公开(公告)号:KR101724918B1
公开(公告)日:2017-04-07
申请号:KR1020150139716
申请日:2015-10-05
Applicant: 현대자동차주식회사 , 기아자동차주식회사 , 주식회사 캠스 , 주식회사 노루비케미칼
IPC: C09D133/06 , C09D175/06 , C08J7/04 , B05D7/24 , B05D7/00
CPC classification number: C09D175/06 , B05D7/53 , C08F220/18 , C08F220/28 , C08F220/32 , C08F2220/1825 , C08F2220/281 , C08F2220/325 , C08G18/246 , C08G18/4063 , C08G18/718 , C08G18/73 , C09D5/00 , C09D7/48 , C09D133/068 , C09D163/00 , C08L33/06 , C08L75/06
Abstract: 본발명은핫스탬핑필름용클리어도료조성물및 이를이용한도장방법에관한것으로, 보다상세하게는아크릴수지및 폴리에스터폴리올수지에에폭시변성아크릴수지및 2종의광흡수제를혼합하여부착력을개선하고단파장및 장파장을동시에차단하여내후성을향상시킬수 있으며, 반응형실리콘을포함하는경화제를혼합함으로써내치핑성, 내오염성및 내수성을향상시킬수 있는핫스탬핑필름용클리어도료조성물및 이를이용한도장방법에관한것이다.
-
公开(公告)号:KR101704138B1
公开(公告)日:2017-02-08
申请号:KR1020140179397
申请日:2014-12-12
Applicant: 현대자동차주식회사 , 기아자동차주식회사 , 주식회사 노루비케미칼
IPC: C09D175/14 , C09D175/06 , C09D7/12
CPC classification number: C08G18/6216 , C08G18/4063 , C08G18/42 , C08G18/44 , C08G18/73 , C08G18/755 , C08G18/758 , C08G18/7621 , C08G18/7671 , C09D175/04
Abstract: 본발명은 1 코트도장용질감도료조성물에관한것으로서, 더욱상세하게는질감이우수하고내화학성이뛰어난우레탄수지본연의특성과내화학성과소재밀착성이우수한아크릴수지본연의특성을모두가지는아크릴변성우레탄수지를기재로포함하는 1 코트 1 베이킹시스템에적용이가능한 BTX-FREE 타입의환경친화적질감도료조성물에관한것이다.
Abstract translation: 一层一次烘烤涂料用涂料组合物包括树脂,颜料,溶剂和一般添加剂。 树脂是通过聚合聚碳酸酯二醇,聚酯二醇,丙烯酸树脂和异氰酸酯单体制备的丙烯酸改性聚氨酯树脂。 使用一层一层烘烤涂料的涂料组合物可以提供柔软的质地,优异的耐化学性和粘附性。
-
33.
公开(公告)号:KR101417114B1
公开(公告)日:2014-07-16
申请号:KR1020080100841
申请日:2008-10-14
Applicant: 현대자동차주식회사
Abstract: 본 발명은 자동차 무도장 외장부품용 폴리프로필렌/클레이 나노복합재 및 이의 제조방법에 관한 것으로서, 더욱 상세하게 설명하면, 유기화 클레이, 무수말레인산이 그래프트된 폴리프로필렌 및 용융지수(MI) 1 ~ 20 g/
10분 인 폴리프로필렌 수지를 함유하는 (a)마스터 배치; 용융지수(MI) 15 ~ 35 g/
10분 인 (b)폴리프로필렌 수지; (c)자외선 안정제; 및 (d)열 안정제;를 포함하는 자동차 무도장 외장부품용 폴리프로필렌/클레이 나노복합재에 관한 것이다. 본 발명의 나노복합재는 상기 유기화 클레이, 무수말레인산이 그래프트된 폴리프로필렌 및 용융지수(MI) 1 ~ 20 g/
10분 인 폴리프로필렌 공중합체를 용융 컴파운딩하여 마스터 배치를 제조한 후, 상기 마스터 배치와 폴리프로필렌 공중합체, 자외선 안정제 및 열 안정제를 최적의 비율로 다시 용융컴파운딩하여 제조한다. 본 발명의 나노복합재는 저온 내충격성, 웰드라인 강도, 내후성이 우수하고, 성형품의 외관 품질이 우수하며, 도장 공정 삭제를 통한 원가절감이 가능할 뿐만 아니라, 무기물 함량이 적기 때문에 경량화가 가능하여 사이드실 몰딩, 루프랙 커버 등 자동차 무도장 외장부품에 적용할 수 있다.
