는 제조방법을 제공하여 점성 및 포화자화값의 증대, 분산성향상 및 그 효과의 상승을 가질 수 있도록 하는데 그 특징이 있다.

    구리 함유 휘수연광의 전처리 방법
    30.
    发明公开
    구리 함유 휘수연광의 전처리 방법 无效
    处理含有多晶硅的铜的方法

    公开(公告)号:KR1020150064258A

    公开(公告)日:2015-06-11

    申请号:KR1020130146129

    申请日:2013-11-28

    CPC classification number: C22B34/34 C22B1/00

    Abstract: 본발명은구리함유휘수연광의전처리방법에관한것으로, 더욱구체적으로구리함유휘수연광과황산을혼합하는단계; 상기혼합후 가열하여황산화반응시키는단계; 상기황산화반응후 물을넣고교반하여수침출시키는단계; 상기수침출후 고체와액체를분리하는단계; 및상기분리된고체를건조시키는단계를포함하는구리함유휘수연광의전처리방법에관한것이다.

    Abstract translation: 本发明涉及一种预处理含铜辉钼矿的方法,更具体地说,涉及一种用于预处理含铜辉钼矿的方法,该方法包括以下步骤:将含有铜和硫酸的辉钼矿混合; 在混合后,进行硫酸化反应作为含有铜和硫酸的辉钼矿; 经硫酸化反应后用水搅拌浸出水; 水浸后分离固体和液体; 并干燥分离的固体。