公开(公告)号:CZ9501745A3
公开(公告)日:1996-01-17
申请号:CZ174595
申请日:1994-11-16
Applicant: BAXTER INT
Inventor: LARRY ROSENBAUM , WILIAM ANDERSON , LECON WOO , DEAN LAURIN , BUAN ANGELES LILIAN , LING MILAEL T K , DING YUAN-PANG SAMUEL , HAYWARD DENISE S , HOPPESCH JOSEPH P , NEBGEN GREGG , WESTPHAL STANLEY
IPC: A61L27/00 , A61L31/00 , C08L23/02 , C08L23/06 , C08L23/08 , C08L23/10 , C08L23/16 , C08L23/20 , C08L23/26 , C08L29/04 , C08L31/04 , C08L51/06 , C08L53/00 , C08L53/02 , C08L67/00 , C08L75/00 , C08L77/00 , C08L101/00 , C08L101/12 , C08L23/14
CPC classification number: C08L23/02 , C08L23/0815 , C08L23/0846 , C08L23/0853 , C08L23/0869 , C08L23/10 , C08L51/06 , C08L53/00 , C08L53/02 , C08L77/00 , C08L101/00 , C08L2203/02 , C08L2205/08 , C08L2666/04 , C08L2666/20 , C08L2666/14 , C08L2666/24 , C08L2666/02
-
公开(公告)号:NO952802L
公开(公告)日:1995-09-15
申请号:NO952802
申请日:1995-07-14
Applicant: BAXTER INT
Inventor: LAURIN DEAN , BUAN ANGELES LILLIAN , WOO LECON , LING MICHAEL T K , DING YUAN-PANG SAMUEL , ANDERSON WILLIAM , ROSENBAUM LARRY A , HAYWARD DENISE S , HOPPESCH JOSEPH P , NEBGEN GREGG , WESTPHAL STANLEY
IPC: A23L7/10 , A23L7/196 , A61L31/00 , B32B27/08 , B32B27/32 , C08L23/08 , C08L23/10 , C08L25/04 , C08L53/00 , C08L53/02
Abstract: A multiple layer structure comprising a skin layer composed of a polypropylene copolymer with styrene ethylene-butene styrene block copolymer within a range of 0-20% by weight skin layer, and, a radio frequency ("RF") susceptible layer adhered to the skin layer. The RF layer has a first component of a propylene based polymer, a second component of a nonpropylene polyolefin, a third component of a radio frequency susceptible polymer, and a fourth component of a polymeric compatibilizing agent.
-
公开(公告)号:ZA9408816B
公开(公告)日:1995-07-11
申请号:ZA9408816
申请日:1994-11-08
Applicant: BAXTER INT
Inventor: LAURIN DEAN , BUAN ANGELA LILLIAN , WOO LECON , LING MICHAEL T K , DING YUAN-PANG SAMUEL , ANDERSON WILLIAM , ROSENBAUM LARRY A , HAYWARD DENISE S , HOPPESCH JOSEPH P , NEBGEN GREGG , WESTPHAL STANLEY
IPC: A61L27/00 , A61L31/00 , C08L23/02 , C08L23/06 , C08L23/08 , C08L23/10 , C08L23/16 , C08L23/20 , C08L23/26 , C08L29/04 , C08L31/04 , C08L51/06 , C08L53/00 , C08L53/02 , C08L67/00 , C08L75/00 , C08L77/00 , C08L101/00 , C08L101/12 , C08L
CPC classification number: C08L23/02 , C08L23/0815 , C08L23/0846 , C08L23/0853 , C08L23/0869 , C08L23/10 , C08L51/06 , C08L53/00 , C08L53/02 , C08L77/00 , C08L101/00 , C08L2203/02 , C08L2205/08 , C08L2666/04 , C08L2666/20 , C08L2666/14 , C08L2666/24 , C08L2666/02
-
公开(公告)号:PA8449201A1
公开(公告)日:2000-05-24
申请号:PA8449201
申请日:1998-03-20
Applicant: BAXTER INT
Inventor: LAURIN DEAN , ROSENBAUM LARRY A , BUAN ANGELES LILLIAN , HOPPESCH JOSEPH P , ANDERSON WILLIAM , LING MICHAEL T K , NEBGEN GREGG , WOO LECON , DING YUAN-PANG SAMUEL , WESTPHAL STANLEY , HAYWARD DENISE S
IPC: B29K101/12 , B29K255/00 , B32B23/14 , B32B27/32
Abstract: UNA ESTRUCTURA DE CAPA MULTIPLE COMPRENDIENDO UNA CAPA DE SUPERFICIE COMPUESTA DE UN COPOLIMERO DE POLIPROPILENO CON UN COPOLIMERO DE BLOQUE DE ESTIRENO ETILENO-BUTENO ESTIRENO EN EL RANGO DE 0-20% EN PESO DE LA CAPA DE SUPERFICIE, Y, UNA CAPA SUSCEPTIBLE A RADIOFRECUENCIA ("RF") ADHERIDA A LA CAPA DE SUPERFICIE. LA CAPA RF TIENE UN PRIMER COMPONENTE DE UN POLIMERO BASADO EN PROPILENO, UN SEGUNDO COMPONENTE DE UNA POLIOLEFINA SIN PROPILENO, UN TERCER COMPONENTE DE UN POLIMERO SUSCEPTIBLE A RADIOFRECUENCIA, Y UN CUARTO COMPONENTE DE UN AGENTE POLIMERICO COMPATIBILIZANTE.