무도장, 폴리프로필렌, 나노복합재, 무수말레인산, 유기화 클레이-
公开(公告)号:KR1020120118737A
公开(公告)日:2012-10-29
申请号:KR1020110036299
申请日:2011-04-19
Abstract: PURPOSE: A polyketone composition is provided to maintain durability, chemical resistance, fuel permeability, etc while maintaining performance of polyketone and to remarkably improve impact resistance. CONSTITUTION: A polyketone composition comprises 40-90 weight% of polyketone, 5-40 weight5 of polyamide, and 5-20 weight% of modified rubber. The flow index of the polyketone is 5-70 g/10min, the flow index of the polyamide is 5-70 g/10min and the flow index of the modified rubber is 0.5-30 g/10 min. The polyamide is one or more kinds selected from polyamide 6, polyamide 66, polyamide 6/66 copolymer, polyamide 610, polyamide 612, polyamide 11 and polyamide 12.
Abstract translation: 目的:提供聚酮组合物以保持耐久性,耐化学性,燃料渗透性等,同时保持聚酮的性能并显着提高耐冲击性。 构成:聚酮组合物包含40-90重量%的聚酮,5-40重量%的聚酰胺和5-20重量%的改性橡胶。 聚酮的流动指数为5-70g / 10min,聚酰胺的流动指数为5-70g / 10min,改性橡胶的流动指数为0.5-30g / 10min。 聚酰胺是选自聚酰胺6,聚酰胺66,聚酰胺6/66共聚物,聚酰胺610,聚酰胺612,聚酰胺11和聚酰胺12中的一种或多种。
-
公开(公告)号:KR100738126B1
公开(公告)日:2007-07-10
申请号:KR1020060056066
申请日:2006-06-21
Applicant: 현대자동차주식회사
Abstract: A method for preparing a highly heat resistant UV curable aqueous polyurethane resin is provided to obtain an aqueous polyurethane having improved heat resistance, fast reaction completion behavior and improved surface properties. The method for preparing a highly heat resistant UV curable aqueous polyurethane resin comprises the steps of: reacting a carboxy group-containing diol with a linear diisocyanate in a weight ratio of 1:2 to provide an isocyanate-terminated oligomer; forming a soft segment and a hard segment; mixing the soft segment with the hard segment in a weight ratio of 7:3-9:1 to provide a prepolymer; reacting the prepolymer with a monovalent hydroxy acrylate in a weight ratio of 43:1 to allow the isocyanate terminal to be end-capped with acrylate; dispersing the end-capped product in water to provide an aqueous polyurethane; and curing the aqueous polyurethane resin with UV rays under a dose of 800-1150 mJ/cm^2 for 10-120 seconds.
Abstract translation: 提供一种制备高耐热紫外线可固化含水聚氨酯树脂的方法,以获得具有改善的耐热性,快速反应完成行为和改善的表面性能的含水聚氨酯。 制备高耐热性UV可固化含水聚氨酯树脂的方法包括以下步骤:使含羧基的二醇与直链二异氰酸酯以1:2的重量比反应以提供异氰酸酯封端的低聚物; 形成软段和硬段; 将软链段与硬链段以7:3-9:1的重量比混合以提供预聚物; 使预聚物与单价羟基丙烯酸酯以43:1的重量比反应以允许异氰酸酯末端用丙烯酸酯封端; 将封端产物分散在水中以提供含水聚氨酯; 并在800-1150mJ /平方公分的剂量下用紫外线固化水性聚氨酯树脂10-120秒。
-
-
-
-