公开(公告)号:AU5982499A
公开(公告)日:2000-04-26
申请号:AU5982499
申请日:1999-09-29
Applicant: BASF AG
Inventor: FISCHER MICHAEL , WEBER MARTIN , GINSS CHRISTOPHE , BERZ STEPHAN , KRESS NORBERT
IPC: C08J5/04 , C08F265/04 , C08F279/02 , C08K3/40 , C08K5/00 , C08K7/14 , C08L25/08 , C08L25/12 , C08L25/14 , C08L51/00 , C08L51/06 , C08L55/02 , C08L67/02 , C08L67/03 , C08L101/10
Abstract: The invention relates to a fiber-reinforced thermoplastic moulding material containing the following ingredients in relation to the sum of ingredients A-D and optionally E and F, representing a total of 100 wt. %: d) 10-97 wt. % of at least one aromatic polyester as ingredient A; e) 1-50 wt. % of at least one particle-shaped grafted copolymer with a soft phase glass transition temperature that is lower than 0 DEG C and an average particle size of 50-1000 nm as ingredient B; f) 1-50 wt. % of at least one copolymer made of monomers c1) 50-90 wt. % of at least one vinyl aromatic monomer as ingredient C1 and c2) 10-25 wt. % acrylonitrile and/or methacrylonitrile as ingredient C2, as ingredient C; 1-50 wt. % glass fibers as ingredient D; f) 0-25 wt. % other ingredients that are compatible, can be mixed in a homogenous manner with ingredients A and/or C and can be dispersed therein, as ingredient E; f) 0-10 wt. % usual additives such as UV stabilizers, oxidation retarders, lubricating agents and release agents as ingredient F. The invention also relates to moulded parts made from said moulding materials and used in the interiors of motor vehicles. The invention further relates to the use of moulding materials in the production of moulded parts.
-
公开(公告)号:DE19845289A1
公开(公告)日:2000-04-06
申请号:DE19845289
申请日:1998-10-01
Applicant: BASF AG
Inventor: FISCHER MICHAEL , KNOLL MANFRED , GINSS CHRISTOPHE , BERZ STEPHAN
IPC: C08F265/04 , C08F279/02 , C08K3/04 , C08K5/00 , C08L25/08 , C08L25/12 , C08L25/14 , C08L51/00 , C08L51/06 , C08L55/02 , C08L67/02 , C08L101/00 , C08L67/03 , C08L25/06 , C08L33/18
Abstract: The invention relates to a thermoplastic moulding material containing the following ingredients in relation to the sum of ingredients A C and optionally D-A, whereby said sum corresponds to 100 wt. %: a) 10-98 wt. % of at least one aromatic polyester as ingredient A; b) 1-50 wt. % of at least one particle-shaped grafted copolymer with a soft phase glass transition temperature of less than 0 DEG C and an average particle size of 50-1000 nm as ingredient B; c) 1-50 wt. % of at least one copolymer consisting of monomers c1) 50-90 wt. % of at least one vinyl aromatic monomer as ingredient C1 and c2) 10-25 wt. % acrylonitrile and/or methylnitrile as ingredient C2, as ingredient C; d) 0-25 wt. % other compatible polymers that can be homogenously mixed with ingredients A and/or C or dispersed therein as ingredient D; e) 0-10 wt. % usual additives such as carbon black, pigments, UV stabilizers, oxidation retarders, lubricating agents and mould-release agents as ingredient E. The invention also relates to moulded parts made of said moulding materials, used in the interiors of motor vehicles, in addition to the use of said moulding materials in the production of moulded parts.
-
23.