-
公开(公告)号:NO302870B1
公开(公告)日:1998-05-04
申请号:NO952802
申请日:1995-07-14
Applicant: BAXTER INT
Inventor: LAURIN DEAN , BUAN ANGELES LILLIAN , WOO LECON , LING MICHAEL T K , DING YUAN-PANG SAMUEL , ANDERSON WILLIAM , ROSENBAUM LARRY A , HAYWARD DENISE S , HOPPESCH JOSEPH P , NEBGEN GREGG , WESTPHAL STANLEY
IPC: A23L7/10 , A23L7/196 , A61L31/00 , B32B27/08 , B32B27/32 , C08L23/08 , C08L23/10 , C08L25/04 , C08L53/00 , C08L53/02
Abstract: A multiple layer structure comprising a skin layer composed of a polypropylene copolymer with styrene ethylene-butene styrene block copolymer within a range of 0-20% by weight skin layer, and, a radio frequency ("RF") susceptible layer adhered to the skin layer. The RF layer has a first component of a propylene based polymer, a second component of a nonpropylene polyolefin, a third component of a radio frequency susceptible polymer, and a fourth component of a polymeric compatibilizing agent.
-
公开(公告)号:AU686697B2
公开(公告)日:1998-02-12
申请号:AU1099895
申请日:1994-11-16
Applicant: BAXTER INT
Inventor: LAURIN DEAN , BUAN ANGELES LILLIAN , WOO LECON , LING MICHAEL T K , DING YUAN-PANG SAMUEL , ANDERSON WILLIAM , ROSENBAUM LARRY A , HAYWARD DENISE S , HOPPESCH JOSEPH P , NEBGEN GREGG , WESTPHAL STANLEY
IPC: A61L27/00 , A61L31/00 , C08L23/02 , C08L23/06 , C08L23/08 , C08L23/10 , C08L23/16 , C08L23/20 , C08L23/26 , C08L29/04 , C08L31/04 , C08L51/06 , C08L53/00 , C08L53/02 , C08L67/00 , C08L75/00 , C08L77/00 , C08L101/00 , C08L101/12
Abstract: A polymer based composition for fabricating into articles is described. The composition comprises: a polypropylene in an amount by weight from 40-90% of the composition and having a melting temperature greater than 130 DEG C; a radio frequency susceptible polymer in an amount by weight from 5-50% of the composition and having a dielectric loss greater than 0.05 at 1-60 MHz and ambient temperature to 250 DEG C, the susceptible polymer being selected from (1) polymers containing at least one segment selected from the group consisting of urethanes, esters, ureas, imides, sulfones, and amides, and (2) ethylene copolymers having 50-85% ethylene content copolymerized with at least one monomer selected from the group consisting of acrylic acid, methacrylic acid, ester derivatives of acrylic acid with alcohols having 1-10 carbons, vinyl acetate, and vinyl alcohol; a compatibilizing polymer in an amount by weight from 5-30% of the composition, the compatibilizing polymer conferring compatibility between the radio frequency susceptible polymer, and the polypropylene, the compatibilizing polymer being a styrenic block copolymer with hydrocarbon soft segments, and wherein the composition has an optical haze value of less than 30% for the composition processed into a film of about 0.299 mm in thickness measured in accordance to ASTM D-1003, a mechanical modulus of less than 2758x10 Pa when measured according to ASTM D-882 and the composition exhibits no strain whitening after being strained at moderate speeds of about 50 cm per minute to about 100% elongation.
