硬化性エポキシ樹脂組成物およびその製造方法
    37.
    发明申请
    硬化性エポキシ樹脂組成物およびその製造方法 审中-公开
    可固化的环氧树脂组合物及其生产方法

    公开(公告)号:WO2003037985A1

    公开(公告)日:2003-05-08

    申请号:PCT/JP2002/011395

    申请日:2002-10-31

    Abstract: The invention relates to (1) a curable epoxy resin composition comprising (A) an amine−modified epoxy resin of a nongel state which is obtained by reacting an epoxy resin with a polyamine and (B) boric acid and/or a boric ester, (2) a powder of the curable epoxy resin composition and a process for its production, and (3) a process for production of heat−resistant laminated sheets by using the curable epoxy resin composition. The invention provides (1) a curable epoxy resin composition capable of giving a cured article having a high glass transition temperature and excellent mechanical properties, (2) a powdery curable epoxy resin composition having a high glass transition temperature, excellent mechanical properties and excellent storage stability and a process for its production, and (3) heat−resistant laminated sheets made by using the resin compositions and having excellent heat resistance and mechanical properties.

    Abstract translation: 本发明涉及(1)一种可固化环氧树脂组合物,其包含(A)通过使环氧树脂与多胺反应获得的胺改性环氧树脂和(B)硼酸和/或硼酸酯, (2)可固化环氧树脂组合物的粉末及其制造方法,(3)使用该可固化环氧树脂组合物制造耐热层压片的方法。 本发明提供(1)能够赋予玻璃化转变温度高,机械特性优异的固化物的固化性环氧树脂组合物,(2)具有高玻璃化转变温度,优异的机械性能和优异的储存性的粉末状固化型环氧树脂组合物 稳定性及其制造方法,(3)使用该树脂组合物制成的耐热性和机械性能优异的耐热层压片。

    高炉炼铁的节能富氧方法
    39.
    发明申请

    公开(公告)号:WO2014082428A1

    公开(公告)日:2014-06-05

    申请号:PCT/CN2013/075654

    申请日:2013-05-15

    Applicant: 王林 田妍妍

    Inventor: 王林 田妍妍

    CPC classification number: C21B5/00

    Abstract: 一种高炉炼铁的节能富氧方法,其中高炉炼铁的富氧喷煤工艺中的氧气,是由制氧设备直接进入高炉鼓风机与空气混合,形成氧气质量含量为21-31%的富氧空气,该富氧空气在高炉鼓风机内经压缩后进入热风炉加热至1000-1400°C,再直接进入高炉内参加炼铁反应。该方法不仅能使氧气混合均匀,可提高稳定性,而且不需要再配备专用的氧气压缩机,可有效地减少设备投资及设备的维护费用,既能降低能耗又能降低生产成本而且环保。同时,对高炉炼铁的原有生产线改造非常方便,只要把制氧设备的氧气出口与高炉鼓风机进气口连接即可。