公开(公告)号:CA2864919A1
公开(公告)日:2013-09-06
申请号:CA2864919
申请日:2013-02-28
Applicant: CORNING INC
Inventor: FADEEV ANDREI GENNADYEVICH , CHANG THERESA , BOOKBINDER DANA CRAIG , PAL SANTONA , SAHA CHANDAN KUMAR , DEMARTINO STEVEN EDWARD , TIMMONS CHRISTOPHER LEE , PEANASKY JOHN STEPHEN
Abstract: Low-friction coatings and glass articles with low-friction coatings are disclosed. According to one embodiment, a coated glass article may include a glass body comprising a first surface and a low-friction coating positioned on at least a portion of the first surface of the glass body. The low-friction coating may include a polymer chemical composition. The coated glass article may be thermally stable at a temperature of at least about 260°C for 30 minutes. A light transmission through the coated glass article may be greater than or equal to about 55% of a light transmission through an uncoated glass article for wavelengths from about 400 nm to about 700 nm. The low- friction coating may have a mass loss of less than about 5% of its mass when heated from a temperature of 150°C to 350°C at a ramp rate of about 10°C/minute.
-
公开(公告)号:MX383888B
公开(公告)日:2025-03-14
申请号:MX2015006899
申请日:2015-05-29
Applicant: CORNING INC
Inventor: CHANG THERESA , DANA CRAIG BOOKBINDER , DANIELSON PAUL STEPHEN , DEMARTINO STEVEN EDWARD , FADEEV ANDREI GENNADYEVICH , MORENA ROBERT MICHAEL , PAL SANTONA , PEANASKY JOHN STEPHEN , SCHAUT ROBERT ANTHONY , TIMMONS CHRISTOPHER LEE , VENKATARAMAN NATESAN , VERKLEEREN RONALD LUCE
Abstract: Los contenedores de vidrio descritos en la presente son resistentes a la deslaminación, tienen fuerza mejorada y mayor resistencia al daño; en una modalidad, un contenedor de vidrio puede incluir un cuerpo que tiene una superficie interior, una superficie exterior y un grosor de pared que se extiende entre la superficie exterior y la superficie interior; por lo menos la superficie interior del cuerpo puede tener un factor de deslaminación menor o igual que 10; el cuerpo también puede tener una capa tensada compresivamente que se extiende desde la superficie exterior del cuerpo en el grosor de pared; la capa tensada compresivamente puede tener una tensión de compresión de superficie mayor o igual que 150 MPa; se puede poner un revestimiento lúbrico alrededor de por lo menos una porción de la superficie exterior del cuerpo, de modo que la superficie exterior del cuerpo con el revestimiento lúbrico tenga un coeficiente de fricción menor o igual que 0.7.
-
公开(公告)号:MX378553B
公开(公告)日:2025-03-07
申请号:MX2014010334
申请日:2014-08-27
Applicant: CORNING INC
Inventor: BOOKBINDER DANA CRAIG , CHANG THERESA , DEMARTINO STEVEN EDWARD , FADEEV ANDREI GENNADYEVICH , PAL SANTONA , PEANASKY JOHN STEPHEN , SAHA CHANDAN KUMAR , TIMMONS CHRISTOPHER LEE
Abstract: Se describen revestimientos de baja fricción y artículos de vidrio con revestimientos de baja fricción; según una modalidad, un artículo de vidrio revestido puede incluir un cuerpo de vidrio que comprende una primera superficie y un revestimiento de baja fricción posicionado en por lo menos una porción de la primera superficie del cuerpo de vidrio; el revestimiento de baja fricción puede incluir una composición química polimérica; el artículo de vidrio revestido puede ser térmicamente estable a una temperatura de por lo menos aproximadamente 260°C durante 30 minutos; una transmisión de luz por el artículo de vidrio revestido puede ser mayor que o igual a aproximadamente 55% de una transmisión de luz por un artículo de vidrio sin revestir para longitudes de onda de aproximadamente 400 nm a aproximadamente 700 nm; el revestimiento de baja fricción puede tener una pérdida de masa de menos que aproximadamente 5% de su masa cuando se calienta de una temperatura de 150°C a 350°C en una velocidad de rampa de aproximadamente 10°C/minuto.