-
公开(公告)号:CO4290439A1
公开(公告)日:1996-04-17
申请号:CO94051219
申请日:1994-11-09
Applicant: BAXTER INT
Inventor: LARRY ROSEMBAUM , ANDERSON WILLIAM , WOO LECON , LAURIN DEAN , BUAN ANGELES LILLIAN , LING MICHAEL TK , DING YUAN-PANG SAMUEL , HAYWARD DENISE S , HOPPESCH JOSEPH P , NEBGEN GREGG , WESTPHAL STANLEY
IPC: A61L31/00 , A23L7/10 , A23L7/196 , B32B27/08 , B32B27/32 , C08L23/08 , C08L23/10 , C08L25/04 , C08L53/00 , C08L53/02
Abstract: 1. UNA ESTRUCTURA DE CAPA MULTIPLE COMPRENDIENDO:P UNA CAPA DE SUPERFICIE; UNA CAPA SUSCEPTIBLE A RADIOFRECUENCIA ("RF") AD- HERIDA A LA CAPA DE SUPERFICIE, LA CAPA RF TENIEN- DO UN PRIMER COMPONENTE DE UN POLIMERO BASADO EN PROPILENO, UN SEGUNDO COMPONENTE DE UNA POLIOLEFI- NA SIN PROPILENO, UN TERCER COMPONENTE DE UN POLI- MERO SUSCEPTIBLE A RADIOFRECUENCIA, Y UN CUARTO COMPONENTE DE UN AGENTE POLIMERICO COMPATIBILIZAN- TE; LA ESTRUCTURA TENIENDO PROPIEDADES FISICAS EN EL RANGO DE a = 70%; c 1.0; e > 0.1% f
-
公开(公告)号:BR9405786A
公开(公告)日:1996-03-26
申请号:BR9405786
申请日:1994-11-16
Applicant: BAXTER INT
Inventor: LAURIN DEAN , BUAN ANGELES LILLIAN , WOO LECON , LING MICHALEL T K , DING YUAN-PANG SAMUEL , ANDERSON WILLIAM , ROSENBAUM LARRY A , HAYWARD DENISE S , HOPPESCH JOSEPH P , NEBGEN GREGG , WESTPHAL STANLEY
IPC: A61L27/00 , A61L31/00 , C08L23/02 , C08L23/06 , C08L23/08 , C08L23/10 , C08L23/16 , C08L23/20 , C08L23/26 , C08L29/04 , C08L31/04 , C08L51/06 , C08L53/00 , C08L53/02 , C08L67/00 , C08L75/00 , C08L77/00 , C08L101/00 , C08L101/12
Abstract: A polymer based composition for fabricating into articles is described. The composition comprises: a polypropylene in an amount by weight from 40-90% of the composition and having a melting temperature greater than 130 DEG C; a radio frequency susceptible polymer in an amount by weight from 5-50% of the composition and having a dielectric loss greater than 0.05 at 1-60 MHz and ambient temperature to 250 DEG C, the susceptible polymer being selected from (1) polymers containing at least one segment selected from the group consisting of urethanes, esters, ureas, imides, sulfones, and amides, and (2) ethylene copolymers having 50-85% ethylene content copolymerized with at least one monomer selected from the group consisting of acrylic acid, methacrylic acid, ester derivatives of acrylic acid with alcohols having 1-10 carbons, vinyl acetate, and vinyl alcohol; a compatibilizing polymer in an amount by weight from 5-30% of the composition, the compatibilizing polymer conferring compatibility between the radio frequency susceptible polymer, and the polypropylene, the compatibilizing polymer being a styrenic block copolymer with hydrocarbon soft segments, and wherein the composition has an optical haze value of less than 30% for the composition processed into a film of about 0.299 mm in thickness measured in accordance to ASTM D-1003, a mechanical modulus of less than 2758x10 Pa when measured according to ASTM D-882 and the composition exhibits no strain whitening after being strained at moderate speeds of about 50 cm per minute to about 100% elongation.
