21.
公开(公告)号:EP3074542A4
公开(公告)日:2017-11-29
申请号:EP14863663
申请日:2014-11-24
Applicant: UNITED TECHNOLOGIES CORP
Inventor: CHIN HERBERT A , HALUCK DAVID A , OGDEN WILLIAM P , MOULIN MICHAEL A
IPC: C21D1/06
CPC classification number: C21D9/38 , C21D1/06 , C21D6/002 , C21D7/13 , C21D2211/008 , C23C8/02 , C23C8/22 , C23C8/32 , F16C33/32 , F16C33/34 , F16C33/62 , F16C2204/72 , F16C2223/12 , F16C2223/16
Abstract: A method for cost effectively case hardening a component formed from a martensitic stainless steel material with a desired metallurgical condition for high temperature, high rolling contact fatigue, corrosion and spall initiation and propagation resistance bearing performance. The method describes a method to significantly reduce the carburization or carbo-nitriding process times for appreciable reduction in manufacturing cost. The Method includes the steps of: forming the component from a martensitic stainless steel material having an ASTM grain size of 9 or finer; and subjecting the component to one of a carburization and a carbo-nitriding treatment with significantly lower case hardening times for manufacturing cost-effectiveness.
-
公开(公告)号:EP2971210A4
公开(公告)日:2016-11-16
申请号:EP14764684
申请日:2014-01-15
Applicant: UNITED TECHNOLOGIES CORP
Inventor: CHIN HERBERT A , OGDEN WILLIAM P , HALUCK DAVID A , SPITZER RONALD F
CPC classification number: F16C33/62 , C21D6/002 , C21D9/36 , C21D9/40 , C22C38/00 , C22C38/02 , C22C38/22 , C22C38/24 , C22C38/30 , C22C38/38 , C22C38/44 , C22C38/46 , C22C38/48 , C22C38/50 , C22C38/52 , C22C38/58 , C23C8/22 , C23C8/26 , C23C8/32 , C23C8/38 , F16C19/02 , F16C33/32 , F16C2202/04 , F16C2204/72 , F16C2206/58 , F16C2240/18 , F16C2240/40 , F16C2240/48 , F16C2360/23
Abstract: A rolling element bearing includes a plurality of bearing components, which include one or more rolling elements, an inner ring and an outer ring. A first of the bearing components includes martensitic stainless steel configured with a core and a hardened case. The martensitic stainless steel of the core includes approximately 8% by weight or more chromium. The martensitic stainless steel of the hardened case has a grain size that is substantially equal to or finer than ASTM grain size #7. The martensitic stainless steel of the hardened case includes approximately 6% by weight or more chromium, and carbon. Molecules that include the carbon are substantially uniformly dispersed within the hardened case.
-
23.
公开(公告)号:EP2849920A4
公开(公告)日:2016-06-01
申请号:EP13790177
申请日:2013-04-12
Applicant: UNITED TECHNOLOGIES CORP
Inventor: CHIN HERBERT A , OGDEN WILLIAM P , HALUCK DAVID A , MCCUTCHAN SEAN , SPITZER RONALD F , KELLER ALLEN V
CPC classification number: C21D7/06 , B24B1/00 , B24B11/02 , B24B19/06 , B24B31/02 , C21D1/76 , C21D9/36 , C21D9/40 , C23C8/02 , C23C8/26 , C23C8/36 , C23C8/50 , C23C8/80 , F16C33/32 , F16C2223/02 , F16C2223/10 , F16C2240/18 , F16C2360/23 , Y02P10/212 , Y10T29/47
Abstract: A method of treating bearing rolling elements or bearing rings after a hardening and temper heat treatment is disclosed. The method may include treating the bearing rolling elements in a tumbling treatment and then in a duplex hardening treatment. The method may include treating the bearing rings in a peening treatment and then in a duplex hardening treatment. The duplex hardening treatment may also include at least one sequential process segment consisting of subjecting the bearing rolling element & rings to a nitriding process to increase the surface hardness and compressive residual stress. The combined two-step process produces a deep surface/sub-surface residual stress greater than the depth of the maximum operating von-Mises shear stress along with an ultra-hard surface with high magnitude of compressive residual stress. In so doing, the bearing ring and rolling elements will have significantly enhanced rolling contact fatigue resistance and resistance to surface imperfections and debris.
-
公开(公告)号:EP2890871A4
公开(公告)日:2015-09-09
申请号:EP13832481
申请日:2013-06-04
Applicant: UNITED TECHNOLOGIES CORP
Inventor: SHAH DILIP M , CHIN HERBERT A , MARCIN JOHN JOSEPH , REYNOLDS PAUL L , SUCIU GABRIEL L , GENEREUX PAUL D
CPC classification number: C21D9/085 , B22D27/045 , C21D1/26 , C21D8/105 , C22C19/03 , C22C19/056 , C22C38/00 , C22F1/10 , C30B29/52 , C30B33/02 , F01D5/02 , F05D2220/323 , F05D2230/40 , F05D2240/60 , F05D2300/171 , F05D2300/501 , F05D2300/606 , Y02T50/672
Abstract: High modulus turbine shafts and high modulus cylindrical articles are described as are the process parameters for producing these shafts and cylindrical articles. The shafts/articles have a high Young's modulus as a result of having high modulus crystal texture along the longitudinal axis of the shaft/article. The shafts are produced from directionally solidified seeded single crystal cylinders that are axisymmetrically hot worked before a limited recrystallization process is carried out at a temperature below the recrystallization temperature of the alloy. The disclosed process produces an intense singular texture and results in shaft or cylindrical article with a Young's modulus that is at least 40% greater than that of conventional nickel or iron alloys or conventional steels.
-
-
-