公开(公告)号:MY123030A
公开(公告)日:2006-05-31
申请号:MYPI9904178
申请日:1999-09-27
Applicant: BASF AG
Inventor: FISCHER MICHAEL DR , WEBER MARTIN DR , GINSS CHRISTOPHE , BERZ STEPHAN , XDF NORBERT KRE
IPC: C08J5/04 , C08F265/04 , C08F279/02 , C08K3/40 , C08K5/00 , C08K7/14 , C08L25/08 , C08L25/12 , C08L25/14 , C08L51/00 , C08L51/06 , C08L55/02 , C08L67/02 , C08L67/03 , C08L101/10
Abstract: A GLASS-FIBER-REINFORCED THERMOPLASTIC MOLDING COMPOSITION COMPRISES, BASED ON THE TOTAL OF COMPONENTS A TO D AND, IF DESIRED, E AND F, WHICH IN TOTAL GIVE 100% BY WEIGHT, A) AS COMPONENT A, FROM 10 TO 97% BY WEIGHT OF AT LEAST ONE AROMATIC POLYESTER, B) AS COMPONENT B, FROM 1 TO 50% BY WEIGHT OF AT LEAST ONE PARTICULATE GRAFT COPOLYMER WHOSE SOFT PHASE HAS A GLASS TRANSITION TEMPERATURE BELOW 0ºC AND WHOSE MEDIAN PARTICLE SIZE IS FROM 50 TO 1000 NM, C) AS COMPONENT C, FROM 1 TO 50% BY WEIGHT OF AT LEAST ONE COPOLYMER MADE FROM THE FOLLOWING MONOMERS C1) AS COMPONENT C1, FROM 50 TO 90% BY WEIGHT OF AT LEAST ONE VINYLAROMATIC MONOMER, AND C2) AS COMPONENT C2, FROM 10 TO 25% BY WEIGHT OF ACRYLONITRILE AND/OR METHACRYLONITRILE, D) AS COMPONENT D, FROM 1 TO 50% BY WEIGHT OF GLASS FIBERS, E) AS COMPONENT E, FROM 0 TO 25% BY WEIGHT OF OTHER COMPATIBLE POLYMERS HOMOGENEOUSLY MISCIBLE WITH COMPONENTS A AND/OR C OR DISPERSIBLE IN THESE, AND F) AS COMPONENT F, FROM 0 TO 10% BY WEIGHT OF CONVENTIONAL ADDITIVES, SUCH AS UV STABILIZERS, OXIDATION RETARDERS, LUBRICANTS AND MOLD-RELEASE AGENTS. MOLDINGS MADE FROM THESE MOLDING COMPOSITIONS AND USED IN MOTOR VEHICLE INTERIORS ARE ALSO DESCRIBED, AS IS THE USE OF THE MOLDING COMPOSITIONS TO PRODUCE THE MOLDINGS.
-
公开(公告)号:DE59910301D1
公开(公告)日:2004-09-23
申请号:DE59910301
申请日:1999-09-29
Applicant: BASF AG
Inventor: FISCHER MICHAEL , WEBER MARTIN , GINSS CHRISTOPHE , BERZ STEPHAN , KRESS NORBERT
IPC: C08J5/04 , C08F265/04 , C08F279/02 , C08K3/40 , C08K5/00 , C08K7/14 , C08L25/08 , C08L25/12 , C08L25/14 , C08L51/00 , C08L51/06 , C08L55/02 , C08L67/02 , C08L67/03 , C08L101/10
Abstract: The invention relates to a fiber-reinforced thermoplastic moulding material containing the following ingredients in relation to the sum of ingredients A-D and optionally E and F, representing a total of 100 wt. %: d) 10-97 wt. % of at least one aromatic polyester as ingredient A; e) 1-50 wt. % of at least one particle-shaped grafted copolymer with a soft phase glass transition temperature that is lower than 0 DEG C and an average particle size of 50-1000 nm as ingredient B; f) 1-50 wt. % of at least one copolymer made of monomers c1) 50-90 wt. % of at least one vinyl aromatic monomer as ingredient C1 and c2) 10-25 wt. % acrylonitrile and/or methacrylonitrile as ingredient C2, as ingredient C; 1-50 wt. % glass fibers as ingredient D; f) 0-25 wt. % other ingredients that are compatible, can be mixed in a homogenous manner with ingredients A and/or C and can be dispersed therein, as ingredient E; f) 0-10 wt. % usual additives such as UV stabilizers, oxidation retarders, lubricating agents and release agents as ingredient F. The invention also relates to moulded parts made from said moulding materials and used in the interiors of motor vehicles. The invention further relates to the use of moulding materials in the production of moulded parts.
