Abstract: A pleat type knitted fabric is provided to give natural pleats and excellent surface feeling on a fabric even without performing a separate mechanical process, by knitting the fabric using yarns having different shrinkage rates. A pleat type knitted fabric comprises a fabric and pile yarns arranged slopingly with respect to the fabric. The fabric is knitted by using a latent crimp yarn and a general yarn at a ratio 1:1-2:1. The latent crimp yarn has a thermal shrinkage rate of 10-30% at 60-130‹C and a restoration rate of 30-70%. The general yarn has a thermal shrinkage rate of no more than 10% at 60-130‹C. The fabric has pleats by under-lapping the latent crimp yarn with respect to the general yarn.
Abstract translation: 提供褶皱型针织物,即使不进行单独的机械加工,也可以通过使用具有不同收缩率的纱线编织织物,从而在织物上产生天然褶皱和优异的表面感觉。 褶皱型针织物包括相对于织物倾斜布置的织物和绒头纱线。 织物通过使用潜在卷曲纱线和一般纱线以1:1:2:1的比例编织。 潜在卷曲纱线在60-130℃下的热收缩率为10-30%,恢复率为30-70%。 一般纱线在60-130℃时的热收缩率不超过10%。 织物通过对潜在卷曲纱线相对于一般纱线进行欠研磨而具有褶皱。
-
公开(公告)号:KR100778778B1
公开(公告)日:2007-11-28
申请号:KR1020070014923
申请日:2007-02-13
Applicant: 코오롱글로텍주식회사
CPC classification number: D06C15/04 , B32B3/30 , B32B5/245 , B32B2305/022 , D06C7/02 , D06C15/02 , D06C23/04 , D06C2700/31 , Y02P70/637
Abstract: An apparatus and a method for performing lami-embo treatment on a textile are provided to improve the quality in lami-embo of a textile, by giving the optimum temperature condition for maximizing the lami-embo of the textile using a pair of preheating rolls so as to perform uniform lami-embo treatment on the textile. A pair of preheating rolls(10,10') preheats a textile layer and a foam layer, which constitute a textile. A pair of embossing and engraving roll(20,30) performs lami-embo treatment on the preheated textile. A cooler(40) cools the treated textile. The cooler has a cooling fan type. The preheat temperature of the textile ranges from 130°C to 195°C.
Abstract translation: 提供了一种用于对纺织品进行拉伸处理的装置和方法,以通过使用一对预热辊使纺织品的最大温度条件达到最佳温度条件来提高织物的纤维素的质量,因此 对纺织品进行统一的熏蒸处理。 一对预热辊(10,10')预热构成织物的织物层和泡沫层。 一对压花和雕刻辊(20,30)对预热的纺织品进行拉伸处理。 冷却器(40)冷却经处理的纺织品。 冷却器有冷却风扇类型。 纺织品的预热温度范围为130°C至195°C。
-