-
公开(公告)号:CA2864919C
公开(公告)日:2020-06-30
申请号:CA2864919
申请日:2013-02-28
Applicant: CORNING INC
Inventor: FADEEV ANDREI GENNADYEVICH , CHANG THERESA , BOOKBINDER DANA CRAIG , PAL SANTONA , SAHA CHANDAN KUMAR , DEMARTINO STEVEN EDWARD , TIMMONS CHRISTOPHER LEE , PEANASKY JOHN STEPHEN
Abstract: Low-friction coatings and glass articles with low-friction coatings are disclosed. According to one embodiment, a coated glass article may include a glass body comprising a first surface and a low-friction coating positioned on at least a portion of the first surface of the glass body. The low-friction coating may include a polymer chemical composition. The coated glass article may be thermally stable at a temperature of at least about 260°C for 30 minutes. A light transmission through the coated glass article may be greater than or equal to about 55% of a light transmission through an uncoated glass article for wavelengths from about 400 nm to about 700 nm. The low- friction coating may have a mass loss of less than about 5% of its mass when heated from a temperature of 150°C to 350°C at a ramp rate of about 10°C/minute.
-
公开(公告)号:CA2891781C
公开(公告)日:2019-05-28
申请号:CA2891781
申请日:2013-11-22
Applicant: CORNING INC
Inventor: CHANG THERESA , DANIELSON PAUL STEPHEN , DEMARTINO STEVEN EDWARD , FADEEV ANDREI GENNADYEVICH , MORENA ROBERT MICHAEL , PAL SANTONA , PEANASKY JOHN STEPHEN , SCHAUT ROBERT ANTHONY , VENKATARAMAN NATESAN , VERKLEEREN RONALD LUCE , TIMMONS CHRISTOPHER LEE , BOOKBINDER DANA CRAIG
IPC: C03C17/00 , B32B17/06 , B65D1/40 , B65D25/14 , C03C17/30 , C03C17/32 , C03C17/42 , C03C21/00 , C09D179/08
Abstract: The glass containers described herein have at least two performance attributes selected from resistance to delamination, improved strength, and increased damage resistance. In one embodiment, a glass container may include a body having an inner surface, an outer surface and a wall thickness extending between the outer surface and the inner surface. A compressively stressed layer may extend from the outer surface of the body into the wall thickness. The compressively stressed layer may have a surface compressive stress greater than or equal to 150 MPa. A lubricous coating may be positioned around at least a portion of the outer surface of the body. The outer surface of the body with the lubricous coating may have a coefficient of friction less than or equal to 0.7.
-
公开(公告)号:CA2877742C
公开(公告)日:2019-05-28
申请号:CA2877742
申请日:2013-06-28
Applicant: CORNING INC
Inventor: ADIB KAVEH , BOOKBINDER DANA CRAIG , CHANG THERESA , DANIELSON PAUL STEPHEN , DEMARTINO STEVEN EDWARD , DRAKE MELINDA ANN , FADEEV ANDREI GENNADYEVICH , HAMILTON JAMES PATRICK , MORENA ROBERT MICHAEL , PAL SANTONA , PEANASKY JOHN STEPHEN , SAHA CHANDAN KUMAR , SCHAUT ROBERT ANTHONY , SCHIEFELBEIN SUSAN LEE , TIMMONS CHRISTOPHER LEE
Abstract: Delamination resistant glass containers with heat-tolerant coatings are disclosed. In one embodiment, a glass container may include a glass body having an interior surface, an exterior surface and a wall thickness extending from the exterior surface to the interior surface. At least the interior surface of the glass body is delamination resistant. The glass container may further include a heat-tolerant coating positioned on at least a portion of the exterior surface of the glass body. The heat- tolerant coating may be thermally stable at temperatures greater than or equal to 260°C for 30 minutes.
-
公开(公告)号:RU2671328C2
公开(公告)日:2018-10-30
申请号:RU2017146886
申请日:2013-02-28
Applicant: CORNING INC
Inventor: FADEEV ANDREI GENNADYEVICH , CHANG THERESA , BOOKBINDER DANA CRAIG , PAL SANTONA , SAHA CHANDAN KUMAR , DEMARTINO STEVEN EDWARD , TIMMONS CHRISTOPHER LEE , PEANASKY JOHN STEPHEN
IPC: B32B17/06 , A61J1/06 , C03C17/30 , C09D179/08
Abstract: Изобретениеотноситсяк фармацевтическимупаковочнымматериалам, вчастностистекляннымконтейнерам, такимкакампулы, трубки, пробирки, икасаетсяпокрытойфармацевтическойупаковки. Упаковкавключаетстеклянныйкорпус, включающийпервуюповерхностьи вторуюповерхность, противоположнуюпервойповерхности, которыйявляетсястекляннымконтейнером, выполненнымизборосиликатнойстекляннойкомпозиции, иперваяповерхностьпредставляетсобойвнешнююповерхностьстеклянногоконтейнера; антифрикционноепокрытие, расположенноепоменьшеймереначастипервойповерхностистеклянногокорпуса, приэтомантифрикционноепокрытиесодержитполимер, выбранныйизгруппы, содержащейполиимиды, фторполимеры, полимерынасилсесквиоксановойосновеи кремнийорганическиеполимеры; ислойсвязующеговещества, расположенныймеждуполимероми первойповерхностьюстеклянногокорпуса, причемкоэффициенттрениячастипокрытогостеклянногоизделияс антифрикционнымпокрытиемсоставляетпоменьшеймерена 20% меньше, чемкоэффициенттренияповерхностинепокрытогостеклянногоизделия, изготовленногоизтакойжестекляннойкомпозиции. Изобретениеобеспечиваетсозданиефармацевтическойупаковки, обладающейповышеннымсопротивлениемк механическимповреждениям. 6 н. и 23 з.п. ф-лы, 46 ил.