-
-
公开(公告)号:BR9914201A
公开(公告)日:2001-07-03
申请号:BR9914201
申请日:1999-10-01
Applicant: BASF AG
Inventor: FISCHER MICHAEL , KNOLL MANFRED , GINSS CHRISTOPHE , BERZ STEPHAN
IPC: C08F265/04 , C08F279/02 , C08K3/04 , C08K5/00 , C08L25/08 , C08L25/12 , C08L25/14 , C08L51/00 , C08L51/06 , C08L55/02 , C08L67/02 , C08L101/00
Abstract: A thermoplastic molding composition comprises, based on the total of components A to C and, if desired, D and E, which in total give 100% by weight,a) as component A, from 10 to 98% by weight of at least one aromatic polyester,b) as component B, from 1 to 50% by weight of at least one particulate graft copolymer whose soft phase has a glass transition temperature below 0° C. and whose median particle size is from 50 to 1000 nm,c) as component C, from 1 to 50% by weight of at least one copolymer made from the following monomersc1) as component C1, from 50 to 90% by weight of at least one vinylaromatic monomer, andc2) as component C2, from 10 to 25% by weight of acrylonitrile and/or methacrylonitrile,d) as component D, from 0 to 25% by weight of other compatible polymers hormogeneously miscible with components A and/or C or dispersible in these, ande) as component E, from 0 to 10% by weight of conventional additives, such as UV stabilizers, carbon black, pigments, oxidation retarders, lubricants and mold-release agents.Moldings made from these molding compositions and used in motor vehicle interiors are also described, as is the use of the molding compositions to produce the moldings.
-
公开(公告)号:DE19845317A1
公开(公告)日:2000-04-06
申请号:DE19845317
申请日:1998-10-01
Applicant: BASF AG
Inventor: FISCHER MICHAEL , WEBER MARTIN , GINSS CHRISTOPHE , BERZ STEPHAN , KRES NORBERT
IPC: C08J5/04 , C08F265/04 , C08F279/02 , C08K3/40 , C08K5/00 , C08K7/14 , C08L25/08 , C08L25/12 , C08L25/14 , C08L51/00 , C08L51/06 , C08L55/02 , C08L67/02 , C08L67/03 , C08L101/10 , C08L25/06 , C08L33/20
Abstract: The invention relates to a fiber-reinforced thermoplastic moulding material containing the following ingredients in relation to the sum of ingredients A-D and optionally E and F, representing a total of 100 wt. %: d) 10-97 wt. % of at least one aromatic polyester as ingredient A; e) 1-50 wt. % of at least one particle-shaped grafted copolymer with a soft phase glass transition temperature that is lower than 0 DEG C and an average particle size of 50-1000 nm as ingredient B; f) 1-50 wt. % of at least one copolymer made of monomers c1) 50-90 wt. % of at least one vinyl aromatic monomer as ingredient C1 and c2) 10-25 wt. % acrylonitrile and/or methacrylonitrile as ingredient C2, as ingredient C; 1-50 wt. % glass fibers as ingredient D; f) 0-25 wt. % other ingredients that are compatible, can be mixed in a homogenous manner with ingredients A and/or C and can be dispersed therein, as ingredient E; f) 0-10 wt. % usual additives such as UV stabilizers, oxidation retarders, lubricating agents and release agents as ingredient F. The invention also relates to moulded parts made from said moulding materials and used in the interiors of motor vehicles. The invention further relates to the use of moulding materials in the production of moulded parts.
-
-
-
-
-
-