알킨으로부터 알켄의 선택적 수소화 반응용 촉매
    31.
    发明公开
    알킨으로부터 알켄의 선택적 수소화 반응용 촉매 有权
    碱选择性加氢催化剂

    公开(公告)号:KR1020120117252A

    公开(公告)日:2012-10-24

    申请号:KR1020110034893

    申请日:2011-04-14

    CPC classification number: B01J23/89 B01J35/08 B01J35/10 C07C5/08

    Abstract: PURPOSE: A catalyst for selective hydrogenation of alkynes to alkenes is provided to rapidly convert alkynes to alkenes by carrying palladium and metal oxide mixtures containing iron and copper in the shell parts of silica particles. CONSTITUTION: A catalyst for selective hydrogenation of alkynes to alkenes includes a process in which palladium and metal oxide mixtures containing iron and copper are carried in the shell pores of silica particles with core-porous shell structures. The molar ratio of copper atoms and iron atoms in the metal oxide mixtures is 1:00.5-2.9. The content of the palladium in the shell pores is in a range between 0.01 and 10 weight%. The content of the metal oxide mixtures in the shell pores is in a range between 0.01 and 10 weight%.

    Abstract translation: 目的:提供用于烯烃选择性氢化为烯烃的催化剂,用于通过在二氧化硅颗粒的壳体部分中载带含有铁和铜的钯和金属氧化物混合物,将炔烃快速转化成烯烃。 构成:用于烯烃选择性氢化为烯烃的催化剂包括其中含有铁和铜的钯和金属氧化物混合物在具有核心多孔壳结构的二氧化硅颗粒的壳孔中携带的方法。 金属氧化物混合物中铜原子和铁原子的摩尔比为1:0.5-5-2.9。 壳孔中钯的含量为0.01〜10重量%。 壳孔中的金属氧化物混合物的含量在0.01至10重量%的范围内。

    초상자성 특성을 갖는 마이크론 크기의 실리카 코어/자성체쉘 입자 및 그 제조 방법
    32.
    发明公开
    초상자성 특성을 갖는 마이크론 크기의 실리카 코어/자성체쉘 입자 및 그 제조 방법 有权
    具有微尺度的超级磁性特征的二氧化硅核/磁性粒子及其方法

    公开(公告)号:KR1020100044432A

    公开(公告)日:2010-04-30

    申请号:KR1020080103566

    申请日:2008-10-22

    Abstract: PURPOSE: A super-paramagnetic porous micro particle formed with a silica shell and a silica core, and a manufacturing method thereof are provided to maintain a super-paramagnetic property of the micro particle, and to easily disperse the particle into a water-soluble organic solvent. CONSTITUTION: A manufacturing method of a super-paramagnetic porous micro particle with a spinel structure in a pore formed with a silica shell and a silica core comprises the following steps: dispersing a meso porous silica particle in a core-shell type to a polar solvent including a metal oxide precursor; inserting a surfactant to the solution from the previous step after adding a non-polar solvent; refluxing the mixed solution after heating; and heating the manufactured super-paramagnetic porous micro particle again.

    Abstract translation: 目的:提供由二氧化硅壳和二氧化硅芯形成的超顺磁性多孔微粒及其制造方法,以保持微粒的超顺磁性,并容易地将颗粒分散于水溶性有机物 溶剂。 构成:在由二氧化硅壳和二氧化硅芯形成的孔中具有尖晶石结构的超顺磁性多孔微粒的制造方法包括以下步骤:将核 - 壳型的中孔多孔二氧化硅颗粒分散到极性溶剂 包括金属氧化物前体; 在加入非极性溶剂后,将表面活性剂插入前一步骤的溶液中; 加热回流混合溶液; 并再次加热制造的超顺磁性多孔微粒。

    산화철을 포함하는 코어-쉘 복합체
    34.
    发明授权
    산화철을 포함하는 코어-쉘 복합체 有权
    包含氧化铁的核 - 壳复合物

    公开(公告)号:KR101800807B1

    公开(公告)日:2017-11-23

    申请号:KR1020160150580

    申请日:2016-11-11

    Inventor: 허남회 김유진

    Abstract: 티타늄철석(ilmenite) 광석으로부터수득되는금속염화물을물에녹인후 철성분만을선택적으로침출하여소결과정없이산화철을제조하는방법, 상기방법에의해제조된산화철및 상기산화철에금속산화물을코팅하여제조되는코어-쉘복합체에관한것이다.