-
公开(公告)号:CZ174695A3
公开(公告)日:1996-01-17
申请号:CZ174695
申请日:1994-11-16
Applicant: BAXTER INT
Inventor: ROSENBAUM LARRY A , ANDERSON WILIAM , WOO LECON , LAURIN DEAN , BUAN ANGELES LILIAN , LING MICHAEL T K , DING YUAN-PANG SAMUEL , HAYWARD DENISE S , HOPPESCH JOSEPH P , NEBGEN GREGG , WESTPHAL STANLEY
IPC: A61L31/00 , A23L7/10 , A23L7/196 , B32B27/08 , B32B27/32 , C08L23/08 , C08L23/10 , C08L25/04 , C08L53/00 , C08L53/02 , B32B27/00
Abstract: A multiple layer structure comprising a skin layer composed of a polypropylene copolymer with styrene ethylene-butene styrene block copolymer within a range of 0-20% by weight skin layer, and, a radio frequency ("RF") susceptible layer adhered to the skin layer. The RF layer has a first component of a propylene based polymer, a second component of a nonpropylene polyolefin, a third component of a radio frequency susceptible polymer, and a fourth component of a polymeric compatibilizing agent.
-
公开(公告)号:PL310403A1
公开(公告)日:1995-12-11
申请号:PL31040394
申请日:1994-11-16
Applicant: BAXTER INT
Inventor: LAURIN DEAN , BUAN ANGELES LILLIAN , WOO LECON , LING MICHAEL T K , DING YUAN-PANG SAMUEL , ANDERSON WILLIAM , ROSENBAUM LARRY A , HAYWARD DENISE S , HOPPESCH JOSEPH P , NEBGEN GREGG , WESTPHAL STANLEY
IPC: A61L27/00 , A61L31/00 , C08L23/02 , C08L23/06 , C08L23/08 , C08L23/10 , C08L23/16 , C08L23/20 , C08L23/26 , C08L29/04 , C08L31/04 , C08L51/06 , C08L53/00 , C08L53/02 , C08L67/00 , C08L75/00 , C08L77/00 , C08L101/00 , C08L101/12 , C08L23/00
Abstract: A polymer based composition for fabricating into articles is described. The composition comprises: a polypropylene in an amount by weight from 40-90% of the composition and having a melting temperature greater than 130 DEG C; a radio frequency susceptible polymer in an amount by weight from 5-50% of the composition and having a dielectric loss greater than 0.05 at 1-60 MHz and ambient temperature to 250 DEG C, the susceptible polymer being selected from (1) polymers containing at least one segment selected from the group consisting of urethanes, esters, ureas, imides, sulfones, and amides, and (2) ethylene copolymers having 50-85% ethylene content copolymerized with at least one monomer selected from the group consisting of acrylic acid, methacrylic acid, ester derivatives of acrylic acid with alcohols having 1-10 carbons, vinyl acetate, and vinyl alcohol; a compatibilizing polymer in an amount by weight from 5-30% of the composition, the compatibilizing polymer conferring compatibility between the radio frequency susceptible polymer, and the polypropylene, the compatibilizing polymer being a styrenic block copolymer with hydrocarbon soft segments, and wherein the composition has an optical haze value of less than 30% for the composition processed into a film of about 0.299 mm in thickness measured in accordance to ASTM D-1003, a mechanical modulus of less than 2758x10 Pa when measured according to ASTM D-882 and the composition exhibits no strain whitening after being strained at moderate speeds of about 50 cm per minute to about 100% elongation.
-
-
-
-
-
-
-
-
-