-
公开(公告)号:AU2016247214A1
公开(公告)日:2016-11-10
申请号:AU2016247214
申请日:2016-10-21
Applicant: CORNING INC
Inventor: ADIB KAVEH , BOOKBINDER DANA CRAIG , CHANG THERESA , DANIELSON PAUL STEPHEN , DEMARTINO STEVEN EDWARD , DRAKE MELINDA ANN , FADEEV ANDREI GENNADYEVICH , HAMILTON JAMES PATRICK , MORENA ROBERT MICHAEL , PAL SANTONA , PEANASKY JOHN STEPHEN , SAHA CHANDAN KUMAR , SCHAUT ROBERT ANTHONY , SCHIEFELBEIN SUSAN LEE , TIMMONS CHRISTOPHER LEE
Abstract: A glass container comprising: a glass body having an interior surface and an exterior surface, wherein at least the interior surface of the glass body has a delamination factor of less than or equal to 10; and a heat-tolerant coating bonded to at least a portion of the exterior surface of the glass body, wherein the exterior surface of the glass body with the heat-tolerant coating has a coefficient of friction of less than about 0.7, wherein the coefficient of friction is a maximum coefficient of friction measured relative to a second glass container in a vial-on-vial testing jig under a normal load of 30 N, the second glass container having a body formed from a same glass composition and comprising the heat-tolerant coating on an at least a portion of the outer surface of a body of the second glass container and subjected to the same environmental conditions prior to measurement.
-
公开(公告)号:MX2015006887A
公开(公告)日:2015-09-16
申请号:MX2015006887
申请日:2013-10-23
Applicant: CORNING INC
Inventor: DEMARTINO STEVEN EDWARD , SCHAUT ROBERT ANTHONY , FADEEV ANDREI GENNADYEVICH , CHANG THERESA , TIMMONS CHRISTOPHER LEE , PEANASKY JOHN STEPHEN
Abstract: De acuerdo con una modalidad, un contenedor de vidrío puede incluir un cuerpo formado de una composición de vidrio de tipo I, clase B, de acuerdo con el estándar ASTM E438-92. El cuerpo puede tener una superficie interna, una superficie externa y un grosor de pared que se extiende entre la superficie externa y la superficie interna; el cuerpo también puede incluir una capa tensada compresivamente que se extiende hacia adentro del grosor de la pared desde por lo menos una de la superficie externa y la superficie interna; se puede poner un revestimiento lúbrico sobre por lo menos una porción de la superficie externa del cuerpo, en donde la superficie externa del cuerpo con el revestimiento lúbrico tiene un coeficiente de fricción menor o igual que 0.7.
-
公开(公告)号:SG11201504073WA
公开(公告)日:2015-06-29
申请号:SG11201504073W
申请日:2013-10-23
Applicant: CORNING INC
Inventor: CHANG THERESA , DEMARTINO STEVEN EDWARD , FADEEV ANDREI GENNADYEVICH , PEANASKY JOHN STEPHEN , SCHAUT ROBERT ANTHONY , TIMMONS CHRISTOPHER LEE
Abstract: The glass containers described herein have at least two performance attributes selected from resistance to delamination, improved strength, and increased damage resistance. In one embodiment, a glass container may include a body having an inner surface, an outer surface and a wall thickness extending between the outer surface and the inner surface. At least the inner surface of the body may have a delamination factor less than or equal to 10. A tenacious inorganic coating may be positioned around at least a portion of the outer surface of the body. The outer surface of the body with the tenacious inorganic coating may have a coefficient of friction less than or equal to 0.7.
-
-
-
-
-
-
-
-
-