    Abstract translation: 从矿石中得到的金属氯化物之后钛拍击(钛铁矿)溶解在水中,选择性浸出由cheolseong分钟,这是通过涂布在铁氧化物的金属氧化物和通过上述方法制造的铁氧化物制备产生未经烧结过程中的铁氧化物的方法 核壳复合体。

    무용매 조건의 1,3,4-옥사디아졸 합성법
    36.
    发明授权
    무용매 조건의 1,3,4-옥사디아졸 합성법 有权
    1,3,4-恶二唑在无溶剂条件下合成

    公开(公告)号:KR101778358B1

    公开(公告)日:2017-09-13

    申请号:KR1020150027006

    申请日:2015-02-26

    Abstract: 본발명은 1,3,4-옥사디아졸을합성하는방법으로서, a) 무용매조건에서, 기계적분쇄법으로히드라지드화합물과알데하이드화합물을반응시켜 N-아실히드라존화합물을합성하는단계; 및 b) 무용매조건에서, N-아실히드라존화합물에아이오딘계산화제를첨가한후 산화고리화반응으로 1,3,4-옥사디아졸을합성하는단계를포함한다. 본발명에따른무용매반응에의한 1,3,4-옥사디아졸합성법은매우높은선택성과용이한방법으로 1,3,4-옥사디아졸을높은수율로합성할수 있으며핸들링이쉽다는장점이있다. 또한, 용매내부의소량의물에의해다른부산물이생성되는것을방지할 수있으며이는합성되는중간물질이물에의해출발물질로돌아가는일도방지할 수있다.

    Abstract translation: 本发明涉及1,3,4-恶二唑的合成方法,其包括以下步骤:a)在无溶剂条件下通过机械粉碎使酰肼化合物与醛化合物反应合成N-酰基腙化合物; 并且b)在没有溶剂的情况下,向N-酰基腙化合物中加入碘计算剂,然后通过氧化环化反应合成1,3,4-恶二唑。 根据本发明的1,3,4-恶二唑合成方法可以通过极高的选择性和易于处理的方法以高产率合成1,3,4-恶二唑 有。 另外,可以防止溶剂中的少量水产生其他副产物,这可以防止合成的中间体通过水返回原料。

    금속 나노입자 제조 방법
    37.
    发明授权
    금속 나노입자 제조 방법 有权
    金属纳米材料的制备方法

    公开(公告)号:KR101691501B1

    公开(公告)日:2016-12-30

    申请号:KR1020140012084

    申请日:2014-02-03

    CPC classification number: B22F9/24 B22F1/0018

    Abstract: 본원은, 금속나노입자의제조방법에대한것으로서, 구체적으로는히드라진-이산화탄소결합화합물을금속산화물또는금속이온화합물과반응시키는것을포함하는, 금속나노입자의제조방법에관한것이다.

    Abstract translation: 本公开内容涉及制备金属纳米颗粒的方法,特别涉及一种制备金属纳米颗粒的方法,所述方法包括使肼 - 二氧化碳结合的化合物与金属氧化物或金属离子化合物反应。

    젤형 하이드라진의 제조 방법
    40.
    发明授权
    젤형 하이드라진의 제조 방법 有权
    凝胶型HYDRAZINE的制备方法

    公开(公告)号:KR101542795B1

    公开(公告)日:2015-08-07

    申请号:KR1020140032538

    申请日:2014-03-20

    Inventor: 허남회 이병노

    Abstract: 본원은, 젤형하이드라진의제조방법에관한것으로서, 구체적으로는용매없는조건에서하이드라진과이산화탄소가 2:1 비율로결합된젤형의무수화합물을선택적이고정량적으로제조하는방법에관한것이다.

    Abstract translation: 本申请涉及一种制备凝胶型肼的方法,其中更具体地,其中肼和二氧化碳以2:1的比例彼此结合的凝胶型无水化合物在溶剂型肼中选择性和定量制备, 自由条件。

Patent Agency Ranking