헤테로폴리산계 촉매의 촉매수명을 연장하는 방법
    33.
    发明授权
    헤테로폴리산계 촉매의 촉매수명을 연장하는 방법 失效
    延长杂多酸催化剂催化寿命的方法

    公开(公告)号:KR1019930005312B1

    公开(公告)日:1993-06-17

    申请号:KR1019910007014

    申请日:1991-05-01

    Abstract: This relates to prolonging the life of heteropolyacid catalyst of formula HaXbYcMdOf in acid-catalyst reaction or oxidation. The life of catalyst is prolonged by supplying at least one of 0.1-10000 ppm piridine or nitrogen contained organic cyclic compound, amine, and ammonia continuousl or periodically in gas-phase oxidation in the presence of a catalyst. In the formula, H is proton; X is alkali, alkali earth, rare earth, and one or group of cations of Fe, Cu, Ag, Tl, Pb and Bi; Y is Si,P,Ge,As; M is V,Mo,W; O is oxygen; and each of a,b,c,d is tom ratio.

    Abstract translation: 这涉及在酸催化剂反应或氧化中延长式HaXbYcMdOf的杂多酸催化剂的使用寿命。 通过在催化剂存在下,在气相氧化中连续或周期性地供给0.1-10000ppm的吡啶或含氮的有机环状化合物,胺和氨中的至少一种来延长催化剂的寿命。 在该式中,H是质子; X是碱金属,碱土金属,稀土元素,以及Fe,Cu,Ag,Tl,Pb和Bi的一种或多种阳离子; Y为Si,P,Ge,As; M是V,Mo,W; O是氧; a,b,c,d分别为汤姆比。

    메타크릴산 제조용 고체촉매 및 그 제조방법
    36.
    发明授权
    메타크릴산 제조용 고체촉매 및 그 제조방법 失效
    用于制备甲基丙烯酸的催化剂及其制备方法

    公开(公告)号:KR1019900004118B1

    公开(公告)日:1990-06-16

    申请号:KR1019880008099

    申请日:1988-06-30

    Abstract: A catalyst of formula P, Mo12As0.2-2.0Cs0.1-1.0V0.1-2.0Tl 0.1-2.0 Cu0.1-2.0X0.1-0.5Oa [where X= Pd, Pb, Ba or Ca; a= bal. no. for prepg. methacrylic acid is prepd. by (a) adding soln. of B (contg. Tl(C2H3O2), CsNO3, Cu(NO3)2. 2.5H2O and nitrate of the X) to aq. soln. of A(contg. H3PMo12O40, H3AsO4 and V2O5) to coppte, (b) heating at 40-100 deg. C on a stirrr to obtain slurry, (c) vacuum-drying at 20-100 deg. C and molding, and (d) calcining for 3-15 hr at 320-400 deg. C in the air or N atm.. The methacrylic acid is prepd. by contacting methacrolein with O in the presence of the catalyst.

    Abstract translation: 式P的催化剂,Mo12As0.2-2.0C0.1-1.0V0.1-2.0Tl 0.1-2.0 Cu0.1-2.0X0.1-0.5Oa [其中X = Pd,Pb,Ba或Ca; a = bal 没有。 为prepg。 甲基丙烯酸是制备的。 通过(a)添加soln。 的B(连续T1(C2H3O2),CsNO3,Cu(NO3 )2.2.5H2O和X的硝酸盐) SOLN。 的A(连续H3PMo12O40,H3AsO4和V2O5)来处理,(b)在40-100℃加热。 C,以获得浆料,(c)在20-100℃真空干燥。 和(d)在320-400度煅烧3-15小时。 C在空气中或N atm ..甲基丙烯酸是制备的。 通过在催化剂存在下使甲基丙烯醛与O接触。

    바이오매스 기반의 나일론 6-모폴리논 공중합체 및 이의 제조방법
    37.
    发明公开
    바이오매스 기반의 나일론 6-모폴리논 공중합체 및 이의 제조방법 有权
    基于生物量的尼龙6​​-MORPHOLINONE共聚物及其制备方法

    公开(公告)号:KR1020150014178A

    公开(公告)日:2015-02-06

    申请号:KR1020130089514

    申请日:2013-07-29

    Abstract: 하기 화학식 1 및 2의 반복단위를 갖는 나일론 6-모폴리논 공중합체는, 흡습성, 성형성 및 기계적 물성이 우수할 뿐 아니라, 바이오매스를 원료로 할 수 있는 환경 친화적인 고분자로서, 자동차산업, 전기전자산업, 포장재산업, 의류/섬유산업, 건축부품산업 등의 분야에서 유용하게 사용될 수 있다.
    [화학식 1]

    [화학식 2]

    Abstract translation: 本发明涉及具有化学式1和2的重复单元的尼龙6-吗啉酮共聚物。更具体地,尼龙6-吗啉酮共聚物具有优异的吸湿性,成形性和机械性能,并且可以用于各种领域,例如载体 ,电子电器,包装材料,服装/织物和建筑零件行业,作为可以使用生物质为原料的环保聚合物。