33.
    发明专利
    未知

    公开(公告)号:DE19919827A1

    公开(公告)日:2000-11-02

    申请号:DE19919827

    申请日:1999-04-30

    Applicant: BASF AG

    Abstract: Production of polyisocyanate polyaddition products comprises reacting isocyanates with isocyanate-reactive compounds in the presence of a compound (I) capable of reacting with tertiary amines. Independent claims are also included for the following: (1) mixtures for preparing polyurethane polyaddition products (sic), comprising isocyanates or isocyanate-reactive compound and (I); (2) mixtures of isocyanates and (I); (3) polyisocyanate polyaddition products containing nitrogen bonded to carbon through four bonds.

    34.
    发明专利
    未知

    公开(公告)号:DE19902802A1

    公开(公告)日:2000-08-03

    申请号:DE19902802

    申请日:1999-01-25

    Applicant: BASF AG

    Abstract: Polyurethane with a loss factor of 0.2-0.8 is based either on (a) a prepolymer obtained by reacting a polyisocyanate with a polyester polyol or polyether polyol with secondary hydroxyl group(s) and a molecular weight of 300-1200 or; (b) a polyol component containing other polyester polyol(s) or polyether polyol(s) with primary and secondary OH groups and a molecular weight of 300-1200. A process for the production of polyurethane (PU) with a loss factor of 0.2-0.8 involves bringing into contact (A) a component containing compound(s) which react with isocyanate and (B) a polyisocyanate component. In this system, either (1) component (B) is a prepolymer obtained by reacting a first polyester polyol or polyether polyol with at least one secondary hydroxyl group and a number-average molecular weight (MW) of 300-1200, or at least two of these, with an NCO group-containing compound, or; (2) component (A) contains other polyester polyol(s) or polyether polyol(s) with primary and secondary OH groups and MW of 300-1200. Independent claims are also included for (i) PU obtained by this process, with a loss factor of 0.2-0.8 and also with a natural frequency of 30-500 Hz and/or a dynamic elastic modulus of 1-50 N/cm ; (ii) a method for obtaining PU with a loss factor in the above range or also with at least one of the other properties in (i), by incorporating polyester polyol(s) or polyether polyol(s) with MW in the above ranges into the PU; (iii) formed articles containing PU as in (i).

Patent Agency Ranking